When doing sulfamate nickel plating, certain breakdown products are generated whose exact molecular formulas are not known, but which are known to be stress relaxers. One of these breakdown products goes by the name of AUP, or "the magic stress reducer" (and possibly a few other names). I have a number of literature articles which note the existence of this product and its effects, and offer some attempts at exact analysis of the material.

But I once saw, and cannot seem to find now, a published article about how to engineer the production of this stress reducer in the plating cell. I know there is a published technique where sulfurized nickel anodes are used in the main plating cell, but there is an auxiliary cell or overflow cell where electrolytic nickel anodes are employed in order to generate the stress relaxer. I remember that this cell design was reputed to allow plating at very high current density (over 200 ASF) with near zero stress and, I believe, no need for other addition agents.

If anyone has any recollection of this and can point me to the article I would appreciate it!


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


++

In 1990, Dr. S. Alec Watson published one of the most comprehensive papers on the subject that is (or was) available thru the Nickel Development Institute page. Just type NiDI and search on technical papers.

Best regards,

Guillermo Marrufo
Monterrey, NL, Mexico


++

Ted, I have a copy of an electroforming guide produced by INCO, which mentions the formation of stress reducer (azodisulfonate)when using insoluble platinum electrodes or high currents on nickel anodes. I have got it in pdf format if you want a copy, or you can download it from INCO's site.

Regards,

Richard Guise
- Lowestoft, U.K.


++

Ted,

Guillermo is correct but more specifically you want Technical Series # 10052 "Nickel Sulphamate Solutions" By Dr.Alec Watson.

Russell Richter
Gar Electroforming Div.

Danbury, CT, USA


++

Thank you very much Guillermo, Richard, Russell!


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com