Letter 10096 Ultra high molecular weight polyethlene (uhmwpe)
I'm looking for properties of uhmwpe (ultra high molecular weight polyethlene) which is using as a surgical implant raw material and sterilization methods of this material. Also, is there an application to keep its dimensions stable?
Hi ! May I suggest you go a website and just type in 'uhmwPe' and contact those people. There are definitely DIFFERENT types of uhmwPe! Ranging from around 2,000,000 molecular length (and weldable!) to around 5 or 6,000,000. In other words, some are better than others and some, obviously, cost more, too. A major manufacturer is SIMONA in Germany. They could/should be able to give you full information on sterilization etc., if they bother to reply (sometimes they sure don't want to be bothered!). Cheers!