Home of the finishing HOTLINE since 1989

-----

Brighteners for Gold Plating


Q. I am making a brightener for a decorative gold bath, do I want to use cobalt sulphate heptahydrate or cobalt sulphate mono-hydrate?

Jerry Hammie
GPEAA, Inc. - Naples, Florida
1998



1998

A. I am sorry: English not perfect...

Gold plating is very kind of bath. Generally brightener is cobalt, cadmium, indium, etc.

The concentration of brightener is usually very low include.

acid type : 0.5g/l - 1g/l

EDTA 2Na is good low current part, and as Brightener react. Organic brightener is not used yet.

Welcome to Korea 2002 world cup games...

Thank you

Kyuong min, KIm
platech - suwon(2002 Worldcup game state), Korea




Multiple threads merged: please forgive chronology errors and repetition  🙂



Q. I am using a citric acid gold bath, I want to make my own brightener using EDTA and Cobalt, but I need a formula for the brightener. Help!

Jerry hammie
- Gold Plated Emblems
1998



A. Cobalt sulphate 9 gram, and edta 15 gram, and indium sulphate 0.4 gram

Majed Ja
- Bethlehem Palestine
August 12, 2011




Q. I was wondering what citric acid does in the formula when making a bath? Also I was wondering how I can find this. I was also wondering if there is a substitute that I can use? Please help me find this and any other useful information on this topic. I will give the recipe to anyone who responds. Thank you.

Kim A [surname deleted for privacy by Editor]
- McCord, Saskatchewan, Canada
2000


"Gold Plating Technology"
by Reid & Goldie
-- hard to find & expensive; if you see a copy cheap, act fast!

goldie
on Amazon
or eBay
or AbeBooks
(affil link)

A. Hi Kim. See if a library has Reid & Goldie "Gold Plating Technology". It covers everything about gold plating.

sidebar There's nothing wrong with wanting to privately exchange information with someone, but this isn't the site for it. We're not a matchmaking service for individuals to barter their knowledge with each other; we're here for Public education. Anything anyone wishes to share is posted for all to share.

Luck & Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.




Q. Hello please send me the latest formulas of the best ways for gold plating and chrome plating if required. If you have any books about this subject please send me.

Khaled Sibai
- Suadi arabia
2000


A. Hi Khaled. I suggested an excellent gold plating book above. For chrome plating I suggest your start with our "Introduction to Chrome Plating".

Luck & Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.




Q. I would like to know the formula for citric acid .

Megan Smith
- Atco, New Jersey
2001


A. citric acid = C3H6O3

Rishi Aggerwal
- India
2003


A. citric acid = C6 H8 O7

Samira [surname deleted for privacy by Editor]
- Phoenix, Arizona, USA
2004



Q. Hello,
I currently work in a small plating shop doing hard gold plating on kovar pins, copper, nickel, gold.

We don't have access to any type of analysis, our problem is our gold looks really good for the first 5 or 6 minutes of plating then it starts to get really dull after that; we usually plate for 10 minutes.

Bill Coppell
- Alvin Texas
November 28, 2020


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"