Letter 16059 ELECTRO POLISHING OF S.S. 420 GRADE [India]++ DEAR SIR, I WANT TO DO ELECTRO POLISHING ON STAINLESS STEEL 420 GRADE STRIPS PRODUCT KNOWN AS RIDERLESS HEALD'S USED IN TEXTILE WEAVING THE THICKNESS OF PRODUCT IS 0.30MM, WIDTH IS 5.50MM & LENGTH IS 280MM TO 410MM. PLEASE GUIDE IN THE ABOVE MATTER. MR. ASHOK M. NAIR
++ Most of our "must have" books include good chapters on electropolishing, including the Metal Finishing Guidebook, the Electroplating Engineering Handbook, and ASM's Metals Handbook, Vol. 5.
++ Proprietary electropolishing processes for ss-400 series are available in India. Ramesh Khare