50000. Seeking anodizing of Nissan 350 z
engine parts
{9/18/08}
50001. Need lacquers and lacquer coating
machine for buttons and buckles
{9/18/08}
50002. How to clean Brass sign? ![]()
50003. Seeking sulphuric acid in 5-gallon
containers
50004. Plating to meet 1000 hours of salt
spray [India]
50005. Passivation Problems With
Forgings ![]()
50006. Coating / plating for high
reflection at 532nm? [Washington]
50007. Sodium carbonate determination
[Maryland]
50008. Need zinc-nickel coating job
shop [India]
{9/18/08}
50009. Need titanium nitride coating on
alumina and zirconia [India]
50010. How to achieve large pores at
titanium surface
50011. Anti-oxidant material for copper
foil [Syria]
50012. Green residue after application of
salt-vinegar paste and Simichrome [Washington, DC]
50013. How much hex chromium is produced in
an HHo Generator
50014. Electrochemical etching to mark
tools [New York]
50015. How to prep and paint brass
letters [Ohio]
50016. Looking to restore old copper water
boiler [West Virginia]
50017. Is there at an home test for
rhodium?
50018. Where can I find equipment to powder
coat tiles? [New Jersey]
50019. Process for silver plating of flange
nuts [India]
50020. Seeking copper or rust color powder
coating
{9/18/08}
50021. At what pH is Zn(OH)2 completely
dissolved in water?
50022. Kitchen Faucet Finish Question
[Washington]
50023. Need Cadmium Anodes, sodium
Dichromate, & Trichloroethylene
{9/19/08}
50024. Titanium oxide layer thickness
measurment [India]
50025. What are the Extraction or recovery
processes for gold, silver and copper [India]
50026. Chemical polishing of molds
[India]
50027. Want someone to remove black nickel
plating
{9/19/08}
50028. Watts nickel plating
hardness
50029. Testing a hardcoat anodize seal
[New York]
50030. Reflector Direct Vaccum
Metalizing
50031. Electroplating failure
analysis
50032. Compatibility of mixing stainless
steel & galvanized hardware [Alaska]
50033. What types of metal corrode?
50034. Chloride limits for Alkaline
Etch [Kansas]
50035. Cleaning up a Winchester Model 1906
pump action 22
50036. Timeline of change from hexavalent
to trivalent chrome [Wisconsin]
50037. Floor covering for anodizing
line
50038. How to prep new resin for DI
service?
50039. E-coatings, are they toxic?
50040. Sudden high pH in e-coat
bath
50041. Facing Separation or Delamination
During Wire Spray
50042. How to do electroless tin plating
over electroless nickel
50043. Sn plating looks like Zn after
Autoclave test ![]()
50044. Required leaching practice for anode
bags and filters [Wisconsin]
50045. Hard anodize/taber testing
[Kansas]
50046. Please help with satin finish on
stainless angle
50047. How do you get the look of lead
coated copper without the price?
50048. Need to refinish 6000 series
aluminum boat parts [Maryland]
{9/23/08}
50050. Remove Paint from Aluminum Window
Frames
50051. Cooling coil material for HF acid
etch bath? [India]
50052. What is anticorrosive to chromic
acid in bath [Thailand]
50053. E-coating material [India]
50054. Difference between yellow and white
galvanizing?
50055. Is vacuum necessary for baking of
electroless nickel? [India]
50056. Chrome Peel from Plastic
Substrates
50057. Percentage of nickel in zinc-nickel
acid, alkaline and sulphate baths [India]
50058. Black spots on Zn plated and
trivalent chromated (bright) parts [India]
50059. Nickel plating an Aluminum/Copper
assembly [Washington]
50060. Zinc Plating Cosmetics
50061. Mixing sodium di-chromate in
passivation [Montana]
50062. Blisters on zinc plated sheet
metal [India]
50063. Machining techniques for milling
nickel chrome plating on aluminum [Wisconsin]
50064. Etching time for aluminum
extrusions? [UAE]
50065. Painting of 316 SS after
passivation
50066. Quick rusting after washing of
rotors [India]
50067. Evaluation of Plating Depth
50068. Bright nickel vs sulfamate nickel as
an undercoating
50069. Need water softener powder /
Boraxo
5007. Stripping PVD coatings
50070. A few deep scratches in my one day
old black fridge!
50071. Removing gold plating from a brass
ingot [Mississippi]
50072. Recycling chrome
50073. Cad class 1 red dye
50074. Need plating of 1018 Shaft to pass
500 hrs of humidity test [Indiana]
{9/25/08}
50075. Need Coated Stainless Sheet Metal
Screws
{9/25/08}
50076. Need a Temperature Control Box for
rust experiment
50077. Stripping powder coating
[Minnesota]
50078. Coating question for Kickstarter
.... not sure what it is
50079. Iron Entry Door damaged by concrete
and HCL overspray [Kansas]
50080. Why is copper roof brown, not
green? [Washington]
50081. Spec for Hot tin dip? [New
York]
50082. How to get compatible color with
epoxy? [Vietnam]
50083. Powdercoating Galvaneal
50084. Comparision of different GI
sheets [India]
50085. Calculate dispense volume of liquid
copper sulfate [Virginia]
50086. Chromic Acid Anodizing is not
passing salt spray test [India]
50087. Chrome plating aluminium die
castings
50088. Corrosion inhibitor for sulfamic
acid
50089. Who takes Phosphate Sludge?
[India]
{9/26/08}
50090. A good copper electroplating
solution
50091. Inspection of Clear Alodine
[Wisconsin]
50092. Does black oxidizing change the
thickness of a part? [Alabama]
50093. Skip plating problems
50094. Need help with nickel brush plating
questions
50095. Electrodeburring on SCM-440
Martensite
50096. SS304L above seawater
environment
50097. Corrosion between a black anodized
aluminum part and a yellow zinc plated part
50098. Removing chrome and cadmium from
ground water [Thailand]
50099. Left All-Clad Stainless Steel in
Self-Cleaning cycle in Oven [Ohio]
50100. Stainless bolts in aluminium
[Vermont]
50101. On precipitating Nickel from
wastewater
50102. Steel knives by Victorinox corrode
and pit from my well water
50103. Electrolysis of copper weathervane
and lead flashing [Channel Islands]
50104. Filling in pits by brush plating
copper
50105. Steel I beam preservation and
finish
50106. Oil rubbed finish
50107. Removing clear coat
[Indiana]
50108. Removal of electrolysis within
drilled wells [Washington]
50109. Polishing Pitted Old Road Bike
Rims
50110. Protective Clear Coat for White Gold
Ring?
50111. Environment and public safety
issues
50112. Acid tin plating problem after
soldering [India]
50113. Black anodised parts now turning (or
turned) slightly crimson/reddish
50114. Stains from Deep Brazing then clear
iridite.
50115. Best electropolishing chemical
composition? [India]
50116. Coating on Hardened EN31?
[India]
50117. Corrosion of power connector
[Denmark]
50118. Need barrel plating
{9/30/08}
50119. Looking for chromed plastic license
plate frames
{9/30/08}
50120. Hard chrome thickness and hardness
measurement equipment
50121. Patina for pewter
50122. Need brush gold plating service
[Washington]
{9/30/08}
50123. Stripping/polishing/lacquering Brass
Knobs -- where? [New York]
{9/30/08}
50124. Need to plate a faucet in dull
nickel / brushed chrome [New York]
{9/30/08}
50125. Need car dipping service
{9/30/08}
50126. Chrome plating of plastic parts
[Mexico]
{9/30/08}
50127. Want to buy Sodium M Nitrobenzene to
strip nickel plating on steel [Thailand]
{9/30/08}
50128. Looking for used gold brush on set
up for small projects. [Washington]
{9/30/08}
50129. Bathtub gets Blue/Green
stains
50130. Determining max. temp SS304
experienced from its Blue color?
50131. Need reliable electrode material
selection for KOH?
50132. Salt Spray Woes.... Please help
[New Jersey]
50133. Clearcoat solvent bubbles
problem [Portugal]
50134. CED paint temperature
[India]
50135. Peeling E Coat [Ohio]
50136. E-Coat Cost? [India]
50137. Electroless nickel on copper/brass
material
50138. To reduce the failure of Zinc
Plating Components [India]
50139. Black Spots in Acid Zinc Plating at
Lcd After Trichrome Passivation [India]
50140. Smoky/Milky surface observed in HCD
areas after Plating with blue passivation [India]
50141. Electroplating of stainless steel
mesh with platinum [South Africa]
50142. Hardcoat as a dynamic seal
surface [North Dakota]
50143. 1/16" 6061 Warping After Type III
Anodize
50144. Air Moisture Causing Stainless Steel
to Rust
50145. Rust issue after Electro Chem
deburr
50146. Standard for waterjet
blasting
50147. Is "Sweep Blasting" supposed to
remove existing primer? [India]
50148. Why the grain-like surface
appearance on Inconel 907?
50149. Chrome Coffee Table Base
50150. Finishing treatment for a new WRC
shingle roof?
50151. What causes temporary marks on
table, not water marks?
50152. Care of Indian Head Pennies
50153. Stripping chrome from duplex LDX
2101 alloy basis metal
50154. Rough plating in nickel sulphamate
plating [Malaysia] ![]()
50155. Electroplating of gold over
aluminium alloy [India]
50156. Plating specification for solderable
copper plated aluminum wire [Indiana]
50157. Galvanized wire properties
[Ireland]
50158. Transferring Hull cell analysis to
plating bath? [Ireland]
50159. Where to get corrugated metal
panels [New Jersey]
50160. Nickel-Chromium plating thickness
issue on non-alloy steel rod [Slovenia]
50161. Required Thickness of Copper on
Steel for Outdoor Exposure
50162. Life of Platinized Anodes
[India]
50163. Electroless gold plating
[Switzerland]
50164. Why the powder painting peel off
from the galvanized metal? [Mexico]
50165. Color spec for zinc olive drab
[Minnesota]
50166. 75 Volt 1000 Amp Rectifier
needed
{10/3/08}
50167. How to separate copper from
silver
50168. Can iridite be colored white??
[New York]
50169. Copper plated motorcycle
tank
50170. Replacement Class 3 Form III
50171. Need TDC II (thin dense
chromium?)
{10/6/08}
50172. Conductive, Corrosion resistant,
RoHs compliant, Ground Point coating on steel tube
50173. QQ-P-35 Type 2 vs MIL-S-5002
50174. pH stabilization problems in copper
accelerated salt fog chambers [Ohio]
50175. Gold plating over low percentage of
gold alloy
50176. Gas permeability of elecroplated
ABS/HIPS
50177. Chrome plating ABS tubes from
inside [India]
50178. Copper migration through sulfamate
nickel plating [New York]
50179. Nickel Etch
50180. Cleaning an anodized part in an
alkaline cleaner
50181. Evidence of Improved Corrosion
Resistance after Laser Marking
50182. Masking of caliper in bore area for
brake application [India]
50183. Why Passivate if Parts Already Pass
the ASTM A 967 Requirements?
50184. Problems with 316 and 420 SS rusting
after laser etching
50185. Best finish for supermarket
trolleys
50186. Need precision matte black
e-coat
{10/7/08}
50187. Metal bars stamped with "P" found
near old gravel pit in NW [Iowa]
50188. Ni-B Electroless plating
[Mexico]
50189. Making corrugated iron look old but
not rusty
50190. Chemicals for grey-bluing (not
blacking) early Winchester and Marlin barrels.
50191. Retro steelcase color matched
[Iowa]
50192. Spray chrome finishes [South
Dakota]
50193. Will chromate passivation keep brass
looking natural and protect the finish. [Germany] ![]()
50194. How to differentiate two parts
having Dacromet and Geomet coating? [India]
50195. Looking for mirror finished copper
plate [India]
{10/7/08}
50196. Need used plasma nitriding
equipment [Croatia]
{10/7/08}
50197. WHY DOES BATTERY ACID DISSOLVE
METALS BUT NOT PLASTICS?
50198. Tin plating using easy chemical
process [India]
50199. NORAX BELTS ---seeking a
distributor/supplier [Washington]
{10/8/08}
50200. Need to find Hawes Lemon Oil
50201. High temperature black spectral
coating [Indiana]
50202. Black spots in Zinc Trivalent
Plating [India]
50204. SHELL AND TUBE HEAT EXCHANGER TYPE
SELECTION [India]
50205. Vibratory finishing Steel,
Stainless, Steel and Aluminum [New York]
50206. Plating thickness checking in hot
condition [India]
50207. Laser Etching a Zamak Housing with
Coating [Ireland]
50208. What is Mirco # 3 [Ohio]
50209. Silver (Ag) plating on ABS - Best
method
50210. What Are the Electrical Properties
of Chromate Conversion Coating over Zinc?
50211. Sealing of anodised aluminium and
testing of sealed layer [India]
50212. HARD CHROMIUM FAILURE ![]()
50213. Corrosion for nickel plated
material
50214. Maximum recommended potential to
earth ground for electroplating copper wire [South Carolina]
50215. Coloring - the stainless
steel
50217. Removing Chrome from wheels
[Virginia]
50218. Throw / Covering Power in Barrel
Plating
50219. Impossibility of building up more
than 10 microns of electroless nickel [Portugal]
50220. High Gloss Epoxy powder cures to
dull finish
50221. Silver Anode Supplier
{10/9/08}
50222. Another way to color
aluminum?
50223. 304 SS pipe corrosion in liquid
ammonia / ammonia solution [Switzerland]
50225. Micro porous nickel problem
[India]
50226. Difference between Stainless Steel
grade 304 and 202 [New York]
50227. Ceramic Metaloids plastic
material
50228. Anodizing on LM6 Grade Aluminum
Gravity Die Casting [India]
50229. What is clear chem coat per
SPG-MPS-006?
50230. Inconsistency in Black Dye
Appearance on 7075 [Tennessee]
50231. Alternative to Magni coating
[India]
50232. Galvanize plating comparision to
copper plating as to rust inhibiting
50233. White Residue Problem in Black
Oxided Stainless
50234. Finishing of Sony T77 Digital Camera
- Stainless Steel
50235. Water eating away at copper
roof
50236. Different Density of Zinc
[Mexico]
50237. What happens during slow
plating?
50238. Looking for phosphiric acid anodize
per sae arp 1524
{10/10/08}
50239. Seeking shop to strip and re-nickel
plate a motorcycle frame
{10/10/08}
50240. RWC testing machine for my small
factory [India]
{10/10/08}
50241. Pretreatment for alumium for powder
coating using 3 stage spray wash. [New York]
50242. Zinc plating finish that looks
tarnished [Indiana]
50243. Black conductive plating
50244. Colour of yellow zinc
[Malaysia]
50245. Dissolution of the copper core from
the hollow jewellery
50246. Galvanic Corrosion between trivalent
chrome plated parts and stainless steel [Ohio]
50247. Seeking a flat black conductive
plating
{10/10/08}
50248. Zinc plating sealer [India]
50249. Decorative acid-wash on plate
steel
50250. RED ALMOST RUST LOOKING SPOTS ON
CARBON STEEL AFTER ZINC PLATING [Indiana]
50251. Electroplating Nickel-Boron
Alloys
50252. Nickel tin alloy [India]
50253. Deburring round pipe
[Minnesota]
50254. White spots on 22ct high polished
gold rings [India]
50255. Brass-plated lamp is rusted
50256. Corrosion resistance of stainless
vs. plated cabinet pulls
50257. Cleaning up the splinters from cut
pipe
50258. Powder coating without
baking
50259. Potential for Galvanic Action
between Stainless Steel and Iron Phosphate [North Carolina]
50260. Best book for ion nitriding
process [India]
50261. Acid cleaning cast iron pipe with
HCL [South Africa]
50262. Altrernatives to Liquid Penetration
Test? [Malaysia]
50263. Need procedure for Yellow
Passivation on Zinc [India]
50264. Blisters in Cadmium Plating
[India]
50265. Corrosion and pitting during
pre-anodize clean and etch on 7075-T7351?
50266. White spots after spray phosphating
(10 Stages Zn phosphate) [India]
50267. Want to restore patina to 18k
antique jewelry [Ohio]
{10/15/08}
50268. Copper plating [Kentucky]
50269. Hard Material that is not attacked
by piranha and HF
50270. What types of metal can you
chrome? [Iowa]
50271. Paint recommendation to refinish
Antique "Cast Iron" Water Fountain?
50272. Please advise dyi solution for
preventing metal kitchen cabinet knob corrosion
50273. Removing oxidation on aluminum that
was clear coated [Wisconsin]
50274. Cad Plate on a Copper-Aluminum
Bushing?
50275. Painting Spec for Nitrogen Tank
[Nigeria]
50276. ASF vs. Thickness guide? [South
Carolina]
50277. Tarnishing on copper plating
[India]
50278. Repairing damaged/oxidized Silver
Coatings on Connectors
50279. Substitute for MEK in
Gunwash?
50280. Solvents for PVDF
50281. Problems in Blackodising
[India]
50282. Etching bath and procedure for
titanium tubing
50283. High Temperature Water Resistant
Coating for Steel Pipe
50284. Water recycling question
50285. Discoloration on pure tin
product [Thailand]
50286. Need black oxide coating on 50,000
fasteners
{10/15/08}
50287. Titanium passivation versus
anodizing [Minnesota]
50289. Book with the best titrations
available
50291. Speckles problem in acid tin
plating
50292. Satin gold bath content
composition [India]
50293. Naming Finishes
50294. Need IVD coating service in
Europe
{10/17/08}
50295. Need Nickel Carbonate on a regular
basis [India]
{10/17/08}
50296. Need NADCAP Supplier for NAS
4006
{10/17/08}
50297. Need Sulfamate Nickel, ID Plating,
280.0" Lengths, 30.0" ODs, 14.0"IDs [Wisconsin]
{10/17/08}
50298. Wanted: Information on Powder Coat
Equipment
{10/17/08}
50299. Where can I purchase the Electronic
Grade Sulfuric Acid and H2O2
{10/17/08}
50300. Need PVD coating system
{10/17/08}
50301. Need automatic electroplating
plant
{10/17/08}
50302. Need help regarding removing tar
residue from 30,000 sf of existing concrete floor.
50303. What would be the proper treatment
of air conditioning evaporators for marine use. [Maryland]
50304. Galvanized pipe for fryer filter
[Delaware]
50305. What is Electrolytic
Galvanizing
50306. Need help for finishing: what is
ELp-Fe/Ni (92)-P10/AT [Malaysia]
50307. H2O2 and biological wastewater
treatment [Germany]
50308. Is environmental experience a good
start for a plating career? [South Carolina]
50309. Testing procedure for phosphate
accelerator [Pakistan]
50310. Stainless Steel....Black Oxide
Finish [Massachusetts]
50311. Electroless Copper Plating for
Micro-probing Transistors [Texas]
50312. Techni-White, Albaloy, Miralloy,
Optalloy, White Bronze, copper/tin/zinc alloy plating and Salt Fog
test per ASTM B117 [Massachusetts]
50313. Trivalent Zn Black Peels off
[India]
50314. Black chromate turns khaki green
(military green) after two weeks [India]
50315. Black zinc plating doesn't stick to
stainless steel [Singapore]
50316. Alternative material for 6061-T6
[India]
50317. Seeking faucet replating in
Ontario [Canada]
{10/21/08}
50318. Need Roll Bar Plating [Virginia]
{10/21/08}
50319. Need copper plating of bicycle frame
and fork [Oregon]
{10/21/08}
50320. Hydrogen Embrittlement of 1144
stressproof [Nebraska]
50321. Fluxing after hot dip
[Germany]
50322. CHROME SCRATCH REPAIR [New
Jersey]
50323. Zinc Nickel Plating [India]
50324. Roughness in copper plating bath
[India]
50325. Problem in tin plating
[India]
50326. Nickel sulphate bath pores
[Turkey]
50327. Can blue passivation pass nsst for
72 no WR? [Malaysia]
50328. Salt spray on SS 416 [India]
50329. Teflon coating vs. hard chrome
plating ? [Saudi Arabia]
50330. Need Chemical Stripping of HVOF
coatings [Arizona]
{10/22/08}
50331. Need a supplier for Mannitol,
Sulfamic Acid, and other chemicals [Philippines]
{10/22/08}
50332. What is the current status of
theoretical understanding of hard chrome plating [Greece]
50333. Painting and Distressing a Tin Tile
Mirror [New York] ![]()
50334. Clear coat mosiac in bottom of clay
birdbath [Michigan]
50335. Repair nickel-plated finish
scratches [Kentucky]
50336. Removing orange tint from Teak
[California]
50337. Replacing wheels. How are
aftermarket wheels? [Rhode Island]
50338. Corrosion in new digital camera
[UK]![]()
50339. Chroming equipment for my motor
cycles [Scotland]
50340. Tarnished Baldwin candlestick lamps
need help! [South Carolina]
50341. What is Sweet blasting?
[UAE]
50342. What is Pewter finish
[Canada]
50343. Standards for crosshatch loss for
aluminum boats [Missouri]
50344. Punching holes in powder coated
sheetmetal [New Hampshire]
50345. Want a Dupli-cell for zinc-iron
plating [Costa Rica]
50346. Passivating Heat Treated
Titanium [Canada]
50347. Please describe Zinc Phosphating to
someone familiar with anodizing [Kentucky]
50348. Champagne gold stainless steel
[Philippines]
50349. Salt fog protection for different
types of plating [Malaysia]
50350. Seeking Opinion on Anodic and
Cathodic cycles involved with Cleaning and Material activation
[Ohio]
50351. Seeking dip-spin zinc plater in the
North/South Carolina area [North Carolina]
{10/24/08}
50352. Disintegration of silver paint in
satin gold bath [India]
50353. GOLD PLATING INSIDE WAVEGUIDES
[UK]
50354. Chrome on aluminium without
zincate [Isle of Man]
50355. Does gold induce galvanic coupling
in a copper etching system? [California]
50356. WHERE TO BUY CED PAINT
[Thailand]
{10/24/08}
50357. Hydrogen embrittlement in quenched
steel [Argentina]
50358. Trying to satisfy a client wanting a
patina copper bar front [Ireland]
50359. Possible to plate a textile
sculpture? [Ohio]
50360. Removing Gold Electroplating from a
22-lb Bolt [Iowa] ![]()
50361. Artist seeks technical advice on
plating project [California]
50362. What is Nigresene coating?
[Singapore]
50363. Why does the hot dipped tin coated
copper wire blackens @ 155 C ? [India]
50364. Phosphating before painting
[Turkey]
50365. Is SS304 is a good cost cutting
solution for SS316 ? [India]
50366. Need refinishing of fancy
COPPER/BRONZE/BLACK antique grill [New York] ![]()
{10/27/08}
50367. Why does Baking Soda Blasting
prevent rust? [Belgium]
50368. Nickel-Phosphorus plating
[Israel]
50369. Plated layer (Cu-Ni-Cr)cracking
[Vietnam]
50370. Titanium tubes need etching/cleaning
in preparation for TIG welding [California]
{10/28/08}
50371. Need to cover a non-food counter top
for sales counter in retail [Alabama]
50372. Is a galvanized steel tub ok for my
dogs to drink out of? [Idaho]
50373. Problem of hardchrome plating not
depositiing on weld joints [India]
50374. Proper equipment for wheel and rim
chroming? [South Africa]
50375. What is proper Rhodium Plating
Thickness and how to measure it? [India]
50376. Galling on Rotating Stainless
Flanges [Tennessee]
50377. Non Cyanide Plating on Zinc Die Cast
(Zinc Alloy) [Thailand]
50378. Titanium and stainless anodizing
process information [Pakistan]
50379. Passivation for Stainless 318
[Israel]
50380. Reducing the friction coefficient of
stainless steel on steel [Israel]
50381. ISO 1320:1192 an active or inactive
standard [Mississippi]
50382. Cadmium plating adhesion problem on
15-5 PH [India]
50383. Need shop to apply conductive black
plating on stainless steel strip [Malaysia]
{10/30/08}
50384. Chromate passivation solution is
stripping the cadmium plating [Ireland]
50385. Yellow Iridite for aluminum parts to
be painted [Florida]
50386. Suggested Tank Lining for 98%
Sulfuric Acid? [UAE]
50387. Adding ammonium chloride in powder
form to surface of hot-dip bath and it's effects on the environment
and humans [Australia]
50388. Teflon paint removal --non chemical
immersion type solution needed [California]
50389. Material for handling 80~95%
Sulfuric Acid @ 280~320C and 1atm [Taiwan]
50390. Chemicals for brightening of ss
components? [India]
50391. Bike mfgr. needs etching service on
titanium tubes [California]
{10/30/08}
50392. What is most cost efficient at
resisting corrosion on steel surfaces? [China]
50393. Abrasion resistance of type 3 vs
type 2 anodizing [Utah]
50394. Need oven to burn sweeps
[Florida]
50395. Forcing Chrome to Tarnish [New
York]
50396. Help with carbonate build up in
Albaloy bath [Massachusetts]
50397. Help seeking research literature
review sources regarding chrome plating acceptability [Ohio]
50398. Jeweler doing rhodium plating needs
good electrochemical cleaning salt [India]
{10/30/08}
50399. Need Spare Parts for our salt spray
chamber [Turkey]
{10/30/08}
50400. Does Zinc Plating on 17 HRC steel
need hydrogen embrittlement relief? [India]
50401. Need Help With Paint for
Refrigerator Door Handle
50402. Hot Black Oxide on Copper
[Colorado]
50403. Need Nickel plating on
carbon/epoxy [California]
{10/31/08}
50404. Colour of electroless NiB bath and
stability [India]
50405. High emissivity, high temperature
resistant coating for surface temperature measurement using
IR-pyrometer [Germany]
50406. Stainless only tools for finishing
SS - how critical [Virginia]
50407. Honda ST1300 motorcycles thermostat
failure [Georgia]
50408. Painting a cast aluminum product to
the best quality finish [Colorado]
50409. Galvanising tank material
[Nepal]
50410. What kind of galvanizing for a
hollow metal door [Puerto Rico]
50411. Pulse Plating for Palladium?
[Texas]
50412. BLISTERS IN PLATING 8740 MATERIAL
WITH CADMIUM (AMS-QQ-P-416 TY.II CL.2) [California]
50413. Plating on Molybdenum
[California]
50414. TSA OR BSAA INSTEAD OF CAA,
CONVERSION COATING [Turkey]
50415. Purpose of Zinc Bath
[Alabama]
50416. Boric Sulfuric Electrolyte
Analysis [New York]
50417. Change in frictional properties
after passivation [Texas]
50418. What does iron phosphate do to hot
dip galvanized steel [Florida] ![]()
50419. Zinc Phosphate Nubbing on Clean vs.
Coated Racks [Michigan]
50420. How would you finish a composite
field hockey stick? [UK]
50421. Patinating copper plating
[Massachusetts]
50422. Need AgC Plating Literature
please [India]
50423. Cooling system for hard
anodizing [Indonesia] ![]()
50424. Anodizing, is it food safe?
[Canada]
50425. Silica removal by anion
exchanger [Iran]
50426. Deflashing chemicals for
leadframes? [Philippines]
50427. Do's and Dont's for new E coat paint
shop [India]
50428. How to make Galvanizing Flux?
[India]
50429. Threaded steel rod, zinc plated with
trivalent chromate screwed into aluminum plate
[Massachusetts]
50430. Etching mild steel tubing for good
adhesion of urethane coating [Wisconsin]
50431. Zinc Phosphate - Lubricity
[Michigan]
50432. What is the allowable extent of
magnetism in CF8m castings? [India]
50433. Artist neeeds Au plating on
Bronze [Maine]
{11/5/08}
50434. Looking for process distributor of
5-stage iron phosphate [Texas]
{11/5/08}
50435. Removing hot dip zinc coating from
wash tub [Alabama]
50436. Electroplating tin on copper
[Pakistan]
50437. Is Trivalent Chrome Passivation and
Electrolytic Process? [Turkey]
50438. Trouble shooting for
electroplating [Malaysia]
50439. Brush Plating Titanium??
[California]
50440. Problem in Nickel Chrome Plating
[India]
50441. Chrome Plating of Striped Cylinder
Liner [India]
50442. Formulation of copper strike/plating
bath for stop off of nitriding [Canada]
50443. Peeling problem in nickel-chrome
plating [Canada]
50444. Implications of adding selective
Gold over Stainless Steel 301-1/2 hard [Mexico]
50445. Tin plating testing points
[India]
50446. Eliminate bulk anodize
burns/voids [California]
50447. Anyone seen this aluminum anodizing
defect? [Michigan]
50448. Coating on etched aluminum foil
[New York]
50449. Will anodized stainless steel seize
with another stainless steel part ? [Canada]
50450. Need baby shoes pewtered.
[Colorado]
{11/7/08}
50451. Artist needs bronze sheet plated on
one side with 18-22k gold [Maine]
{11/7/08}
50452. Need worn coffee machine parts Brass
Plated [Georgia]
{11/7/08}
50453. Need powder coating system for wood
and MDF board [India]
{11/7/08}
50454. Why are car wheels made of
steel? [India]
50455. Restoring the dark brown finish to
copper sinks [Texas]
50456. Allergic to White Gold engagement
ring, what to do? [Canada]
50457. Removal Of Thin Stroke Ni
Electroforms [Florida]
50458. pH drop in Nickel Sulphamate
installation [Portugal]
50459. What chemicals will remove black
stains on steel at weld areas? [Turkey]
50460. Citric Acid Passivation Problems
[Australia]
50461. Is phosphate coating making our
springs squeak? [Texas]
50462. Pencil Hardness failure issue on abs
finish [California]
50463. HCL titration analysis
[Texas]
50464. Need shop to do plating of ABS
plastic with brass [Mississippi]
{11/10/08}
50465. Want copper plating of Harley Ultra
Fire Fighter wheels [Alabama]
{11/10/08}
50466. Want to buy dead flat optical
paint [Florida]
{11/10/08}
50467. How to determine the composition of
a coin [Canada]
50468. Automotive use of Stainless Steel
Fasteners in Aluminum Block [New Zealand]
50470. Sodium Bicarbonate Analysis [New
York]
50471. Removed screen paint from plastic
HDBE crates with sulfuric acid [India]
50472. Clear coat for high polish
brass? [Wisconsin]
50473. Soldering of galvanized versus
galvannealed metal [North Carolina]
50474. Is anodizing of galvanised sheet
steel possible (PGI) [Australia]
50475. Effect of citric acid on a
electroless nickel plated surface [Portugal]
50476. What is the better finish
specification for steel close to the sea? [UAE]
50477. Questions about military finishing
spec. MIL-STD-171? [Florida]
50478. Green Aluminum Oxide Powder on a
supposedly anodized component [Illinois]
50479. Copper Heat Exchanger Corrosion
[Canada]
50480. Aluminum plenum needs nickel plating
in Tulsa, OK [Connecticut]
{11/12/08}
50481. Want New Holand Spin Dryer
[Massachusetts]
{11/12/08}
50482. Need screw painting equipment
[Canada]
{11/12/08}
50483. Painting screws in large volumes.
How is it done? [Canada]
50484. ALUMINIUM ANODIZING FAILURE
[Italy] ![]()
50485. Seeking iron plating deposit on
parts [Oregon]
{11/13/08}
50486. Need antique silver plating
chemicals [Turkey]
{11/13/08}
50487. Need a very good varnish
[Turkey]
{11/13/08}
50488. How to build a "hot tank" for metal
cleaning? [Canada]
50489. Need customized electrolytic
reduction cell [India]
{11/13/08}
50490. Need Gold Potassium Cyanide
Machine [India]
{11/13/08}
50491. Wanted: someone to help me setup and
learn to do MIL-C-5541 at my plant [New York]
{11/13/08}
50492. Vertical soldering 24 gauge
bonderized box rain gutter. [California]
50493. Need rusty steel sheets for book
covers [New York]
50494. What does MFCr3 mean?
[Malaysia]
50495. ASTEC QP4412? [Delaware]
50496. How to keep up with revised
Specifications? [Michigan]
50497. Order Entry Software for Metal
Finishing [Georgia]
50498. Re-Use of Spent Sulfuric Acid.
[India]
50499. Use of copper sulfate to protect
metal [Texas]
50501. Bronze Finish is rusting and
flaking [UAE] ![]()
50502. Passivation of 316 Stainless - Bath
required? [California]
50503. Electrolytical removal of low
alloyed steel plate [Sweden]
50504. Help = 5 stage Pre-Cleaner /
Phosphate coating for Powder paint system [Massachusetts]
50505. Removing snap ring burr on an
interrupted cut on work hardened spline [Michigan]
50506. Silver Plating or Coating a timber
beam [Greece]
50507. Nickel plating vs. e-coating?
[Massachusetts]
50508. Customs officer says 400 series is
not stainless steel [India]
50509. Need 5 cherry doors stripped in dunk
tank [Minnesota]
{11/14/08}
50510. Technology supplier for
manufacturing of sodium polysulfide [Thailand]
{11/14/08}
50511. Nambe metal bowl has dark stain
[Iowa]
50512. Trying to strip chrome nickel and
copper from a thousand car wheels a week [Florida]
50514. Can I use Cvd system for metallizing
and tiN COATING? [India]
50515. Aluminium etching question
[South Africa] ![]()
50516. How to produce titanium-like finish
on stainless steel [Indiana]
50517. Anodizing and alodizing
[Australia]
50518. Acid zinc barrel inconsistent blue
chromate [New Zealand]
50519. Need Information on Paint Sludge
Recylcing in the UK [England]
{11/17/08}
50520. Turquoise Collector, was given 250
lbs. of Silver Ore from 92 yr. old miner's Wife. [Arizona]
50521. Immersion silver tarnish issue after
wave reflow in RoHS environment [Malaysia]
50522. Using steel plate on a bar table
[California]
50523. Can we do decorative chrome from our
hard chrome tank? [Tennessee]
50524. Are there alternatives to
passivation? [Illinois]
50525. 17-4 forging rust on un machined
surface [Georgia]
50526. Avoiding corrosion from stainless
cleat on aluminum "tinnie" [Australia]
50527. Apartment complex asks about proper
repainting of old galvanized doors [Pennsylvania]
50528. New plant having some problems with
CED electrocoating [India]
50529. Erosion of the zinc passivated
surface in storage [India]
50530. We are powder coating aluminum
sheet, but paint is peeling off [India]
50531. Best coating for black exhaust
tips? [Wyoming]
50532. Science project: Hydrochloric acid
affect on different metals. [Michigan]
50533. Need chrome dipping (not
electroplating) equipment [Canada]
50534. Molded or formed plastic needs a
good mirror finish [California]
50535. Quantifying the effectiveness of
scale removal [Michigan]
50536. Removing scratches from lexan
drive-thru windows [Illinois]
50537. Need bronze statue repair and
restoration [New Jersey]
{11/20/08}
50538. Want polishing and plating of old
glass doorknobs, hinges, etc. [Georgia]
{11/20/08}
50539. Need derusting (slight) and
refinishing of four Toyota RAV/4 wheels [Illinois]
{11/20/08}
50540. Need a shop to take white rust off
galvanized coils in northeastern USA [Pennsylvania]
{11/20/08}
50541. Need Passivation Consultant for
Nitric [Pennsylvania]
{11/20/08}
50542. Seeking Parkson Clarifiers
[Michigan]
{11/20/08}
50543. Need my wheels chromed [Texas]
{11/20/08}
50544. Protective Coating for a Solar Power
Pond Project - Reg [India]
{11/20/08}
50545. Need hot dip galvanizing unit for
nuts and bolts [Oman]
{11/20/08}
50546. Requirement for a PVDF coating
plant [India]
{11/20/08}
50547. Stainless steel street rod uses
aluminum rivets. What now? [Pennsylvania]
50548. Thermal conductivity of chromate
conversion coating [North Carolina]
50549. Is there danger of hydrogen
embrittlement from acidic passivation of titanium? [Israel]
50550. We plate copper on Zammak, what
changes are needed to plate on iron [Pakistan]
50551. Digital printing on anodized
aluminum [Canada]
50552. Seal issue with nickel fluoride and
hot flashed part [Michigan]
50553. Anodizing and molding
[Pennsylvania]
50554. In A967 passivation, does the 25% by
vol. Nitric represent industrial (65%) or full strength Nitric?
[Mississippi]
50555. Can I use a PC power supply for
anodizing? [Michigan]
50556. Copper Size for DC low-voltage
high-amperage [Malaysia]
50557. IR Oven creating dirt in powder
coating process [Canada]
50558. Corrosion on sharp edges metal parts
with polyester powder coating [Malaysia]
50559. Corrosion Resistant Plating for Cold
Rolled Steel [California]
50560. Corrosion resistance of Hard Chrome
at pH 1 [South Africa]
50561. Crazing problem on welded assemblies
made from 5052 H32 aluminum [California]
50562. Electropolishing Problem [New
Jersey]
50564. Delayed Blisters in Alkaline Zinc
Electroplating [Michigan]
50565. Need to ASTM A463 Alumize coat SAE
J1392 HSLA steel [Michigan]
{11/21/08}
50566. Titanium chemistry in HF and HNO3
chemical milling [New York]
50567. Appearance issue on zinc-nickel
plated parts (heat treated parts) [Indonesia]
50568. HARD ANODIZING COATING THICKNESS NOT
BUILDING UP [India]
50569. Interpreting salt spray results on
e-coated zinc plating [South Africa]
50570. Lacquering Nickel and Brass
[North Carolina]
50571. Welding problems on plated
terminals [Mexico]
50572. Mismatched Stainless Kitchen
Appliances [Louisiana]
50573. Using ammonia in pickling
solution [Iran]
50574. E-coating facility [Florida]
{11/21/08}
50575. Shot blasting to a SA-2-1/2
surface [India]
50576. Inhibitor for stainless steel
pickling? [Malaysia]
50577. Need rebrassing of candleholders and
lamp items [New Jersey]
{11/25/08}
50578. Electroplating steel components with
copper [Pakistan]
50579. Mixed bleach with phosphoric acid
and inhaled it [Kentucky]
50580. Is nickel plating or tin plating
better for a wine press? [Canada] ![]()
50581. How to treat spent Nickel solution
containing Nitrobenzene Sulfonate [Malaysia] ![]()
50582. Trivalent Yellow passivation failing
in 13-20 hrs salt spray [India]
50583. How to deliberately accelerate
crazing and cracking problems of powder paint [Turkey] ![]()
50584. Converting rhodium dip plating
solution for use in pen plating [India]
50585. Pipe Ramming Sleeve. Protection of
the steel casing [Ireland]
50586. Construction manager needs
oil-rubbing of large bronze sheets [New York] ![]()
{11/26/08}
50587. Need someone to Re-enamel old
bathtubs [Jamaica W. Indies]
{11/26/08}
50588. How can you tell if a screw or nail
is galvanized or zinc coated? [Oregon]
50589. Marbleized blackening effect on
copper [Texas] ![]()
50590. Suitability of Cr Plating on SGI
base metal for Sea Water application [India]
50591. Segment of aluminum piano hinge
needs a black anodized finish [Washington]
{11/26/08}
50592. Spots on Alu extrusion from PVC
protection tape [Singapore]
50593. How to plate copper on paint
[Singapore]
50594. Electroless Nickel Poor Finish on S7
Tool Steel [Kansas] ![]()
50595. Need cold blackodizing process
[India]
{11/28/08}
50596. Want consistent 2-tone plating on
acid tin [India]
50597. Artist seeking to recreate natural
rich dark brown brass patina [UK]
50598. Looking for a shop that can do
e-coating and metal stripping near NJ/NY/PA [New Jersey]
{11/28/08}
50599. Flatware is claimed as 18/8 but not
so marked [Connecticut]
50600. How to prevent micro-flaking of cast
aluminum 383? [Oregon] ![]()
50601. Can I use EGI sheets for outdoor
applications? [India]
50602. Seeking clear high temperature
adhesive for glass [Egypt]
{11/28/08}
50603. How to chemically determine Na + and
K+ in salts? [Egypt]
50604. Tell me about Aluminium
Sputtering [India]
50605. Comparison of 440C with SS 321 for
valves for steam service [India]
50606. Urgent Solution Needed for Chroming
failure. Chrome specs suspected [Florida]
50607. Rust proof coating [India]
50608. Need for CR6-free internally and
externally plated hydraulic tube [England]
{11/28/08}
50609. Passivation of electroless nickel --
theory and practice [Argentina]
50610. Excessive decarburization due to
zinc plating and baking [Minnesota]
50611. Best acid dip for powder coating
[Maine]
50612. Galvanising Ash Generation
Benchmarking [Mexico]
50613. White spot appears on bright
nickel/chrome plated faucet [South Korea]
50614. Seeking a supplier of electroless
boron baths [Turkey]
{12/2/08}
50615. Can't chromate spot weld marks on
aluminium chassis [Singapore]
50616. Renew Old Flagpole for 100th
Anniversary Celebration [New Jersey]
50617. Painting to prevent build up in
preheater fans [India]
50618. Hard Anodize Ripple Problem
[Utah]
50619. Will Ameron 2/400 adhere to
sandblasted Inconel? [Louisiana]
50620. Stainless Steel is suffering black
patches after passivation [UK]
50621. Need chrome plating and polishing in
Mexico [California]
{12/2/08}
50622. Adhesion problems while
powdercoating over clear zinc, chromate ROHS compliant
[Minnesota]
50623. Which rusts 1st? [Trinidad and
Tobago]
50624. E-coating on silver [New
Hampshire]
50625. What to do about the vin #
sticker [Louisiana]
50626. Differences between hot and cold
sealing (advantages and disadvantages) [Egypt]
50627. Want to buy Gearless
Contractometer [China]
{12/3/08}
50628. Electroless Nickel Plating on
Gold? [Sweden]
50629. Solid oxide fuel cell
construction [Alabama]
50630. Weatherproof Clear Coating to Keep
Polished Brass Shiny [Maryland]
50631. Scratched chrome [Alabama]
50632. Zinc Phosphate pretreatment ASTM
number? [India]
50633. Excessive water carryover into our
fume scrubber [Phillipines]
50635. Ni plating spot check?
[Michigan]
50636. Hydrogen Embrittlement in
Electroless Ni Plating [England]
50637. Red dot in 24k gold electroformed
product [Hong Kong]
50638. Is my chromate conversion system up
to par? [Florida]
50639. Machining after Passivation
[California]
50640. Corrosion of SS316 in 1.2 pH buffer
solution [India]
50641. Pumping Sodium Hypophosphite
[Michigan]
50642. Twisting of cold rolled steel sheet
during PVC coating [Turkey] ![]()
50643. Paint Biocompatible ISO 10993 or USP
Class VI [Arizona]
{12/4/08}
50644. Wood cookstove surface plate
repair [Pennsylvania] ![]()
50645. CHROME PLATING SAFETY ISSUE
[China]
50646. Making Hard Chrome Harder
[California]
50647. Electroplating Printed Circuit
boards [New Zealand]
50648. Looking for a zinc plater in
Northern Mexico [Michigan]
{12/5/08}
50649. Nedox coating on aluminum plate 6061
alloy [Wisconsin]
{12/5/08}
50650. Platinizing Tungsten
[Maryland]
50651. Options for low VOC clear coat
finishes on steel [Virginia]
50652. Home made electroless plating
solution [Tennessee]
50653. How to rid house of toxic Rustoleum
paint used in shower stall [California]
50654. Searching for "Plating" by P.C.
Baldwin [Wisconsin]
50655. Non insulated anodes in cyanide zinc
tank [Venezuela]
50656. Watts Nickel bath gassing too
much [Colombia]
50657. Nickel Chrome plating ability due to
pin hole [Indonesia]
50658. 21 questions for the most brilliant
scientist [Michigan]
50659. Etching process for Pt-Rh wire
[India]
50660. Cement art on eg baskets, sandals
etc [South Africa]
50661. How do I restore a copper finish on
a 120 year old steel fireplace mantle? [Illinois]
50662. Paint stripper and aluminum
[Texas]
50663. Subjecting 304L to PWHT
temperatures [Alabama]
50664. Analysis of copper plating solution
(acid based) [India]
50665. Electric insulation properties of
powder coated surfaces [Tennessee]
50666. BLACK OXIDE FOR STAINLESS STEEL
17-4 [Malaysia]
50667. 4 stages for degreasing and
polishing aluminium rivet heads [Iran]
50668. CONTROL OF RESIDUAL PHOSPHATE
[Italy]
50669. Restoring black lacquer finish on
antique furniture [Virginia]
50670. Anode bags maintenance?
[China]
50671. How to deal with Paint Sludge
[Indonesia]
50672. Permanent colors on tin metal
[England]
50673. Inside blowing of 73 od pipes
[India]
50674. Peel Off and Pin hole problem on SG
Iron Hard Chrome Plated surface after Grinding [India]
50675. Possible Negative Effects of
Exposure to Iron Phosphate Wash on Brass and Zinc-plated Forged
Steel [Florida]
50676. Preparing a 1940 truck grill for
chrome [California]
50677. Do copper utensils contains any
trace of lead in it? [UK]
50678. How to make Aluminum Sheet look like
new shiny COPPER (no patina)? [Florida]
50679. Hexavalent and trivalent salt spray
hours? [India]
50680. De-galvanising sheet metal
[India]
50681. Removing chrome from aluminum wheels
and painting them [Pennsylvania]
50682. Black Chrome Specification [New
Jersey]
50683. Anodizing Assemblies - trying to
minimize / avoid bleeding [New York]
50684. Current carrying capacity of nickel
plated plastic? [Minnesota]
50685. Looking for a non hexavalent
corrosion resistent primer for use on carbon steel
[Connecticut]
50686. Chrome plating defect at seam
[Italy] ![]()
50687. My Copper Valleys... [Ohio]
50688. Pre-bond cleaning of magnesium
[Connecticut]
50689. Changing household appliances from
black to white [Louisiana]
50690. Need info on cadinum vs yellow
zinc [Alaska]
50691. About chemical masking [China]
![]()
50692. Trivalent Phosphate VS Hexavalent
for inline cleaning prior to inline painting [Ohio]
50693. Help with removal of melted/burnt-on
Teflon [New York]
50694. Using furniture stripper on my brass
bed...should I? [Minnesota]
50695. Risk and safety statements in
various languages (MSDS) [Belgium]
50696. Help in getting BAC approved for
chemfilm and topcoat approved [Missouri]
50697. Design of equipment for dip spin
coating [India]
50698. Explosive limits of powder in powder
coating? [Scotland]
50699. What's FH galvanized steel G60?
[China]
50700. PVC Extrusion tooling corrosion
resistance E Nickel vs. Chrome [Australia]
50701. Removing recast layer after EDM
process on hardened A286 Nickel alloy [New York]
50702. Need surface grinding of an 18"
level [Texas]
{12/16/08}
50703. Seeking X ray fluorescence (XRF)
-secondhand machine [UAE]
{12/16/08}
50704. Etching Silver coated acrylic
[Argentina]
50705. How to Strip Silicon Carbide
[India]
50706. Aluminum cylinder permanently in
salt water [Canada]
50707. Black stains formation
[India]
50708. Development of a Capacitive Mercury
level sensor [India]
50709. Blue Zinc is turning yellow over
time [India]
50710. What are the specs for brass hull
cell test panels? [China]
50711. Can micro-crack density be too
high? [Tennessee]
50712. How to calculate plating
thicknesses [China]
50713. Converting part per million to
ounces per gallon for a dilute chromate seal [Texas]
50714. Do I need to Anapol if shot blasting
stainless steel? [England]
50715. Cleaning electroless nickel plated
aluminium post plating. [England]
50716. Phosphate sludge disposal
problem [India]
50717. Does the zinc-phosphate finishing
(or pre-finishing) layer become an electrical conductor? [New
York]
50718. Interpretating Corrosion
Specifications [UK]
50719. Need Copper Coating of Large
Stainless Steel Screens [California]
{12/17/08}
50720. Black Nickel Plating -
Solderability [Malaysia]
50721. Need Universal Black Finish to
replace Enequist Electroblack [Australia]
{12/17/08}
50722. Need Gold plating on dog's rabies
tags [Montana]
{12/17/08}
50723. What plating will not cause hydrogen
embrittlement when welded? [Ohio] ![]()
50724. Need olive drab Zinc plate
[Pennsylvania]
{12/17/08}
50725. Need Sulfamate Nickel Plating of
internal bore [New York]
{12/17/08}
50726. Need kolesterising service for our
washers [India]
{12/17/08}
50727. Want to buy continuous hot dip
galvanizing line [Spain]
{12/17/08}
50728. Plating shop needs nickel
hypophosphite [Iran]
{12/17/08}
50729. Info on "Finish Process per ES12717,
METHOD III" please [Canada]
50730. Help to remove fingerprints from
powdercoated surface needed [New Zealand]
50731. Chrome Plating hydraulic piston rods
for marine applications [UK]
50732. Spots on nickel plate over high
polished brass [Colombia]
50733. Want organic additive to reduce
electroforming to one third of the normal process time
[India]
50734. Ni sulfamate grows too warm
[Iowa]
50735. Finishes on aluminum
[Georgia]
50736. Corrosion on Clear Coated Die-Cast
A380 Aluminum Parts for Gym Equipment [California]
50737. Corrosion of GA or Zinc plating
without passivation [India]
50738. Need chrome plating of a metal table
base [Ohio]
{12/19/08}
50739. Process for Titanium Oxidizing?
[Canada]
50740. Removing grey tarnish on a 92.5
silver ring [Philippines]
50741. Need Phosphoric anodizing ROM
costs [Washington]
{12/19/08}
50742. Recommended jeweler in Los Angeles
for rhodium plating [California]
50743. Looking for coating chemical for
ink-jet printing on metal [Georgia]
50744. How to Coat Plastic Spheres with
Zinc? [California]
50745. How to detect stain on a silver
plated lead frame? [Malaysia]
50746. A967 or AMS 2700? Which is the right
passivation spec to use? [Massachusetts]
50747. Too much silver plates onto cathode
plates in copper refinery [India]
50748. Repairing Scratches on Ceramic flat
top Stove Help [Tennessee]
50749. Refinishing my heavily etched brass
table top [Illinois]
50750. Ruined oiled bronze bath faucet
[Texas]
50751. Cleaning an antique brass or copper
dog [Mississippi]
50752. Bronze to Oil Rubbed Bronze [New
Jersey]
50753. How can I strip hard chrome from
different metals? [Florida]
50754. High Absorptivity, Low Emissivity
Paint [New York]
50755. Packing standards for painted/powder
coated finished goods [India]
50756. Blemishes / scabbing on fresh Galv'd
steel [Great Britain]
50757. Sulfuric Acid Anodize
[Alabama]
50758. Resists for chemical milling mold
texturing [Sri Lanka]
50759. Need silver plating brightener
(black powder) [India]
{12/23/08}
50760. Best coating for 7075 aluminum
alloy [Iran]
50761. Plating onto glass [UK]
50762. Sink drain with rust stains [New
Jersey] ![]()
50763. Chrome plating inflatable vinyl
toy [California]
50764. Nodular extra chromium deposit at
inside of dia 40mm rings [India]
50765. Passivating 304 and 308 SS, salt
spray problems [Mexico] ![]()
50766. Rusting problem in phosphated
surface [India]
50767. Need hard coating and nickel acetate
sealing [Florida]
{12/23/08}
50768. Need phosphatizing tanks
[Venezuela]
{12/23/08}
50769. Electroforming problem due to
excessive 2 butene [Turkey]
50770. Ultrahard Coating/Plating for
Titanium? [Oregon]
50771. Electroless ruthenium or iridium on
aluminum [Maryland]
50772. Is galvanized steel used for
automobile bodies? [India]
50773. De-rusting a rusty buckknife
[Kentucky]
50774. Safety of galvanized barbeque
[Australia]
50775. Want to powder coat a chrome snare
drum [Idaho]
50776. Galvanic effect pros n cons with
copper and aluminum [India]
50777. How can I restore the black
highlighting that was originally on my sterling silver flatware ?
[New York]
50778. Detecting presence of Clear Chromate
Alodine Iridite [Illinois]
50779. Process to decorate architectural
grilles to match 'cor-ten' steel? [California]
50780. Advantages of electrodeposition over
conventional powder coating [India]
50781. Nervous employee seeks plating
jobs [Missouri]
50782. How to Recover Gold From
Solution [India]
50783. Need supplies for glass coating in
vacuum machine [India]
{12/23/08}
50784. Wear rate calculations
[India]
50785. Step-like defect in LCD area of tin
plating [India]
50786. Incomplete Anodize Finish and
Surface Imperfections [Ohio]
50787. Re-finishing Chrome Parts [New
Jersey]
50788. Where I can find good plastisol with
good price [Jordan]
{12/26/08}
50789. Need Help with setting up a Surface
Temper Etch Line [Canada]
{12/26/08}
50790. Need dilute sulphuric acid (Lots I
promise) [UAE]
{12/26/08}
50791. Painting procedure for aluminium
castings used in chemical measurement instruments [India]
50792. Delay tarnish in copper
electroformed pieces for later silver or gold plate
[Colombia]
50793. Staining/blemishes in
electrogalvanizing step ladders [Kazakhstan]
50794. Need pinkish brown patina on bronze
piece for next week. Help! [Massachusetts]
50795. Wanted: sandblasting and clear
coating of 1970s steel desk [Georgia]
{12/26/08}
50796. Hydrochloro acid pickling vs shot
blasting [India]
50797. Electroless Ni-B coating is dark not
shiny [Iran]
50798. Change chrome shower parts to oil
rubbed brass [Illinois]
50799. What is a correct method of
measuring micron plating on 925 silver [India]
50800. Aluminum alloy and surface finish
preferred for marine use [India]
50801. Stainless steel nut vs mildsteel
bolt [India]
50802. Need rechrome of 20" rims
[Delaware]
{12/29/08}
50803. Need chroming done for my 2001 cbr
929 [New Jersey]
{12/29/08}
50804. Need Hardcoat Anodizing 6061-T6
Machined Round Stock [New Jersey]
{12/29/08}
50805. Need bronzing of a small organic
item (baby snake) [Ohio]
{12/29/08}
50806. Need replating and full-plating of
watches [Russia]
{12/29/08}
50807. Need brass antique finish chemicals
and electroplating chemicals [India]
{12/29/08}
50808. Rusting remover with nails!
[Texas]
50809. Color sanding chrome fx?
[Colorado]
50810. Refinishing "antique" electrical
breaker-box cover [Texas] ![]()
50811. How to antique white wood kitchen
cabinets [Kentucky]
50812. Restoring the inside of a wood
stove [Rhode Island]
50813. Did I ruin my silver with
bleach? [California]
50814. 1960s GM chrome plating
[Wisconsin]
50815. Best method of Centrifugal Casting
of Brass Rods [India]
50816. Shavings from CF8M are lower in
chromium content than spec. Possible? [India]
50817. How to dissolve sulfamic acid and
make it into liquid form [Pakistan]
50818. Matte wrinkled oil paint
[Nigeria]
50819. Solvent Bonding ABS to ABS
[Florida]
50820. Water Based Anti Rust Coating for
Wire Nail Coils [India]
50821. Dross control in galvanising
[India]
50822. Reducing the variation of hardchrome
plating [India]
50823. Rhodium plating problems
[Pakistan]
50824. Achieving polished, durable finishes
on 6061 Aluminum [California]
50825. 240 grit polish to a 'Y' strainer
body [India]
50826. How to polish copper [Egypt]
50827. Need help on learning to finish
brass horns [Oklahoma]
50828. Galvanic Corrosion between Brass and
Aluminum [Egypt]
50829. Need help finding a company to blue
large fireplace items [Tennessee]
{12/30/08}
50830. Is 85% copper 15% zinc jewelry
toxic?
50831. Yellow Zinc/Silver Zinc??
[Pennsylvania]
50832. Electropolishing with weak acid?
[Maryland]
50833. Want to private label electrolytic
silver cleaning plate [Australia]
{12/30/08}
50834. Controlling white rust in
galvanizing [India]
50835. Need 20-year protection by
electrogalvanizing [India]
50837. Using stainless steel for PVD
[Pennsylvania]
50838. Regarding tin plating on aluminium
alloy [India]
50839. Need chrome plating in Mexico
[California]
{1/2/09}
50840. Need Printing (graphics/text) onto
Anodized Aluminum finished components [Michigan]
{1/2/09}
50841. Finishing a processional cross
[Nebraska]
50842. Rusted Metal Used in Home
Interior? [Washington]
50843. Recovery Of Fine Processed Gold
Dumped As Waste In The River [New Guinea]
50844. Repairing Fibreglass Acid Bath
[Australia]
50845. Which process need for miror effect
polishing for hard chrome 5-8 micron on copper [China]![]()
50846. Cleaning 304 SS rusty pipes and
fittings at site [UAE] ![]()
50847. Black coatings for 304 stainless
[California]
50848. Need shop for EN, Chrome, and Grind
work [California]
{1/5/09}
50849. Need chromate touchup pen for yellow
zinc plating [New York]
{1/5/08}
50850. Diffuse titanium in vapor
[India]
50851. Is there any such thing as sterling
silver plate? [Australia] ![]()
50852. Cleaning Chrome-Plated Steel Swords
for Display [Texas]
50853. Can hubcaps for a 1955 Chevrolet be
regalvanized to look new [Texas]
50854. Alternative for TCE
[Philippines]
50855. Nickel plating (Bright) Process
capablity and control charts [India]
50856. Capacity of P-nitrobenzene sulfonic
acid as a gold stripper [India]
50857. Stripping racks or hangers in
minimum time [India]
50858. Darkening on the galvanized coated
steel (both galvanized plain and galvanized skinpass) [India]
50859. Adherence problems with
galvanizing [Brazil]
50860. Line mark and dent mark obsevered in
chrome plated rod [India]
50861. Small hand tool for removing flash
from rubber product [India]
50863. Need fabricator for zinc
tabletop [Texas]
{1/7/09}
50864. Finishing a wine cellar tasting
table [Florida]
50865. Material of construction for
manganese phosphate tank [New York]
50866. Can cast 316L stainless be
galvanized and how would it perform in seawater? [New York]
50867. How to remove acid from zinc in
plating [Mexico]
50868. Pickling problem for carbon steel
pipes [Iran]
50869. Polishing on a vertical CNC milling
machine? [New Hampshire]
50870. Does real stainless steel get
rainbow color/blue tinting ? [Texas] ![]()
50871. Can I use AISI 1010 as alternate to
Q345E steel? [India]
50872. Can MIL-PRF-85582 replace
MIL-PRF-23377? [Missouri]
50873. Locating lost parts in a plating
tank [Florida]
50874. Soldering problem on
electrogalvanized iron wire [India]
50875. Nylon-11 based polyamide coating
won't stick to ductile iron parts [Indiana]
50876. Better terminology than "A-A-A
Passivation"? [Illinois]
50877. Descaling heat treated 303SS
[Arizona]
50878. Black "rub" on stainless food
equipment [Washington]
50879. Looking for chrome plating equipment
on plastic to start a fam. business [Mexico]
50880. Difference between a virgin raw
material and a reprocessed material [India]
50881. How to minimize spangles [Saudi
Arabia]
50882. Cracking in silver plating
[Canada]
50883. Plating peeling on phosphor bronze
springs [Georgia]
50884. Life expectancy for plating chromium
bath [Mexico]
50885. Thickness of anodize coatings
[Texas]
50886. Restoring my brass and glass
tables [California]
50887. Passivate modified gold-plated 303
SST SMA connector [New York]
50888. Damaged the finish on copper table -
HELP!!! [New Jersey] ![]()
50889. Want to Black Chrome my "bike"
[Wisconsin]
50890. What do I use to finish a tin mirror
frame from Mexico? [Massachusetts]
50891. Method of analysis for Palladium
activator solution for plating on ABS? [Colombia]
50892. What fasteners to avoid corrosion in
this home renovation? [Australia]
50893. Alternatives to gold cyanide
bath [Italy]
50894. Differences of plating (nickel, blue
zinc, rainbow zinc) [Malaysia]
50895. Training for Barrel Nickel
Plating [Vermont]
50896. Metals compatibility with Deionized
water [Minnesota]
50897. Recommendations for a flexible paint
system to paint graphite/epoxy bike? [California] ![]()
50898. How I can get a good appearance of
Alodine 600? [China] ![]()
50899. Need Chrome plating of ABS
plastic [Denmark]
{1/13/09}
50900. Need my old wrought iron front porch
stair railings stripped and refinished [Kentucky]
{1/13/09}
50901. Seeking zinc-iron plater in
Wisconsin [Michigan]
{1/13/09}
50902. How Can I Remove the Gold Plating
from Stainless Steel Watch Strap [Italy] ![]()
50903. Lighting design for powder coating
oven [New Hampshire]
50904. Preparing Titanium for Paint
[Oregon]
50905. Bright (hard) gold plating process,
brown at first, then goes bright, why?? [Virginia]
50906. Why a pH control in chromic
anodize? [Georgia]
50907. ZINC PHOSPHATING [India]
50908. How to destroy an ominous stainless
steel object so I can rest [Australia]
50909. Black Chrome Plating Please??
[Texas]
{1/13/09}
50910. How do I get the color green from
flame treatment of steel? [Colorado]
50911. Restore anodized alum sheets?
[South Carolina]
50912. Hardened chrome rods [India]
50913. SS301 / 07 x 16H6 Heat Treatment
[India]
50914. Stress Relief Annealing Type 301
Stainless Steel [Illinois]
50915. Looking for a school to take classes
in plating [Massachusetts]
50916. Resistivity probe installation
[Texas]
50917. White rust on 5/16" Galvanized
Spring Steel Rod [Minnesota]
50918. ENI Flaking off of 3003 Alum
[California]
50919. Heat treated electroless nickel
coloring as gun finish. [Idaho]
50920. Question about anode to cathode
ratio on watts bath [Colombia]
50921. Acid Copper doesnt look right
[Kentucky]
50922. In Hard Chrome plating, how do
platinised titanium compare with lead anodes [India]
50923. Non-Cyanide Zinc Plating Problem
[India]
50924. Can E Polish Bath be used for
Electro Plating [New York]
50925. Suggestions for plating gold on 303
stainless steel without nickel or copper underplating
[Nevada]
50926. Need the surface treatment on
Inconell [Hong Kong]
50927. Surface treatment for SUS sink
[Hong Kong]
50928. Chemical etch needed for roughening
electroplated nickel surface [Illinois]
50929. Need pickling and pacification of ss
pipe in Minnesota [Wisconsin]
{1/13/09}
50930. Seeking Fluidized Bed Paint
Stripping [Iowa]
{1/15/09}
50931. Coating to make Titanium
non-conductive for handheld device in work environment [Rhode
Island]
50932. Magnesium determination in magnesium
chromate solution [UK]
50933. What type of Nitric Acid dissolves
silver? [Missouri]
50934. Scratch removal on refrigerator
doors [New Jersey]
{1/15/09}
50935. Ferretic Nitricarburizing
[Michigan]
50936. Alkaline zinc-nickel plating
[Malaysia]
50937. Hard gold plating solution
needed! [Malaysia]
50938. Low Frequency Pulsed Anodizing on
the Cheap? [New York]
50939. Need a used beta back scanner
[Arizona]
{1/15/09}
50940. Seeking plastisol coating of
d-rings [Ohio]
{1/15/09}
50941. Where can I get details of
sheradizing process and machinery [India]
{1/16/09}
50942. Changing chrome to oil rubbed
bronze [Colorado]
50943. Melonite vs Tennifer process for
golf club heads? Which is the best? [California]
50944. Touching up Bronze Plating on
Antique Clock [California]
50945. I have the "want to" to learn
chroming!!! [Texas]
50946. Restoring blackening on anodized 14k
ring [California]
50947. General question to every engineer
of power plant [India]
50948. I am looking for a new watchcase
plater [Washington]
{1/16/09}
50949. Tone of Brass vs. Nickel plating for
alto trombone? [Texas]
50950. Voltage for a copper plating science
project? [India]
50951. Anodizing process to match silver
matte [India]
50952. Metal Furniture Mfgr. Seeks
Decorative Brass Plater [Indiana]
{1/16/09}
50953. Safely cleaning chromium plated
copper [South Carolina]
50954. Seeking chrome dipping
[Virginia]
{1/16/09}
50955. Want consulting services on gun
blueing process [India]
{1/19/09}
50956. Seeking Used Plating Lines
[Michigan]
{1/19/09}
50957. Plating carbon steel with stainless
steel [Washington]
50958. Titanium Cladding Passivation in PX
Oxidation Reactors [Iran]
50959. Need chrome plating of multiple
aluminum window channels - for assembly and retail sale
[Louisiana]
{1/19/09}
50960. High Phos Nickel Electroplating
[California]
50961. How to identify mild steel in mixed
iron scrap [Nigeria]
50962. Want to strip trivalent chromate but
not the zinc plating [India]
50963. Getting Started in Anodizing
[Connecticut]
50964. Best way to work harden 316
stainless to make pen nibs [California]
50965. Refurbishing scratched formica
bedroom dresser [North Carolina]
50966. Removing latex paint from a wrought
iron circular stairway [Oregon]
50967. Welding silver wire jewelry
[Egypt]
50968. Stainless Steel is oxidizing due to
floor tile dust? [Indiana]
50969. Acidified thiourea silver polish
stained stainless steel sink [Ohio]
50970. How to stain teak table darker?
[Washington]
50971. Appearance of white rust on acid
zinc parts [England]
50972. Aluminum extrusions marred with
black spots by graphite runout beam [India]
50973. Best electrode coating for good
adhesion? [Iran]
50974. How was this brown/purple wash done
on Galvanized wrought iron fence? [California] ![]()
50975. Seeking high-temp adhesive for
sharpening-stone to metal [New York]
50976. Who can rechrome the front and back
bumpers of my Pontiac Chieftian 1951 Hardtop [Illinois]
{1/19/09}
50977. Need good price on anodizing and
passivation supplies [Canada]
{1/19/09}
50978. How to calculate hex chrome air
emissions from a tank [North Carolina]
50979. Chromic Acid Anodising Colour seems
off [England]
50980. ERW pipe for Sea Water Line
[Turkey]
50981. Jeweler wants black immersion
plating for gold and 316SST [Belgium]
50982. What is reddish-orange substance on
anodizing tank cathode? [Colorado]
50983. Where to get Transom wood [New
Jersey]
50984. Rhodium plated Yellow Gold!? They
cant do what I want! [Australia]
50985. When electroplating copper my finish
is rough and grainy [Texas]
50986. What would make Brass magnetic?
[New York]
50987. Standards or tests for How clean is
clean ? [UK]
50988. Translating "galvanically protected"
to Polish [Poland]
50989. What type of metal and finish for a
food storage container [California]
50990. What is the purpose of additive and
accelerator in zinc phosphating? [Malaysia]
50991. Electroplating steel clips as proof
of ownership [Africa]
50992. Plumbing wholesaler needs replating
of chrome into satin nickel [South Carolina]
{1/21/09}
50993. Selective matte tin plating
[Arizona]
50994. How to achieve Aqua Blue Patina?
[South Africa] ![]()
50995. Problem of silvering the hologram
master [Massachusetts]
50996. Stripping method for titanium carbon
nitride ? [India]
50997. Copper sulphate test over hard
chrome plated surface [India]
50998. How would I find my parents stolen
rings? [Texas]
50999. Sterling Silver Tableware Badly
Tarnished [Florida]