Letter 13707

Wood stain removal  

 

How do I remove a white heat mark from a mahogany coffee table. The table was protected by a coaster but obviously something has gone wrong. The coffee cup was not particularly hot and it could be some other type of stain but it is the same shape as the coaster. Will I need to have the table stripped professionally.

Shirley Mason
- Wakefield, Yorkshire, England, GB


 

Rub area with cloth dipped in mixture of cigarette ashes lemon juice or salad oil, Or rub with a cloth dipped in lighter fluid followed by a mixture of Rottenstone [link is to product info at Rockler] and salad oil wipe dry and wax or polish.

Jenna Marie
- Elgin, Il 60087


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 





 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com