Nickel free silver plating for jewelry


1998

I am a jewelry manufacturer and electroplater and am facing problems with nickel free silver plating.

I hv already tried white bronze as a base plating before silver plating but haven't been successful with controlling the tarnishing and palladium plating before silver plating turns up to be too expensive.

Mandeep Singh


1997

Hi Mandeep,

With reference to your father's visit in Holland a few weeks ago, I hope that the Degussa company came up with the solution for the problem you are facing.

Bye,

Herman

Herman Tiggeler
Accessa BV


Another possibility is a bright cobalt deposit.

Uwe Berger
- Blasberg, Germany
1998



In a related letter, Ken Lemke stated that cobalt might have the same problems as nickel in causing allergic reactions.

tom & pooky   toms signature
Tom Pullizzi
Falls Township, Pennsylvania
1997



1998

Tom,

a medical test (patch test) in Germany showed that cobalt gives not the same reaction as nickel.

One reason can be that normally you have more contact to nickel than to cobalt. So perhaps it is only an alternative for nickel for the next years.

There are some shops in Germany using cobalt as a substitute for nickel.

Uwe Berger
- Blasberg, Germany


try BRONZES NF NICKEL FREE FROM ENTHONE-OMI OR DECOREX FOR PALLADIUM

ROBERTO ARIAS
- metalquimica
1998


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"