Burnishing


I'm a student of the Technical University of Gdansk, Poland. Ball burnishing is the subject of my master thesis. I would be very grateful if somebody could contact me by my mail address. I need all the information about ball burnishing : web sites, literature, companies' names, etc.

Krzysztof Z [last name deleted for privacy by Editor]
- Poland
1998


I need information about Black Burnishing of metal Components like Textile Spinning Rings. I am the Chief Executive of a Leading Textile Machinery Manufacturer in India

S C A [last name deleted for privacy by Editor]
- Coimbatore, INDIA
1999


Hallo,

I am a metal worker and I need to find out what the ball burnishing process involves and if there are any companies in the uk that offer the service. How have you got on with your inquiry? Maybe you could let me have some basic information on the process as I am interested to know the limitations ie, what type of surface it can be applied to etc.

Good luck with your thesis,

Adam R [last name deleted for privacy by Editor]
- London
2001



2005

Please send me some info if you have it by this time.
I am working on burnishing
thanks,

Peter Koorapati
- Australia



2005

Roller Burnishing is a Super-finishing process. It is a Cold Working process which produces a fine surface finish by the planetary rotation of hardened rollers over a bored or turned metal surface. Since all machined surfaces consist of a series of peaks and valleys of irregular height and spacing, the plastic deformation created by roller burnishing is a displacement of the material in the peaks which cold flows under pressure into the valleys. The result is a mirror-like finish with a tough, work hardened, wear and corrosion resistant surface. Lapping and Honing is eliminated.

ADVANTAGES OF ROLLER BURNISHING
Mirror Finish in One Pass, Accurate Sizing, Close Tolerances, Eliminates Lapping & Honing.
Improved Metallurgical Properties - Work Hardened Surface, Increase in fatigue strength.
No Additional Machine Investment - attachable to any Standard Machine Tool Already Present in the Shop.
Long Tool Life No Operator Skill Required Low Torque & Power Requirements Maximum Parts Interchangeability.


Yashwant Pawar
- Mumbai, MS, India



2006

The method of roller burnishing is a cold rolling process without removal of metal. A set of rollers is used to roll on the component surface with adequate pressure. As a result all the pre-machined peaks gets compressed into valleys thus giving a mirror like surface finish.

Advantages of Roller Burnishing are

1. Fantastic Mirror like surface finish

2. Consistent dimensional tolerance and Repeatability

3. Single Pass Operation offers very less cycle time

4. Increases the Surface Hardness

5. Reduces the Reworks and Rejections

N. Srinivasan
burnishing tools - Coimbatore, Tamil Nadu, India



2006

I'm a graduate student-mechanical department-HoChiMinhCity University of Technology. I'm now studying about ball or roller burnishing process. There's hardly any literatures about this subject in Vietnam, and it's difficult to find out the full literatures on internet. Hence, I need and hope everybody can help and support me. If someone has e-books or literatures, please contact or send them to me.
Thanks and have a good day to everybody

Quang.

Dang Thien Quang
HoChiMinhCity University of Technology - HoChiMinh City, VietNam



dears,
can I get the some information abt ball burnishing. And also I need some paper to related to ball burnishing process.

parmar haresh
Engineer - surat,gujrat, India
November 18, 2009


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"