Q. Dear friends.
Is there anyone expert in electrodeposition of lead dioxide (PbO2) on titanium and ceramic substrate?
- Tehran, iran
July 22, 2021
A. Hi Cyrus.
Although PbO2 is conductive, I don't know whether PbO2 can be electrodeposited, although electrodeposition of lead followed by oxidation via some method certainly sounds very feasible.
I think you might get a more enthusiastic response by posting your own situation and asking a specific question than by asking people to step forward, credentials in hand :-)
Luck & Regards,

Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
July 2021
September 10, 2021
Book on electrodeposition of lead dioxide on titanium:
The Electrodeposition of Lead Dioxide on Titanium
by
D. Gilroy, R. Stevens
Electricity Council Research Centre, 1979.
Ex USSR book on electrodeposition of lead dioxide:
E.A.Dzafarof :Elektroosazhdeniye,svoistva i primenenie dvuokisi svinca(Electroplating,properties and use of lead dioxide),Baku 1967.
Russian book on electroplating of PbO2: �"жафаров Э.А. «Электроосаждение, свойства и применение двуокиси свинца».
(Electoplating, properties and uses of lead dioxide, 1967, 103 pages)
You can download it (free)at galvanicrus.ru webpage.
Hope it helps and good luck
- Cerovski vrh 157 Croatia
⇩ Similar, related, Q&As -- oldest first ⇩
Q. I WOULD LIKE THE COATING METHODS AND TECHNOLOGY/EQUIPMENT PURCHASE OF THE COATING OF LEAD DIOXIDE COATING ON THE CERAMIC SUBSTRATE RODS FOR DEVELOPING OUR SYSTEM.
Nalan Alikasifoglu2003
Q. I need literature about lead dioxide manufacture and its coating methods on ceramic rods. please help or give me the guideline for the same. I will be very thankful to you in this regard.
MUHAMMAD SAADULLAHA. Take lead ingot and burn in oxygen and then do thermal spraying of it. I have seen this process in a factory in India.
Rajiv SanghaviQ. Does anyone have thermodynamic data for the two allotropic forms of lead dioxide, specifically the standard free energy of formation?
Roger Altman