Chemical deburring of titanium




I am a mfg eng. working on developing a chemical deburring method for titanium. I am interested in any references or articles relevant to this subject. I would also appreciate any chemical formulations that would warrant investigation.

Matt Adams
1998



1998

Dear Matt:

If you can vibratory finish your part, REM Chemicals out of Southington, CT. offer a very good physicochemical process for deburring/refining Titanium components such as jet engine airfoils and surgical implants.

Good Luck,

Bill

Bill Boatright



Look on page 627 of "Modern Electroplating" edited by Lowenheim [on AbeBooks, eBay, or Amazon affil links] , for a one sentence entry on electropolishing Ti. A rather nasty mixture. You will need an excellent exhaust system for a lab or pilot plant testing.

James Watts
- Navarre, Florida
1998


Hi, Matt:

I believe we have done some previous work together on your electropolishing unit. Please talk to me before you consider using Lowenheim's formulation!

Thanks and best regards,

Ed Bayha
Metal Coating Process Corporation - Charlotte, North Carolina
1998



2001

There is another proprietary method that uses salty solutions to electropolish titanium.

Anna

anna_berkovich
Anna Berkovich
Russamer Lab - Pittsburgh, Pennsylvania
(ed. update July, 2025: sorry, Anna has retired)


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"