Poor adhesion of silver plating on PMMA


I would like to know which are currently the best practices to deposit silver onto a PMMA film. I think silver has a poor adhesion to PMMA and therefore some kind of pretreatment is required. Probably by using an interface layer of SiO2 adhesion could be enhanced. I would like to know also if this process is easier on PET.

Looking forward to hear any advice on the topic,

Jose C. Arboiro
Instituto de EnergÌa Solar - Spain
1998



What does PMMA and PET stand for?

tom & pooky   toms signature
Tom Pullizzi
Falls Township, Pennsylvania
1997


PMMA stands for PolyMethyl MethAcrylate and
PET for PolyEthylene Terephthalate

Regards

Jose C. Arboiro
Instituto de EnergÌa Solar - Spain
1998



I would like to known if anyone has been able to make photoconductive polycarbonate or a polycarbonate + PMMA blend? My needs are for a transparant film. rjm

Robert Miller
1999


we are working on silver coatings on textiles. We have been working on two different fabrics, PET and nylon. PET has better adhesion than nylon (I am not sure about PMMA) ..we also did post treatment by coating some resin to improve the adhesion.

Nurmalasari
- Taiwan
May 16, 2011


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"