Hydrogen embrittlement




I'm interested in chrome plating a bicycle frame. I understand that there is a phenomenon known as hydrogen embrittlement. Is it possible to alleviate this condition and regain the plated object's pre-plating strength? Also, is this true of all plating or only chrome?

Eliot Glaser
1998



1998

Hydrogen embrittlement applies only to high-strength steel; your bike may be a common low strength steel, or aluminum or magnesium (maybe even titanium). Hydrogen embrittlement can happen from any plating, and some other processes like pickling, but it is worst with chrome plating because chrome is so inefficient that it generates a tremendous amount of hydrogen.

Assuming the bike doesn't break during plating (it's very unlikely, but has occasionally occurred with certain highly stressed items like springs), baking will relieve the problem if done quickly (most people recommend within 2 hours).

But do you really understand what is involved in chrome plating? First, you can't do it yourself for environmental and safety reasons; secondly you need to apply other plating (probably copper, then nickel) before the chrome plating; third, the part has to be polished and buffed before plating or it will look terrible.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey



I have found out that phosphor bronze is highly prone to hydrogen embrittlement. Are othe copper alloys also prone?

Is beryllium copper prone to the problem of hydrogen embrittlement?

Yashawant V.Deval
Deval Utensils factory - Pune, INDIA
1998



Dear Sir

I am also looking for the test to be conducted for the Hydrogen Embrittlement in Bolts. Could you please suggest some advanced technique for the same? I am currently looking for the them who are working on this topic. Could you please suggest me to whom I should contact for the same topic.

I anticipate that you will consider my request and hoping for your reply.

Thanking you

sincerely yours

Vinay Deodeshmukh
University of Nevada Reno - US
2000


Would hydrogen Embrittlement be an issue with 1144 Stress Proof steel?

Jim Shrake
- Houston, Texas
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"