What is the lower temperature limit for copper oxidation in ambient atmosphere?




Q. I am currently working on a project that involves furnace brazing copper. In seeking to control oxidation, we are using nitrogen as a backing gas in the furnace. The top temperature reached in the furnace is 1350 F. Does anyone know at what temperature copper begins to form significant oxidation in an ambient atmosphere, that is, how cool does the copper need to be before we open the furnace door?

Thanks!

Richard Carter
PVI, LLC - Ft. Worth, Texas
2002



Suggestion: Do a few trials using different final temperatures and see what the highest acceptable temperature is, for your specific conditions.

Bill Reynolds
Bill Reynolds [deceased]
consultant metallurgist - Ballarat, Victoria, Australia
We sadly relate the news that Bill passed away on Jan. 29, 2010.

2002


A. We have been studying copper oxidation for over two years to determine the complex reactions involved in copper oxidation at room temperature to 500 °C. Between room temperature and 100 °C copper forms a thin Cu2O layer; at about 150 °C a complex oxide forms Cu3O2; and at 200-300 °C CuO forms. Significant oxidation occurs when CuO begins to form. You should cool copper to below 150 °C to be sure that only a protective thin film has formed.

David L. Cocke
Lamar University - Beaumont, Texas
2002



Q. to Mr David L. Cocke

Dear David,
I am interested in the catalytic action of the copper surface when distilling alcohol.
Do you have any observations about how much time the oxide layer forms on pure copper at room temperature in air?
Thanks in advance.

Atanas Atanasov
- Plovdiv, Bulgaria
January 9, 2019



January 2019

thumbs up sign  Hi Atanas. David's posting was from 17 years ago; I doubt that he monitors this page or is reachable through his e-mail address from so long ago, but we'll try :-)

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




Q. Hi,

Our process is to flame treat the plastic package surface before marking for better mark adhesion. As the plastic package is molded along with copper leadframe, suspecting the possibility of oxidation. Would like to check whether this flame treatment at 300 °C for about 1~2 seconds will cause any oxidation? Visually no findings of oxidation.

Regards,

MADURAKAVI DEIVANAYAKAN
Semiconductor assembly - Chennai,TamilNadu, INDIA.
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"