What chemicals or chemical pastes are effective in removing discoloration from 304 stainless steel after T.I.G. welding? If the compounds are proprietary, who is the supplier and where can they be bought?

Lin Emery
studio - New Orleans, LA, U.S.


+++

There are a variety of ways to clean the weld discoloration. TIG welding usually leaves the least of this problem, but you always have some.

1) Use a nitric acid/ hydrofluoric acid paste (pickle paste). This is very hazardous and should be handled with extreme care and knowledge.
2) Grit blast with non-iron containing grit, then passivate.
3) Wire brush with 316ss brush or Scotchbrite cloth to clean off discoloration, then passivate.
4) Electrically remove the discoloration with proprietary chemicals and equipment. This method can be fast and easy.

Contact us if you want info on this. We cannot name it here.


Lee Kremer

Stellar Solutions, Inc.

Algonquin, IL, USA


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 





 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com