Hi there, I'm a chemist and currently working on catalyst
synthesis for hydrogen reforming. thus,I would like to enquire on
zirconia powder as a support material of the metal that we are going
to use.
I need the zirconia in the form of 12/20 mesh size with chemical
composition of 94.78 wt% zirconia oxide, 4.29 wt% calcium oxide, 0.57
wt% silica, 0.27 wt% titanium dioxide, 0.09 wt% ferric oxide.
porosity of 33-36%, specific gravity of 5.3-5.6 g/cc, surface area
less than 1 square meter per gram.
Please do contact me for further details and thank you.
Regards,
Senthamarai Padmanabhan
alternative energy - SHAH ALAM, SELANGOR, MALAYSIA


 |
|