Help with drying system for nickel chrome plating plant



Q. Can anybody help in our search for a decent drying system?

We run a manual shop producing gold, nickel & chrome on all types of base metals inc stainless, diecast, plastic.

The dryer will need to cope with about 120 jigs per hour.

Steve Sudlow
plating shop - U.K.
1998


A. If you have steam or hot water available, there should be no difficulty in building a workable box-type dryer for racks of plated work. The secret is to not to get cheap on the recirc fan. You want to blow the water off with warm AIR, not dry it on with radiant heat.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
1998


Low Pressure
Regenerative Blower
regenerative_blower
on Amazon
or eBay
(affil link)

A. If you come out of a warm/hot rinse tank, you can rig a system that uses excess air from your regenerative blower in a drying box setup at very little cost.If you do not have a regenerative blower, consider getting a good used one. The intake is filtered and it is oil free.

James Watts
- Navarre, Florida
1998


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"