Titration
Is there a titration process for the determination of nickel in a watts bath, would this be the same for the nickel chloride or nickel sulfamate.
Robert Sachs
Sybron - Ontario, Canada
It is the same titration as for sulfamate nickel.
James Totter, CEF
- Tallahassee, Florida
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.