How to make a brass table chrome silver!

++

I have a pair of glass topped solid brass tables that have a high polish brass finish. I would like to figure out the best possible way to refinish the gold brass color to be high polish chrome silver finish instead. Any suggestions?

Thanks,

Mary Newcomb
- Stamford, Connecticut, USA


++

Plating something with silver or chrome is not a do-it-youself project. A plating shop can do it though. Silver would be very pretty, but tarnish prevention and removal might be overwhelming. Nickel-chrome plating would leave you with a durable and low maintenance finish.
pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search