The I.S. Meter - alive or dead?


Twenty some years ago one could buy in Britain an instrument for measuring internal stress during deposition (electro- and otherwise) called I.S. Meter. Its action was based on the extension or contraction of a thin metal strip kept in tension as a stressed deposit was being plated onto it.

Does anyone know if these instruments are still being manufactured by anyone anywhere in the world? Any information would be greatly appreciated.

Thank you, Berl

berl stein berl sig
"PlaterB" Berl Stein
NiCoForm, Inc.
supporting advertiser
Rochester, New York
nicoform
1997


Berl,

Martin Marietta in Orlando was rumored to be using a continuous input device run thru a computer to maintain absolute zero stress in electroforming. Oak Ridge's electroforming department may have some knowledge of this also.

Other than that, the only thing that I am aware of is the stress tabs, a moderately accurate estimation of stress that is much faster than a contractometer.

James Watts
- Navarre, Florida
1997



Might be worth a try to ask Wm. Cannings of the UK if the instrument you are seeking is still available.

Ken Lemke
Ken Lemke
Burlington, Ontario, Canada
1997



1997

Further to Mr. Lemke's discussion, The Canning Handbook mentions a device "devised by Hoar and Arrowsmith" described in Electroplating and Metal Finishing 1968, 21, 85 and Trans. Inst. Institute of Metal Finishing 1957, 34, 354, Trans. Inst. Metal Finishing 1965, 43, 84, and Trans. Inst. Metal Finishing 1964, 42, 68.

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



1997

Hi Berl,

When I worked at Sel_Rex a long time ago they marketed IS meters which they got from Czechoslovakia. Sel-Rex is now owned by Enthone-OMI. Perhaps they still have them or know where to get them.

Cheers!

Bob

Bob Teichmann
Avon Products, New Jersey

Ed. note: This is a very old thread (14 years!), but all threads on finishing.com are monitored and still "alive", so updates are welcome.


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"