Letter 19014 Technical assistance request for sheet galvanizing line [Iran]+++ Gentlemen, We are a hot dip galvanizer in Iran that now intended to install a small sheet galvanizing line for galvanizing steel sheets with thickness equal or more than 1.5mm. We are requesting your technical help in this regard, to buy a new or used line for us or technical assistance to fabricate some parts in Iran and buying some parts from abroad. We will be thankful if you answer how you can help us. Mansour Mirhendi