what kind of safety precautions are commonly used for chromating spray application to strip steel?

heather essary
- woodhaven michigan usa
2002



Reduced to the basics, do not get it in your body or clothes, don't eat it, don't drink it, don't smoke it and don't breathe it. Net result, protective clothes and a particle mask as a minimum since you will have some very fine spray or mist with a spray system. James Watts
- Navarre, Florida
2002




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"