(Cycles thru suppliers).


Letter 14046

Seeking metallic plated fine fiber [Colorado] 

 

Electroless plating of our fine continuous polymer fibers (4-6 micron diameter, 1000+ filaments per unwoven bundle) with 2-3 micron thick coating around each fiber of copper or nickel, followed by a thin electrically insulative coating. Need R&D quantities by this summer, production capability of 5000 lbs/yr. by early 2003. Final product is used in electronics packaging materials.

Jay B [last name deleted for privacy due to age of posting]
- Longmont, CO, USA


Dear Reader: there is no provision for public reply to this particular letter because it is not a technical question but a commercial inquiry to which our advertisers will reply in private --

I want to post a question or inquiry of my own.
 
I am a supporting advertiser and want to reach the inquirer privately.






     