We have an electroplating plant in which we plate fashion good accessories like buttons, buckles, washers, eyelets, zipper pulls. etc. The size of material to be plated varies from (diameter 1 mm to 10 cm). Our major problem is choice of a correct lacquer and lacquer machine which can apply the lacquer on the objects smoothly and give a pleasent and shiny look.

Our finishes are
antique copper, antique brass, tin, white bronze, antique silver, black nickel free

Can any body select one or more suitable lacquers and methods of application (my major problem is antique silver which becomes yellow even after applying lacquer on it)