Seeking Electroless Nickel Plater [India] 

 

We are located in Bangalore in a very keen to find a good electroless nickle plater. The present plater results in either peel off of dullness. The finished product during assembly is crimped. During crimping the plating peels. The plating is done on Aluminium 6061 material. What is the reason for this ?