Stripped rims are oxidizing [Louisiana] 

++

I have a CBB929RR and I had stripped the paint of my rims and now they are oxidized BAD, what can I do??? I have re sanded them and re sanded... I have re polished over and over. What are my options?

Thanks,

Rich Melillo
- Gretna, LA


++

Lacquer! Polish them, then immiediately degrease and lacquer them, doesn't look much different from bare polished aluminium, except it doesn't corrode, I've used acrylic car lacquer with great success on copper and aluminium