Letter 11040

S-N curves PtRh-20 material 

 

I am searching for so called S-N (Stress vs Cycles), curves, for PtRh 20 materials at elevated temperatures(1000 C), because I think we have a fatigue problem. S-N curves for PtRh 20 at room temperare could also help me a lot.

Thanks in advance,

Joris van der Steen
LG.PHILIPS Displays - Netherlands