(Cycles thru suppliers)


Letter 10032

Problems in Bluing  

 

I want to know the exact composition of the bluing salt used for the bluing of M.S. Also the chemical composition of chemical Degreaser (Alkaline). Also could you guide that some parts developed white powder at many areas after one day of bluing. Could you propose remedy for it?

Thank you,

Tayyab S [name deleted for privacy]
- Islamabad, Pakistan


May 26, 2008

Hi, Tayyab. We have an FAQ on Black Oxide and Cold Blackening to introduce the general technology. Beyond that, the Metal Finishing Guidebook goes into more depth about the technology. But in most plating shops in the west, the shops buy proprietary alkaline degreaser process and black oxide (bluing) processes, and the exact compositions are held as trade secrets which no one can share with you. Good luck.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, NJ


Dear Reader: please choose what you want to do.

I want to answer or follow-up on this question (in non-commercial fashion).
 
I want to post a question on a different subject.
 
This letter is within a monitored forum, very much "alive" here in 2008. If you spot any broken links or obsolete info, please advise!





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com