Archives of the finishing com Hotline

[Letters 40000 to 40999]

The finishing.com Hotline includes more than 50,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.

 

40000. Reasons for Solderability Problem in Sip Socket (Berg Pins) [India]
40001. Improving adhesion of TGIC powder over hot dip galvanized steel [Arizona]
40002. Vacuum cadmium [Michigan]
40003. Electroless nickel over babbitt alloy [Brazil]
40004. Plating electroless nickel on gold coated wafer [South Korea]
40005. An uncomfortable smell from Bath's solution [Singapore]
40006. Silver plating Peels off copper [India]
40007. Seeking Plating Shop for Sculpture [England] {3/24/06}
40008. Need motorcycle parts rechromed, small parts [California] {3/24/06}
40009. Need quotations for a color coating line [Vietnam] {3/24/06}
40010. Need My Wheels Powder Coated [Florida] {3/24/06}
40011. Need Used "Countertop" Salt Spray Booth [Wisconsin] {3/24/06}
40012. Seeking Acid Zincate Process [Maryland] {3/24/06}
40013. School Electroplating Project Didn't Work [Iowa]
40014. How to get platinum coating on molybdenum metal [India]
40015. 3 to 5 year black ring and bleached water stain 24inch oak window sills [New York]
40016. How to precipitate gold from H202? [Virginia]
40017. The best way to paint an aluminum ultralite wheelchair [North Carolina]
40018. Kitchen sink color restoration [South Carolina]
40019. Chrome wheels are discoloring [California]
40020. How do I put an "oil rubbed" finish or blackened bronze finish on a beaten copper sink? [Alabama]
40021. Blue coloration on stainless steel when subjected to heat [India]
40022. Alocrom / Alodine 1200 ROHS compliance [UK]
40023. Can any deionizer remove or reduce the actual level of salt tds [Pakistan]
40024. Using Oxygen gas for Cyanide oxidation [Texas]
40025. Separation of zinc from steel mils sludge [Turkey]
40026. How do you verify the copper sulphate spot test of passivated steel? [Georgia]
40027. Fluoride determination in HF/Nitric titanium etches [UK]
40028. Difference between two plating notes for RoHS compliance [India]
40029. What chemical to use for Titanium Etch [Maryland]
40030. Will a high SO2 environment embrittle 316SS bolts? [Zambia]
40031. Above what tensile strength do screws require de-embrittlement? [UK]
40032. Pockmarks from Malcomizing [California]
40033. Replate Nickel over Nickel [Ohio]
40034. Pitting in 2024-T4 used in aerospace [Canada]
40035. Aluminum Etch Prep turning Aluminum Black [Indiana]
40036. Electrodeposition of organic phosphated metals [India]
40037. Seeking chrome and gold plating [Nigeria] {3/27/06}
40038. Need Liquid Primer for powder coating of electro galvanised sheets [UAE] {3/27/06}
40039. Purification of copper [Australia]
40040. pH of rust [Maryland]
40042. "MIL-C-5541 class 3" versus "MIL-a-8625 type III class 2" [Spain]
40043. Hot-corrosion related problem [India]
40044. I want to paint a polystyrene life buoy (currently white) red [South Carolina]
40045. Removing unwanted splashed tin coating from outside of antique copper tea kettle [Kansas]
40046. How can I paint my wood burning stove [Georgia]
40047. Need Advice on Refinishing Brass Lamp Outside my Front Door [Georgia]
40048. How to electroplate lead on printed circuit boards [India]
40049. Remove cement from ceramic tile [Florida]
40050. ABOUT STANDARD OF BS1706-FE-ZN5 [China]
40051. SPRAYING GOLD METALLICS [Oregon]
40052. Avoiding orange peel in clear coat [Oregon]
40053. Salt spray resistance for E D [India]
40054. Repolishing the black spot on titanium coated stainless steel sheets which is observed on time of welding [India]
40055. Brass plating on hinges [India]
40056. Zinc Iron Plating [India]
40057. Re-anodizing cast aluminum [Canada]
40058. Citric vs. Nitric passivation for titanium human implant [Massachusetts]
40059. Intergranular attack on Nimonic 105 alloy [Scotland]
40060. Interference of phosphating layer with press fit [India]
40061. Slag removal on sheet metal [North Carolina]
40062. 1045 Steel has become magnetic [Oklahoma]
40063. Scaling of heat treated screws made from boron steel material [India]
40064. Want rhodium plating on sterling silver jewelry [California] {3/28/06}
40065. Chrome plate ABS in Mexico [Michigan] {3/28/06}
40066. Double zinc coating before powder coating [Malaysia]
40067. Help with finishing of steel custom stairs [Texas]
40068. How to judge whether plating passes B117 12hours or 96hours? [China]
40069. ASTM spec for yellow chromate adhesion testing [Arizona]
40070. Pitting in bright silver anodizing [Australia]
40071. Coating Contributing to Fatigue Failure of 7075? [California]
40072. Having a problem plating pewter [Philippines]
40073. New startup needs plating equipment and supplies [Spain] {3/28/06}
40074. What reagent for examining grain boundaries of 7075 T6 [China]
40075. Plating Surgical Instruments [Kentucky] {3/28/06}
40076. Need automated chrome plating system [Thailand] {3/28/06}
40077. Knowledge of D M Plant [India]
40078. Chrome plating on plastic [Maryland] {3/29/06}
40079. Need 1963 Lincoln bumpers rechromed reworked [Georgia] {3/29/06}
40080. Need HDG Advisor [India] {3/29/06}
40081. Temperature rise reduction with Tellurium Copper [Connecticut]
40082. Underground copper water lines [Ohio]
40083. Galvanic Action to my aluminum boat [Colorado]
40084. How to glue pennies together? (Canadian cents) [Canada]
40085. Varying color of firearms "blue" by changing percentages of nitrates [Nevada]
40086. Cleaning filter coth in line with 2%HCL Solution [Texas]
40087. Teflon Coating Test Methods [China]
40088. Hydrogen Bakeout [Canada]
40089. Stainless Steel Pretreatment [Thailand]
40090. Thick Ni-P layer [Taiwan]
40091. Leveled rhodium for electronics industry [Oregon]
40093. Haze in Chrome LCD areas [Arizona]
40094. Gold plating peel off [India]
40095. Acid Chloride Zinc [Illinois]
40096. Nickel plating is flaking [Florida]
40097. Tri Chrome Coating For FE/ZN 12 [California]
40098. Spangle and shiny metal - Architectural anodising [New Zealand]
40099. Color inconsistency during hard anodizing of aluminum alloy 6063 component [India]
40100. Sealing Process for Hard Anodize MIL-A-8625 [Ohio]
40101. Minimal pretreatment tank to reduce pretreatment time before powder coating [India]
40102. Ferrous metal phosphating and passivating [Zimbabwe]
40103. Want to buy gold refining equipment [Thailand] {3/30/06}
40105. I would like to know about a cost or other related details for establishing a new plant for coating [Tanzania]
40106. TCE Disposal [Texas]
40107. RAL chart for Colour Specification [India]
40108. What the process steps for powder coating diecast aluminum? [California]
40109. CORROSION in a Marine Envrionment [California]
40110. Questionable Plating Practices Observed During Vendor Review [Arizona]
40111. Zinc Barrel Plating Current Density [Hong Kong]
40112. Need literature on anodising and electro-colouring on aluminum [India]
40113. Mil-C-5541 Class 3 and Class 1A [Iowa]
40114. Replacement to Mineral Spirits [India]
40115. Need my bumper replated [Georgia] {3/31/06}
40116. Startup needs chrome plating materials [Philippines] {3/31/06}
40117. Need copper relining for kitchen pots [New York] {3/31/06}
40118. Where can I get my rims redipped in chrome? [Michigan] {3/31/06}
40119. How to prepare anodizing film of aluminum alloy with electric particles? [China]
40120. Powder coating stainless steel sink [Maryland]
40121. Nonionic surfactant analysis using HPLC method and their separation [Sweden]
40122. Lab test to determine if steel panels are galvanized [Michigan]
40123. What pre-treatment for powder coating electroless nickel aluminum casting [South Africa]
40124. Detailed rhodium plating process [Indonesia]
40125. Electroforming mandrel question [Massachusetts]
40126. SS316 in waste heat recovery [Sri Lanka]
40127. Checking if article was actually hot dipped [Philippines]
40128. Sealer after powder coating [Pennsylvania]
40130. Browning Blacking Bluing of Brass [Sweden]
40131. Repainting galvanized garage doors? [Kentucky]
40132. Need flexible metallic coating for polyurethane resin [Canada] {3/31/06}
40133. Need Devilbiss XVA53C Paint Booth INSTALL DIRECTIONS [Maryland] {3/31/06}
40134. Etching a pattern in aluminum before anodizing [South Africa]
40135. What coating is required for brass water-service fittings? [Iran]
40136. Max. Hard Chome plating Thickness [India]
40137. Repairing crack or hole in rinse tank [Georgia]
40138. Dichromate -passivation of zinc plated medium carbon steel [Massachusetts]
40139. Rusty yellowish surface after pickling [Turkey]
40140. Need hard chroming done on a 1.5" square area [Pennsylvania] {3/31/06}
40141. Chemically removing copper sheet dents and scratches [Philippines]
40142. STANDARD NITRIC/FLUORIDRIC PICKLING/PASSIVATION OF AISI 430 [Italy]
40143. Etching nickel phosphorous [China]
40144. Looking for Anodized Aluminum Nameplate material in sheets [California] {3/31/06}
40145. Used/surplus buffs available? [Washington] {3/31/06}
40146. Need Powder Coating on set of wheels [Michigan] {4/5/06}
40147. Want custom lacquer finish on tuba [Washington] {4/5/06}
40148. Need Clear Polyester Finishing of Wood Dashboards [South Carolina] {4/5/06}
40149. Need aluminum brushing machine like Emmebi [Bangladesh] {4/5/06}
40150. COD in post treatment wastewater and pre treatment wastewater [Malaysia]
40151. How to do oxidation test for AZ91D [Malaysia]
40152. Molibdenium coating [Iran]
40153. Cyanide silver plating process and nickel sulfamate base plating process [India]
40154. How to rust nickel [Alabama]
40155. Temp. resistance of powder coated motorcycle parts [Canada]
40156. Finishing a bronze fountain [Florida]
40157. Lacquer for silver plate [Illinois]
40158. Why after greening operation on Xray tube of SS fails and coating not adhering properly [India]
40159. Need rust prevention chemical for recirculating water in art fountains [Vermont]
40160. Hexavalent chromium prohibition on USA cars? [Brazil]
40161. Anodizing vs. RoHS [California]
40162. Scrapping a rectifier, advice needed [Louisiana]
40163. Why are layers of pp balls used in dm water storage tanks? [India]
40164. How to strip and re-nickel-chrome parts [Georgia]
40165. Dishwasher resistance failure of organic coated glass tumblers [Turkey]
40166. Why are we doing alkaline zinc plating? [India]
40167. I AM IN DESPERATE NEED OF HELP WITH MY CHROME TANK [South Carolina]
40168. Uneven deposit in the bore [India]
40169. Tin plate Blistering [Australia]
40170. How to convert the color of GALVANIZED IRON to SILVER? [Philippines]
40171. Need a reliable decorative chroming system [Finland]
40172. Rust is coming out from bottom side of door stiffner in MS [India]
40173. Seeking qualified plating services supplier [China] {4/6/06}
40174. Need chrome plating of valve covers [Michigan] {4/6/06}
40175. Remove the anodizing from a grille to a 1964 Falcon [New Jersey] {4/6/06}
40176. Seeking Endurion Process Chemistry [Germany] {4/6/06}
40177. Need anode hooks made of nickel [Michigan] {4/6/06}
40178. Need fume control additive for chrome plating [California] {4/6/06}
40179. Single replacement lab w/ copper sulfate !!help!! [California]
40180. Capacity enhancement of a chilling plant [India]
40181. Can chromium be deposited by physical vapor deposition [Philippines]
40182. Can pregnant women safely work on Arsenic analysis? [Pennsylvania]
40183. Need help repairing ring with great sentimental value! [Ohio]
40184. Welding steel to a galvanized baffle. HELP [Texas]
40185. Discoloration of silver plated flatware following use of dishwasher detergent. Can it be removed? [Georgia]
40186. Trivalent chromate plating with black finish [Ohio]
40188. Coating other than lacquering copper and brass rolled products [India]
40189. Nickel-Cad diffusion bake time [Connecticut]
40190. Yellowish color on stainless steel [Singapore]
40191. Aqueous Cleaner or Non Flammable Solvent to Flush Fuel from Metal Box Prior to Soldering [California]
40192. STAINLESS FOUNTAIN has RUST formations. Please Advise [Arizona]
40193. WHITE GOLD TURNING YELLOW [Pennsylvania]
40194. Galvanized Tin Kitchen Countertops [Texas]
40195. NEED ROUND NICKEL ANODES 2 INCHES BY 36 INCHES [Wisconsin] {4/6/06}
40196. Need company to manufacture patented product [Florida] {4/5/06}
40197. Seeking pot metal refinisher for tail light housings for a '61 T-Bird [New Jersey] {4/5/06}
40198. Updating a 1956 Buick Special bumpers [North Carolina] {4/5/06}
40199. Used open face spray booths needed [California] {4/5/06}
40200. Need water transfer printing equipment [California] {4/5/06}
40201. Spontaneous Combustion [Washington]
40202. Why federal law requires all coins to bear the word Liberty [Florida]
40203. Selectively leaching Cu from Monel [Washington DC]
40204. Suppliers for tin/gold and tin/silver electroplating solutions [UK]
40205. Electro refining [UK]
40206. Copper functional test [Malaysia]
40207. Painting on Gear Box [India]
40208. Sand coatings? [Canada]
40209. Acid cu [Massachusetts]
40210. Can I plate tin directly to 304 stainless? [Ohio]
40211. Coatings for Aluminum Busbar [Colombia]
40212. Electroplating Rose [India]
40213. Brown stains on chem film [Washington]
40214. Color of oxalic anodizing after Hot DI seal [Singapore]
40215. Laser Engraving Polished Aluminum [California]
40216. Heat and acid resistant material having mechanical strength of mild steel [India]
40217. High conductivity/fingerprint resistant coating [California]
40218. How to increase life of Biometrics sensor housing [India]
40219. Need chroming of large stainless plates - 7X18 feet [Maine] {4/7/06}
40220. Need gold plating and chrome plating of SM 58 Microphone screens or grills [New Jersey] {4/7/06}
40221. Hard anodisation [India]
40222. Thinking of starting a E Coat Job shop? [Wisconsin]
40223. Electroless nickel plating of heat treated steel and steel hardness relationship [Virginia]
40224. Where can I get 304 stainless steel wool [New York]
40225. EXACT VOLTAGE BREADOWN (PER MIL) FOR HARD ANODIZE TYPE 3 [Israel]
40226. Galvanic action between stainless steel pin fixing to an aluminum window restictor [Ireland]
40228. Electroplating copper to glass [Arizona]
40229. Why machined part of MS bright material is difficult to Zn plate ? [India]
40230. Electropolishing - Looking for a company in Guangdong [China] {4/7/06}
40231. Seeking electropolishing on 6061-T6 parts [Minnesota or North Dakota] {4/7/06}
40232. Diamond like carbon coating [India]
40233. Phosphating on aluminum alloys [Pakistan]
40234. What is the best way to achieve a "Scotch-Bite" finish? [Missouri]
40235. Stripping of Plastic Painted Parts [India]
40236. Cost of plastic paint shop idle running condition [India]
40237. Stainless steel coloring without electrical power [Egypt]
40238. Composite hardchrome plating - Reg [India]
40239. Optimum conditions for elctroplate copper with copper pyrophosphate bath on steel substrates? [Italy]
40240. Tin Plate Bumping/Blistering in Lead Free Environment [North Carolina]
40241. Blistering of silver/nickel on machined aluminum [England]
40242. Chrome titanium coating house ornaments [Trinidad and Tobago]
40243. Plating both outside AND inside of a tube - Can it be done with zinc? [Minnesota]
40244. Chromic acid anodize can it be stripped and reworked without edging the aluminum [Florida]
40245. Need auto dipping services [California] {4/7/06}
40246. Want to buy PTFE coating material [England] {4/7/06}
40247. Need Used Nordson Powder Coat Gun [Utah] {4/7/06}
40248. Is it possible the corrosion rate of carbon steel which have weld seam higher than without weld seam? [Malaysia]
40249. Cleaning auto transmission [Louisiana]
40250. In new solution after doing 35 pcs my rhodium pieces started looking black [India]
40251. Trivalent Plating Chemistry [India]
40252. RoHS Compliance of clear and yellow Irridite aluminum finishes [New Jersey]
40253. Is zinc and clear coating RoHS compliant? [Illinois]
40254. Eloxated aluminum [California]
40255. What is Electro Galvanising [India]
40256. What is Altizizing? [Sweden]
40257. Automating Surface Tension Measurements [Pennsylvania]
40258. Measuring the gold thickness by gravematric method [UAE]
40259. Coloring Stainless Steel [Pennsylvania]
40260. Cleaning electroless nickel tank [South Korea]
40261. Process worker would like some info on the Scientific Definition for Chromic Anodising? [Wales]
40262. 32 finish on A36 Carbon Steel [Idaho]
40263. Looking for a scratch resistant aluminum finishing method for 6061 and 5052 [Wisconsin]
40264. Restriction in usage of Stainless Steel Piping in Closed Hot Water Heating System [Canada]
40265. Seeking electroforming/plating services of organic objects [Canada] {4/10/06}
40266. Need my 20 inch rims powder coated [New Jersey] {4/10/06}
40267. ALUMINUM BRIGHTENING SOLUTIONS OR ALUMINUM BRIGHTENERS [India] {4/10/06}
40268. Need a Black Lacquer Dye for 302 ST [Connecticut] {4/10/06}
40269. Need to plate through holes in PCB [California]
40270. Seeking a fabricator to assist in the molding and chrome appearance finish of plastic [New York] {4/11/06}
40271. Need Class "A" E-Coat and Powder Processor in SE or South Central USA [Michigan] {4/11/06}
40272. Need coating of Molybdenum foil in coils with nickel [Israel] {4/11/06}
40273. Reenamel old cast iron sink [North Carolina] {4/11/06}
40274. Need firearm Hard Chromed in Northern VA/WV [West Virginia] {4/11/06}
40275. Inquire about Water Transfer Printing [India] {4/11/06}
40276. Need Masking Tape for powder coating [India] {4/11/06}
40277. Need system for busbar plating [Colombia] {4/11/06}
40278. Acid Etching Aluminum [Australia]
40279. Need help with GM 4347M Specification [Mexico]
40280. Corrosion Test on Copper Cladding Cookware [Indonesia]
40281. Iron Content Test for Nitric Acid Passivation Baths [Michigan]
40282. Titanium surface prep for organic coating [Pennsylvania]
40283. Recycling of clinker of zinc pot [Egypt]
40284. BLACKENING OF STAINLESS STEEL [California]
40285. Flat Black Coating for Stainless Steel [Florida]
40286. Bleed out under copper and steel interface [Florida]
40287. Brass strip material corrodes and fractures after tin plating [North Carolina]
40288. Scratches and patches on cadmium plating [India]
40289. Industry standard for cosmetics on clear chromate, aluminum [Idaho]
40290. Gold alodine plating problem [Minnesota]
40291. How to use citric acid to clean a steam sterilizer [Australia]
40292. Satin finish on a metal surface? [Arizona]
40293. Zinc Ammonium Chloride Effects on Metals [Illinois]
40294. Troubles with trivalent chromium precipitation [Brazil]
40295. Mottled surface appearance of hard coated 6061 AL after repeated autoclave cycles [Florida]
40296. Chemical info on acid engraving [Georgia]
40297. Seeking Teflon Coating Service [Indonesia] {4/12/06}
40298. Want wall posters of Plating Specs [Arizona] {4/12/06}
40299. Galvanized contact poisoning? [Washington]
40300. Aluminum vs. Stainless Steel Piping for Aquaculture Saltwater Application [Ecuador]
40301. Electrolyte for Electropolishing Conductive Graphite [California]
40303. Bubbles in Finish from Water Left on Surface [North Carolina]
40305. Duration of accelerated weathering test [Malaysia]
40306. Rework chemical for sn-bi plated leadframe [Taiwan]
40307. A60 Galvanized versus electro-galvanized steel [California]
40308. Adhesive bonding to electroless nickel [Arizona]
40309. HOW TO AVOID CHROME SEALING AFTER PHOSPHATING TO AVOID POLLUTION [India]
40310. Want red anodized motorcycle wheels [Pennsylvania] {4/13/06}
40311. Ozonation sterilization of lake water [Colorado]
40312. Copper roof over the bay window [New Jersey]
40313. Artist wanting to iron plate on copper [Oregon]
40314. Can I cold weld over golf club engravings and then rechrome them? [Oklahoma]
40315. 1959 Ford Galaxy OS door handles needs pits removed and re-chromed [California]
40316. Titanium Nitride coating on stainless steel screws [Texas]
40317. Removing mild tarnish from nickel-plated brass [Wisconsin]
40318. RoHS Compliant Black Oxide? [Canada]
40319. Chrome plating on plastic - ESD problem [Hong Kong]
40320. Etching stainless steel [Hong Kong]
40321. Iron phosphate usage to aid powder coating adhesion [Indiana]
40322. Polishing Hot Rolled? [Missouri]
40323. White Spots on surface after Annealing and Pickling SS [India]
40324. Automated Silver Plating Plant needed [India] {4/13/06}
40325. Need Hard Chromium Additive [Brazil] {4/13/06}
40326. SandBlasting [Kentucky]
40327. Colorant for anodized magnesium [Indonesia]
40328. Strange etching by cup left in sink for two weeks [California]
40329. How to hold Nickel Crowns in a plating tank [New Hampshire]
40330. Marine Grade Alloy [UK]
40331. Removing Aluminum and Chrome Oxidation [Michigan]
40332. Ugly blue paint on brass bed [Ohio]
40333. Stripping powder coat [India]
40334. Galvanized painting pipes [Turkey]
40335. Protection of Stainless Steel Tank for Nickel Bath [Virginia]
40336. Thermal cycle for plated ABS [India]
40337. Printing/Marking Aluminium tube, OD = 8.7mm [UK]
40338. What's the proper way to hang pieces in an acid copper tank? [New York]
40339. Does DS9 passivation fall under ASTM A 380? [Colorado]
40340. Satin finish on stainless steel [California]
40341. How to Start Up A Passivation Operation? [New Jersey]
40342. Electrolysis metal pipe [Pennsylvania]
40343. Want vinyl platisol supplier for chrome plating jigs [India] {4/14/06}
40344. How do you remove oil based primer drops off of concrete? [Washington]
40345. How to remove chrome plating peeling off of rims! [North Dakota]
40346. Scratched up rim [Mississippi]
40347. What size spray paint tip is required to spray Tremclad? [Canada]
40348. Art project neutralizing nitric acid with sodium bicarbonate [Australia]
40349. Standard commercial zinc plating and hexavalent chromium [Illinois]
40350. Anodizing using the barrels [California]
40351. How to hard anodize the inside of a closed end shock tube the same thickness as the outside [California]
40352. Outdoor zinc dining table practical? [Michigan]
40353. Removal of Black Ox from Brass [Rhode Island]
40354. Passivating Aluminum [North Carolina]
40355. Media Blast [Maryland] {4/17/06}
40356. What is the pretreatment for NiP coating on Al sheet by electroless method? [India]
40357. How to codeposit ferrite+BaTio3 along with NiP? [India]
40358. Nitric Acid Testing [Kuwait]
40359. Removal on an antique metal tray of a clear coat finish (unknown) over folk art painted surface [Connecticut]
40361. Powder Coat UnderCured? [California]
40362. Can aluminum wheels be chrome dipped [Michigan]
40363. Hard Chrome Plating Electropolish Finishes [Tennessee]
40364. Anodizing after welding process [Vietnam]
40365. Who can chrome plate alloy wheels in the Montreal area? [Canada] {4/18/06}
40366. Need 4 wheels chromed [New Jersey] {4/18/06}
40367. Need "Corrolube GFS2" Surface Treatment [India] {4/18/06}
40368. Need silk screen ink for printing on rubber [Mauritius] {4/18/06}
40369. Need an electroplating additive made by Ebara of Japan [China] {4/18/06}
40370. Trying electroless CoFe deposition [Brazil]
40371. Peeling chrome wheels [Canada]
40372. Removing zinc coating from a copper penny without hurting the copper [Ohio]
40373. Sulfuric acid (H2SO4) erosion of new Lincoln [Arkansas]
40374. Zinc Corrosion and ASTM D 2565 Procedure B [Oregon]
40375. Stripping electroplated zinc from copper [Illinois]
40376. Lithographed (painted) tin plate sheets cleaning [Romania]
40377. How conductive is powder coat paint? [California]
40378. Quantifying the lubricant content of a dry film can end coating [South Africa]
40379. PCB Ni/Au electroplating crack [Thailand]
40380. Grinding Hardcoat and Holding Flatness and parallelism's of .00005" [New Hampshire]
40381. Chromic anodizing 7075-T7351 aircraft propellers [Israel]
40382. Resistance on Aludine surface [Thailand]
40383. Aluminum anodizing [India]
40384. Adhesion problems w/ powder on cast aluminum [Indiana]
40385. How to achieve 300 hr Salt Spray Resistance using 3 in 1 phosphating solution [India]
40386. SS bolts polishing [India]
40387. Measurement of Ra value of coating [India]
40388. Carbon fiber finish [Singapore]
40389. Need aluminum sheet with front anodized, rear chromated [Italy] {4/19/06}
40390. Stainless appliances: Would you do it again? [Illinois]
40391. Copper Oxidized: National Cash Register [South Carolina]
40392. RoHS and Chromic Acid [California]
40393. Retec - recovery of copper [Sweden]
40394. Cyanide wastewater treatment [Georgia]
40395. Zinc recovery from Dross [Bangladesh]
40398. Surface Roughness [Australia]
40399. Burr Problem of the Part [Singapore]
40400. Need Cobalt Plating [Massachusetts] {4/20/06}
40401. Tractor company needs electrostatic powder samples [Syria] {4/20/06}
40402. I want to double my arching area [Canada]
40403. Sulfur Dioxide Salt Fog Test(ASTM G85-02 Annex 4) [New York]
40404. White Stains on Immersion Tin Surface [Germany]
40405. For white nickel-free plating [India]
40406. Food grade anodising update? [Australia]
40407. Need adhesive tape for adhesion testing [France] {4/21/06}
40408. How do I have to dissolve stainless steel [Belgium]
40409. Regarding the pitting on 316 SS [Saudi Arabia]
40410. Magnetic flow machining with advanced materials [India]
40411. Will clear coat protect copper from spotting? [Florida]
40412. Finishing iron custom staircase [Washington, DC]
40413. Clear coat for auto rims [Texas]
40414. Painting a metal cabinet [New York]
40415. I was wanting to paint a golf cart body [North Carolina]
40416. Aluminum oxide = health risks? [Wisconsin]
40417. Reduction of metal waste in the dental plating industry [Illinois]
40418. Using conductive paint to make high voltage resistors [South Africa]
40419. How to call out gold TiN coating [Canada]
40421. Your thoughts on hardcoat anodizing 5052 alum. [New Hampshire]
40422. Passivation and laser etching [Pennsylvania]
40423. Need Hard Chrome on ID of Hydraulic Cylinder Liner [India] {4/21/06}
40424. Need "Endura Shine" plating process [UK] {4/21/06}
40425. Need Media Supplier Near Pasadena [California] {4/21/06}
40426. Removing 3M scotchlite from aluminum extruded highway sign panel [Canada]
40427. PCB Electroless Nickel/Gold question [Korea]
40428. Need corrosion protection finish for high strength bolts in clean room [California]
40429. Discolored finish after 150degC bake [Singapore]
40430. What colours are available with Alochroming? [UK]
40431. RE HARDCOATING A PART WITHOUT STRIPPING [Massachusetts]
40432. 302 SS nickel wire and salt spray test [Oregon]
40433. Seeking trivalent chrome passivation (Alodine T5900 or equiv) of small aluminum parts [California] {4/24/06}
40434. WANT CYANIDE BASED RHODIUM PLATING SOLUTION [India] {4/24/06}
40435. Wanted: Diamond Turning CNC Consultant For Nickel Plated Mandrels [Illinois] {4/24/06}
40436. Tri-nickel + chrome failing CASS test [Vietnam]
40437. Zinc-Nickel plating [Michigan]
40438. Cloudy electroless nickel deposit [South Korea]
40439. Zinc surge up, how long it will last? [Mexico]
40440. Chromic Anodize - Deterioration of bath [Utah]
40441. Photo-Resist Composition anyone? [Philippines]
40442. What type of bonding clamp is compatible with copper and galvanized steel? [Kentucky]
40443. Seeking spoon ring maker [California] {4/25/06}
40444. Need redipping of chrome car rims [Maryland] {4/25/06}
40445. Gold plating for zinc plates [Pennsylvania] {4/25/06}
40446. How does the phosphoric, citric, and carbonic acid in soda not corrode the aluminum can it is held in? [Maryland]
40447. Which pH level is the most conducive to the corrosion of copper and iron [Malaysia]
40448. Blackening / colouring aluminium by coating [UK]
40449. Removal of rust from marine stainless steel cables used for rigging and subsequent protection [North Carolina]
40450. Remove paint from bath tub [West Virginia]
40451. Uncleanable Aluminum Rims [Kentucky]
40452. Can I clearcoat brushed stainless steel [Connecticut]
40453. Is it possible to strip polished brass, and if so what will be underneath [Arizona]
40454. Restoring brass handles/hardware on Antique Secretary Desk [California]
40455. AMS 2485/G [Taiwan]
40456. Want to know PVDF, CF-8, CF-8M, 16MnDR materials’ compositions [Bangladesh]
40457. Adhesive and optically transparent layer by vacuum coating for gold to stick on glass. [India]
40458. Hard chrome plating adhesive failures [India]
40459. Mold release problem for rotational molding process [West Bank]
40460. Corrosion on the external surface of 1" Alloy 20 pipe [Virginia]
40461. Need tin plating on solder pads only in PCB [India] {4/26/06}
40462. Looking for low emissivity paints meeting MIL-F-14072, P371.2 Type 1 [California] {4/26/06}
40463. Deep-red to near-IR absorbing paint/coating [Switzerland] {4/26/06}
40464. Heat resistant paint for clay products [Florida] {4/26/06}
40465. Need a copper crown gold plated [Louisiana]
40466. Want cast iron cooker - Coal [UK]
40467. Quantity of chemical to use for 16'x3' copper (Hughes book question) [Georgia]
40468. Katrina Took My Soul Away..... [Louisiana]
40469. Mirror like layer is needed instead of pink layer in acid copper electroplating [Egypt]
40470. WANTED: Professional documentation detailing a RoHS Chemical Conversion Coating [Georgia]
40471. Can E-coating be an alternative for zinc galv plating as a rust prevention for metal parts that get powder coated? [Pennsylvania]
40472. Peeling problems in Hot Dip continuous galvanizing Non Ox furnace [Egypt]
40473. Is there an easier way to clean 8.8, 10.9 12.9 grade steel chemically? [South Africa]
40474. Nickel in copper bath [Pennsylvania]
40475. Does nickel coated 302 SS wire need to be passivated to avoid corrosion [Oregon]
40476. Rust in hot phosphated parts [India]
40477. Need Darkening of Copper Clad Wine Cellar Door [Arizona] {4/26/06}
40478. Need Neosepta Cation permeable membrane [Sweden] {4/26/06}
40479. Hard chrome coating on cast iron cylinder [India]
40480. Trivalent Functional Chrome Plating [UK]
40481. How to remove Titanium anodizing non-industrially? [New York]
40482. Need help removing rock like deposits in tank! [California]
40483. Precipitating rhodium out of a rhodium plating solution [Illinois]
40484. What are the decomposition products of Bright Nickel [Thailand]
40485. Second De Embrittlement required after plating? [UK]
40486. Need a body filler before powder coating, compatible with powder coating [Mexico]
40487. What is the Advantage of Powder Coated Stainless Steel Junction Boxes [Saudi Arabia]
40489. Difficulty in zinc plating heat treated parts [India]
40490. Adhesion problems with copper on old zinc parts [Poland]
40491. Problems faced in gold plated metal components [India]
40492. Black spots on satin nickel components [India]
40493. Achieving yellow without a dye station [Canada]
40494. Electro-chemical Deburring [India]
40495. How to quickly remove steel burr on OD [Ohio]
40496. Is copper galvanically safe to use with a ZINC PLATE - Chromate [California]
40497. How to make long lasting (2 years life) Dye Gold Plating on Imitation Jewellery [India]
40498. I want my 4 year old refrigerator painted from white to black [Texas] {4/26/06}
40499. Silica removal [India]
40501. What is zinc die casting plating storage life [Singapore]
40502. Substitutability between galvannealed, hot dip galvanized and electrogalvanized [Canada]
40503. Need anodize and passivate of titanium medical implants [California] {4/27/06}
40504. Need lacquer coating system for gold plated watch bracelets /jewelry [Ireland] {4/27/06}
40505. Where can I buy Ebonol in Brisbane? [Australia] {4/27/06}
40506. Zinc Plated Steel Toxic Fumes? [Georgia]
40507. PVD line water management [Pennsylvania]
40508. Silver plating on carbon for Ag4[Fe(CN)6] dep [Tennessee]
40509. Substrates nodules [Philippines]
40510. Making a chrome bumper paintable [Georgia]
40511. Artist looking for information on corrosives, stains and coloring agents [New Mexico]
40512. How to remove pvc glue from hair and body [Utah]
40513. Removing powder coating from step bars on my pick up [Ohio]
40514. Gold plating lead [Ohio]
40515. Effects of Muriatic Acid on Lungs [California]
40516. AISI material standard to JIS [Indonesia]
40517. Vinyl Coating for Coil Nails [India]
40518. Bubbles in Clear Powder Coat [Ohio]
40519. Bright nickel-free plating wanted cheap [India]
40520. Pin holes in chrome allow corrosion [Colorado]
40521. Polishing raised lettering [Canada]
40522. Aluminium corrosion when used with copper in water [UK]
40523. Chrome Plating Auto Rims in NY or NJ [New York] {4/28/06}
40524. Electroforming a layer of silver solder onto a copper-silver laminate [Florida]
40525. Zinc cyanide poisoning [Minnesota]
40526. Using Deionized Water in Closed Loop Heating System [California]
40527. R.O. WATER REQUIREMENT FOR SS ELECTROPOLISHING? [Pennsylvania]
40528. What are the different ways of passivation for SS 316 L and SS 314 L? [India]
40529. Electropolishing aluminum [New York]
40530. Phosphating Versus Bonderizing [India]
40531. Protection needed for steel pinion in plastic rack [Colorado]
40532. Making a whip saw as my first knife [Michigan]
40533. Thick Film to PCB adhesion deteriorating after Nickel [Indiana]
40534. Setting up to dye aluminum in different colors [Kentucky]
40535. Hard Anodizing 7075 Alum [Massachusetts]
40536. Need cast-iron kitchen sink re-enameled [New York] {5/1/06}
40537. Need electroless silver plating of specialty electrodes [California] {5/1/06}
40538. Need a plant for electro-tinning copper coils [Jordan] {5/1/06}
40539. Procurement of tufftriding salt [India] {5/1/06}
40540. Need a OPC full renewing drum machine [Brasil] {5/1/06}
40541. Chemical Cobalt Plating [Ukraine]
40542. Looking for a thermal target [Turkey]
40543. Cold Enameling does not survive plating [UK]
40544. Chrome plating cda 91300 high tin bronze [Kentucky]
40545. A patina finish of multi colors for a copper backsplash attached to a cast iron sink [New Jersey]
40546. Polishing Stainless Buses and Coaches [Florida]
40547. BBQ Stainless [California]
40548. Best way to remove engraving from sterling silver [South Carolina]
40549. Remove goldplate from s.s. flatware [Canada]
40550. Need to recoat 1943 zinc plated pennies [Georgia]
40551. Recovery of nickel and chrome from stainless steel pickling sludge [India]
40552. I have components that need to be tin/lead plated to MIL-F-14072 F. [Texas]
40553. Need mordant wash for galvanized steel [Connecticut]
40554. Peeling problem in continuous galvanizing [Egypt]
40555. Nickel plating on acid copper plated lead based idols [India]
40556. Flash gold on ABS [Egypt]
40557. Silver - WHY NOW? [Michigan]
40558. Poor adhesion in plating onto titanium [UK]
40559. Suitable valves for concentrated sulfuric acid [Thailand]
40560. Corrosion Preventing Paper for Ferrous Castings in Salt Water? [Pennsylvania]
40561. Surface treatment required for Aluminium Plate [China]
40562. Wanted: To purchase Incralac in 1 and 5 gallon quantities [California] {5/2/06}
40563. Want to buy nitric acid [Philippines] {5/2/06}
40564. Do you know what nitrates are present in the water from electroplating industry? [India]
40565. Influence of surface finishing on AISI 316 on corrosion resistance in marine environments [Norway]
40566. Did Bleach Strip Gold from Wedding Ring? [New Jersey]
40567. Choosing tube mill lubricant for pregalvanized steel [Canada]
40568. Cost reduction for plating of aluminum bus bar [Ohio]
40569. Bothersome fingerprints on Titanium Anodizing [Ohio]
40570. Electroplating solutions [Virginia]
40571. How to remove steel machine screws tapped into aluminum [Canada]
40572. Help--white deposits on my chrome wheels [UK]
40573. REFINISHING METAL 2" TUBULAR HANDRAIL [California]
40574. FINISH: LIGHT CHROMATE CONVERT PER MIL-C-5541 CLASS 3 [Australia]
40575. Salt spray testing of zinc plated iron parts with trivalent chromium passivation [India]
40576. Electropolishing of 304 wire basket [India]
40577. Easiest way to make stainless steel printing plates hydrophilic? [Florida]
40578. What is a different between current and voltage in power supply and why? [Oman]
40579. SOS: Seek help for black oxide short [Singapore]
40580. Acid clean boiler part? [Indiana]
40581. Need rims replated with chrome in NJ or NY area [New Jersey] {5/3/06}
40582. Want cyanide-free gold plating process [India] {5/3/06}
40583. Looking for semi-permeable barrier 0.5 microns [Florida] {5/3/06}
40584. Rust treatment for historic cast iron on stained glass window [Illinois]
40585. Using magnesium hydroxide in metal removal in treating waste water [Utah]
40586. Testing for 304 vs. 316 Stainless Steel? [Canada]
40587. Flawless filler before powder coating [Ohio]
40588. Looking for a blackening solution [India]
40589. How do I maintain the rich dark color of lasering stainless steel? [England]
40590. Is Titanium Plating or Coating on Stainless Steel Possible and How? [Pakistan]
40591. Electroless nickel plating on zinc die castings - found black spot [Malaysia]
40592. Platinum Chrome Blistering [Illinois]
40593. Silver tetrafluoroborate plating [Scotland]
40594. Matte tin plating using cresol sulphonic acid [India]
40595. Durability of different finishes for PC board contacts [Malaysia]
40596. In service passivation of hydrocarbons piping systems above 150 deg.F [China]
40597. Active stainless in galvanized metal lath [Massachusetts]
40598. Jeweler needs silver electroforming service [Canada] {5/5/06}
40599. Need a chrome finish for ABS injection molded parts [California] {5/5/06}
40600. Need anodizing of 6"OD x 96"FW Alum. Roll [South Carolina] {5/5/06}
40601. Need Black Oxide Coating Service [Texas] {5/5/06}
40602. Want Used Oil free Screw Compressor [Pakistan] {5/5/06}
40603. Nextel Suede Coating [UK] {5/5/06}
40604. Want yellow tri chrome passivation process [India] {5/5/06}
40605. How does a mill measure carbon smut on cold rolled [Ohio]
40606. Iridite 7P [New York]
40607. Brass JIS C3604 RoHs Compliance? [Singapore]
40608. Black RoHS conversion coating for aluminum [Virginia]
40609. How to do plastisol, how to do process? [Mexico]
40610. ASTM B117 salt purity [California]
40611. MIL-A-8625 Type III the same as AMS 2469 [Texas]
40612. ***I know why boiling test at 4 hour 100 deg C is required? What is the purpose of this test [Singapore]
40613. How do you get a more SHINY black patina effect on Zinc? [China]
40614. I want titanium coating on stainless steel for coloring [Pakistan]
40615. Hard chrome pre treatment [Ohio]
40616. Bubbles in zinc plate [Massachusetts]
40617. Sodium Contamination In Watt Bath [Arizona]
40618. Gold Plating Thickness (Porosity) [UK]
40619. Which anodizing process is right [North Carolina]
40620. Test to check clear Iridite coating [Florida]
40621. What process can create a scratch proof stainless steel surface? [Malaysia]
40622. Need re-enamelling of an old wall mount sink [Washington, DC] {5/8/06}
40623. Need a chrome finisher to etch our ABS plastic parts in chromic acid solution [Iowa] {5/8/06}
40624. Electroless gold [Delaware]
40625. Non-RoHS stainless steel? [Massachusetts]
40626. Is Rechroming Illegal in New York State? [New York]
40627. Selection of filter press cloth [Turkey]
40628. Titration method for electrolyte - Is this correct? [Canada]
40629. Alkaline Zinc on sheet metal - Recurrent Blistering! [Minnesota]
40630. Woods Nickel Strike ASF [Texas]
40631. Sticky film on my black anodized 6061 [Delaware]
40632. Alochrome/Health and Safety [UK]
40633. What is the natural colour of 7075 Aluminium Hardcoat HAIII [UK]
40634. Conductive powder coat prep [California]
40635. Comparison of plastic chroming techniques [California]
40636. Creating company logo on hot-rolled steel bars [Greece]
40637. Institution where I can get a proper training for Quality Control and Military Standard 105 E? [Poland]
40639. Need epoxy primer powder [UK] {5/9/06}
40640. Black Chrome Wheels [Arizona] {5/9/06}
40641. How do I electro polish sterling silver charms? [UK]
40642. Cleaning copper for soldering purposes [Australia]
40643. Masking fluid for dyeing [UK]
40644. How do I minimize orange peel? [California]
40645. Method of metal plating on plastic [South Africa]
40646. Silver testing supplies [Washington]
40647. Bleach and C.L.R. [Canada]
40648. Looking for suppliers for enamel coating on ferrous parts [India] {5/9/06}
40649. Need vendor for QPQ or salt bath nitrating in North America for large diameter parts [Costa Rica] {5/9/06}
40650. Need yellow chromating of hose fittings [Louisiana] {5/9/06}
40651. Need Stainless Steel pipes/sheets in different colours/finishes [India] {5/9/06}
40652. I need a clear conversion coater for aluminum stampings [Indiana] {5/9/06}
40653. Having trouble rhodium plating silver jewelry [Thailand]
40654. Is there an alternative to Ferroxyl test? [Italy]
40655. Removal of Textured Powder Coating from Bathroom Fixtures [Texas]
40656. Antique black finishing of metal plate [Turkey]
40657. Need RAL shade card [India]
40658. Polyurethane paints [India]
40659. Multilayer electrophoretic lacquer? [India]
40660. Finish for a steel lock [UK]
40661. How to make black color on SS304 steel [Italy]
40662. Black natural finish for steel or iron exterior building parts [California]
40663. Test Method for Evaluation of Electrogalvanized Coated Components [India]
40664. Nickel Chrome Plate temperature thresholds [Illinois]
40665. Wheel chroming [Kuwait]
40666. Plating solution on alternative nickel [Florida]
40667. Hard Anodizing for Corrosion Protection from Methanol [California]
40668. 302 Stainless Steel [Iowa]
40669. How to design 3 Stage Wash System [Indiana]
40670. Cleaning up MONEL 400 after fabrication [Wisconsin]
40671. How to polish the alloy wheel for chrome plating [Thailand]
40672. What do I use to protect aluminum from ethylene glycol+water [California]
40673. Micro inches [Pennsylvania]
40674. "So, Rhodium costs almost twice as much as Platinum - of course I am interested." Gotta love that. [Maryland]
40675. Electroless nickel plating of aluminum parts [UK]
40676. White rust formation on Zinc + Cr+3 finished threads [Brazil]
40677. Where to find Dubois 200 rust inhibitor [California] {5/10/06}
40678. Plating Oxides [Florida]
40679. ALIGRAPH 2, ALUMINIUM GRAPHITE POWDER [Canada]
40680. Need Help with Plating Polished Nickel over Nickel (Replate) [Ohio]
40681. TITANIUM ANODIZING [California]
40682. MIL-C-5541 E - Resistant to Fungi ? [Virginia]
40683. Looking for shop that does RoHS Black zinc with trivalent chromate [Virginia] {5/11/06}
40684. Info about e coating [India]
40685. Black hard chrome problems [New Jersey]
40686. Material plating on titanium for wear resistance [New York]
40687. Corrosive effects of sodium benzoate on magnesium [Texas]
40688. Titanium vs. stainless - scratch resistance [Louisiana]
40689. Chemical Liquid for Stainless Steel [Indonesia]
40690. Solderability of ELECTRO TIN PLATE PER ASTM-B545 [California]
40691. Fingerprint Resistant Coating [Florida]
40692. LOOKING FOR A PRODUCT/ Eurocoating? [Illinois]
40693. Powder coating on cast iron [India]
40694. Line problem on ABS plating [India]
40695. No cyanide in cleaning of gold surface [Turkey]
40697. Sprucing up a copper cup and tray set [New York] {5/11/06}
40698. Seeking zinc plating supplier in Mexico for steel turned hydraulic fittings and adapters [Ohio] {5/11/06}
40699. Aluminum artwork needs repair and resurfacing - help [Canada]
40700. Paint bubbling on galvanized chassis [Canada]
40701. Seeking copper plating of large cylinder [Michigan] {5/12/06}
40702. Bonding strength test for PWBs [Australia]
40703. Stripping Tin on Electroless Nickel [Greece]
40704. Nickel Plating Problem (ph) [Tennessee]
40705. Hard Chrome Plating Bath Contamination [Canada]
40706. Type of coating that ***be used to REPAIR grinded Mil-C5541surface of an Aluminum part [California]
40707. Flash pickling and smut removal on Ti6Al4V [UK]
40708. Need bidet fixtures to be replated to oil rubbed bronze [California] {5/12/06}
40709. Require BORON NITRIDE and WS2 (1micron powder) [India] {5/12/06}
40710. Zr plating [Iran]
40711. Trouble achieving green anodize on odd shape titanium parts [Canada]
40712. Stainless Steel Coffe Table Needs Help (Rust - Scratches) [Georgia]
40713. Tin/lead soldering used on parts with Matte Tin plating [Canada]
40714. Salt tracking problem with PVC plastisol [Missouri]
40715. HOW DO I CARRY OUT MATTE ACID TIN PLATING [India]
40716. Oil for surface grinding aluminum [Australia]
40717. Looking for supplier of palladium powder [South Africa] {5/12/06}
40718. Durable black finish for 18/8 Stainless parts [Indiana]
40719. Yellow Zinc Plate vx. Black Oxide [Georgia]
40720. Surface Finishes for Breadmaker Components [UK]
40721. Want to start business of supplying electro plating chemicals [Michigan]
40722. Powder Coated Patio Furniture [Texas]
40723. Removing Nickel Plating From Paintball Parts [Canada]
40724. Aluminum tank for parkerizing [Nevada]
40725. What metal to use for coffin handles that will be chromed? [India]
40726. Lead sheathing of copper [India]
40727. Difference between Yellow, Green and White Passivation [India]
40728. White powder defect on Black Passivation on Acid Zinc Plating [India]
40729. Pretreatment of areas where welding or grinding remove galvanizing [India]
40730. Want E-coating of Mercury Cougar [Massachusetts] {5/15/06}
40731. Need refinishing of cast-aluminum patio furniture [California] {5/15/06}
40732. Seeking finishing company for Table and Chairs [Michigan] {5/15/06}
40733. Need Electroplating Rectifier [Egypt] {5/15/06}
40734. Need a web metalizer for laboratory use [South Korea] {5/15/06}
40735. Need synthetic HT media [India] {5/15/06}
40736. Need Chrome Plating of plastic auto parts [Washington] {5/15/06}
40737. RoHS and zinc plated hardware [Connecticut]
40738. CASS Test versus ASTM B117 Comparisons? [California]
40739. Stripping of AL Arc Spray Coating from AL-6061-T6 Materials [Singapore]
40740. Black paint fill of stainless steel etched parts [Ohio]
40741. What is the best process to hard plate industrial diamonds to steel to make diamond core drills? [California]
40742. Imbue or change hue of electroless nickel [Illinois]
40743. Substitute for rhodium plating on jewelry [India]
40744. Does anodize improve coating adhesion? [South Dakota]
40745. Performance of powder coating on blasted surface [India]
40746. Effective electro chemical etching process for nickel forming on ss substrate [India]
40747. Best in Class Black Coating [Michigan]
40748. Need Used Plating Tanks [Ohio] {5/16/06}
40749. Need a Nickel Filter [Ohio] {5/16/06}
40750. DIY selective coating [Virginia]
40751. Color fastness of polymer concrete and reinforced moulding compound [Nevada]
40752. Color manipulation of chromate anti-corrosion baths [Texas]
40753. Material for Zinc Melting Pot for Galvanizing [India]
40754. HARD CHROME PLATING OF 10MM DIAMETER CK45 RODS [India]
40755. Nickel Chrome Plating On Aluminum [Turkey]
40756. Laser etching of anodized aluminum [Ohio]
40757. I have brushed aluminum tube to patina in earth tone [California]
40758. Anodising-lead cathodes (RoHS legislation) [Australia]
40759. Rust prevention additive for vibratory compound [South Africa]
40760. High temp non-stick and durable coating? [California]
40761. E-coat [North Carolina] {5/18/06}
40762. Need 1.9 OD galvanized tubing 13 gauge [Nebraska] {5/18/06}
40763. Restauranteur asks if stainless steel okay for lemon juice (citric acid)? [Florida]
40764. Hardening aluminum [North Carolina]
40765. Copper Danglers are F006 Hazardous Waste? [Tennessee]
40766. Spot test for nickel on copper [Washington]
40767. Spot Testing of Nickel in Alloy Steel [India]
40768. Laser Etching of Anodized Aluminum -Is a polished look possible? [Texas]
40769. Corrosion protection A380 cast aluminum with chrome [Michigan]
40770. Need chrome dipping of 18" rims [Michigan] {5/17/06}
40771. Need my 1966 Dodge Coronet bumpers rechromed [South Carolina] {5/17/06}
40772. Need Nickel-Chromium Plating for Aluminum Auto-Trims [Turkey] {5/17/06}
40773. Additive that give brightness to silver plating [India]
40774. Epoxy/ABS system [India]
40775. Polished Chrome vs. Chrome Plated Brass [Washington, DC]
40776. Looking for companies that anodize and sell small beads and bead shapes for jewelry [Pennsylvania] {5/17/06}
40777. How to waste treat nickel boron [California]
40778. Stripping nickel from copper [Turkey]
40779. How to avoid the hydrogen embrittlement problem [China]
40780. High gloss clear TGIC coat turns out flat and dull [California]
40781. Adding Color to the Process of Vitreous Enameling [Arizona]
40782. 24 carat gold colour [India]
40783. Ni3B question Tapping the keg of knowledge here at finishing.com [South Carolina]
40784. Is chrome plating safe for food processing tools or machines? [Indonesia]
40785. ZINC PHOSPHATE COATING [Pakistan]
40786. Need Rims Chrome Plated [Pennsylvania] {5/18/06}
40787. Looking for Yellow Iridium?? plating on magnesium parts [California] {5/18/06}
40788. Alodine and Anodize paint adhesion problems [Canada]
40789. A coating to prevent toner from sticking to rubber rollers [Pennsylvania]
40791. Want to electroform jewelry [India] {5/18/06}
40792. Need system for Teflon Coating on utensils [India] {5/18/06}
40793. I need help to get rid of the nodules in gold plating [Pennsylvania]
40794. Rating of Salt Spray Test [Philippines]
40795. Silver plating - electrolytic chromates [Scotland]
40796. Anodizing Black Dye Smears [Florida]
40797. Salt spray requirements of anodized aluminum [Canada]
40798. Sodium Dichromate sealing of anodized surfaces and temperature degradation [California]
40799. Getting a grip on Sealed Anodized [Japan]
40800. Brass forged component finishing [India]
40801. Corrosion protection for wheels [South Carolina] {5/22/06}
40802. Re-chrome bumpers [Pennsylvania] {5/22/06}
40803. Alodine 1500 agent [Taiwan] {5/22/06}
40804. Need Wheels Refinished [California] {5/22/06}
40805. Looking for Used Copper [New York] {5/22/06}
40806. Corroded Aluminum Door Threshhold [California]
40807. Zinc thickness on galvanized steel conduit [Texas]
40808. HELP! Need a Process Control Specification (not material spec) for Powder Coating [Oregon]
40809. Light blue clouds on electroless Ni-surface [Germany]
40810. Rework on internal thread of size N 10 UNF as gauge not pass after plating [India]
40811. Water break timing [Maryland]
40812. Chemical method to remove rust from carbon steel tank that contains Sulfuric Acid at 98% concentration in explosive atmosphere plant [China]
40813. Elimination of phosphating by adding anything in heat treatment [India]
40814. Acid etching stainless steel panel [Canada]
40815. Need help with solution for mirror finish repair! [North Carolina]
40816. Best coating for aluminum hotplate? [UK]
40817. Seeking chrome plating for rear light guards for Jeep Grand [California] {5/23/06}
40818. Need tube measurement tools [Egypt] {5/23/06}
40819. Monobasic acids [Uganda]
40820. I wish to learn the bronzing trade and purchase supplies [Maryland]
40821. Painting Powder Coated Aluminum [Canada]
40823. RoHs compliance for Stainless Steel Fasteners [Australia]
40824. What is rapid nitriding process? [India]
40825. Corrosion resistance - electroless nickel versus sulfamate nickel [Oregon]
40826. Control of pH in nickel sulfate bath (watts bath) [Nigeria]
40827. Electrodeposit Zinc Plating Affecting Zinc Phosphating [England]
40828. Zinc plating cast iron [Australia]
40829. Nickel plating surface face prior to hard chroming for large bore engine piston rings [Texas]
40830. Cleaning of aluminium castings for race applications [UK]
40831. Salt spray failures in zinc plating [China]
40832. Need stripping and powder coating of auto chassis [Delaware] {5/24/06}
40833. COMPANIES IN THE US THAT CAN CHROME PLATE ALUMINUM WHEELS? [Alabama] {5/24/06}
40834. Want re-chroming of plastic eye-ball air vents for dashboard of 1967 mk2 Ford Cortina [Ireland] {5/24/06}
40835. Need Used Salt Spray Chamber [Belarus] {5/24/06}
40836. Seeking continuous coil coating line [India] {5/24/06}
40837. Plating of platinum in the early 20th century [Florida]
40838. Do you have to remove a powder coating to "repaint" it? [Florida]
40839. Removing tin oxide from tin plated copper tray [Australia]
40840. ALOCHROM 1000 RoHS Compliance [Scotland]
40841. 12L14- ROHS [California]
40842. Can I safely add copper to my diet by boiling pre-1980's pennies with my tea? [New Mexico]
40843. Anionic bed regeneration [Pakistan]
40844. How to make ferrous sulfate as a water flocculant [Georgia]
40845. Suitability of @Kynar Painted Metal Roofing for Collection of Potable Rainwater [Canada]
40846. Polyurethane Powdercoating on Stainless Steel steel AISI304 or AISI210 [UK]
40847. Best way to keep original colour and finish of copper in harsh conditions [UAE]
40848. Powder Coating Automobile Front End Parts [Washington]
40849. Pulsed Current vs Continuous Current Plating [Philippines]
40850. Bright Tin Finish -VS- Matte Tin Finish [California]
40851. Will chemicals used in bright zinc electroplating process hurt Viton? [Ohio]
40852. Dichloromethane (CH2Cl2) effects on black anodize [Minnesota]
40853. Aluprint or Anodic Printing using Inkjet Printers [England]
40854. Question on racking for small parts [Massachusetts]
40855. I need concrete "cons" to Nitric 1 Passivation with sodium bichromate. Please help! [Kansas]
40856. Saltwater resistant fasteners [Florida]
40857. Need chrome plating of valve covers [Wisconsin] {5/24/06}
40858. Where can I get my rims chromed [New Jersey] {5/25/06}
40859. Paint Removal Company for Wooden Doors [Michigan] {5/25/06}
40860. Need gold dipping of a sand dollar [Illinois] {5/25/06}
40861. Need boat cleats rechromed and rub rails mirror polished [Georgia] {5/25/06}
40862. Need satin clear coat for nickel and gold fixtures [Michigan] {5/25/06}
40863. Charcoal filtering nickel sulfamate solution? [California]
40864. RoHS Compliance Confusion - Hexavalent but less than 1000 ppm? [Texas]
40865. Looking for web site with GM Worldwide Engineering standards [Canada]
40866. How to recycle copper and nickel banknote printing plates? [India]
40867. Resistor's resistance drifts up after electroplating [Malaysia]
40868. Zinc Plate Trivalent Chromate blistering after 4 hr 400 Deg F cure bake [California]
40869. Plastisol patching [Turkey]
40870. Cathode selection when electropolishing 416 stainless steel [Ohio]
40871. Clean my hydraulic parts so that could be recycled by filter [Germany]
40872. 316SS Tubing Contamination Problem [Colorado]
40873. Aluminum trailer siding corrosion [California]
40874. Seeking Applicator of DCX Spec PS-8059 (Sermagard) [Michigan] {5/25/06}
40875. Finish for zinc casting [Ohio]
40876. Internal coating of silent check valve damage and corrosion found at swimming pool system [China]
40877. Need Duranodic permanent markers [California] {5/26/06}
40878. Where to get wheels chromed [Virginia] {5/26/06}
40879. Nickel Plating and RoHS requirement [California]
40880. Hardness achievement in high speed self regulating hard chrome bath [India]
40881. Life/wear durability of chrome plating verses nickel boron (i.e. Ultra-Sem) [New York]
40882. Need Cathodic Epoxy Electrocoat per MS-PB60-2 [Ohio] {5/26/06}
40883. Interested in buying silver test strips [United States] {5/26/06}
40884. Finishing process in line for EMT (Electrical Metal Tubes) avoiding white rust on the galvanized [Colombia] {5/26/06}
40885. Need to know how and where from I can order Eli-Lilly first aid kit [Lebanon] {5/26/06}
40886. Agitation air sizing [Zimbabwe]
40887. Reaction of cyanide and bleach? [Texas]
40888. A zinc die casting replating [Hong Kong]
40889. Using caustic to dissolve aluminum [Louisiana]
40890. How to get salt spray of 500 hrs on welded joints [India]
40891. New powder coater needs straight answers [Florida]
40892. Paint touch up on powder coated surface [India]
40893. Color Problem with PVD Deposits [Italy]
40894. Cracks in the chain after yellow zinc passivation [India]
40895. A problem with nickel - chrome plating on zinc substrate [Vietnam]
40896. Hard Plating Small Bores [Rhode Island]
40897. Masking parts during passivation [California]
40898. Powder coat over metallizing better than over phosphatizing? [New York]
40899. Iron Phosphate Lubrication Alternative [Michigan]
40900. I need to hire someone to refinish two vintage chrome tables in Los Angeles [California] {5/31/06}
40901. Need Stainless Steel Sink Polishing Machine [Hong Kong] {5/31/06}
40902. Need Water Immersion Test Equipment [Australia] {5/31/06}
40903. Need a coated copper bracelet manufacturer [California] {5/31/06}
40904. Stainless Steel vs Aluminum Crawfish Boiler [Texas]
40905. ETCHING BRONZE/BRASS WITH LETTERS FOR PRINTING ON LEATHER [Ghana]
40906. Sacaphen coating [Spain]
40907. Alternative to Plastisol? [Australia]
40908. Air voids in cathodic electro coating process [Michigan]
40909. Nitriding case thickness definition [UK]
40910. Main causes of nickel contamination in costume jewelry plating [Hong Kong]
40911. How to recover platinum from the mud of mixed metals like platinum, palladium, rhodium [Pakistan]
40912. Aluminium pickup/crack after anodized process [Malaysia]
40913. Bulk anodizing or cold chemical anodizing of aluminum [Kansas]
40915. Can stainless steel 316L vessel resist for 10% HCl and 10% NaOH [Thailand]
40916. Can you chrome dip my four wheeler brush guards [North Carolina] {5/31/06}
40917. Looking For Rhodium Bath [India] {5/31/06}
40918. Electrolyte for aluminum electroplating [Taiwan]
40919. How to obtain yellow gold precipitate [Nepal]
40920. Faded anodized aluminum [California]
40921. Lacquered Plastic Beads Stick Together [India]
40922. How to make blackened steel rust proof [New York]
40923. Need non peel paint for steel siding [Montana]
40924. Removal of tie dye from hands [Connecticut]
40925. Etching for Aluminium-Boro-Magnesium prepared material [Puerto Rico]
40926. Methanol damaging epoxy paint [New Hampshire]
40927. ZEBRA LINES ON HARD ANODISED COOKWARE [India]
40928. Brass against Aluminum--Need NON-SHINY coating to prevent galvanic corrosion [New Jersey]
40929. Refurbishing nickel-lined copper cookware [Canada] {6/1/06}
40930. Want to know of an opc drum factory [UK] {6/1/06}
40931. Need chemical deburring machine [North Carolina] {6/1/06}
40932. Salvage of ancient sail pulley [California]
40933. What coating is used on the surface of PC Motherboard to protect the copper wires? [Pakistan]
40934. How would I paint a picture on my brand new white fiberglass canoe? [Massachusetts]
40935. Three Step Acid Finishing [California]
40936. Heating Pickle Acids [North Dakota]
40937. Connecting lead anodes to bus bar [India]
40938. Reduction of Boron in Seawater [India]
40939. Soldering onto a aluminum pin [South Africa]
40940. Hydraulic tubing passivation [North Dakota]
40941. What color is Dacromet? [California]
40942. Matte tin plating: thermal resistivity and oxidation [Arizona]
40943. HELP!! Black zinc vs Black oxide [Canada]
40944. Visual Appearance of Sulphamate Nickel [Singapore]
40945. Anodizing over Anodize [Minnesota]
40946. Rainbow Finish on Stainless Steel [Pennsylvania]
40947. Is there a need for iron phosphate coating in a dry film lubrication application? [Michigan]
40948. Need my swing arm plated [New Jersey] {6/1/06}
40949. Low temperature cure powder coatings? [Kentucky]
40950. Plating process for copper [India]
40951. Need laser cutting services and forming using pressbrake [Canada] {6/1/06}
40952. Need rechroming of wheels [Illinois] {6/1/06}
40953. Need powder coating for valve covers [Canada] {6/1/06}
40954. In search of Zinc plater [Michigan] {6/1/06}
40955. Need Trivalent Coating [India] {6/1/06}
40956. Chrome plate truck parts [Michigan] {6/1/06}
40957. Need Black Oxide put on Stainless Steel Part [Pennsylvania] {6/1/06}
40958. Asking for a protocol about gold coated iron particles [Wisconsin]
40959. Electroless Nickel Plating [Pakistan]
40960. Pulse current for trivalent hard chrome plating [UK]
40961. Teflon coating on fiberglass cloth [India]
40962. Optimum pH for tin electro refining [Canada]
40963. Bright nickel process [Indonesia]
40964. Can it be SUS303 if it's rusty and magnetic? [Michigan]
40965. Need Teflon coated aluminum films [Ohio] {6/2/06}
40966. Need black plating on nickel hex panel nut [California] {6/2/06}
40968. I want to sand and prime my car properly. How do I do that? [Canada]
40969. Voltage required to apply e-coat that is used on automobiles [Illinois]
40970. Does hot dip galvanizing adhere on stainless steel? [South Africa]
40971. Boric acid vs Borax pentahydrate [Illinois]
40972. What type of pickling is recommended to clean A286 material [Pennsylvania]
40973. Anodizing a cast A380 aluminum part in light color [California]
40974. Can you suggest good supplier in India, who can do cadmium plating over beryllium copper part? [India] {6/2/06}
40975. Chemical Etching - on Stainless Steel [India] {6/2/06}
40976. Hex chromium, and tri (3+) chromium [India]
40978. Need RoHS antique copper plating [Oregon] {6/5/06}
40979. Need 2 motorcycle pipes chromed [New Jersey] {6/5/06}
40980. Seeking aluminum powder coating line [India] {6/5/06}
40981. We need physical vapor deposition machine for TiN Deposition on Stainless Steel [Pakistan] {6/5/06}
40982. DIP CAR BODY FOR RESTORE CAR [California]
40983. Mirrored headlights? I've seen them but can't find them to purchase [Kansas]
40984. WATER SPOTS ON NEW ALUMINUM WHEELS CLEANERS AND VIN. DIDN'T WORK [Virginia]
40985. Will brass contaminate a rhodium solution even with a pre-plate? [California]
40986. Uranus B6 barrel suitable for chlorhydric pickling? [France]
40987. MSDS [Canada]
40988. How can I remove paint from stainless steel? [Indonesia]
40989. Stoving Enamel [India]
40990. Can we find plateable lexan grade PC? [Hong Kong]
40991. Silver Plating Beryllium/Teryllium Copper Alloys [South Carolina]
40992. Zinc plating of s-832-2 pem clinch nuts [New York]
40993. Wood grain finish on anodized aluminum without mechanical pre-treatment [Sweden]
40994. Need method to clean black spots from hard anodized dye black water sealed on die cast [Pennsylvania]
40995. Avoid SS Side Etching [Taiwan]
40996. Metal finishing in vibratory [Pakistan]
40997. Galvanic corrosion between brass component and aluminum conductor [India]
40998. Need Black-T Coating [Texas] {6/7/06}
40999. Electro-polishing of stainless steel vessels and pipes [India] {6/7/06}


The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.