Letter 11860

Seeking Invar treatment  

 

I need some information on treatment on INVAR-36. We want to use invar in an assembly with an optical component on an instrument that will be used on a satellite. The recommanded treatment we found is given at the end of this letter. Do you know a company that does this treatment on raw material and on the manufactured parts?

"All of the invars should be given a three-step heat treatment for the optimum combination of CTE, strength, and dimensional stability: Anneal at 830ƒC for 30 min/in. of thickness in inert atmosphere and quench in polyalkaline glycol/water solution. Reheat to 570ƒC for 1 hr and air cool. Heat at laeast 48 hr. at 95ƒC and air cool."

Christophe Deutsch
- Quebec, PQ, Canada


Dear Reader, please --
Post a question on a different subject.
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com