Soda acidic

 

How acidic the soda is by testing the ph levels in different brands.

Dany love
- Immokalee, Florida


First of two simultaneous responses --  

No more words or time on answers than questions, so use pH paper.

pic of Ted Mooney Teds signature
Ted Mooney, P.E. RET
finishing.com
Brick, New Jersey


Second of two simultaneous responses --  

Yes, it is, isn't it.

Bill Reynolds
   consultant metallurgist
Ballarat, Victoria, Australia

It is this website's profoundly sad
duty to relate the news that Bill
passed away on Jan. 29, 2010.


ANSWER, or ASK a related Q. POST an unrelated Q.See HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & DevicesUsed & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search