Archives of the finishing com Hotline

[Letters 43000 to 43999]

The finishing.com Hotline includes more than 40,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.

43000. Questions about science experiment results [Georgia]
43001. Need literature on nitriding of stainless steel [India]
43002. How to remove "orange peel" on the surface of nickel electroforming plate [South Korea]
43003. Which are better, 316 or 304 stainless steel pots? [Arizona]
43004. Philharmonic tubist finds 17-4 stainless valves stick [New York]
43005. Is nickel plating safe for oven racks? [India]
43006. Use of titanium as anode [India]
43007. Yellow orange shade after champagne H23 anodizing [Pakistan]
43008. How to get shiny finish on 304 after passivating in nitric acid [India]
43009. Stipple 002 vs VDI equivalent [Massachusetts]
43010. Electrolysis With Metal Toilet Tank Components [California]
43011. What are the effects of chlorides and fluorides on 316 Stainless Steel? [New York]
43012. Need Gold Plating Removed from Silver Bracelet [New York] {11/15/06}
43013. Need a galvanizing plant [India] {11/15/06}
43014. Recovering Zinc from Zinc Chloride for Science Project [North Carolina]
43015. How to mix paint [Nigeria]
43016. Why is anodised coating on aluminum porous [Pakistan]
43017. Hull Cell working [India]
43018. How to maintain a 5 S housekeeping in Lead acid battery manufacturing company? [India]
43019. Original cold rust blue for Imperial (WWI) Artillery Luger [Pennsylvania]
43020. Sterling Silver [New York]
43021. Polarity of Type I Anodize [Arizona]
43022. Polyester Powder Coating After Zinc Plating [California]
43023. Rust on powder coating [Singapore]
43024. Passivation-Hot Dipped Galvanizing [India]
43025. Small blisters on a new product only on the edge after annealing a nickel plated product [The Netherlands]
43026. Sulphuric acid electrolyte gets crystallized at heat exchanger [Turkey]
43027. Seeking anodizing (black) for an 1/8" H Channel [California] {11/16/06}
43028. Need chemicals for Blueish chromate finish [India] {11/16/06}
43029. Need chemical suppliers based in the CT area [Connecticut] {11/16/06}
43030. Need a used truck paint booth [Kentucky] {11/16/06}
43031. Bonding testing of paint [Bangladesh]
43032. How does US 10B wear on a building exterior? [Massachusetts]
43033. Auxillary Anodes in Cu and Ni [Pennsylvania]
43034. Digital Printing onto Anodized Aluminum [Missouri]
43035. Inconsistent black color tone and gloss level with type 2 class 2 [Vermont]
43036. RUST how do I retard it? [Virginia]
43037. Passivation of aluminum alloy [Libya]
43038. How to prevent immersion gold depositing on stainless steel [Minnesota]
43039. White rust [Slovenia]
43040. Pin stuck together during Dull SN plating (Barrel) [Singapore]
43041. Electroless Nickel [Arizona]
43042. Over coating Zinc in Galvanize Wire [California]
43043. Effects on surface friction forces between plastic and zinc coated surface [Turkey]
43044. Gold or gold leaf plating for babies first shoes [UK] {11/17/06}
43045. Need Chrome Plating of Aluminum Wheels in New England [Rhode Island] {11/17/06}
43046. Nano metal powder (carbon) supplier [India] {11/17/06}
43047. Need Type II Chromate Treatment for Cadmium Plating Line [Canada] {11/17/06}
43048. Black oxide/cold bluing liquid required [New Zealand] {11/17/06}
43049. Adhesion of aluminum on glass and adhesion of gold on aluminum [India]
43050. Nickel electrolyte aluminum contamination [India] 2nd Request
43051. DI water corrosion in steam sterilizer [Florida]
43052. Require formula for making cold bluing/black oxide liquid [New Zealand]
43053. Etching titanium to produce crystalline finish? [Maryland]
43054. About PVDF paint for roofing [Philippines]
43055. Aluminum Casting Surface Finish [India]
43056. Measuring the hardness of the anodized layer [Iran]
43057. Need acid dipping of 1985 Monte Carlo ss frame [New York] {11/17/06}
43058. Need Chroming of a Car Part [Connecticut] {11/17/06}
43059. Corrosion prevention on mild steel [India]
43060. How to improve surface finish on a machined aluminum/steel part [Michigan]
43061. Advantages of PVD Coating over Electroplating [India]
43062. Buying chrome or stainless steel heated towel rails [New Zealand]
43063. Chrome-chromium spill [North Carolina]
43064. I want to purchase a plastic chroming system and want some feed back [Georgia]
43065. Using diluted muriatic acid in the home [Oklahoma]
43066. Replacement for MIL-STD-105E [Ohio]
43067. We need the specification and quotation for Shore hardness tester [India] {11/20/06}
43068. Copper-clad Aluminum Wire chemical formula and processing needed [Indonesia]
43069. Wear coefficient values for various materials [India]
43070. Why does my titanium anodizing dull when touched? [China]
43071. Old metal [South Dakota]
43072. Copper pipe to rest on brick or a rock for support in the dirt [California]
43073. Vacuum Vapor Deposition of Lime Glass [Illinois]
43074. Resistance of Rhodium Plating [Denmark]
43075. Addition of Cadmium metal in Cadmium Plating Bath [Pakistan]
43076. Anodizing different alum. types-causes changes in finish [Texas]
43077. Carbide polishing [Canada]
43078. Need aluminum mirror reflective sheet for solar oven panels [Paraguay] {11/21/06}
43079. Need Dacromet provider [India] {11/21/06}
43080. Need chrome plating of new aluminum grille [Washington] {11/21/06}
43081. Seeking new NADCAP-approved metal finishing suppliers [California] {11/21/06}
43082. Need electrodeposition of lacquer for silver [India] {11/21/06}
43083. We Need 100A Remote Rectifiers [Washington] {11/21/06}
43084. Need to set up a barrel plating plant [India] {11/21/06}
43085. Need chroming shop for wheels [Pennsylvania] {11/22/06}
43086. What makes chrome or chrome-plated material difficult to paint? [Australia]
43089. Threshold for Hexavalent cross contamination on Trivalent parts [Kentucky]
43090. TDS Problem in RO plant [Pakistan]
43091. Can the salt solution be recycled after being collected from salt chamber? [India]
43092. Need non-conductive spray paint [New York]
43093. Nitriding 1144 steel shafts [Tennessee]
43094. Comparison betwen galvanizing and powder coating [UAE]
43095. Electroless Nickel plating Versus Nickel Electroplating - Corrosion and Wear Resistance [Minnesota]
43096. Silver plating solution [Philippines]
43097. Sealing of oxide film formed on anodizing [India]
43098. What Passivation Process is recommended for 3156 SS [North Carolina]
43100. Passes after flaming on all ink levels 30 to 56Nm [South Africa]
43101. Need chrome replating of shotgun parts [UK] {11/22/06}
43102. Black oxide in stainless steel [South Carolina] {11/22/06}
43103. Seeking Black Chrome plating on 11L17 steel [Illinois] {11/22/06}
43106. Gold Plating problem [India]
43107. Muriatic acid streaks on versa-loc wall [Pennsylvania]
43108. Brown colour antique mirror [Kuwait]
43109. What is difference between 18/10 and 9 ply surgical stainless steel [Georgia]
43110. Copper Sulphate Test or salt spray test on AISI 416 steel ? [Malaysia]
43111. Need Radar Paint [New York]
43112. Hot Dip Galvanising [India]
43113. HARD CHROME PLATING VAT [India]
43114. Problems with black chrome bath [Colombia]
43115. Durable Chem-Film Coating [California]
43116. Organic Pretreatment with Zero Waste Generation [Philippines]
43117. Passivation Problem on Surgical Instruments [Pakistan]
43118. Trying to get a good surface rms finish on the o.d. on a 3 1/4" 6061 aluminum round [Indiana]
43119. Metal resistancy to 5% ferric chloride solution [Illinois]
43120. Anodized titanium vs. aluminium honeycomb core - corrosion problem [Malaysia]
43121. Need Vendor for Olive Drab Chromate Process [Pennsylvania] {11/24/06}
43122. INSTALLATION AND COMISSIONING NEW PROJECT ON HOT DIP GALVANIZE [India] {11/24/06}
43123. Need small E-coat set up [New York] {11/24/06}
43124. CHROME PLATED ENGAGEMENT RING - TOXIC? [Ohio]
43125. Is Viking-era arsenical bronze safe to wear? [England]
43126. Black Chrome [Colorado]
43128. How to remove PFOS mist suppressant for chromic acid plating bath ? [Belgium]
43129. Can I shorten test time for salt spray [India]
43130. Painting plastic ties [Mexico]
43131. EN/PTFE for temperature sensor? [The Netherlands]
43132. Nickel plating turning dull in few months [India]
43133. No Rinse Chromate Conversion [Wisconsin]
43134. Zinc Phosphate pretreatament [Mexico]
43135. Stainless Steel Coating [India]
43136. I WANT VITREOUS ENAMEL COATING ON CI CASTINGS [India] {11/27/06}
43137. Need stripping of electroless nickel from gun parts for refinishing [Pennsylvania] {11/27/06}
43138. Need bronze yacht hardware replated [Connecticut] {11/27/06}
43139. Pressed tin for meat safe [Australia] {11/27/06}
43140. Ray cook steel and old black oxide refurbished [Texas] {11/27/06}
43141. Need Hard Anodizing in Olive Drab and Dark Tan (Flat Dark Earth) [Utah] {11/27/06}
43142. Where can we directly buy chemicals for anodising [Philippines] {11/28/06}
43143. Need a silver testing machine [India] {11/28/06}
43144. I.R. reflective pigments - Cool coatings [Australia]
43145. Removing gold plating from electric guitar parts [Scotland]
43146. Platinum refining [Maryland]
43147. Remove protective paper from Plexiglass [Illinois]
43148. HOW DO I REFINISH PORCELAIN SINKS [South Carolina]
43149. New copper pipes degrading in historic home. Water unsafe to drink! [Pennsylvania]
43150. PAINT OR COATING WHICH CAN KILL MOLD BUT HAS ZINC OXIDE 1-5 PERCENT [Canada]
43151. Chrome Dipping, bike parts, bumpers rollbars etc [South Africa]
43152. Electromagnetic Radiation from a Rectifier [Australia]
43153. Stripping Chrome from Plastic Car Parts [Canada]
43154. Bright dip vs. pickling of brass [Illinois]
43155. Paint peel off from alloy wheels [India]
43156. Switching from hot dip galvanized [Egypt]
43157. Electroless nickel plating solution recycling [India]
43158. Silicon in electroplated zinc and yellow dichromate [Illinois]
43159. Best Trivalent Plating Thickness [Philippines]
43160. Anodize fading due to heat? [California]
43161. Chrome conversion coating to stop galling? [South Africa]
43162. Bright, Reflective Surface Treatment for Magnesium [California]
43163. Plating thickness [India]
43164. What is the possibility of cracking Aluminum Alloy Wheels When Chrome Plating? [California]
43165. Hexavalent Chromium prohibition [Illinois]
43166. Correcting the effects of caustic etch on polished aluminum [New York]
43167. Does deoxidizing in an iron base deoxidizer solution or a dilute nitric acid solution affect the bond quality provided by the P-2 etch? [California]
43168. Process for plating aluminum with copper to achieve very low interfacial resistance [California]
43169. Repairing mill finish on aluminum [Texas]
43170. Need protective finish applied to copper components [New Jersey] {11/30/06}
43171. Need silver /gold oxidised/anodized finish [India] {11/30/06}
43172. Brinell hardness test (HB) [Egypt]
43173. Cloudy cabinet lacquer [California]
43174. Effect of stainless steel fasteners on aluminum [Florida]
43175. Discarded process acid, Environmental and Economic problem [India]
43176. How do I Solve a Silver Tarnishing Problem?? [Hong Kong]
43177. Electrodeposition coatings as substitute for nickel [India]
43178. Difference between GI and EGI [India]
43179. Crystals forming in Sulfuric Anodize bath [New Jersey]
43180. Aluminum content in anodize solution [Michigan]
43181. What is the method for titanium electro-polishing? [Israel]
43182. Simple etching on carbon and alloy steels [India]
43183. Shot peening of titanium [California]
43184. Need the technology to colour Stainless Steel labels and articles [India] {12/1/06}
43185. Plating alternatives [Illinois]
43186. Does application of Touch-N-Prep bypass MIL-C-5541 salt spray test [Oklahoma]
43187. Magnesium machined part surface treatment [Arizona]
43188. Salt Spray Test on Stainless Steel SUS303 and SUS304 [Malaysia]
43189. Seeking capable company in Utah to manufacture stamp/tumble [Utah] {12/1/06}
43190. Need Poly Tank Saddles [Pennsylvania] {12/1/06}
43191. Silver nitrate's effect on chrome plating [Maryland]
43192. Chrome plating needed on set of stock 17" ACURA wheels [New Jersey] {12/4/06}
43193. Need CBX gold stripping powder [Alabama] {12/1/06}
43194. Requirement of rust preventive oil [India] {12/1/06}
43195. Formula for fresh and salt water? [Colorado]
43196. Nickel plating problem from nickel alto plate [Nigeria]
43197. Discoloration on nickel plated surface [Malaysia]
43198. Type III Anodize conclusive analysis? [Oregon] {12/5/06}
43199. Need chrome wheel dipping [Florida] {12/5/06}
43200. Need a set of 22's rechromed or put in black chrome [Illinois] {12/5/06}
43201. Need the brass finish on an exterior door knob and plate replaced [Kentucky] {12/5/06}
43202. Seeking 18k gold-plating and rhodium-plating for jewellery [Singapore] {12/5/06}
43203. Seeking phosphater to coat a cylinder [Ohio] {12/5/06}
43204. Titanium coating of Al, SC or Cu [Oklahoma] {12/5/06}
43205. Seeking Bright Chrome Plater for Plastic Exterior Truck Grille [Michigan] {12/5/06}
43206. Want to purchase zinc paints [India] {12/5/06}
43207. Need used Vacuum Metallizing plant, and a lacquering line [India] {12/5/06}
43208. Need to buy a Bias buff making machine [India] {12/5/06}
43209. Black oxide (gun blueing) [Oklahoma]
43210. I can't keep a water jacket or storage tank in operation for more than a year [Utah]
43211. Advice on purifying silver nitrate / plating out silver [UK]
43212. What search term do I use to find out about "rebrassing" small decorative items? [California]
43213. Thermal Conductivity [New Jersey]
43214. Hexavalent Substitute [Illinois]
43215. Best way to avoid blackening of polished brass items in coastal areas [India]
43217. Is it possible to coat TiAlN on Nickel electroless plated surface? [China]
43218. Plating of steel to look like polished brass [California]
43219. Trivalent zinc and galvanic corrosion [Illinois]
43220. Aluminum Casting Surface Finish [Denmark]
43221. Need manganese phosphate coat, 4140 steel, 1" Dia. x 3" long 4140, Rc 26-33 [Maine] {12/5/06}
43222. Refurbishing chrome plating on a drum [Maryland]
43223. New Car Rust [New York]
43224. Chemistry question about chrome reduction [Michigan]
43225. Correlation between Neutral Salt Spray and Copper Accelerated Acetic Acid Salt Spray Test [India]
43226. White Rust When Does It Occur After Kynar Coating Is Applied [Florida]
43227. Electric Arc Spraying Compatibiltiy of Stainless Steel on Aluminum [Oklahoma]
43228. Structural alloy for bright dipping [Virginia]
43229. Black Anodizing of Steel to Match a Black Anodized Aluminum Casting [Texas]
43230. Alternative to sulfuric acid for anodizing aluminum [Maryland]
43231. Descaling Molybdenum [Michigan]
43232. Oiled Bronze Colour Stainless Steel [China] {12/6/06}
43233. Need Electroless Nickel Plating on Carbide [Ohio] {12/6/06}
43234. Need non-rack chrome plating for fasteners [California] {12/6/06}
43235. Need Zinc Plating/Galvanizing for steel platforms [New York] {12/6/06}
43236. Need tools and materials to polish graffiti off stainless elevators [New Mexico] {12/6/06}
43237. Need Ra Meter [India] {12/6/06}
43238. Find the copper content in the British penny [Scotland]
43239. Is pearl bright nickel same as satin nickel [Malaysia]
43240. Scale removal from Ro system [Pakistan]
43241. Neurtralizing hcl after metal is dipped [Iowa]
43242. What are the limits of galvanizing? [Oklahoma]
43243. AMS standard for PVD TiAlN? [Minnesota]
43244. Electroless nickel flaking on stainless steel surface [New Mexico]
43245. Optimal length of a plating cells in a continuous application [Illinois]
43246. Durability of Chromed Aluminum Parts [Illinois]
43247. Defect - blistering in sliver plating [Singapore]
43248. Two-step anodizing w/tin sulfate [Ohio]
43249. Require different thickness of silver plating on the same part [New York]
43250. Removal of Chrome From Stainless Steel Substrate [Texas]
43251. I need TiAlN coating machine [India] {12/8/06}
43252. How to differentiate in-situ between a galvanized steel by hot and cold method [Egypt]
43253. Cooling 30% HCl with a tank coil [Iran]
43254. Making aluminum corrode? [California]
43255. What problems do you get when anodising 2014 alloy (T651) and dyeing it black ? [UK]
43256. Cleaning tarnish from Chrome [Indiana]
43257. Vacuum metallizing and lacquering/top coating tequila bottle overcap [California]
43258. Nickel Electroless Plating >40um [Arizona]
43259. Plating of brazing material on copper strip [Korea]
43260. Roughness in Nickel Deposit [Pakistan]
43261. Need silver plated copper wire [Turkey] {12/8/06}
43262. Need anodised aluminium sheets [Australia] {12/8/06}
43263. Fine matte finish on aluminum [Ohio] {12/8/06}
43264. Removal of epoxy sealer from ceramic tile [California]
43265. Silver Removal [Canada]
43266. Case Hardening of Plate Body Armor [Oklahoma]
43267. Chrome replating for chairs [New York] {12/11/06}
43268. Seeking someone who will electroplate cypress needles and leaves [Mississippi] {12/11/06}
43269. Need Pt HTE plating on Ti Grade 2 - contact segment for electroplating [USA] {12/11/06}
43270. Need nickel sulphate [Iran] {12/11/06}
43271. Need Black Metal Dye [Virginia] {12/11/06}
43272. Need Aluminum Oxide Wood Flooring Finish [India] {12/11/06}
43273. The Tarniban Process [Florida]
43274. Powder coating on mdf or wood and its treatment chemicals [India]
43275. Paint brushed effect [Iran]
43276. Want info about about nickel color plating [Syria]
43277. Long Term Environmental Liability Concerns with Anodizing Shop Operation [Indiana]
43278. To maintain acid ratio in zinc calcium phosphate [India]
43279. Using aluminum for a solvent filled parts cleaning station [Washington]
43280. Brown spots on stainless steel tank [Egypt]
43281. Hot Dip Tin Flux [South Dakota]
43282. Clear coating a new gas tank [Illinois]
43283. Electrodes best suited to split water [Florida]
43284. Re-gaining rhodium [Turkey]
43285. Why do metals corrode? [Florida]
43286. How do you take the finish off an old engraved silver trumpet? [California]
43287. Wall stain from hinge [Florida]
43288. Reaction between water and base [Malta]
43289. Dulling application for hot dip galvanization [Turkey]
43290. Cleaning fingerprints off of copper sheeting [New Mexico]
43291. Need anodized aluminum foil [Korea] {12/13/06}
43292. Need Mil-C-5541 and Mil-A-8625 on Beryllium-Aluminum Castings [USA] {12/13/06}
43293. Corrosion SUS 303 versus SUS 400 series [Malaysia]
43294. Titanium etching without HF [Spain]
43295. Zinc Electrowinning [India]
43296. How can I gold plate my copper lures for fishing [Australia]
43297. Magnesium painting options [Michigan]
43298. PVD applied to Trivalent Chrome [New York]
43299. Bright Zinc Plate Per ES1-02-01 [Georgia]
43300. Supplementary coating on Zinc Blue passivation [India]
43301. Blue anodize appearance for different material [Taiwan]
43302. Buffing in Southern California/Orange County [California]
43303. 5 year outdoor corrosion protection for a variety of mild steel and aluminium parts [UK]
43304. LOGOTYPE PRINTED ON STAINLESS STEEL - RESISTANCE [France]
43305. Looking for Moly-phos coating or equivalents [India] {12/14/06}
43306. Cataphoretic coating [India] {12/14/06}
43307. Need TYPE 3 Gold Finish on 21" x 24" PCBs. No Type 1 or 2 Gold [California] {12/14/06}
43308. Need chemicals for chemical polishing of high carbon steel fishhook [Hong Kong] {12/14/06}
43309. COST OF SILVER [Georgia]
43310. Dusty plating of gold onto anode during electro-winning [Australia]
43311. What finish to iridescently color steel art cut with a water jet [Kentucky]
43312. Powder coating wood [Michigan]
43313. Difference between E-coating and Cataphoretic coating [Illinois]
43314. New developments in Autophoretic and Eletrophoretic Coatings [India]
43315. Blisters after zinc plating [Poland]
43316. Gold Plating a handle in a coffee spoon [China]
43317. Stainless steel sculpture electro-polishing [Canada]
43318. Need RIL-Primer P23V40-44 [New Hampshire] {12/15/06}
43319. Trouble in plating a penny with nickel by using a cupronickel alloy [North Carolina]
43320. Tenifer Rifle Barrels [Rhode Island]
43321. Silver wastewater treatment [Washington DC]
43322. Black patches on casting after passivating with trivalent yellow [India]
43323. Tin Lead ST failure [Philippines]
43324. Busbar production procedure [Iraq]
43325. Recommended Stainless Steel Alloy for Electrode Hooks [Georgia]
43326. Client wants hot-dipping but part won't take the heat [Singapore]
43327. Rh plating on internal Pt-coated surface [Ohio]
43328. Plating on zinc products [India]
43329. Lapping of grinded parts [India]
43330. Nails in salt water or nails in tap water [New York]
43331. Can anodizing coatings be made flexible enough to bend without cracking? [Canada]
43332. PHOSPHATING SLUDGE MODIFIER [India]
43334. How to make nickel sulfate for plating [UK]
43335. Repairing Oil Lamp Canisters [Maine]
43336. Paint will peel off galvanized steam vessel [Maine]
43337. Protective N 8 finish [India]
43338. Stripping silver plating from Inconel 718 studs [Florida]
43339. Bare spots on hot tin dip product [Massachusetts]
43340. Electroless Copper [India]
43341. Electroplating cupronickel [Virginia]
43342. Solder Lump build up on tin lead plated terminal [Malaysia]
43343. Finger marks on anodized surface [India]
43345. CORROSION RESISTANCE CHART FOR HASTELLOY [India]
43346. Need decorative plating on abs plastics [Pennsylvania] {12/19/06}
43347. Need Anodize Services [Israel] {12/19/06}
43348. Need Nitric Acid Heating System [India] {12/19/06}
43349. Hydrofluoric Acid Resistant Paint [India] {12/19/06}
43350. Need second hand PVD TIALN coating machine [India] {12/19/06}
43351. SILVER TESTING STRIP [India] {12/19/06}
43352. NEED TO BORROW OR RENT COMMMERCIAL GRADE OZONE AIR CLEANER IN SAN FRANCISCO BAY AREA [California] {12/19/06}
43353. Need a micro plating machine for imitation jewellery products [India] {12/19/06}
43354. Seeking Finishing Consultant [Pennsylvania] {12/19/06}
43355. Need hard chrome catalyst (proprietary additive) [India] {12/19/06}
43356. Need Filter for Hard Chrome Plating [China] {12/19/06}
43357. Dog urine on dark antique finish [Minnesota]
43358. Removing very old paint from copper wall vents [Indiana]
43359. How to paint plastic statues to stay translucent [South Carolina]
43360. How was the plating for old music vinyl records made? [Mexico]
43361. How to strip the silver and brass and how to make a electrocleaner [Philippines]
43362. Avoiding Hydrogen Embrittlement [India]
43363. POWDER COATING ON ZINC COMPONENT [India]
43364. Cryogenic treatment [India]
43365. Hot dip galvanizing flux [India]
43366. Hard chrome plating s g cast iron [India]
43367. Nickel plating pretreatment [Hong Kong]
43368. Zinc plating thickness [India]
43369. CHROME PLATING OF MAG WHEELS [South Africa]
43370. Test for cadmium plating and alternate for Cd plating [India]
43371. Copper finish on aluminium [India]
43372. How do I clean and remove oxidation from the metal trim around my commercial windows [North Carolina]
43373. RUST PREVENTIVE COATING ON TRAIN RAILS [India]
43374. Corrosion of Gold, Frankincense and Myrrh [UK]
43375. Need oil rub bronze on copper tube [Alabama] {12/20/06}
43376. Need shoe bronzing [Georgia] {12/20/06}
43377. Need Chrome/Black Chrome plating Mini bike parts Kansas [Missouri] {12/20/06}
43378. Want to have motorcycle frame nickel plated [Virginia] {12/20/06}
43379. Looking for Wood's Nickel strike and Nickel-Chrome plating on stainless [Ohio] {12/20/06}
43380. Continuous selective reel to reel [Central America] {12/20/06}
43381. Want to set up small hard chroming shop [Nigeria] {12/20/06}
43382. Need flute gold or brass plated [Washington] {12/21/06}
43383. Can't prepare cross section for verifying plating thickness [Colorado]
43384. Preparation of cobalt(ll)thiocyanate [India]
43385. Anodize IAW ASTM B580 Inspection for defects under 500-600X magnification [Massachusetts]
43386. Chrome on plastic/spray on chrome process [Puerto Rico]
43387. Conductive Paint [California]
43388. Electroless Nickel over Copper Whitewash [Minnesota]
43389. Peel off in between bright nickel and semi bright nickel layer [India]
43390. Look of diffused nickel cadmium plate [Serbia]
43391. Where is all the NaOH going? [Connecticut]
43392. Anodized Aluminum Sheets [New York]
43393. Black Cadmium Plating [Florida]
43394. Colour variation in anodized part [Saudi Arabia]
43395. Iron Test for Passivation Bath [Georgia]
43396. Phosphating process [India]
43397. Seeking Zinc Phosphate to meet DOD-P-16232, Type Z, Class 2 [Connecticut] {12/21/06}
43398. We want to rep your nickel iron plating process [China] {12/21/06}
43399. I need photoresist [Egypt] {12/21/06}
43400. DRYING TIME [India]
43401. Recovery of Silver From Electroplating Dragouts [India]
43402. Remove Nikasil Plating [Thailand]
43403. AnSn bonding issue [California]
43405. Pulse form for Nickel Cobalt electroforming [The Netherlands]
43406. Hard Chrome additive [India]
43407. Anodising problems [India]
43408. Need ELECTROPLATING of FRESH ROSES [New York] {12/22/06}
43409. Anode consumption too high [Pakistan]
43410. Tinned Copper Drawing [Egypt]
43411. Over spray problem on auto finish [Tennessee]
43412. Ion Plating [Denmark]
43413. Powder Coating with Primers [Indiana]
43414. Hot DI Seal after Sulfuric Anodize [Arkansas]
43415. Cloth than can hold temperature over 100C and allow high temperature contact with metal [Connecticut]
43416. LOOKING FOR PLASTIC COATING TRAINING / UNIVERSITY [Indonesia]
43417. I need NAS 4006 coating on parts [Ohio] {12/27/06}
43418. 22 inch rim rechroming [New York] {12/27/06}
43419. NEED DEVICE FOR ATOMIZER TEST ACCORDING ASTM F21 [New York] {12/27/06}
43420. SURFACE POROSITY OF NICKEL PLATED TUBES [Iraq] (December 28)
43421. What's the best way to preserve and prevent burning off of bluing on my muzzleloader? [Louisiana]
43422. Stainless steel [Oregon] (December 29)
43423. What type of plastics can be plated? [Japan] (December 26)
43424. Texture of steel [Washington]
43425. What is gold wash? is it plating? It is used on old sterling and is a very thin coating [California]
43426. Difference between using Phospher Bronz and ETP copper as moving contact in a switch [India]
43427. Color etching aluminum [UK]
43428. How to determine Ca++ from phosphate bath [India]
43429. Air bubbles problem [Germany]
43430. Black staining on PBCs vias after electroless nickel/immersion gold plating [Canada] (December 27)
43431. Excessive amount of sodiumcynide in rochelle copper bath [India] (December 29)
43432. Anodizing On Cast Aluminum (ADC 12 grade) [Malaysia] (December 29)
43433. Removal of scale and soot before phosphating without using acid [India]
43434. Vinyl or Brite Coatings for Wire Nails [India]
43435. Need cook top color changed [New York] {12/27/06}
43436. Chrome-like sputtering on aluminum alloy wheels [Singapore]
43437. Need a turn key rust preventative system for train rails [India] {12/27/06}
43438. How to avoid hydrogen embrittlement in plating spring steel? [India]
43439. How to heat HCl for pre-galvanizing pickling [Kuwait]
43440. Nitrates formation [India] (December 29)
43441. Platinium coating by electrochemical method on titanium substrate [India] (December 29)
43442. Need surfactants [India] {12/28/06}
43443. Immersion Tin [India] (December 27)
43444. Chrome plating patch mark can we avoid it? and in which way? [India] (December 28)
43445. 4340 steel material get peel off in Electroless Nickel Plating (plating thick - 25 microns) [India] (December 28)
43446. Formica sheets [California] {12/28/06}
43447. Sn/Pb (60/40)reflow with tin components [Malaysia]
43448. Alodine 12002 VS. 1132 [Florida] (December 29)
43449. Aluminium white rust [India] (December 29)
43450. Technical consultancy [India] {12/28/06}
43451. Alodine colors [California]
43452. Stainless steel sculpture for harsh climate [Canada] (December 29)
43453. Hard anodizing sealing process [India] (December 29)
43454. Hot tub problem [Michigan] (December 29)
43455. Pickling and degreasing of stainless steels [Ireland]
43456. Custom Powder Coating [Indiana] {12/28/06}
43457. Plastic silvering [India] (December 28)
43458. What prevents nails rusting? [Illinois]
43459. Anything new about anodizing of Zinc? [Connecticut]
43460. How do I get my Quicksilver working again, it seems to have stopped [Canada]
43461. REPLACEMENT TO PHOSPHTING IN POWDER COATING PROCESS [India]
43462. Rust in tin plating [India]
43463. Looking for equipment to zinc plate pipes and rods fast [Mexico] {12/29/06}
43464. My $16,000 engagement ring is turning my finger green "help" [Canada]
43465. I want to distress the FRONT of a mirror [Maine]
43466. SANDING ALUMINUM SHEETS [California]
43467. Bath Analysis - AMS 2486 [Massachusetts]
43468. Electroplated Nickel for Food and Drug Product Contact [Illinois]
43469. Where does the Rhodium go when it wears away? [West Virginia]
43470. Seeking electroplating of 72900 copper nickel (spinodal alloy) [Germany] {12/29/06}
43471. How to dissolve Teflon filter paper [Bangladesh]
43472. Preventing tarnishing of silver / natural substances [Arizona]
43473. Thickness control methods for dip-spin coatings [South Korea] (December 29)
43474. EN/PTFE for bearing cage [Israel]
43475. Chemical compositions of metal coatings [India] (December 29)
43476. Copperized Fiberglass Cloth? [Arizona] {12/29/06}
43477. Need E-coating [India] {12/29/06}
43479. Copper anodes inquiry [India] {12/29/06}
43480. Need Bulldog Adhesion Promoter [Canada] {12/29/06}
43481. Rusting [Mississippi]
43482. Electrodes polarity [Italy] (December 29)
43483. Main effects which determine the acetone rub resistance of electrophoretic lacquer [India] (December 29)
43484. Anodizing thickness [Hong Kong] (December 29)
43485. How to do oxlate coating for stainless steel cold forging? [India]
43486. Salt water on chrome rims [Florida] {1/3/07}
43487. Need shop to do Mil-C-5541 Chromate Conversion Coating [India] {1/3/07}
43488. Seeking magnesium refinishing [Illinois] {1/3/07}
43489. Electrocoating Waste Water Treatment [Iran] {1/3/07}
43490. Want to set up hot dip galvanizing plant [India] {1/3/07}
43491. Distributor wants to represent your electropolishing and passivation equipment and chemicals [Thailand] {1/3/07}
43492. How long did it take for the penny to dissolve? [Florida]
43493. "Rust-Look" Spray Paint? [England]
43494. How much or how strong sodium hydroxide [England]
43495. Aluminum Finishing Suggestions [Michigan]
43496. Corroded Aluminum Boat Windows [Connecticut]
43497. Refinishing brass plated coffee tables [New Jersey]
43498. How to dull a chrome finish [California]
43499. I need an oven enamel repair kit [Texas]
43500. Problems in Electrowinning of Ni [Singapore]
43501. Any chemical solution for increasing bonding strength in THERMAL SPRAYING [India]
43502. Nickel free plated jewelry [Sri Lanka]
43503. Castings - black anodise, not grey [UK]
43504. What kind of passivation of 440c is true? [Iran]
43505. Post cleaning of Co-Cr alloy type L605 [Italy]
43506. Phosphating [India]
43507. Powder coat adhesion [New York]
43508. Help with re-paint on motors with metal housing in TN area [Texas] {1/5/07}
43509. Stainless steel flatware decorative black coating refurbished [Ohio]
43510. Electroplating cast iron [Indiana]
43511. Seeking automated second-hand line for powder painting screws [Poland] {1/5/07}
43512. Need infrared powder coating oven [UAE] {1/5/07}
43513. Process for coloring on steel [India]
43514. Yellow chromate adhesion on zinc [Oregon]
43515. Agitation of pickling lines by using compressed air [Egypt]
43516. Checking method of silver plated ss strip [India]
43517. Conductivity drop with top coat over Zinc - Nickel Plating [India]
43518. 416SS and Brass, suggestions for a better Galvanic compatible pair? [Tennessee]
43519. Need my Penn Reels anodized [Maryland] {1/9/07}
43520. Need Zinc Nickel Alloy Plating Plant [India] {1/9/07}
43522. Chemistry question for ASTM B117 pH levels [Michigan]
43523. Difference between ASTM B117 and MIL-STD-202G (method 101E) [Louisiana]
43524. Aluminum casting chromated - need to strip and redo [New York]
43525. Metal temp [India]
43526. What's the weight of the thickness? [New Jersey]
43527. Plating Bubbles [India]
43528. Chroming differences between 304 and 400-series Stainless Steel [Canada]
43529. Tin plating discolouration [India]
43530. AMS 2700 Method 1 Type II Passivation for Medical Device [Colorado]
43531. I need a coating for a reciprocating rod [Minnesota]
43532. Finishes [Indiana]
43533. Corrosion resistance for swimming pool components [Indiana]
43534. Bead wire adhesion [Turkey]
43535. Need list of Hex Chrome free platers [Michigan] {1/9/07}
43536. Full body paint stripping [California] {1/9/07}
43537. Scorched antique copper tea kettle [Washington, DC] {1/9/07}
43539. Nitric acid sales [UK] {1/9/07}
43540. Need a used salt fog testing equipment [Louisiana] {1/9/07}
43541. Metal coating [Jordan]
43542. Color chrome wheels [Florida]
43543. Refinishing chrome on 40 yr. old kitchen stool [Canada]
43544. BENDING SPRING STEEL [Connecticut]
43545. Zn plating ROHS compliance [India]
43546. What aluminum alloy should we use for anodizing/hardcoating load bars? [Rhode Island]
43547. I need some advice on a new start-up of a Electropolish shop and have some thoughts from viewing another shop. [Oregon]
43548. Washing and drying [India]
43549. Etch pure Al-SiCp composites [India]
43550. ALUMINUM ETCH [Indiana]
43551. Achieving dull and blackish surface finish in hot dip galvanizing [India]
43552. Gold plating tungsten powder [Montana]
43553. Effect on adhesion from various heat treatments to electrolytic nickel over 400 series stainless [Pennsylvania]
43554. Anodize in Wet Sulfur Dioxide Environment [New York]
43555. Passivation on aluminum castings [India]
43556. STRIPPING HARD ANODISED PARTS WITH MINIMUM COMPONENT METAL LOSS [Australia]
43557. Alternative to Pickling with HydroFluoric Acid [Trinidad and Tobago]
43558. Polished Brass Plaques [New York]
43559. HI TEMPERATURE ANTI-GALLING COATING [Florida]
43560. Need Iridium Coating of Windscreens, etc. [Minnesota] {1/12/07}
43561. Need my body moulding redone (manual polish, electro polish, bright dip and anodized) [California] {1/12/07}
43562. Need shop to finish 1,000 spring steel clips [Massachusetts] {1/12/07}
43563. Need real-time current density meter [North Carolina] {1/12/07}
43564. Need Aluminum Extrusion Polishing Machine [U.A.E.] {1/12/07}
43565. Painting a DOS coated steel sheet [Venezuela]
43566. Rinsewater disposal in chem-film operation [Georgia]
43567. Powdercoat and achieve 1000 hrs salt spray with little or no pre treatment [Ireland]
43568. What is the type of treatment recommended for electro-galvanizing surface before powder coating? [UAE]
43569. Electrolytic Tinning Process of Copper Wires [India]
43570. Availability of zinc whisker contaminated floor tiles [Illinois]
43571. Control of Ni electroplting bath with additive [Korea]
43572. Alochromed in MIL-C-5541D Class 1A [Singapore]
43573. Need Source for Conductive Rope [Missouri]
43574. Need a finishing shop in Delhi [India] {1/12/07}
43575. Refinish a 25 year old solid brass coffee table to its original luster [New Jersey] {1/12/07}
43576. Need replating of 1950's chairs [New York] {1/12/07}
43577. Need chrome plating of six small six inch high rail stanchions [Georgia] {1/12/07}
43578. Electroplating Zinc onto copper for Gr12 Chemistry Project [Canada]
43579. Solution for electronic waste [India]
43580. Exterior metal surface painting [Indiana]
43581. I'm drowning in grinding dust...help! [Massachusetts]
43582. Reverse electroplating problem [Canada]
43583. Cleaning nickel lined cooking pots [New York]
43584. Using Cold Black oxide and Stripping Black oxide [Illinois]
43585. I'm in search of zinc ceiling panels [California]
43586. Anodizing a barrel [Washington]
43587. I am a girl who needs to give her car some tlc [UK]
43588. E-coating vs galvanized prior to powder coat [Michigan]
43589. Hexavalent conversion to Trivalent Chromium [Georgia]
43590. What is a superior process, galvanizing or e-coating? [New York]
43592. Porosity and corrosion of bright nickel plated components [India]
43593. Our problem is skip plating in nickel [Iran]
43594. Corrosion in centrifugally casted and machined CF8M Seat rings [India]
43595. Where can I dip my rims [California] {1/17/07}
43596. Need pink powder coating of aluminum chairs [Ireland] {1/17/07}
43597. Need copper and nickel plating on nylon [Massachusetts] {1/17/07}
43598. Need MIL-C-83286 Painting service [Florida] {1/17/07}
43599. Need ion exchange resin [Romania] {1/17/07}
43600. Need PVC / PP / HDPE Mist eliminators for Air supply units [India] {1/17/07}
43601. Want an anodizing plant [India] {1/17/07}
43602. Need special Aluminum Alloy test panels [New Mexico] {1/17/07}
43603. Seeking Frit enamels [North Carolina] {1/17/07}
43604. Need wood PU coating plant/ technology [India] {1/17/07}
43605. Need Source for Anti-Tarnish Polymer [Brazil] {1/17/07}
43606. Do coins rust faster in salt water or fresh water [New York]
43607. Low-down on polymer anti-tarnish [Brazil]
43608. Rust removal [Tennessee]
43609. Birthday present for the wife [South Carolina]
43610. Oil rubbed bronze clawfoot tub feet [New York]
43611. Chrome alloy vs. chrome steel [Alabama]
43612. Can Lime Away clean rust stains in my washing machine? [New York]
43613. Getting started [South Africa]
43614. Shelf life of hexavalent chromate vs. trivalent [Texas]
43615. Waste solid residuals from zinc and chromium plating [Colombia]
43616. Bonding galvanized wire [Florida]
43617. Absorptivity values for various color paints [Turkey]
43618. Suitability for Zn-12% Ni plating + Electric Deposit Paint [China]
43619. Where do these fish eyes come from? [Illinois]
43620. Woodgrain effect powder coating [Scotland]
43621. Powder coat and silicone or PVC Plastisol adhesive [Indiana]
43622. Is galvanized iron need to be paint? What paint? [Qatar]
43623. Peroxin test used in electroless nickel plating [India]
43624. Nickel or Other Plating on Copper + Stainless Steel for Service at 600 C [Colorado]
43625. Color of Tin Solution [Arizona]
43626. Want brass plating that looks like gold [India]
43627. Specifying Satin Chrome Decorative Finishes [Nevada]
43628. Adherence test for chromium plating [Colombia]
43629. Direct plating of nickel onto stainless steel [California]
43630. Storage conditions for anodized aluminum [Iran]
43631. Galvanic potential of chromate conversion coating on aluminum in contact with gold [Texas]
43632. Clear Anodizing Thickness [Singapore]
43633. Anodizing aluminium + copper look temperature influences [Belgium]
43634. Green hue on black anodize [New Zealand]
43635. Cracks on the parts which are anodized
43636. To clean austenitic stainless steel tanks by acid pickling and passivation [India]
43637. Very high temperature resistant coating [Iran]
43638. Scratch proof coating for DVD spindles [UAE]
43639. Plastisol coating in Europe [Latvia] {1/18/07}
43640. Chrome Plating aluminum motorcycle parts [New Hampshire] {1/18/07}
43641. Seeking a plating shop who will work my way [Pennsylvania] {1/18/07}
43642. Looking to buy small electric chain hoists [Pennsylvania] {1/18/07}
43643. Touch up paint for Rohm & Haas powder coating [Missouri] {1/18/07}
43644. Need a silver extract machine through x-ray fixture [India] {1/18/07}
43645. Ni-P coated test panels [New Jersey] {1/18/07}
43646. Need to purchase white and pink gold by the ounce [Canada] {1/18/07}
43647. How do you measure rust? [Pennsylvania]
43648. Using Hydrochloric Acid as a Plating Solution [California]
43650. Clear Coating for my Copper Top Bar [Canada]
43651. Gold plating a movie replica [Tennessee]
43652. Meaning in Symbol MFZn-1S-2 [Indonesia]
43653. Use of pulse rectifiers for acid cu and nickel plastic plating [India]
43654. Titanium Pickling Line Help Requested! [Connecticut]
43655. Effect of humidity on taber abrasion test of hard anodize [California]
43656. Black Galvanizing [Canada]
43657. EN Sol'n Turning Black [New York]
43658. Powder coating for aluminum die casting [Florida]
43659. Anodized Aluminum Particles [New Jersey]
43660. Two coats of phosphate? [Michigan]
43661. How to remove surface defects? [India]
43662. Food safety of phosphate coatings [Australia]
43663. Finishing tool steel for corrosion [Illinois]
43664. Looking for black nickel plating [Maine] {1/18/07}
43665. Need patina finish [California] {1/19/07}
43666. Can you gold plate over an existing chrome finish? [California]
43667. What is the voltage requirement for a electrocoagulator? [India]
43668. 2024-T4 AND 2024-T351 MATERIAL [South Dakota]
43669. Tin Alkaline Matte - Plating thickness Accuracy / Wire and Tie (Vs) Jig Plating [India]
43670. Electrical properties of zinc-cobalt plating [Washington]
43671. Remove the glove mark from the surface of anodized aluminum [Malaysia]
43672. HVOF coating contractors need urgently [Nepal] {1/23/07}
43673. Need sulfurizing processor [Virginia] {1/23/07}
43674. Need used zinc electroplating line [Turkey] {1/23/07}
43675. Need zinc ingots [India] {1/23/07}
43676. What happens when copper and amunia mix? [Washington]
43677. Chinese and Japanese conversion of SAE 4130 [Alabama]
43678. How to paint football facemask [Virginia]
43679. Bronze grave markers and copper sulfate degradation [Florida]
43680. Preparation of older aluminum surface for painting [Michigan]
43681. How to clean carved lacquered teak Chinese chest [California]
43682. Preparing a sharpening steel [Australia]
43683. Guidelines for Type I,II,III anodize and chem film [Arizona]
43684. How to dull a shiny nickel finish? [South Africa]
43685. HCI Muratic Acid [North Carolina]
43686. Is it safe to wear the wedding gold wedding band that the mercury turned silver? [Texas]
43687. Refinish Aluminum A/C control yoke [Massachusetts]
43688. What is dross made of and how is it removed [Oklahoma]
43689. Aluminum welding sickness [Canada]
43690. MIL-L-11195 or MIL-DTL-11195? Dipcoating [Mississippi]
43691. Soldering on High-phosphor electroless nickel plated aluminium housing [India]
43692. Is hard chrome plating suitable for leveller/straightener rolls handling hot rolled steel? [India]
43693. Nickel chrome plating on aluminium alloy wheel [India]
43694. White Spots in Zinc Phosphate type 1 Coating as per TT-C- 490E [Tennessee]
43695. Finishing of old titanium [India]
43696. Cleaning tellurium copper [South Dakota]
43697. Pretreatment of Tellur. copper before Silver Plating [Mexico]
43698. Need Epoxy Paint and Coating [India] {1/24/07}
43699. Staining stainless steel [Missouri]
43700. Electropolishing of NiTiAu [Belgium]
43701. Need Brown Architecturally Anodized Parts [Iowa] {1/24/07}
43702. Tool Carts [Ohio] {1/24/07}
43703. Plastic primer [UK]
43704. Frustrated aluminum boat owner needs help with paint problems [Canada]
43705. Removing green residue on copper pipes [England]
43706. Need powder coating on plastics [Canada] {1/24/07}
43707. Plating bumpers [Canada]
43709. Blacken one side of stainless, leaving the other shiny [UK]
43710. Copper Electroplated on Silicon Nitrides -- Viable? What is the story? [China]
43711. Pickling of pipes of hydraulic pipe line [India]
43712. Diffference between Nickel Strike plate and Typical Nickel plating [Michigan]
43713. Need gold plating for a large religious article [Arizona] {1/24/07}
43714. Seeking chrome plating in Barcelona [Spain] {1/24/07}
43715. Paint suppliers [Michigan] {1/24/07}
43716. How easily does decorative chrome surfaces scratch? [Kuwait]
43717. Change brushed nickel to brushed copper or rubbed bronze look? [Florida]
43718. Flatware pitting - production problem? [Canada]
43719. Home built nickel plating system and required items [Texas]
43720. On site disposal of pickling rinsewater [Louisiana]
43721. Restoring 1917 Bronze Plaques From Old Bridge [Tennessee]
43722. Match for polished stainless steel [UK]
43723. Reduce the LPC (Liquid Particle Count) [Singapore]
43724. Effect of alkaline chemical for degreasing the copper metal [Saudi Arabia]
43725. Sink restoration [Michigan] {1/24/07}
43726. Opc drum coating [Iran] {1/24/07}
43727. 7th grade science project on copper plating [New York]
43729. Melting 9k gold [Australia]
43730. Electolysis between stainless steel and steel [Australia]
43732. Gold plating solution by using potassium gold cyanide(68%) [Pakistan]
43733. Rust Problem on Tinned Piano Wire [New York]
43734. Life of mild steel after phosphating [India]
43735. Looking for stripping and nickel-chrome plating in China [Israel] {1/26/07}
43736. Wear Factor for CoCr Mo [South Africa]
43737. How to electroplate a brass trumpet mouthpiece with nickel [South Africa]
43738. What machine is used for chrome plating of plastic? [Brunei Darussalam]
43739. Plating Thickness and Corrosion Resistance Standard [India]
43740. Does platinized titanium anode make particles in nickel bath? [Thailand]
43741. Barrel copper plating [India]
43742. Trivalent Chromate Conversion Coating of Aluminum [Canada]
43743. Electropolishing of 304L SS [Arizona]
43744. Looking for a RoHS compliant, Boeing approved, Chem Film house [California] {1/26/07}
43745. Ion nitriding [Ohio]
43746. Brass industrial parts finishing [India]
43747. Need .25 Synthetic, Pyramid, Tumbling Media [New Hampshire] {1/26/07}
43748. Stripping rhodium from copper wire [Mexico]
43749. Large scale sculptor who needs a mirror finish on a budget [Illinois]
43750. Piping for small point of use DI water station [California]
43751. Immersion silver bath formulation [Malaysia]
43752. Seeking Plasma Spraying on AA7039 [India] {1/26/07}
43753. Seeking Reel/Reel - Vertical Copper Plating Line Services [California] {1/26/07}
43754. Brass faucets re-plated to chrome [Alabama] {1/26/07}
43755. Brabus Monoblock IV Wheels [Florida] {1/26/07}
43756. Need liquid zinc [New York] {1/26/07}
43757. What is best on abs plastic [India] {1/26/07}
43758. Require micro finishing and shining on stainless steel sheets [India] {1/26/07}
43759. Need Heat Treater who uses salt [Mexico] {1/26/07}
43760. Rim straightening machine [Trinidad] {1/26/07}
43761. Is it necessary to purify the plating solution for a small scale nickel electrodeposition process? [France]
43762. Need a deburring electrolyte for laser cut stainless steel thin shims [Oregon] {1/29/07}
43763. Zinc coating electropolishing [India]
43764. Electroplating Brass [Vietnam]
43765. Best Metal to be used as Anodes in Electrolytic Cells [Philippines]
43766. How long has rhodium plating been available? [Washington, DC]
43768. Changing brass finish to a bronzed finish [Virginia]
43770. Cleaning gold plated ceramic [Australia]
43771. Keeping yellow gold...yellow [Texas]
43772. Painting chrome rims [New York]
43774. Restoring Bleach Damage Silverware [California]
43775. Differentiate wet painting and powder coated [Malaysia]
43776. Silver Blistering Mechanism [Connecticut]
43777. WHITE SPOTTING ON BLACK ANODISING [England]
43778. Anodic Seal [Canada]
43779. CASS test vs. ASTM B117 [Philippines]
43780. Silver plating poor adhesion [France]
43781. Plastisol pans [Pennsylvania]
43783. File Cabnet Refinishing Services [Washington] {2/1/07}
43784. Acid Dipping in the Houston Area? [Texas] {2/1/07}
43785. Cost of turnkey plant for silver plating small dia. balls [India] {2/1/07}
43786. I would like to know about Pollution Control board authorized paint sludge recyclers [India] {2/1/07}
43787. Coating to seal ceramic mold [Ireland] {2/1/07}
43788. Rusting a magnet to show how the formation of rust decreases the magnets strength [North Carolina]
43789. Doubts regarding selection of a mandrel [India]
43790. Cubic printing [India]
43791. Nikasil coating [India]
43792. Looking for aluminum casting information [New York]
43793. How to remove chrome from a late stock Harley Davidson springer front end [Texas]
43794. Cadmium Plated Parts [California]
43796. How to start a new galvanising plant? [South Africa]
43797. Fluxes for Zinc Melting [India]
43798. Do I need to use Hard Chrome over E-Nickel when plating D2 Tool Steel? [Ohio]
43799. Clear Coating Raw Aluminum [Utah]
43800. Suitable bath for hard anodising [India]
43801. Alodine 1132 touch-N-Prep Approval For AMS 2473 or AMS474 [Japan]
43802. Hexavalent chomium process free on aluminium [France]
43803. Hex-chrome free alternatives to hard anodizing and Dichromate Seal [UK]
43804. Etching aluminum skin [UK]
43805. Problems masking titanium for type II anodizing [Michigan]
43806. Cleaning of substrate-oxide layer removal [India]
43807. Silicone oil as anti rust [India]
43808. Passivation procedure [Saudi Arabia]
43809. Chrome steel tank [Michigan] {1/31/07}
43810. Need bar stool rings (foot rings) starting w/10 - 12 more later round or square [Indiana] {1/31/07}
43812. Need 'PORCELAIN' Enamel COATING of motor cycle exhaust [Ohio] {1/31/07}
43813. Need mist eliminators [India] {1/31/07}
43814. Looking for equipment to plate motorcycle and snowmobile cylinders [Michigan] {1/31/07}
43815. Need a RAL Standard color chart [California] {1/31/07}
43816. Electroplating copper onto aluminum [Washington]
43817. How do I paint a battery? [Australia]
43818. What infrared lamps to use for powder coating [Saudi Arabia]
43819. Refrigerator refinishing [New York]
43820. Bath Control [Korea]
43821. Plating Rhodium out of a Sulfuric Acid and Hydrochloric Acid Solution [Texas]
43822. Baking of fasteners to relief hydrogen embrittlement [Singapore]
43823. Teflon coating of molds [Illinois]
43824. Powder coating 17-4 steel [Texas]
43825. When does a galvanising waste Zn recovery plant become financially feasible for a small/medium sized galvaniser? [New Zealand]
43826. Welding between dissimilar metals [Florida]
43827. Diminished Results From Salt Spray Tests [Virginia]
43828. What is the advantage of using lacquer coating on zinc plated jobs. What is the salt spray life. [India]
43829. PHOS COPPER ANODES [Mexico]
43830. Positive identification of part marking on anodized surfaces [Minnesota]
43831. Treating old Beechcraft "V-Tail" Bonanza magnesium Flaps bare metal before painting [Florida]
43833. COLORLESS COATING [India]
43834. Cadmium coated bolts / nuts vs. stainless steel bolts for seawater exposure [Florida]
43835. What is this Finish [Canada]
43836. CHROME BATH PROBLEMS [New York]
43837. Need plastic covers chrome plated [Texas] {2/2/07}
43838. SEEKING price to black chrome a 17in. polished AL. dish type wheel for my H-D [Missouri] {2/2/07}
43839. Looking for Chromic Acid Anodizing and Painting [India] {2/2/07}
43840. Paint ABS plastic with silver grey metallic color [Argentina] {2/2/07}
43841. Supplier for Koroseal flexible pvc tank lining material [Michigan] {2/2/07}
43842. Does anyone know how the 2 part epoxy holds up in weather? [Michigan]
43843. Problems plating 24 kt gold on car emblems [Texas]
43844. Nickel recovery by electroplating [Malaysia]
43845. PC power supply for anodizing [New Zealand]
43846. JIS Z 2371 V.S. ASTM B117 [Malaysia]
43847. TRIMITE Low Temperature Acrylic S85-equivalent [Canada]
43848. Black oxidizing on steel components [India]
43849. Wood's strike method [Oregon]
43850. Carbon Content of Cold Rolled Steel Affecting Plating? [Singapore]
43851. Making A New Bronze Plate Bath [Pennsylvania]
43852. Nickel plating cost calculation [India]
43853. Converting RA to UIN [Pennsylvania]
43854. Zinc die cast samples - barrel plating [India]
43855. Quality hardcoat anodizing [Wisconsin] {2/2/07}
43856. Anodizing BMW wheels [New York] {2/2/07}
43857. Need bronze plating in the southeast [Florida] {2/2/07}
43858. Need lathe rim straightening machine [Trinidad] {2/2/07}
43859. Selective etching of iron [Germany]
43860. Remove electroless Ni from gold [Australia]
43861. Removal of nickel finish w/o dipping [Georgia]
43862. AISI 1025 MSFB [Washington]
43863. Short circuit of electrodes of electrocleaner [Florida]
43864. Reducing nickel content in wastewater effluent [Malaysia]
43865. Graphite Coating on 17-4 SS [Wyoming]
43866. How to tell Hot Dip Galv vs. Electroplate [California]
43867. Is water break test also applicable to FR-4? [Philippines]
43868. Silkscreening and Anodizing an Aluminum Surface [Canada]
43869. Teflon coat [Philippines]
43870. We need source for Manganese Phosphating at Chennai [India] {2/6/07}
43871. Recoating of electric fry pan [North Carolina] {2/6/07}
43872. Need a Wet and Powdercoat Painter of Class "A" mag die castings [Minnesota] {2/6/07}
43873. Need consultant to setup an electropolishing plant [India] {2/6/07}
43874. Setting up x-ray film wash for silver [Malaysia] {2/6/07}
43875. Electroless through hole plating on pcb [Indonesia]
43876. High-Strength Electroformed Copper Parts [California]
43877. Making paint with copper [India]
43878. Electrofoming onto shells with silver or gold [England]
43879. Black finish for stainless steel [England]
43880. I WANT TO MAKE METAL YARD ART [Arizona]
43881. Copper plate cast iron bench ends using copper sulfate? [Canada]
43882. Vapor Hone Media [USA]
43883. Oil rubbed bronze flexibility [Florida]
43884. Black spot on zinc plated parts [India]
43885. To strip hardchrome plating from aluminum plate [India]
43886. Powder coating [Massachusetts]
43887. Black Oxide grey color on Sae J2340 High Strength Steel [Mexico]
43888. Hot-dip galvanizing plant - relatively small scale [Argentina]
43889. Dull finish [India]
43890. Poor adhesion appears in nickel from base metal [Philippines]
43891. Copper anode appearance [Virginia]
43892. Space Flight Gold Plating / Soldering [California]
43893. Cost of several aluminum plating [Massachusetts]
43894. Is there any product (e.g. soap) that can accelerate black spots on Zn Plated materials? [Brazil]
43895. How to Seal Chrome Plated Pipe Thread Plumbing Components at high pressures [Pennsylvania]
43896. Unexplainable Pitting of 6061 Aluminum Parts [Connecticut]
43897. Resist for etching with ferric chloride [Canada]
43898. Pickling of titanium [New York]
43899. Micro Etching Process for Identification [India]
43900. Need IVD Aluminum coater in the southeast [South Carolina] {2/6/07}
43901. Tin metal in tin electro refining [Canada]
43902. Rusting Stainless Steel [Nebraska]
43903. Bathroom fixtures [Iowa]
43904. Treatment for Silver Nitrate in wastewater [Washington]
43905. ABS plastic plating procedure [India]
43906. Duplex Nickel plus hard chrome plating thickness vs Duplex Nickel decorative chrome thickness [India]
43907. Need Steel Blasting and Prep [Ohio] {2/7/07}
43908. Metal finishing and treatment [Malaysia]
43909. Demineralisation water's impact on aluminium casting [India]
43910. Protective coating for MEA system [UAE]
43911. CAN 6061-T6 BE REPLACED WITH 6082-T6 CONSIDERING WEAR RESISTANCE [UAE]
43912. Restoring antique toy car [New York]
43913. Brass Chandelier [Ohio]
43914. Seeking supplier for passivation of springs and powder painting of springs. [Illinois] {2/7/07}
43915. Al grades for hard anodising for electrical resistance [UK]
43916. Bloody red color and a black spot [Philippines]
43917. Carbide removal from 300 series stainless steel [California]
43918. Need Manganese Phosphate Coating on Alloy Steel [Pennsylvania] {2/7/07}
43919. PVD Provider in India [Wisconsin] {2/7/07}
43920. Hazards of bathtub refinishing/resurfacing dust? [Washington]
43921. Want to remove mineral oil from sandblasted steel...help! [New York]
43922. Decor potassium cyanide gold plating solution [Florida]
43923. Copper + hydrogen chloride [Texas]
43924. Need Aluminum Vapor Deposit Per Mil-C-83488 [Florida] {2/9/07}
43925. Need Diamond Black or TC50 coating for cutting tools [Arizona] {2/9/07}
43926. Public artist needs help on Gazebo with Creative Shingling [Colorado]
43927. Powder Coating a very detailed piece - no coverage problem [Canada]
43928. Tin Plating, Missing Pages [Arizona]
43929. Seeking painters familiar with Mil specs and CARC in particular [Vermont] {2/9/07}
43930. Source for RILSAN COATING/PUCOATING for MS fabricated rollers [India] {2/9/07}
43931. Need olive drab conversion coat on zinc that is RoHS compliant [Minnesota] {2/9/07}
43932. Need hot dip tinning reel-to-reel machine [Korea] {2/9/07}
43933. Need gas nitriding equipment [Egypt] {2/9/07}
43934. What chemical could you dissolve in water to make a zinc coating stick to the iron? [England]
43935. Newbie on electroplating with acid copper [Saudi Arabia]
43936. Discoloration of copper and bronze brake pads [Oklahoma]
43937. Chemical to make aluminium dull quickly without long term damage? [UK]
43938. Aluminum Wheel Restoration [New Jersey]
43939. How to adjust the subsidence rate of salt spray [China]
43940. Gray scale formation is salt spray [India]
43941. Prepaint cleaning-heavy equipment [Canada]
43942. Regarding plating peel off [India]
43943. Dirty substrate causes poor adhesion? [Philippines]
43944. Post-Nickel Plating Cleaning/Rinsing (critical cleanliness!) [Utah]
43945. Plating magnesium [Illinois]
43946. Rusting of 303 stainless vs. 416 stainless [New York]
43947. Silica scale removal [New Zealand]
43948. Bright Dipping of Copper [Massachusetts]
43949. Sulfurizing Process = Lubricating cast iron? [Virginia]
43950. WHITE RUST ON ELECTROLESS NICKEL PLATED PARTS [California]
43951. I want addresses in India for re-coating of cookware [India] {2/9/07}
43952. Need non-porous Tantalum anodization [California] {2/9/07}
43953. Need selective blackening on Brass Parts [Minnesota] {2/9/07}
43954. Need Zinc (Gray) Phosphate [Alabama] {2/9/07}
43955. Uniform Tantalum Oxide on large area, thin Tanatalum foil [California]
43956. Silver ring turned black [North Carolina]
43957. Hard Chrome Replacement Technologies [UK]
43958. Bend Strips for Electroless Plating [New York]
43959. Applying Aeroglaze Z306 Flat Black Thermal Control Paint to Nickel Plated Aluminum [Texas]
43960. Blackening of stainless steel [China]
43961. Pimples on hot dip galvanizing [South Dakota]
43962. Brown Stains on E-less Ni/Au plating on Silicon Wafer [Philippines]
43963. What is the best pre-penetrant aluminum etch that will not destroy the substrate [New York]
43964. COMPATIBILITY OF 18-8 STAINLESS STEEL WITH 304 [New York]
43965. O-ring that wears through hard chrome? [Ohio]
43966. Source for zinc, cadmium and zinc-nickel plating [India] {2/13/07}
43967. Seeking anodizing of pair of valve covers [Georgia] {2/13/07}
43968. Need Chrome parts changed to Black Chrome [Indiana] {2/13/07}
43969. Need job shop for mechnical cadmium plater [New Jersey] {2/13/07}
43970. Need automotive paint booth [Alabama] {2/13/07}
43971. Diaphragm Valves with Ceramic Coating [Malaysia] {2/13/07}
43972. How do you replate a brass roman tub faucet? [Washington] {2/13/07}
43973. Seeking jobber for coating MIL PRF 23377....25,000 pcs [Ohio] {2/13/07}
43974. Autobody shop needs crossflow paint booth [Illinois] {2/13/07}
43975. Post dip wanted after clear electrophoretic lacquer [India] {2/13/07}
43976. Need powder coating removal bath system [New Zealand] {2/13/07}
43977. Need traveling temperature recorder [India] {2/13/07}
43978. Electroless Nickel [Iran]
43979. What solutions to use to Electropolish Co-Cr Alloy (L605) [California]
43980. Diffusion of platinum plating into metal substrate [Canada]
43981. Dietz number for magnesium make up of wheels [Pennsylvania]
43982. Detecting the presence of Nikasil (in any form) in SAE 10W30 oil [Pennsylvania]
43983. Platinum, Palladium or Rhodium? [North Carolina]
43984. Removing tar from copper flashing [North Carolina]
43985. Porting and Hot Tanking [Belize]
43986. Wheels/compounds [Ohio]
43987. Is Nickel Plating ROHS compliant? [Illinois]
43988. FRP Coating on a Painted Surface [India]
43989. Lowering chrome results in my effluent [New Jersey]
43990. Question about NaOH attack [Georgia]
43991. What purchases and/or training is needed to do black oxide in house? [Wisconsin]
43992. What is Blackodizing? [India]
43993. CVD / Stainless Steel problem [Tennessee]
43994. Coating porous Titanium sintered discs with Platinum - Techniques and Suppliers [Canada]
43995. Increasing zinc metal concentration in acid zinc solutions [UK]
43996. Gold plating defects [Massachusetts]
43997. Replacement for nickel plating over zinc (zamak) alloy [Colombia]
43998. Color fastness for anodized aluminum parts [California]
43999. Suitable bath for hard anodising [India]


The finishing.com Hotline has been on the Internet since '95 and includes more than 40,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.