39000. Plasma Teflon Coating [India]
39001. Gold Nickel Adhesion decreased due to oxide layer [Minnesota]
39002. Metal finish similar to grinding but without using a grinding machine for metal plates [India]
39003. Need steel tanker desk refinished [California] {1/13/06}
39004. Need chrome stripped from wheels then prepped and refinished [Virginia] {1/13/06}
39005. Need galvanized license plate bracket refinished [North Carolina] {1/13/06}
39006. CAT-A-LAC 643-1-1 ALUMINUM PAINT SOURCE? [California] {1/13/06}
39007. High heat resistant for BBQ coating [Malaysia] {1/13/06}
39008. Recipe to oxidize brass, copper and pewter [Australia]
39009. Plating School? [Pennsylvania]
39010. Bonding polyurethane tread to a nylon 6/6 30% glass filled hub [Michigan]
39011. What's "thick Au" ? [China]
39012. What wear plating is best for hard S7 steel and corrosion resistant to bleach? [Nevada]
39013. Roughness/pitting on flat vertical surfaces in Bright Ni [Australia]
39014. Nickel plating of inner diameter [Serbia]
39015. Color variation on conversion coated aluminum [Canada]
39016. Want a visual Ra comparision chart [Wisconsin]
39017. Sulphuric acids additions via a stainless pipe [Ireland]
39018. Need ceramic coating applicator [Canada] {1/16/06}
39019. Aluminum basket in stainless steel stock pot [Texas]
39020. Remove calcium from Nickel Sulphate solution [India]
39021. Need High Gloss (Mirror) Finish on our pressure cast aluminum components [India] {1/17/06}
39022. Measuring surface conditions on anodized aluminum extrusions [Georgia]
39023. Paint removal for old cast iron stove [Pennsylvania]
39024. Not able to get more than 950 HV hardness in hard chrome plating consistantly [India]
39025. Looking for someone in the world to do silver electroforming on non conductive small objects [Australia] {1/17/06}
39026. Zinc coating thesis [Philippines]
39027. Hard anodizing of aluminum cookware costing and setup parameters [Egypt]
39028. Specimen preparation for electrochem testing [Indonesia]
39029. Alternative to zinc and colour customer asking for trivalent finish on future orders [England]
39030. Definition of blackening stainless steel [Massachusetts]
39031. Could you help me about step and thickness of plating? [Thailand]
39032. Pickling and Passivation bath for stainless steel 316Ti [Hong Kong]
39033. Inspection of ZAMAK coated with Ni/Cr [Egypt]
39034. Want to do "bad" electroforming [UK]
39035. Corrosion caused by incorporation of drag-out? [California]
39036. Masking Film Usage [Ohio]
39037. How to depassivate stainless steel for nitrocarburizing [Peru]
39038. Measure free fluoride ions concentration without adding any buffer or ph collecting solutions [India]
39039. Chrome, Cad, Zinc or Nickel plating best for Paper Machinery [Canada]
39040. Anodizing for Mic-6 and C-250 [Israel]
39041. Need my Yamaha frame polished [Illinois] {1/17/06}
39042. Need fenders dipped [Florida] {1/17/06}
39043. Plastic pieces triple coated to give chrome finish [New Jersey] {1/17/06}
39044. In search of shop to strip and powder coat 4x19" Rims [Texas] {1/18/06}
39045. Need anodizing of a cast aluminum part with some stainless pins [California] {1/18/06}
39046. Need aluminum processing chemicals (Alodine, Iridite, Accelagold) per MIL-C-5541 [Texas] {1/18/06}
39047. Need technology license and electroplating machine for diamond dental burrs [Turkey] {1/18/06}
39048. Looking for a used Taber Abrader [Kentucky] {1/18/06}
39049. Browning a sheet of copper to use for a kitchen island [Ohio]
39050. K-v problem [Oklahoma]
39051. RoHS compliance plating [California]
39052. Tantalum polishing [Hong Kong]
39053. How much gap between anode and cathode for plating? [India]
39054. I need to dull the burnished areas of an aluminum trailer [Ohio]
39055. Solder removal from gold coins [Nevada]
39056. Pin holes and pitting in copper plating of Ni Cr plated plastics [India]
39057. Electropolishing [India]
39058. Need silver plating over aluminum [Maryland] {1/19/06}
39059. Need SureCoat Gun [Canada] {1/19/06}
39060. AMS, MIL-SPEC CONVERSION TABLES [Kansas]
39061. Need to plate Tin to specification ASTM A599M, is it Electroplating? [Mexico]
39062. Tarnish Resistance Coating for Silver [New Jersey]
39063. Looking for wood-grain lamination on aluminum [California] {1/19/06}
39064. Dry chemicals to solution [Washington]
39065. Removal of discoloration on stainless steel caused by plasma cutting [New Jersey]
39066. SS got burr after stamping [Singapore]
39067. Home painting of aluminum sheet [South Africa]
39068. Help - need info on AMS 2433B spec [Massachusetts]
39069. Reducing energy waste in baking coated aluminum/steel parts [Malaysia]
39070. I live in a warehouse with a zinc plating co. [Canada]
39071. Leadframe Plating, NiNiP vs Full Ni (without NiP) [Philippines]
39072. Brownish red gloppy stuff in copper plating experiment [Illinois]
39073. Variegated appearance in sulfuric anodic coating [Costa Rica]
39074. Electroless chemical polishing of stainless steel parts [Canada]
39075. Can steel be silver plated? [New Hampshire]
39076. Used trumpet has some kind of rusting under the keys [Idaho]
39077. Custom etching of gun barrels [Oklahoma]
39078. Faded black stereo components: Can black color be restored? [Virginia]
39079. Need Bright Aluminum Finish - Mirror Like [Georgia]
39080. Need alternative to cyanide stripping of gold [New Hampshire]
39081. How to refinish my grandpa's tin bread box [Florida]
39082. Galvanizing plant [Ethiopia]
39083. Spalling of Sulfuric anodized (Black) 2024 aluminum [California]
39084. Electropolishing: History facts wanted [Germany]
39085. Electroplating, electrocoating, electrodipping [Hong Kong]
39086. Need plating on ZA-27 Alloy with satin finish [California] {1/20/06}
39087. Detection of oil/grease on aluminum surface [India]
39088. Sandblasting WC-Co inserts before coating [Czech Republic]
39089. Joining Polypropyene Sheet [New Zealand]
39090. Metal finishing to blacken silhouettes [Montana]
39091. Need PTFE coated onto gold plated nitinol wire [Colorado] {1/20/06}
39092. Aerospace epoxy primers [UK]
39093. Name of machine that makes aluminium roofing sheets [Nigeria]
39094. Chrome plating wheels [Georgia] {1/20/06}
39095. Laser Etching Soft-Touch Paint [Illinois]
39096. Oxidizing laser engraved jewelry [New Jersey]
39097. Removing Paint from Copper Ship Lanterns [Canada]
39098. Test methods to distinguish hot dip galvanizing and electroplating [India]
39099. Need chrome plating for motorcycle parts [Texas] {1/20/06}
39100. Pot metal manipulation [Virginia]
39101. Need my bumpers plated [New Hampshire] {1/23/06}
39102. Need Brass Bed Cleaned [Texas] {1/23/06}
39103. Would like to have some engine parts stripped and dipped in Chrome [Florida] {1/23/06}
39104. Need replating of nickel onto inside of solid copper crepe pan [Texas] {1/23/06}
39105. Want plasma electrolytic oxidation equipment [Pakistan] {1/23/06}
39106. Need info on TD coating [Georgia] 2nd Request
39107. Need on-site removal of sharp protrusions on sheet shear bed [New Jersey] {1/24/06}
39108. Need hot bluing of steel tubing [Canada] {1/24/06}
39109. Want technology for coating on pistons [Pakistan] {1/24/06}
39110. Want automatic makeup and analysis of metal cleaning solution [Wisconsin] {1/24/06}
39111. Biosorption of heavy metals using fungal biomass as adsorbent [India]
39112. Filter press cloth cleaning [Malaysia]
39113. MAGNETIC INFLUENCE OF ANODIZE COATING [Israel]
39114. Black anodized aluminum [Belgium]
39115. Looking to Powder Coat wheels [New York] {1/24/06}
39116. Vacuum Metallization on plastic parts needed in USA [California] {1/24/06}
39117. Need black chrome coating for Ti / Ni parts [Utah] {1/24/06}
39118. Electro Polishing Machine [Malaysia] {1/24/06}
39119. Removing rust from powder coated surface [California]
39120. Abrasion Resistance plating for 300 Series stainless steel [Missouri]
39121. Looking for a source for Dow plating [California] {1/24/06}
39122. Need to set up a Galvanizing plant [India] {1/24/06}
39123. Steel Smut Composition [Australia]
39124. Ruthenium plating onto titanium [North Carolina]
39125. Prep for Anodized Aluminum Bumpers? [New Jersey]
39126. Desire info on chrome plating plastic and metal, and on vacuum forming plastics [Ohio]
39127. Replacement idea for glass heaters in EN bath? [India]
39128. What will be problem having pinholes and pitting when doing hardchroming? [Singapore]
39129. Surface finish and cracking of anodized 7075 [Illinois]
39130. Cleaning oxide layer thermal deburred parts [The Netherlands]
39131. Hot water tank-s.s 316L 317L [Chile]
39132. Need porcelain enameling service [Pakistan] {1/25/06}
39133. Need powder coating stripped from (not) hoffman boxes [Florida] {1/25/06}
39134. Need Teflon coating on SS304 sheet [India] {1/25/06}
39135. Corrosion of stainless steel by 1M sulfuric acid [Korea]
39136. Differences between Trivalent Zinc Clear vs. Zinc Yellow Chromate (289A) [Mexico]
39137. RoHS testing for Hex chrome in chrome plated brass [Virginia]
39138. PVC glue - At what low temperature does PVC glue not mend [Maryland]
39139. Coating Molybdenum foil with 0.5um Electroless Nickel Coating [Israel]
39140. Problem with rhodium pen plating process [Greece]
39141. Micro Kote and Tri-Ni finishing [China]
39142. Need Anti-Gall coating on screws [Connecticut] {1/25/06}
39143. Want to run Decoral oxide process [Pennsylvania] {1/25/06}
39144. UK Distributers (Other than Mankiewicz) of Nextel products [Scotland] {1/25/06}
39145. Mil-C-5541 Electrical Resistance Testing [California] {1/25/06}
39146. How to make sulfuric acid [Georgia]
39147. Pitted stainless bath grab bar [Connecticut]
39148. Making steel look like old dutch silver [California]
39149. Chromate conversion alternative for aluminum heat sinks? [Illinois]
39150. How to bond PVDF sheets into a steel tank [UK]
39151. POWDERCOAT TEST PROCEDURES NEEDED [Florida]
39152. For finishing of M2 steel, is blackening suitable? Application is for -170 degree celcius [Singapore]
39153. Electroless Ni Plating over BeCu and surface imperfections [California]
39154. Corrosion protection and electrical conductivity of magnesium die cast alloy substrate [Illinois]
39155. Stripping plastisol from plating racks [California]
39156. Need stripping and rechroming of weld star wire automobile rims [New York] {1/26/06}
39157. Need unichome plating on u-bolts [Texas] {1/26/06}
39158. Lost the results of my daughters science experiment [Georgia]
39159. Estimated cost of precipiating heavy metals out of a solution [Texas]
39160. Zinc plating at home for newbies [Norway]
39161. Polished Brass Faucets - Can they be Re-plated? [Ohio]
39162. Headlight reflectors of my vintage car [Philippines]
39163. COLOR CLASS 3 [Texas]
39164. Passivating 304V SS single-use medical device [Pennsylvania]
39165. Looking for coating for temp and corrosion requirements applied to complicated geometry [Michigan]
39166. Will powder coat bond to a kitchen sink to restore the porcelain look? [Indiana]
39167. Plating over aluminum starts peeling [Philippines]
39168. Anode dimension for better anode consumption [Philippines]
39169. Peeling off and brittleness in the epoxy coating [India]
39170. Getting copper coating on non-conductors [South Africa]
39171. Matt Black Finish Required [England]
39172. Causes of solder tombstoning effect? [Philippines]
39173. Coating with Al a beryllium mirror covered with a thin 125microns optical layer of nickel [Chile]
39174. Looking for company doing tin cobalt plating on casting parts [Malaysia] {1/26/06}
39175. Want black chrome for motorcycle [Tennessee] {1/26/06}
39176. Need 2 lamp bases plated in brass or similar look [Florida] {1/26/06}
39177. Seeking auto body acid dipping shop [Indiana] {1/26/06}
39178. Need titanium anodizing equipment and supplies for low-volume production [India] {1/26/06}
39179. We want a finish for cast iron which lasts long and is wooden grain [India] {1/26/06}
39180. Blackening copper for computer cooling [Ohio]
39181. Plating gold without cyanide [Australia]
39182. Galvanized wall covering - HUGE QUESTION [Arizona]
39183. Will copper color change indoors [Texas]
39184. Clearcoat required for Countertop Refinishing [Canada]
39185. Parkerized Coat v. Hard Anodizing Coat v. Powder Coat [California]
39186. Need process for Acid Zinc plating with trivalent black passivation [India]
39187. Oxalic Acid Spot Test as per AMS 2485-J (Coating Black Oxide) [France]
39188. Electroless Nickel-Zinc Plating [Australia]
39189. Surface finish specs for ElectroDeposited Zinc plating [California]
39190. Friction Hinge problem [Ohio]
39191. Need my bumpers rechromed [Georgia] {1/26/06}
39192. 50% Sulfuric Acid Tank [Tennessee]
39193. Require small amount of potassium cyanide [Florida] {1/26/06}
39194. Patina on kitchen cabinet (not a gun) [Utah]
39195. Hardness of white gold vs. yellow gold [Canada]
39196. What we should do to reduce the fluctuated dross in a bath? [Macedonia]
39197. How to best improve our pretreatment cleaning process? [Iowa]
39198. Hydrochloric Acid Test after Permanganate [Indiana]
39199. Porosity problem [Malaysia]
39200. Hard materials with little wear resistance [Michigan]
39201. Need Copper Sulphate / Copper Oxide [India] {1/27/06}
39202. How do I set-up a galvanizing plant [South Africa] {1/27/06}
39203. Need used paint booth [Georgia] {1/27/06}
39204. Need 3 to 6 Kw Teflon or PTFE heaters [California] {1/27/06}
39205. Black chrome plating using ionic liquids [UK]
39206. LOW VOC verus ISO free - which is safer? [Canada]
39207. Cleaning copper disc without abrasives [England]
39208. Green collection on copper tubing - is this a serious situation ? [New York]
39209. Voltage/amperage relationships in plating baby shoes [Israel]
39210. Crevices and powder coating [India]
39211. Alternative to chrome in place of sealing after anodizing [India]
39212. Right method of PT of HR sheet [India]
39213. Want wear resistant alternative to chrome plating for copper dies [Kentucky]
39214. Need boron reduced electroless nickel plating [Pennsylvania] {1/27/06}
39215. Want black chromium on my bike parts [Tennessee] {1/27/06}
39216. Looking for a company can give us powder coating services in Phoenix [Arizona] {1/27/06}
39217. Need polypropylene balls [India] {1/27/06}
39218. Teach me to make nameplates [Missouri] {1/27/06}
39219. Looking for a process: color etch on stainless steel [Canada] {1/27/06}
39220. Air compressors [Pakistan] {1/27/06}
39221. Roughness vs Tensile Strength [Indonesia]
39222. Migration of aluminum through copper plating [India]
39223. Can an aluminum piston be plated to restore compression? [Pennsylvnia]
39225. Rhodium analysis-Rh metals and rhodium minerals [Korea]
39226. Remove copper buildup on carbide tooling balls [Tennessee]
39227. Scratch resistance of powder coating on metal [Michigan]
39228. Anodizing sputtered Ti film [Ohio]
39230. Peel-off strength of Electroless Nickel on Aluminum [UK]
39232. Peel off problem in lead-free plating [Philippines]
39233. Brown staining of Cr III conversion coating with a lithium based sealant [UK]
39234. Analysis of Anodized Aluminum Part shows Strontium [Utah]
39235. Fingerprints [Indiana]
39236. Cleaning of aluminum investment castings [India]
39237. Corrosiveness, Rusting of Pre-Hardened P-20 Steel [Indiana]
39238. Looking for electropolishers [Connecticut] {1/31/06}
39239. Re-chroming a 1999 F-250 front bumper [South Carolina] {1/31/06}
39240. Need replating of our bathroom plumbing fixtures [Illinois] {1/31/06}
39241. Need mortise door lock hardware cleaned and plated satin nickel [Alabama] {1/31/06}
39242. Seeking bright chrome plating for high volume production of luggage racks [Michigan] {1/31/06}
39243. Need anodising equipment [India] {1/31/06}
39244. Need quotation for some plating products [Peru] {1/31/06}
39245. Need transparent colored coatings for light bulbs - range of colors [Massachusetts] {1/31/06}
39246. Galvanization Measurement Instrument for Galvanized Steel Sheet Metal [Egypt] {1/31/06}
39247. Need coloring kits for inlaying letters/numbers on firearms [Wisconsin] {1/31/06}
39248. Need Nickel S-Rounds [Ohio] {1/31/06}
39249. Need Used Plating Equipment [Ohio] {1/31/06}
39250. Need consultant for manufacture of phosphating chemicals [India] {1/31/06}
39251. Which is better, stainless steel or anodized aluminum? [New York]
39252. Treeing (dendrites) in Ni Sulfamate Electroforming [Virginia]
39253. Food processor drive shaft [Washington]
39254. Voltage and sulfate requirements [Indiana]
39255. CHROME VS STAINLESS STEEL [Illinois]
39256. Iridite 14 - 2 Testing procedure [Arkansas]
39257. Removal of coating from Stainless Steel? [Michigan]
39258. What is proper method for finishing Cast iron surfaces in two pack PU [pre-treated with sand blasting] [India]
39259. Problems with black powder coating [UK]
39260. Rust on Electroless Nickel Coated Motors [Kentucky]
39261. Sulfamate nickel plate over 304L stainless steel in a high speed rotating member [Texas]
39262. Decorative Nickel -Chrome plating on SS 409 Silencers [India]
39263. Chemical Polishing of 2014 aluminum alloy [Portugal]
39264. A durable coating for an aluminum diecasting [Pennsylvania]
39265. Cleaning Fingerprints From Clear Trivalent Conversion Coated Aluminum [Washington]
39266. Which one is the best stainless steel [India]
39267. Need tin-zinc plating for my fasteners [Thailand] {2/1/06}
39268. Seeking supplier to provide plating per GMW 4700M [Michigan] {2/1/06}
39269. Want Skinpass Line [Iran] {2/1/06}
39270. Need olive drab chromate touch up process [Pennsylvania] {2/1/06}
39271. Selective etching of Ag (silver) [Pennsylvania]
39272. Salt Spray Test Specification for NC Acrylic Paints [India]
39273. Gavanneal Popping or Outgassing in E-Coat [Michigan]
39274. Why it is necessary to add boric acid to acid tin bath plating [India]
39275. How to reduce brittleness in Nickel Plating [India]
39276. In need of an Aluminum Bright Dip that does not contain nitric acid [Kansas]
39277. Why do we use 15-18%HCl for pickling [India]
39278. Surface Contamination of Stainless Steel Resulting in Red Rust Spots [Florida]
39279. Looking for paint removal, acid dip, neutralize and e-coat for old car fenders doors [Ohio] {2/1/06}
39280. NEED A BLACK COATING [South Dakota] {2/1/06}
39281. Seeking "Kanigan Niptef" finish [Ohio] {2/1/06}
39282. Who can advise on Conductive coating of Glassdoors for Display Refrigerators [Swaziland]
39283. Need release agent and two pack paint for in mould coating [Australia] {2/2/06}
39284. Safe disposal of liver of sulphur used on silver [Florida]
39285. Stainless steel turns black upon sterilization [England]
39286. Anodizing film color is wrong [Pakistan]
39287. BIG problem with black powdercoat on 7/8" 14 gauge HR tubing [New York]
39288. Recommended plating for automotive connectors [The Netherlands]
39289. Nickel Stripping from Brass Material [Pakistan]
39290. Rhodium Pen Plating Problem [India]
39291. Adhesion of Cr/Gold on oxidised wafer [India]
39292. Pt plating: surface finish versus allowable strain [California]
39293. I WANT TO REMOVE RUST CONTAMINATION FROM 347-H SS PIPE IN THE FIELD [Oklahoma]
39294. Nylon 66, glass filled - etching the surface in preparation for adhesive bonding [Ohio]
39295. De-coating of HSS and Tungsten Carbide tools [South Africa]
39296. Nitric acid in anodizing bath? [Costa Rica]
39297. Metallized European skull mounts [Oklahoma]
39298. Hot dipped galvanized bracket on stainless steel pipe [New Zealand]
39299. I NEED A CLEAR COAT AND PAINT SYSTEM FOR WOOD CRANKBAITS [Kentucky] {2/2/06}
39300. Having adhesion problems when painting urethane to urethane? [California]
39301. Need bathroom faucets refinished from chrome to oil rubbed bronze [Texas] {2/2/06}
39302. Looking for Zinc -Trivalent Yellow Chromate plater [Illinois] {2/2/06}
39303. Seeking brush plating for new auto body letters and logos [Pennsylvania] {2/2/06}
39304. Need A Vapor Degreaser [Texas] {2/2/06} 39305. Matte tin finish for electronic components [Massachusetts]
39306. Need immersion tinning process [Italy] {2/3/06}
39307. Need consultation to set up a manufacturing plant for epoxy powders [India] {2/3/06}
39308. Additives for acid zinc chloride [Argentina]
39309. Trivalent Chromium Passivation [England]
39310. Galvanize adhesion problem [UAE]
39311. Brushed Nickel [Turkey]
39312. Chromizing of cold rolling work rolls [Egypt]
39313. Regarding specification for saccherometer in phosphating [India]
39314. Attaining a superior finish in stellite with lapping emeries [India]
39315. Need Electroforming Equipment Processes and Supplies [Nevada] {2/3/06}
39316. Rate of oxidation on metals [Georgia]
39317. What solution should I use for electroplating with copper? [Missouri]
39318. How can I find weight percent of alumina in composite coating? [India]
39319. Where can I get a ball hone, 240 grit, Aluminum oxide to use on Nikasil [Washington]
39320. Experimenting with Steel Patinas [New York]
39321. Metallic blue ceiling lights [California]
39322. Sponge plating [New Jersey]
39323. Galvanized finish RoHS compliant? [Illinois]
39324. Pre galvanized steel RoHS compliant? [California]
39325. Welding on chrome plated surface [Canada]
39326. Powder coating standard [Mexico]
39327. Plasma Nitriding on Steel Tubing [Illinois]
39328. Bluish Color of Sn-plating over Ni After 3X Reflow (eak Temp @ 260degC) [Philippines]
39329. Cathode material for Chromic Acid [Illinois]
39330. Citric vs Nitric Passivation [California]
39331. Contaminated 2mm and 4mm drilled holes from machining [Colorado]
39332. Corrosion Resistance Needed for Steel Stampings with Tight Flatness Requirements [Canada]
39333. Nickel Plating? [California]
39334. Brass chandelier needs re-plating [California] {2/6/06}
39335. Need inorganic high ratio zinc silicate coating to astm b117-63t [Connecticut] {2/6/06}
39336. SS Passivation techniques for home shops [California]
39337. HOW MANY MICRON IS 23 KARAT IN GOLD PLATING [South Africa]
39338. Need media blasting shop in Miami area [Florida] {2/6/06}
39339. Enamel for Storage Water Heater [Malaysia] {2/6/06}
39340. What dissolves gold [South Africa]
39341. Colorless alodine [Romania]
39342. Aluminum 1100 Grain Boundary Etch [Massachusetts]
39343. Cleaning/Sealing copper flashing [North Carolina]
39344. Need help with Iron Plating using Ferrous Iron Fluoborate Process [Mexico] {2/6/06}
39345. Getting even finish with chromate conversion [Pennsylvania]
39346. Needing tail-light and hood ornament rechromed [Indiana] {2/6/06}
39347. Hazards of Tin-Bismuth Alloy at High Temperature [Texas]
39348. RE SURFACING HURRICANE LAMPS [Florida]
39349. Aluminum Corrosion [Washington]
39350. Shelf life extensions for Magnesium treatment AMS M-3171 Type VI [California]
39351. What paint do I use for mural on an aluminum fishing boat? [Oregon]
39352. I need help on making my own conductive paint to make flowers plating [Mexico]
39353. Looking for a shot blasting jobshop in Pune [India] {2/6/06}
39354. Heat-coloured titanium [Australia]
39355. Coating on inside surface of aluminum tubes used in heat exchangers [India]
39356. About cleaning section of anodizing aluminum [Turkey]
39357. How long will it take for electrolysis to eat through a copper pipe? [Oregon]
39358. White Bronze or Imitation Rhodium [Pakistan]
39359. Need rechroming of car wheels [Illinois] {2/7/06}
39360. I would like to find a good rechromer [South Carolina] {2/7/06}
39361. Need metal marking machines [China] {2/7/06}
39362. Need a set of cabinet hardware replated with copper [Virginia] {2/7/06}
39363. Need chrome door lock replated [Canada] {2/7/06}
39364. Finger prints on stainless steel [Oregon]
39365. Powder coating to coat a steel gas tank [California]
39366. Hexavalent Chromium Removal from Groundwater Leachate [Pennsylvania]
39367. Tell me about bright nickel [Colorado]
39368. Tank stripping of kitchen cabinets [New Jersey] {2/8/06}
39369. Need New Tank and Chemical Suppliers [Utah] {2/8/06}
39370. Zinc removal from wastewater [Pennsylvania]
39371. Painting tin plated aluminum [Pennsylvania]
39372. Yellow Foam Mold Coatings [California]
39373. Need to know how to coat a ceramic coffee cup with powder paint [India]
39375. Late developing white stain on black oxide [Pennsylvania]
39376. PVD Titanium Nitride : Why gold color did not in same shade around workpieces? [Thailand]
39377. Electroless Nickel Immersion Gold vs. Immersion White Tin [Florida]
39378. Have new polymer that is not glass filled, need conductive coating [California]
39379. Reduction of lead impurities on lead free plating solution [Philippines]
39380. Metal chips [Philippines]
39381. 17-4 Hot Roll [California]
39382. Stainless Screws binding on stainless PEMS [Connecticut]
39383. Need T-Fal Coating or equivalent [California] {2/9/06}
39384. Need a vendor to bronze a firefighters uniform [California] {2/9/06}
39385. Seeking anodization of bicycle rims, spokes [Missouri] {2/9/06}
39386. Need Nano Metal Powder of Silver, Gold, Copper, Nickel etc [India] {2/9/06}
39387. Cleaning Ti [Florida]
39388. Urgent questions about acid wash for steel! [Texas]
39389. Is it possible to return to the aluminum look for aluminum with bronze finish? [Illinois]
39390. TRICHLOROETHYLENE REPLACEMENT [Canada]
39391. Unknown microfinish symbol [Michigan]
39392. FEP teflon coating process [New Jersey]
39393. EFFECT OF SILVER BRIGHTENERS ONTHE ELECTRICAL CONDUCTIVITY [Mexico]
39394. High conductivity plating on beryllium copper or not? [UK]
39395. Selective removal of AlF and AlxOyFz contaminates from anodize surface [Arizona]
39396. ELECTOLYTIC PICKLING [India]
39397. Do you plate PFZnNi-5D? [Missouri] {2/10/06}
39398. Need sample pack of metal finishes [New Jersey] {2/10/06}
39399. Need good factory for spray and UV coating [China] {2/10/06}
39400. Seeking Classified Material Plating Shop [Texas] {2/10/06}
39401. How can I remove copper nickel layers from a copper core without attacking the copper core? [Washington]
39402. Fish eye problem in electroless nickel plating [India]
39403. Titanium Nitride Color during PVD process [India]
39404. ZINC PHOSPHATE TT-C-490 [Arizona] {2/10/06}
39405. Need lettering removed/filled in on rifle barrel [Arizona] {2/10/06}
39406. Building a platinum plating equipment for teaching [Venezuela]
39407. Cleaning of polishing mops [UK]
39408. Conductive, corrosion resistance aluminum [North Carolina]
39409. Treating Brass [New York]
39410. Need bananas plated [New York] {2/10/06}
39411. Need phosphoric acid anodize for aluminum sheet .016-.050. [Texas] {2/10/06}
39412. Selection of coating resistance value for coal tar enamel on pipe lines [UK]
39413. Specific conditions for titanium anodizing [Argentina]
39414. Re tinning a pot [Virginia]
39415. Hardness Measurement [Malaysia]
39416. Sulphuric Acid Resistance for Concrete Walls [Dominican Republic]
39417. How to maintain pH in rinse water tanks of pickling [India]
39418. HCL scrubber system [Malaysia]
39419. Phosphating Sludge Removal [Malaysia]
39420. Clear coating for copper pots - prevent tarnishing [Illinois]
39421. Electroless Nickel or Nickel Electroplate: Motorcycle Frame [Michigan]
39422. I want to electroform dead scorpions and bugs. Would this be like plating a flower? [California]
39423. Hard Chrome over Hard Chrome in Aerospace [Canada]
39424. Organic flux reaction on Type II yellow zinc plate [Illinois]
39425. Brushing aluminum to obtain grain [Canada]
39426. Pickling of steel rod [South Africa]
39427. Compatibility of Nitinol and Stainless Steel Stents [Germany]
39428. Seeking anodixed and protective coated 24g Aluminum [California] {2/13/06}
39429. Pvd coating machine for decorative and functional purpose [India] {2/13/06}
39430. Need vacuum metallizing equipment [India] {2/13/06}
39431. Zn 5CC DIN 4042 [India]
39432. Automotive paint ovens/thermal calculations [Iran]
39433. Problems with cad plating [Texas]
39434. Electrical properties of yellow zinc chromate on steel [Massachusetts]
39435. Masking for tin plating on nickel plated component [India]
39436. Stainless Steel Electro Polishing [South Africa]
39437. Pitting on a brass substrate [Oregon]
39438. Aluminum to Steel doors [Illinois]
39439. Need our brass parts pvd coated [India] {2/14/06}
39440. Changing the look of brass [North Carolina]
39441. Eliminating boron in waste water [Israel]
39442. Parylene Adhesion to Brass [California]
39443. Autophoretic chemical supplier [Iran]
39444. How to dry the parts after oiling on black oxide surface [China]
39445. Surface pitting on chrome plated PC/ABS [Indiana]
39446. How to keep nickel electroform bright in long term use? [Thailand]
39447. Arsenic Plating [Australia]
39448. Liquid mask [UK]
39449. Brass plating [New York] {2/14/06}
39450. DI water pilot plant [UAE] {2/14/06}
39451. Approximate investment for a chrome plating set up [India] {2/14/06}
39452. Titanium Anode Baskets [California] {2/14/06}
39453. NEED OF CHEMICALS AND MACHINERY FOR DIAMOND ELECTROPLATING [TURKEY] {2/14/06}
39454. Electropolishing of NiTi (nitinol) [Israel]
39455. Stripping Pitted Chrome from Aluminum Car Wheels [Georgia]
39456. Electrolysis in pet watering system [New Jersey]
39457. Galvanic Corrosion - Rheostat - Nichrome Winding - Brass Wiper [California]
39458. Blueing process [India]
39459. Perfect utilization of the steel pickling liquor [Egypt]
39460. HCl resistant coating for steel structures [India]
39461. Black spots in hot dip zinc coated wire [Sri Lanka]
39462. Electroless Nickel Plating for wet sour service applications [UAE]
39463. Phosphoric Acid Anodizing [Louisiana]
39464. Replacement for Hard Anodize in a Casting [Pennsylvania]
39465. Need Inexpensive Process to apply MIL-A-8625, Type III, Class 2 Anodize to Interior A356 Aluminum [Minnesota]
39466. Re-anodising aluminium [UK]
39467. Suitability of nimonics with acids [India]
39468. Aluminum casting into hot dip galvanised tube -outdoor use [UK]
39469. Seeking reconditioning of football facemasks [North Carolina] {2/15/06}
39470. Teflon coating on aluminum [Massachusetts] {2/15/06}
39471. Need process for titanium coating on cookware [Iran] {2/15/06}
39472. Plastic dip [Michigan]
39473. Zinc Embrittlement [India]
39474. Chromium and Electrocoagulation [UK]
39475. How to eliminate solvent popping in twin pack polyurethane paints [Ireland]
39476. EN over 304 Stainless [Connecticut]
39477. Tin plating copper parts with stainless (sus 302/303) hardwares, any problem? [Thailand]
39478. Acetic Acid for ph [Florida]
39479. Clear anodised parts are coming out pink [England]
39480. Aluminum Dust and how do you dispose of it properly after polishing? [Ohio]
39481. To prepare a coating of Ni-P-(ZnMn)Fe2)4-BaTiO3 by EL method [India]
39482. Copper effect of ammonium chloride on hot brass [UK]
39483. Teflon application on holders, skids and fixtures [Mexico]
39484. Powder Coat thickness tolerance on machined parts and holes [South Carolina]
39485. Furnace brazing / annealing and chrome plating [Italy]
39486. Curbed my rims [Florida] {2/16/06}
39487. Manual of the salt spray tester [Malaysia]
39488. Decreasing Copper Content of our Descaler Solution(Pre-treatment) [Philippines]
39489. How to make an Aluminum finish looks like blued steel [California]
39490. How to paint or "touch up" fake brass faucets? [Pennsylvania]
39491. Need BLACK ENDURION FINISH on steel rods [New Hampshire] {2/16/06}
39492. Heat Treatment effects- nickel plating [New York]
39493. Stripping of Electroless Nickel Plating on Brass [India]
39494. How much mileage can one get out of a pound of Chromic Acid in a conversion bath? [Ohio]
39495. 303 stainless and Hf containing pickle [Ireland]
39496. U.V. stable, anodized Aluminum [California] {2/17/06}
39497. Need my bumper rechromed [New York] {2/17/06}
39498. 18K gold plating [Oman]
39499. 6061 Aluminum boat part corrosion [Texas]
39500. Coating material NS 3100 F Metallic [Florida]
39501. CEE - BEE J-3 Tests [Arkansas]
39502. How to make chromating/alodine surface harder? [Malaysia]
39503. Why use Nitride [Florida]
39504. Dull finish galvanizing [Australia]
39505. WHAT IS THE DIFFERENCE BETWEEN PRE-GALVANIZED AND PRE-ZINC COATED? [Malaysia]
39506. Is standard anodizing acceptable for the pills ? [Illinois]
39507. 430SS become dull after chemical polish [Singapore]
39508. Copper on aluminum [UK]
39510. Liquid water [Ohio]
39511. Safety concern about grinding anodize coating [Oklahoma]
39512. Outhouse appearance wanted [Michigan]
39513. How to remove ink stains from a brushed stainless steel refrigerator? [Louisiana]
39514. Different results anodising aluminum grades 6061 vs 6082 using 'home setup' [South Africa]
39515. Stripping silver conductive paint from inside a copper mold [New York]
39516. Cyanide-iron complex treatment [Mexico]
39517. Electrolysis of water as a science fair project [Tennessee]
39518. What adheres paint to chrome? [Colorado]
39519. Sand Blasting - Standards [India]
39520. Copper exposed on parts that are supposed to be nickel [Philippines]
39521. Is Powder Coating best for adhering to stainless? [Indiana]
39522. Reverse Zinc Plating [New Mexico]
39523. Powder Coat Failure--Aluminum Railing [Tennessee]
39524. No Chemical Treatments In Waste System? [Pennsylvania]
39525. Need black chrome [New York] {2/17/06}
39526. DO PINHOLES IN THE RIMS MAKE AIR LEAK FROM THE TIRES? [Florida]
39527. Adhesive for Teflon belt ends joining [India]
39528. RoHS COMPLIANCY [Georgia]
39529. Need Calibration and Repair of Thickness Tester [Philippines] {2/17/06}
39530. Vacuum evaporation on glass beads [India]
39531. Nickel and tin recovery [Malaysia]
39532. Want know-how in imitation jewelry [India]
39533. Aqua bead blast specification [South Africa]
39534. Need low-copper salt for salt fog testing per ASTM B 117 [Arizona] {2/17/06}
39535. Cooling Tower Blockage [UK]
39536. Electroplating onto Aluminum (Nickel onto Aluminum) [India]
39537. Need aluminum reflectors [India] {2/21/06}
39538. Seeking brass polishing of fan blades in the Miami/Broward area [Florida] {2/21/06}
39539. Anodize aluminum bike components [Puerto Rico] {2/21/06}
39540. Zn plating plant and knowhow required [India] {2/21/06}
39541. Trying to get that mirror like finish on my Semi Truck Stainless trim [Georgia]
39542. Color plating motorcycle parts? [Colorado]
39543. Polishing Stainless Steel Bolts in Vibratory Tumbler [Wisconsin]
39544. Line graining small aluminum blocks - best practices [California]
39545. Need gold purity checking machine [India] {2/21/06}
39546. PCB Etching - Transfer process [Nigeria]
39547. Help drilling out a titanium bolt [Norway]
39548. Need gold colored appearance for my aluminum 17 in wheels [Florida]
39549. Need best cleaner for anodized antique copper plated items [Ohio]
39550. Need North American availability of European Aluminum Conversion Coating [Michigan] {2/22/06}
39552. Need a line for pickling of carbon steel sheets with environment friendly process [India] {2/22/06}
39553. Looking for Sales Rep Company [Ohio] {2/23/06}
39554. Require Electronic Laser Engravure Machine for Cylinders [India] {2/23/06}
39555. Zinc plating and Cr6 [Pennsylvania]
39556. High Copper Concentrations in Treated Wastewater [Singapore]
39557. Bus bar rating [India]
39558. Sodium Dichromate Testing? [Arkansas]
39559. Epoxy Paint (MIL-PRF-22750) Over Anodized Aluminum [Virginia]
39560. Salt bath nitriding Vs TiN [India]
39561. Reworking electroless nickel plating [California]
39562. Inactive chrome electroplating bath [Iran]
39563. Aluminum Bright Dip [Kansas]
39564. Corrosion problem after phosphating process [Indonesia]
39565. Post-cleaning passivated stainless steel parts cres 303 type [New Mexico]
39566. Zinc Phosphate and Protecting Aluminum [Florida]
39567. Mn-Phosphating SST hrs life [India]
39568. Need rhodium plating solution [Vietnam] {2/23/06}
39569. Clear durable coating needed for mirror finish stainless steel sheets [Texas] {2/23/06}
39570. Need Halar (ECTFE) Powder Coating [Montana] {2/23/06}
39571. Seeking crusaval [Pakistan] {2/23/06}
39572. Need blasting rooms, new or used [Florida] {2/23/06}
39573. Need platinum wire electrodes [Canada] {2/23/06}
39574. Stainless steel spoon that have darkened during normal use [Arizona]
39575. Does chrome gets converted to hexavalent chromium after hard chrome plating [India]
39576. 2 problems with TOC during analyzing the electroplating solution [Hong Kong]
39577. Rust inhibiting coatings for steel hinges [Pennsylvania]
39578. CrN on Steel [Ohio]
39579. Heat resistance on aluminum diecast part finished with Alodine [Hong Kong]
39580. Chromic anodizing process [Canada]
39581. Pickling after glass-blasting [Turkey]
39582. Use of 316L for marine propeller [Thailand]
39583. Need Black Chem Film [California] {2/23/06}
39584. Need chrome plating of a plastic center hub [California] {2/23/06}
39585. Need to Get A Sword Powder Coated [Canada] {2/23/06}
39586. Can you powder coat a pistol? [Oregon] {2/23/06}
39587. Looking for a paint booth [Pennsylvania] {2/23/06}
39588. Need 1 gallon of pre-mixed Alodine 1500 [New York] {2/23/06}
39589. Teflon Food Grade Coating [California]
39590. Vapor blasting a lambretta scooter [England]
39591. Polishing aluminum rims for a dull matte finish [Arizona]
39592. Yellowing of stainless steel tailpipes [New York]
39593. Tolerancing based on delta E [Georgia]
39594. My black oxide won't turn black [New York]
39595. White rust problem [Jordan]
39596. Corrosion Resistance for Conversion Coat (MIL-C-5541 Class 1A) [Korea]
39597. Coating for aluminum parts [Canada]
39598. Compatibility of aluminum rivets on a stainless steel substrate over time [Texas]
39599. Seeking stainless steel polisher to remove scratches on new refrigerator [New Jersey] {2/24/06}
39600. Need immersion tin plating process for flexible copper clad laminates [India] {2/24/06}
39601. Need silver recovery cell [Saudi Arabia] {2/24/06}
39602. Why alodine steel [Pennsylvania]
39603. Chrome touch up for repairing some peeling [Vermont]
39604. Zinc plating on 1144 CF Stressproof material [Pennsylvania]
39605. Ni Plate melting? [Scotland]
39606. Test for Nickel and or Chrome plating thickness on brass substrate [Oregon]
39607. Have 68 Oldsmobile trying to restore, need chrome re-finished or dipped [Delaware] {2/24/06}
39608. Dongguan Area Anodize [China] {2/24/06}
39609. Looking for microsection equipment [Texas] {2/24/06}
39610. How to convert to CO2 concentration as the resistivity of DI water known [Singapore]
39611. Dubpernell test method [Mexico]
39612. Chemical to strip coated jig [Malaysia]
39613. Electroplating Gold with Gold Anodes [Connecticut]
39614. Gold plating blistering on a copper terminal [Mexico]
39615. Electrocleaner lifespan and testing [Pennsylvania]
39616. Solidification/stabilization technology for heavy metal laden waste [India]
39617. How to paint plastic car molding [Canada]
39618. Black deposits developing between a stainles steel sliding contact and galvannealed coating [Minnesota]
39619. What is causing this on Zinc electrodeposit? Hydrogen Entrapment? [Mexico]
39620. Potassium hydroxide pre-clean solution temp inquiry [Philippines]
39621. Seeking Chrome Plating of 1954 Chevy PU grill [Washington] {2/24/06}
39622. How do I restore an object with so much rust? [South Carolina]
39623. Corrugated iron roof nightmare...Suggestions? [Canada]
39624. Heat resistant clear coat needed for my copper plated stove [North Carolina]
39625. Looking for professional spray painter in Toronto to spray chrome bookcases? [Canada] {2/28/06}
39626. Restoration of 50's Chrome table and chairs St. Louis area [Missouri] {2/28/06}
39627. Seeking market research data, final finishes [Hungary]
39628. Simple Electroplating [Illinois]
39629. Gold Electro Chemical Deposition using Cyanide Solution [Singapore]
39630. CrVI residue on hard chrome plated suface [India]
39631. Stick the diamond crystal onto matrix [India]
39632. What clear coat can protect against fingerprints and stains on copper parts in a high temp environment? [Florida]
39633. Vacuum impregnation [California]
39634. Nickel Gold Plating [Philippines]
39635. Need portable silver extracting machine [Botswana] {3/1/06}
39636. Welding on boriding surface [India]
39637. At what temp. will a custom brass and copper fireplace surround discolor? [Pennsylvania]
39638. GILLESPIE ANTIQUE RESTORER [Kentucky]
39639. How to clean a WW 1 bayonet [Tennessee]
39640. Removing chrome from aluminum [New Jersey]
39641. ANNOUNCEMENT: OSHA issues 5 micrograms of Cr(VI) per cubic meter of air as the new 8-hour PEL value. [California]
39642. How to Break a Tin Gel [Indiana]
39643. Rhodium electroless - problem [Poland]
39644. Insulation resistance in zinc plated olive green passivation in comparision with zinc plated yellow passivation [India]
39645. Lead-free, Zinc ED plating [Singapore]
39646. Elimination of descaling after heat treatment in chain plates [India]
39647. Calculation for correct volts and amps for electropolishing [Pennsylvania]
39648. How could I get a "No 4 Ground Finish"? [Colombia]
39649. Hardening aluminum for nikasil coating for high pressure [Michigan]
39650. Brushed nickel finish on aluminum [Canada]
39651. Setup a small factory to galvanized angle-bar 16ft x 2" x 2" manufacturing [Singapore] {3/1/06}
39652. Need heat seal lacquers for aluminum to plastic [Iran] {3/1/06}
39653. Need process chemistry for trivalent passivation [India] {3/1/06}
39654. RoHS testing for Cr6 under paint [New Zealand]
39655. McDonnel Douglas STF1004? [Alabama]
39656. Testing method [Iran]
39657. How can I make beautiful black patination on copper? [India]
39658. Cataphoretic coating of tantalum carbide [India]
39659. Possibility to spray the water-based Telfon material onto the stainless steel material S304 grade [Singapore]
39660. Mixing Practice and Keeping Induction Time for Painting [Korea]
39661. Powder coating peels off, when a bolt is tightened on a punched hole in sheet metal door [India]
39662. Poor coverage of electroless copper on polyester [India]
39663. Hard anodizing process [Vietnam]
39664. Parts cleaning problem [Illinois]
39665. Is Black Oxide MIL-C-13924 class 4 the same as Black Passivate? [Massachusetts]
39666. Process clarification on powder coating? [India]
39667. Brass faucet replating [Texas] {3/1/06}
39668. Need a supplier of bronze plating service [Spain] {3/1/06}
39669. Hard anodized coating thickness measurment gauge [India] {3/1/06}
39670. Need GPC and SPC powder [India] {3/1/06}
39671. Need polishing equipment for new project [Syria] {3/1/06}
39672. Protecting wrought iron: Samuel Yellin's work [Florida]
39673. SOLID BRASS TO OIL-RUBBED BRONZE [California]
39675. Lightening metal car parts [Pennsylvania]
39676. STEP test equipment [Connecticut]
39677. Removal of Cloisonne by Chemical Stripping [New Jersey]
39678. Test methods [India]
39679. Copper Electroforming, heavy (.25 inch+) deposits, problems with bubbles [Virginia]
39680. Chrome Plating vs. Ion Nitriting. Can the two be combined? [Ohio]
39681. What is the definition of room temperature for the plating industry [Massachusetts]
39682. Masking Problems [India]
39683. How to seal on a nickel plating surface? [China]
39684. Trouble in zinc plating already electroless nickel plated of low carbon steel casting valve [Illinois]
39685. Seeking cathodic epoxy electrocoat [Michigan] {3/2/06}
39686. Need to refinish 2 plates surrounding my white, 50 year old, gas stove burners [New York] {3/2/06}
39687. POOL CAGE Black Anodized Aluminum FADING...RE-Anodizing, is it possible? [Florida]
39688. Patent number of Kodak KPR3 negative photo resist? [Utah]
39689. Al-Si Alloy parts go moldy [China]
39690. How to solder on a nickel plating surface [China]
39691. How to prevent oxidation and finger prints from hand made bronze metal mirrors [India]
39692. Powder coating fiberglass body of 1934 Roadster-Frazer Nash [Texas]
39693. Galvanization line [Sudan] {3/2/06}
39694. NEED A 1000 LTR DAY WATER TREATMENT /R O / D M / INSTALLATION [India] {3/2/06}
39695. Need salt chamber [Poland] {3/2/06}
39696. Outdoor protection of bronze [Arizona]
39697. How to treat spent acid in pickling plant in cold rolled steel mill [India]
39698. CED Paint conductivity is dropping [India]
39699. Can't meet surface finish spec in grinding chrome plate [India]
39700. Want a hard thick coating for aluminum [Italy]
39701. Wanted for Gold Leafing on Wooden Picture Frames [India] {3/3/06}
39702. Need vermiculite coating on fibreglass webbing [UK] {3/3/06}
39703. Need Case Hardening on Firearms [Oklahoma] {3/3/06}
39704. Want Powder Coating of Alloy Wheels [Ohio] {3/3/06}
39705. Working on arsenic detection in lab [Pennsylvania]
39706. Electroless Pt [Virginia]
39707. Dark Metallic or Cobalt Plating [Canada]
39708. Removing severe lime scale from toilet bowls, shower doors and dishwasher [New Jersey]
39709. Chrome furniture [Puerto Rico]
39710. Is Black Oxide Coating on Fastners RoHs Compliant? [Ohio]
39711. Copper coating on aluminum wire [India]
39712. Increasing the hardness and high temperature resistance [Indonesia]
39713. Black Streaks in Chromic Anodize Salt Spray Panels [New York]
39714. Oxide film on stainless steel (X46 Cr 13, 1.4034) after eroding [Switzerland]
39715. Coating for aluminum 7075: H2S and NACE compatible [Canada]
39716. Help cleaning aluminum intake manifold [Virginia]
39717. Solder flakes on QFP packages [Malaysia]
39718. Problems with zinc plating coming off threads during die application [Iowa]
39719. Wash Primer to Prevent Filiform Corrosion Under Lacquer on Brushed Steel [Ohio]
39720. CHEMICALS/PROCEDURE /SYSTEM FOR MIRROR FINISH TO STAINLESS STEEL BALLS [India] {3/3/06}
39722. WOW! What a wonderful company! [Maryland]
39723. Ammonium Hydrosulphide v Liver of Sulpher [England]
39724. Epoxy Mold Compound : Why Toxic? [Philippines]
39725. Removing piston ring layer [Malaysia]
39726. UV withstandability of CED coating [India]
39727. Stainless knives rusting [Australia]
39728. How to make the aluminum surface to be like the skin of an orange(with lots of small surfaces to reflect)? [China]
39729. Need chrome over ABS plastic [Canada] {3/6/06}
39730. Relining Copper Pots [New York] {3/6/06}
39731. Need cast-iron kitchen sink re-enamelled (porcelain -- NOT acrylic !) [Virginia] {3/6/06}
39732. Need Powder Coating of MDF pieces [Washington] {3/6/06}
39733. Need Machine Shop to Turn/Re-surface 14" Mag. Wheels [Florida] {3/6/06}
39734. Need Gold Plating of BMX Bike Parts [Florida] {3/6/06}
39735. Silver plating [Nebraska] {3/6/06}
39736. Need anodized aluminium tubes for OPC drums laser printer [Malaysia] {3/6/06}
39737. Production e coat on small aluminum parts [Michigan] {3/6/06}
39738. Need white gold plating solution [New York] {3/6/06}
39739. Need small quantity of Incralac [Canada] {3/6/06}
39740. Need a source of yellow Macalube for fasteners [UK] {3/6/06}
39741. Periodic Table [California]
39742. Reactions between acids and metals [New Jersey]
39743. Aluminum, finishing of bar stock [Massachusetts]
39744. Will heating a copper pipe emit cyanide gas? [Louisiana]
39745. Copper Paint treatment [Mauritius]
39746. Aspiring millionaire scrap dealer, needs direction b4 ordering new Ferrari [Australia]
39747. What is essential to electroless nickel process? [Oregon]
39748. Rechroming golf clubs [The Netherlands]
39749. Painting a Shower Frame [Georgia]
39750. Marine grade anodizing for blocks, coolers, radiators [Massachusetts]
39751. What's the best way to strip chrome? [Pennsylvania]
39752. What is Fe/Zn 5 c 2C F-010 [Texas]
39753. Substitute for PVC lining to be used for D.M. water plants/ETP plants [India]
39754. How to determine the purity of nitric acid? [Philippines]
39755. Polishing of Tiny Brass Components [India]
39756. Surface Treatment [India]
39757. Volume resistivity of adhesives [India]
39758. Need an optimum painting method over a galavanised surface [Australia]
39759. Black Oxiding for Tin Electroplate? [Massachusetts]
39760. Zinc electrolyte specifications (galvanizing) [Egypt]
39761. Which type of vacuum pump for metallizing [India]
39762. PVD Zirconium Nitride [California]
39763. Adhesion of electroless nickel onto nickel iron alloy [UK]
39764. Is there a Practical Upper Limit for Hard Chrome Hardness? [Georgia]
39765. PO2 conversion coating for Thixo Mag? [Washington]
39766. Alternate coating for moulds [India]
39767. Corrosion, compatibility [Singapore]
39768. Shop ceiling restoration [Minnesota]
39769. Cross drill before or after powder coating? [Wisconsin]
39770. Zinc Cyanide over 12L-14 Steel [Minnesota]
39771. How do I obtain 5-15 g/l dissolved aluminum in my electrolyte [Canada]
39772. Need Graphics on Mannequins [Colorado] {3/7/06}
39773. Need fusion bonded epoxy lining process and painting of valves [India] {3/7/06}
39774. Extra thick layer of hard chrome plating [Canada] {3/7/06}
39775. Need Black Pearl Finish on carbon steel golf clubs [Oklahoma] {3/7/06}
39776. Need aluminum wheel refinished [New Jersey] {3/7/06}
39777. Need Silver Plating on Rexolite [New Hampshire] {3/7/06}
39778. Need a system to apply an antique gold/bronze finish to spin casted medallions [Illinois] {3/7/06}
39779. Remove metal solder from silver dollar [Missouri]
39780. Contamination issues from refinishing woodstoves [California]
39781. Restore patina on antique brass sink basin [New Jersey]
39782. Smut from silver plating bath [New York]
39783. Require chrome plating thickness of piston for hydraulic applications [UAE]
39784. Suitable finish on brass component when used in high humidity coast area [India]
39785. How do I know if it is electronic grade sulfuric acid? [Canada]
39786. Testing Chromate Treatment Prior to Painting [Missouri]
39787. Info please on graphitic corrosion rates of high phosphorus grey iron? [Australia]
39788. Corten steel for ship repair [Singapore]
39789. Plating and RoHS compliance [Wisconsin]
39790. Dissolve molded clay [New York]
39791. Cast Aluminum Fork Legs [Maine]
39792. Paint a mural on a polyethylene water tank [Bahamas]
39793. International Standard AS AFTN-A240 [Oregon]
39794. Measuring thickness of sulphamate nickel plating [Scotland]
39795. We are in trouble to do nickel plating [India]
39796. Black Hex Chrome vs Black Tri Chrome [Ohio]
39797. Most easy method to convert gold potassium cyanide to metallic [India]
39798. Paint Stripping Dip Tank [Tennessee]
39799. Wholesaler needs fashion jewelry with excellent gold and silver plating [Australia] {3/12/06}
39800. Need fenders plated [Pennsylvania] {3/12/06}
39801. WANT MY RIFLE REFINISHED [FLORIDA] {3/12/06}
39802. Seeking anodizing of 6061 structures [Pennsylvania] {3/12/06}
39803. WANT PORCELAIN ENAMELED SHEETS FOR WHITE BOARDS [Turkey] {3/12/06}
39804. Used DC Reversing Switches and a Filter Needed [Ohio] {3/12/06}
39805. Jeweler Needs Potassium Cyanide [Alaska] {3/12/06}
39806. Want electrostatic powder coat system [Viet Nam] {3/12/06}
39807. Need digital inks for anodized aluminum [California] {3/12/06}
39808. Need Process Monitoring Equipment for phosphatizing line [Iowa] {3/12/06}
39809. Need Electrostatic liquid painting guns for PVDF Coatings [India] {3/12/06}
39810. Need to find a refiner for gold potassium cyanide [New Jersey] {3/12/06}
39811. Selective Coating for Solar Panel Absorber [Hong Kong]
39812. Pre-paint cleanup of steel part after stripping chrome, nickel and copper [California]
39813. Acid for concrete patio got on Stainless Steel BBQ [California]
39814. Stripping oxide coatings from aluminum [Malaysia]
39815. Chemical Conversion Coating REMOVAL on Aluminum [Canada]
39816. Oven Dry For Chromate [Singapore]
39817. Pinholes and dirt in paint problem on aluminum [South Africa]
39818. Marring test equipment [Georgia]
39819. Galvanized versus e-coat [Michigan]
39820. Electroless Nickel and Immersion Gold Undercut the LPISM [Malaysia]
39821. Magnetic chrome? [Maine]
39822. Bubbles problem on Ni-Cr plated materials [Philippines]
39823. Chrome reactivator [California]
39824. Removing a cement tile with colour layer from chrome plated moulds [India]
39825. Painting anodized aluminum [Ohio]
39826. Stains on stainless steel after alkaline cleaning [Connecticut]
39827. Titanium reaction with HCL and HF [Philippines]
39828. Surface finishing of aluminum alloys
39829. Protecting steel pipes from exhaust fumes [Namibia]
39830. Need a brass bell plated [Georgia] {3/14/06}
39831. RESISTANT MASH SEAM WELDING OF GALVANEALED SHEET [India]
39832. Powder coating - problems in pretreatment [Turkey]
39833. How to prevent copper plated/copper sinetered products from oxidation/finger prints [India]
39834. High Electrical Relay Insertion Force [Georgia]
39835. 1000 hrs salt spray [India]
39836. Pre-treatment 6061 aluminum [Massachusetts]
39838. Galvanized steel: How to tell if steel is coated, how to remove coating [Maryland]
39839. Alodine Color without Chromium [New York]
39840. Post anodize cleaning [Canada]
39841. Need reel-to-reel silver plating [Singapore] {3/14/06}
39842. Hard Anodizing Question [California]
39843. How do we get nickel or nickel-chrome plating on aluminum sand casting product surface [India]
39844. Properties of diamond-like-carbon [Portugal]
39845. Need to electroform name plates and labels [India] {3/15/06}
39846. Electropolishing of gold alloys [South Africa]
39847. Future trends of technology to replace Cathodic Electro Deposition [India]
39848. I have two questions to ask you. Could you please reply and explain them for me? [Thailand]
39849. How to know if chemical stripping of hardcoat attacked my aluminum [Mexico]
39850. Silver deposit - Purity analysis [Switzerland]
39851. Peeeling of chrome plating on bathroom towel warmer [Scotland]
39852. Need dip tank service for rusty antique car body [New York] {3/15/06}
39853. Zinc dross in the galvanising industry [Zimbabwe]
39854. Black anodizing changes to yellow [Iran]
39855. Acids [England]
39856. Alodine and Araldite Compatibility [Portugal]
39857. Need chrome for my motorcycle wheels [North Carolina] {3/15/06}
39858. Jobshop who does black endurion finish [New Hampshire] {3/15/06}
39859. Fine line adhesive tapes for electroless nickel [Israel] {3/15/06}
39860. Does water conduct electricity? [California]
39861. Sodium chloride eats up molds [Florida]
39862. Aluminum nitride metallization [Oklahoma]
39863. RoHS compliant alternative to Zinc Phosphate bond coat [Illinois]
39864. Melt-coated bronze [New York]
39865. Tank material for Nitric Stripping [Wisconsin]
39866. pH sensor shock [California]
39867. Plating Stainless Steel [South Carolina]
39868. Masking ecoat parts that have already been ecoated [Illinois]
39869. Need Gold Plating [Hong Kong] {3/15/06}
39870. Looking for vacuum metallizing supplier [Indonesia] {3/16/06}
39871. Finishing suppliers for automotive industry [Mexico] {3/16/06}
39872. Need a faucet refinished [Bahamas] {3/16/06}
39873. Reaction of Mg and H [France]
39874. Making of phenyle [India]
39875. Cold Rust Bluing Problem [New Zealand]
39876. Difference between grease and gel? [India]
39877. Oxidation of copper [Florida]
39878. Removing galvanizing from the interior of a galvanized steel tank [Washington]
39879. Rohs compliance of finishes [Ohio]
39880. Determination of chloride in turbid solutions [Egypt]
39881. Copper Testing Final Effluent [Scotland]
39882. Powder Coat [California]
39883. Nickel Plating Time Failure [Philippines]
39884. Ideal ratio of point TA/FA in zinc phospating [Indonesia]
39885. Mild corrosion and stain in 7075 alloy [California]
39886. Does humidity effect to rust level? [India]
39887. Is there a corrosion protection coating that can go under autophoretic coating? [England]
39888. Decreasing Copper Content of our Descaler Solution(Pre-treatment) [Philippines]
39889. Compatibility of hard anodized 6061-T6 aluminum billet machined part with EN plated 7075 aluminum blllet machined part [North Carolina]
39890. Zinc Phosphate Coating for automotive industry [Pennsylvania] {3/17/06}
39891. Solder Cleaning Machines [Wisconsin] {3/17/06}
39892. Is tremclad toxic to animals? [Canada]
39893. Seismic compliance for plating line installation [California]
39894. Powder peels off/inspection [Pennsylvania]
39895. Looking to silver/metal plate plastic cutlery [Canada] {3/17/06}
39896. French process furnace [Vietnam] {3/17/06}
39897. Enquiry for setup of red Oxide Plant and purchase of machinery required [India] {3/17/06}
39898. Small chroming bath setup [Australia] {3/17/06}
39899. EXAMPLES OF MONOBASIC, DIBASIC and TRIBASIC ACIDS [Philippines]
39901. Blueing of Steel [Delaware]
39902. Dissolution and analysis of titanium [India]
39903. 98% sulphuric acid [Australia]
39904. Digestion procedure [Maryland]
39905. Difference between Class I and Class III Iriditing [Maryland]
39906. Chem treated cyanide zinc finish, on steel [Illinois]
39907. Steps for hot dip galvanizing [UAE]
39908. Suitability of using nickel metallizing on MS for application with strong halide attack [India]
39909. Plating Electroless Nickel on Aluminum Substrate [South Korea]
39910. Guideline for aluminum cleaning [India]
39911. Phosphate bath problem [India]
39912. Black Passivation and Black Trivalent Plating [Singapore]
39913. Selective Passivation / 15-5 PH / Citric Acid [Connecticut]
39914. Sandblasing Companies [Canada] {3/20/06}
39915. Pewter Coffee Service [Massachusetts] {3/20/06}
39916. Conducting substrates [India] {3/20/06}
39917. Coating equipment and formulation [India] {3/20/06}
39918. Setting up a hot dip galvanising plant [Nigeria] {3/20/06}
39919. Coating for metal high temp and chemical resistant [Indonesia] {3/20/06}
39920. Suitable epoxy/paint coatings for chemical resistant [India] {3/20/06}
39921. Need electroplating machines [Saudi Arabia] {3/20/06}
39922. Polipropylene sheet [California] {3/20/06}
39923. BUFFING WHEEL 20\" X 7\" 8 PLY [California] {3/20/06}
39924. N-95 PARTICULATE RESPIRATOR 8210 3M [California] {3/20/06}
39925. HIGH STRENGTH FLAP BRUSH WHEEL A/O MEDIUM [California] {3/20/06}
39926. TRIPOLI BROWN LIQUID COMPOUND [California] {3/20/06}
39927. INCO S ROUND NICKEL ANODES [California] {3/20/06}
39928. TRICLOROETILENE 10,000 GL [California] {3/20/06}
39929. Oven [Canada] {3/20/06}
39930. Pennies [New York]
39931. Boriding at fluidised bed reactor [Turkey]
39932. Tin sheets for steel deck [Philippines]
39933. Solubility of ammonium bifluoride at different temperatures [India]
39934. Student/Educational Electroplating -- Why Sugar? [North Carolina]
39935. Fiber Optic Uncladding Techniques [Singapore]
39937. BLACKENING NICKEL PLATED ITEMS [North Dakota]
39938. Blackening zinc plate [North Dakota]
39939. Living in mystery with a nickel allergy on my hands [Maine]
39940. Darkening oil rubbed bronze locksets [California]
39941. Durable black finish [UK]
39942. Old cheap bed [Texas]
39943. Bronze Finishing [Missouri]
39944. Industrial or Military Spec for Application of Trivalent Chromate Finish to Zinc Electroplate [New Jersey]
39945. RoHS / WEEE compliant replacement for black e-coat of aluminum [Oregon]
39946. Hydrochloric Acid Spectrophotometric Analysis [Canada]
39947. Charcoal filtering Nickel Sulfamate? [California]
39948. Cathodic paint problem [India]
39949. I want to paint a pole barn that is covered in galvanized steel [South Dakota]
39950. Epoxy finishing of hand ground steel [New York]
39951. Metal blackening process [Malaysia]
39952. Help? Random uneven thickness on flat surfaces with sulfamate nickel [Massachusetts]
39953. Silver plating in barrel [Serbia]
39954. Selective Plating using Platinum [New York]
39955. Density of current in the cadmium plating process [Italy]
39956. Steel tubing and CR plating [Arizona]
39957. Anodise cookware [India]
39958. IRON in a HCL pickle tank? [Illinois]
39959. Reason for Sludge formation in Acid Tanks [India]
39960. Requirement for Used Automatic Electroplating Plant [Pakistan] {3/21/06}
39961. Auto Paint Booth Lighting that adheres to Florida Fire Codes [Florida] {3/21/06}
39962. Looking for a product to "hide" or make scratches blend in on anodized cast surfaces [Illinois] {3/21/06}
39963. Seeking PVA substitute [Israel] {3/21/06}
39964. Stainless Steel Samples [New Jersey] {3/21/06}
39965. Product of Nitric acid and Sulphuric acid [England]
39966. How do I extract silver [Texas]
39967. Refinishing an enameled iron double sink [Texas]
39968. How to Age A Shiny Brass Plated Fireplace Door [Pennsylvania]
39969. How to perform Bleach Test on a Black Anodized Part? [California]
39970. Chemical Conversion Coating [India]
39972. Hard aluminum anodizing [Italy]
39973. Distributor is seeking copper sulphate and copper oxide [India] {3/22/06}
39974. Titanium Dry Etching [New Jersey]
39975. What kind of paint do I use on polyethylene resin "wicker" furniture? [Utah]
39976. Need to know everything about chroming to open up a shop of my own? [California]
39977. Confusing ASTM-B 650 for plating thickness [Virginia]
39978. Leadframe plating [UK]
39979. CLEANING SILICONE CONTAMINATED PARTS [Virginia]
39980. Discoloration of 100%Sn on top of a PPF leadframe [Singapore]
39981. Differences b/w electroless and electrolytic nickel plating [India]
39982. How do I tone down a brass coffee table? [Florida]
39983. Refinish Resin Tabletop? [California]
39984. Calibration of Timer for Water Immersion Tanks on Passivate Line [Kansas]
39985. Mechanical Zinc [China]
39986. Knowledge about Alodine [Canada]
39987. Can't get rid of sealing smut [Philippines]
39988. Need Chrome Wheels Rechromed [Washington] {3/22/06}
39989. Need consultation on, and equipment for, Aluminizing Steel Strip or Steel Pipe [Belgium] {3/22/06}
39990. Need salt spray cabinet for our lab [Pakistan] {3/22/06}
39991. Painting plastic kitchen doors [England]
39992. Procedure for hard chrome plating onto electroless nickel coating [Greece]
39993. Calculating acid zinc barrel plating production rate [Hong Kong]
39994. Black anodized (Type 2,Grade 2) [China]
39995. What type of coating techniqe should follow for coating on Needles? [India]
39996. FDA approved powder coat [Texas]
39997. Need polishing materials and accessories [Egypt] {3/23/06}
39998. Can automobile mag wheel rechroming still be done? [Texas]
39999. Good inhibitor for biological growth [Pennsylvania]


The finishing.com Hotline has been on the Internet since '95 and includes more than 40,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2006