Letter 15049
Etching of 3000 series aluminium
[Australia]
++
I am having trouble etching a 3000 series aluminium. Have tried
caustic, Tuckers, Kellars, Barkers, dilute and concentrated HF with
water. I only have success in revealing the precipitates and cannot
resolve the grain boundaries. Can anybody out there help me out??
Matthew Hogan
Melbourne, Victoria, Australia
April 2, 2007
It's better to anodise it .