Anodizing MMC


We want to anodize MMC material (Al30Si70). Who has experience and can tell use about the procedure.

Any advice would be appreciated.

Jan-Henk Pennings
TNO METALS RESEARCH INSTITUTE
1998



The Canning Handbook [on eBay, Amazon, AbeBooks affil links] states that high Si alloys are unsuitable for anodizing. Perhaps someone is doing some research in this area, or you could tell us something you may have discovered. METALAST has set up a research laboratory for anodizing, and Anodizer's Plaza (available from our WWW links page) is also run by specialists at university.

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania
1998


Please contact me to get more info. regarding the anodization of MMC which we successfully performed.

Samir Elomari
Canadan Space Agency
1998



Proper netiquette demands, in public forums such as this, that information be freely shared on line, not in private correspondence. Each letter which is posted "improves the breed", as winners spawn other winners when playing the ponies. Letters sent in private do not share this benefit, as inbreeding causes the swift end of the question. It's the diminishing gene pool problem, no matter how smart the original pair of question/answer, you need to mix in some fresh ideas.

tom pullizzi animated    tomPullizziSignature
Tom Pullizzi
Falls Township, Pennsylvania
1998


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"