Outgassing problem on lamp reflector





 

On a parabolic reflector used with an HID lamp, discoloration is taking place on the coated surface. The base material of the reflector is aluminum 6061-T6 per astmb209 or ASTM B221. There is a 10-16 microinch roughness height called out on the parabolic surface and the coating is specified as follows:

MIRROR, ALUMINIZED COATING IN ACCORDANCE WITH
MIL-M-13508 WITH A MAGNESIUM FLUORIDE PROTECTIVE
FILM TO WITHSTAND TEMPERATURE OF 500 °F

Apparently, due to the high temperature environment created by the HID lamp, outgassing of the coating material is occurring, primarily the fluoride. I would greatly appreciate any information and advice regarding this matter as well as any suggestions of possible alternative processes.

Thank you in advance,

Edward J. Hile, III
Goodrich Hella Aerospace - Oldmar, Florida


A spec is a spec, and if the customer wants MgF, then...

However, it seems to me a film of Al2O3, ZrO2 or even SiO2 might be adequate protection for an aluminum visible light reflector (HfO2 if you really need thermal protection); the caveat here is without more information on mechanical stress, thermal cycling, environment and other parameters the part may be subjected to, it is hard to give a definitive answer.

MgF2 is used in optics frequently as a polarizing material and because it is fluorescent under electric lights. There maybe reasons for the MgF2 spec other than protecting the reflective surface.

Dale Woika
Surface Conversion Sciences - Bellefonte, Pennsylvania, USA
 



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"