Aluminum Rack Systems for anodizing




I NEED INFORMATION ON ALUMINUM RACK SYSTEMS WHERE USED IN THE ANODIZING INDUSTRY. BOOKS, MAGAZINES,ARTICLES, ETC. I AM NEW TO THIS INDUSTRY AND NEED TO LEARN ALL I CAN.

GERALD PETERS
DISTRIBUTING
1998



--

I'm also new to the industry so I feel a little silly giving a response, but here goes:

We make most of our racking systems in-house out of aluminum and Titanium. Titanium, while expensive, is great because it lasts a long time and there is no need to strip the fixture between runs. Aluminum works but becomes sharp (safety hazard), flimsy and always needs to be stripped and repaired.

If you can afford the Titanium do it.

James A. Corier


For titanium racks, which is the best way to go for long term.

David A. Kraft
- Long Island City, New York
--



I need help on how to solve a problem of pitting on the aluminium surface. This happens once in six months. Usually I change the entire bath solution and make it up fresh. Is there an alternative. What causes this pitting which appears as small black dots on the alu. sheet? Thanks Deepak

Deepak Ratan
1999


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"