Letter 12003

Corrosion effect of traceable residue of carbon dioxide in aqua ammonia on the carbon steel piping 

 

I would appreciate if you can give me any comment on the effect of traceable residue of carbon dioxide in aqua ammonia to the carbon steel piping. The concentration of carbon dioxide is about 30 ppm in aqua ammonia.

Best regards,

Ji Ok Kim
- Seoul, Korea


 

Carbon dioxide will form carbonic acid with water, in a sealed system, I would think that the alkalinity of the ammonia would tend to neutralize this acid. Is there free oxygen in this system?

Tom Pullizzi
Platronica.com
Falls Township, PA


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com