We are currently working on a small NASA explore program and looking for a supplier to supply us with terminal lugs. It would have to be nickle finish instead of electro tin plated for the simple reason this will be in space and would grow wiskers if electro tin plated.

Could someone furnish us with the suppliers that can supply the terminal lugs and any information regarding electro plating that would with-stand the space enviroment.

The terminal lugs will vary in size from #2, through #10 and will have a insulated sleeve on the crimped end.