Heat Aged Solderability on Bright Plated Tin 

 

Has anyone ever heat aged a bright tin (MSA based) electroplated deposit at or above 155C for more than 8 hours and seen more than 95% coverage for soldering?

Brian Scaria
- Waterbiry, CT


 

I wouldn't think so.

Tom Pullizzi
Platronica.com
Falls Township, PA