The Process of Electrostatic Powder Coating

Q. Could you please forward to me detailed info on the process involved with Electrostatic Powder Coating

S Slevin
- Erlangen Germany
1998


SUGGESTED POWDER COATING BOOKS
for Shops & Engineers


powdercoat_pietschmann2023
"Industrial Powder Coating: Basics, Methods, Practical Application" by Judith Pietschmann (2023)
avail from eBay, AbeBooks, or Amazon

powdercoat_liberto2003
"User's Guide to Powder Coating" by Nicolas Liberto (2003)
avail from eBay, AbeBooks, or Amazon

powdercoat_utech2002
"High Performance Powder Coating" by Bob Utech (2002)
avail from eBay, AbeBooks, or Amazon

powdercoat_liberto1994
"Powder Coating. The Complete Finisher's Handbook" by Nicolas Liberto (1994)
avail from eBay, AbeBooks, or Amazon

powdercoat_sys_lehr1991
"Powder Coating Systems" by William Lehr (1991)
avail from eBay, AbeBooks, or Amazon

powdercoat_tech_harris1976
"The Technology of Powder Coatings" by S.T.Harris (1976)
avail from AbeBooks, or Amazon

"Fundamentals of Powder Coating by Emory Miller & David Taft (1974)
avail from AbeBooks, or Amazon

(as an Amazon Associate & eBay Partner, we earn from qualifying purchases)

A. Hi, cousin Slevin. We can give you general info here: the parts must be cleaned, phosphated (if steel) or chromated (if aluminum), dried, electrostatic sprayed with the powder (which can be either thermoset or thermoplastic), and baked to fuse the powder into a plastic coating. For a little more on the subject, please see our on-line article by Mario Pennisi. But this is a subject that fills whole libraries, so "detailed info" will require a book.

Good luck!

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
1998


A. A very good general overall information book is "Fundamentals of Powder Coating" It is available through the Society of manufacturing Engineers.

The book has had several reprints and if it is not available SME has other similar publications available.

Society of Manufacturing Engineers
One SME Drive PO Box 930
Dearborn. MI 48121-0930 USA
Tyrone L. Caley
Jefferson City Missouri


A. On top of those nice recommendations, I would also recommend PCI [The Powder Coating Institute], the industry association charged with the advancement of powder coating technology in the marketplace.

Craig Burkart   Craig Burkart signature
Craig Burkart
- Naperville, Illinois


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"