Activating polished nickel without dulling

-----

Can someone please help me find a procedure for activating polished sulfamate nickel without dulling the surface finish ?

Seanshop


Hi, Seanshop. Electrocleaning, followed by a dip in stabilized citric acid, is touted by video disc manufacturers. Sounds like it's worth a shot. Good luck!

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey