27000. Painting HDG steel for use in salt water [Louisiana]
27001. Seeking anodizing of large 6061 assembly [South Dakota] {1/27/04}
27002. Applying color to a laser engraved graphic on a color anodized part [South Carolina]
27003. Need pricing for water treatment chemicals [Florida] {1/27/04}
27004. Patchy Hard Coating of 2024 [North Carolina]
27005. INFO ON STARTING GALVANIZING BUSINESS [South Africa] {1/27/04}
27006. Effect of aluminizing on E-glass fiber [Libya]
27007. Ferro-nickel electroplating [Iran]
27008. Copper plating [Texas]
27009. Stripping protective coating from brass [Texas]
27010. Problems polishing silver [Wisconsin]
27012. Seeking blaster/stripper for Aluminum Body Panel from a '71 Land Rover [New York] {1/28/04}
27013. Nedox plater [California] {1/28/04}
27014. Post-phosphate oil or other material sought [California]
27015. Need Copper plating on our mirror polished T316L stainless steel sheet [Texas] {1/29/04}
27016. Chemical conversion coating on aluminum alloy [California] {1/29/04}
27017. Gold dipping of chrome work [Illinois] {1/29/04}
27018. Need a deruster shop [Iowa] {1/29/04}
27019. Nickel Brush Plating [Connecticut] {1/29/04}
27020. Acrylic Coating for Dye Sublimation [Curacao] {1/29/04}
27021. Floating silicon balls for hot water sealing bath [China] {1/29/04}
27022. Anodizing shop needs hairlining machine [China] {1/29/04}
27023. Effect of Temperature on Corrosion [California]
27024. Finding out the weight of US coins [California]
27025. Chemistry Lab help [Canada]
27026. Stripping away gold tubing from quartz [Texas]
27027. How to dissolve copper while leaving nickel unchanged [Michigan]
27028. Detecting thin aluminum phosphate coating [Hong Kong]
27029. Coating a Decorative Sheet Metal Heat Shield [New York]
27030. Painting metal parts of a desk [California]
27031. Standards for color fastness to light [Tennessee]
27032. EN pits [New York]
27033. Constant current vs. voltage anodizing [Minnesota]
27034. MIL-C-5541 Class 1A vs Class 3 [Kansas]
27035. Electrolytic Passivation [Texas]
27036. Stainless Finishing [California]
27037. Coating for aluminum heat sink [Massachusetts]
27038. Need PVD equipment [New Zealand] {1/29/04}
27039. Recipes of gold, silver and copper brush plating baths? [Colorado]
27040. YELLOW NICKEL [Serbia and Montenegro]
27041. REFINISHING AN OLD BRASS BAR [Georgia]
27042. Refinishing chrome bathroom fixtures to brushed nickel [Michigan]
27043. What is the difference between Chromate and Chromium coatings? [Massachusetts]
27044. Data Source Request for Surface Absorption or Reflectance To Visible Light [Singapore]
27045. Why use AMS QQ P 35 for aerospace instead of ASTM A 967? [Ireland]
27046. Hot Sealing with PVC lined tank [Saudi Arabia]
27047. Risk of do not use phosphate? [Mexico]
27048. Adhesion problem. Nickel over stainless steel 430 [Poland]
27049. Package Contamination on our IC [Indonesia]
27050. Shock rod macrocracks in chrome plating [Brazil]
27051. Silver plating was very dull and not mend [Thailand]
27052. Black spot problem in Zinc Iron Yellow Barrel Plating [India]
27053. Cleaning stainless steam sterilizers [Texas]
27054. A131 #4 Finish on aluminum [New York]
27055. Severe corrosion in a wet steam system [India]
27056. Plating failure of chrome finish on main winch of new sailboat [Maryland]
27057. Thin Dense Chrome Plate vs Chrome Plate [New York]
27058. Fabric mfgr. needs wear coating for cutting blades [New Hampshire] {1/30/04}
27059. Seeking silver or aluminum coating on optical glass [China] {1/30/04}
27060. Oxidation-Reduction [Canada]
27061. Electrospark coating technology or micro welding [India]
27062. Selective etching of aluminum oxide [Missouri]
27063. Possibility of use of silver plated copper wire in distribution transformer [India]
27064. Businessman wants to start a chroming business [Virginia]
27065. Polishing some 73 year old Vintage Headlights for Automobiles [New Hampshire]
27066. How to I age raw brass? [Oregon]
27067. Finishing and polishing stainless steel [New York]
27068. Chemicals for the Shor Simplicity refining system [UK]
27069. How to clean "Flash Gold" [New York]
27070. Chrome fire surround staining [UK]
27071. Magnesium Alloy refinish [New Jersey]
27072. Custom trophy gold finish [California]
27073. pH of incoming rinse water [Connecticut]
27074. Solderability problem with tin plating [Singapore]
27075. Surface profile of Galvannealed steel [Texas]
27076. Need process for 108 hours in CASS Test [India]
27077. Can I anodize on top of existing anodic film [New Zealand]
27078. Alternative to elelctropolishing 304 SS [Georgia]
27079. Where can I get items dipped in chrome [Ohio] {1/30/04}
27080. Seeking chrome plating [Illinois] {1/30/04}
27081. Need maskant for turbine blade stripping [Italy] {1/30/04}
27082. Looking for high heat resistant finish on glass fibre braided cables [India] {1/30/04}
27083. Problem with Cyanide Mixture waste treatment [Arizona]
27084. Painting a bronze pool fountain [Texas]
27085. Questions Regarding Tinted E-Coat Processes [Indiana]
27086. How can I tell if brightener has been used? [Indiana]
27087. Titanium tumbling media for 6RMS finishing [California]
27088. Alternatives for ni-cr plating of brass [North Carolina]
27089. Electroplating Hard Material [UK]
27090. How to replace the inside coating of a microwave with tape [Mexico]
27091. Hard chrome on aluminum IDs [Illinois] {2/2/04}
27092. Plasma treatment of nylon parts [California] {2/2/04}
27093. Need copper finish repair on new wall fountain [New Jersey] {2/2/04}
27094. Seeking refinishing of brass faucets to nickel [Texas] {2/2/04}
27095. Growing shop need chroming / polishish service [California] {2/2/04}
27096. Need provider - plate plastic with real or fake gold and silver [Texas] {2/2/04}
27097. Need homopolymer poly to coat underground conduit [Georgia]{2/2/04}
27098. HAVE YOU EVER CLEANED RUST WITH CLOROX? [No. Carolina]
27099. Best substrate to Spin coat PDMS onto [Pennsylvania]
27100. Hunting for Steel Pickling Companies [Michigan]
27101. Etchant for ALN? [Iran]
27102. Help me polish aluminum bike parts [California]
27103. Casting then anodizing 6061Al? [Michigan]
27104. FeCl lack of depth-of-etch on brass plates [Scotland]
27105. How do I strip chrome from aluminum? [Illinois]
27106. Non-stick coatings for stove drip pans [So. Dakota]
27107. Harmonica mouthpiece allergy? [U.K.]
27108. Want to circular scar a stainless steel table top [Missouri]
27109. What things can be chromed? [Washington]
27110. Getting rid of brass finish on lamps to another finish [So. Carolina]
27111. Federal Color 11350 (Red) available? [Panama Canal]
27112. Dichromate Precipitation [New York]
27113. Can I do magnetic particle inspection after plating? [India]
27114. Titration for iron content in electropolishing solution [India]
27115. Gold stripping with Muriatic Acid [Tanzania]
27116. Solderability Failure at heel area [Singapore]
27117. Electroless Nickel in Saltwater Environment [Utah]
27118. Hard Times In Hard Chrome Plating [New York]
27119. I want to remove nitrates from silver cyanide bath [Thailand]
27120. Need to do Invar (Iron,nickel,chrome) alloy plating [Wisconsin]
27121. Is painted Alodine 1200 heat affected? [Québec, Canada]
27122. Electrical bonding use of Alodine 1200 and 1201 [Kansas]
27123. Liquid masking materials? [Washington]
27124. Copper streaks during the pickling of low carbon steels [Kentucky]
27125. 303ss passivation problems [New York]
27126. Material Suggestion for CO and CO2 at 200 deg C [Pakistan]
27127. Corroded coupling bolts [Pennsylvania]
27128. Looking for Non-Pitter 22 Special [California] {2/3/04}
27129. Need Sonic Cleaner 15-20 gallon ASAP [Minnesota] {2/3/04}
27130. Need APPROVED shop for applying Mil-P-53084 [New York] {2/3/04}
27131. SILVER EXTRACTION MACHINE [India]{2/3/04}
27132. Copper wire: need to produce & maintain a bright surface finish [Oregon]
27133. PAINTING PROCESS ON CYCOLOY PLASTIC [India]
27134. Effect of temperature on voltage of an electrochemical cell [B.C., Canada]
27135. Anodized parts have ghost-like stain [So. Africa]
27136. I want to have my refrigerator painted [Virginia] {2/3/04}
27137. dk rhodium [India]
27138. How to dispose of used zinc chloride MTL 50% [California]
27139. Teflon Impregnated Anodize [Massachusetts]
27140. Polymers and defoamers [New Jersey]
27141. Seeking finishing facility Ciudad Juarez area [Mexico] {2/4/04}
27142. DOW23 finish for Magnesium Alloy [New Jersey] {2/4/04}
27143. Seeking nickel plating on aluminum up to 12' [California] {2/4/04}
27144. DYE SUB SUBSTRATE COATING [Washington] {2/4/04}
27145. Zinc plating for 300 - 500 deg F [Kentucky]
27146. Yellow iridite and chromate treatments [Oklahoma]
27147. Acid Dipping for my 1948 Chevy, worth it? [Alabama]
27148. Requesting annealing procedure for 304SS [India]
27149. Finishing zamak alloy [Romania]
27150. Residual stress due to shot-peening [UK]
27151. CPVC vs. copper to plumb a house [Georgia]
27152. HOW TO PICKLE/PASSIVATE HASTELLOY C-276 [South Africa]
27153. Need synthetic diamond powders [India] {2/4/04}
27154. Need a shop that does hologram mastering [India] {2/4/04}
27155. Abrasive wear testing...materials abrasive [Spain]
27156. Lead free plating chemistry [Philippines]
27157. Teflon Coating [Mississippi]
27158. Applying aqueous phosphate coating to maximize primability and corrosion resistance [Georgia]
27159. Pitting on anodized aluminum frame - need technical help [Florida]
27160. Hard chrome plating - coefficient of friction [India]
27161. Electroless Nickel [Mexico]
27162. Are poly tags flame treated both sides? [Connecticut]
27163. Clusters of tiny dot found on tin plated surface [Singapore]
27164. Need Alkali Etch information for Aluminum [Illinois]
27165. Passivity vs. corrosion rate [Canada]
27166. Need chlorine corrosion resistance at 1200 C [Iran]
27167. Dissimilar metal aluminum/304 stainless galvanic corrosion [Georgia]
27168. Materials and coatings for pistons [South Africa]
27169. CF12 Heat Treatment [Iran]
27170. Adhering copper sheet/rool to block fence [Arizona]
27171. Best Reflectivity Coating for Headlight Reflectors [Wisconsin]
27172. PCB Classes [India]
27173. Adhesion testing in PCB manufacture [England]
27174. Compatibility of chrome and powder coat used on the same surface [Ohio]
27175. OEM wants to painting galvannealed electrical enclosures [West Virginia]
27176. MIL-C-5541 class 1A [China]
27177. Influence of electrochemical deburring on surface to be anodized [Spain]
27178. Contamination from mild steel rollers on to stainless steel sheet [England]
27179. Need helmet windscreen iridium coating [Nevada] {2/5/04}
27180. Chrome dipping my rims [California] {2/5/04}
27181. Electropolish nitinol (Ni, Ti alloy) [Poland]
27182. Need rubbery finish on steel jewelry [UK]
27183. Sculptor needs a color stain for stainless [Texas]
27184. Drilling equipment mfgr. paints "noiseless steel" [Pennsylvania]
27185. How to electropolish rhenium and ruthenium? [Spain]
27186. High temp. Ash corrosion [Ecuador]
27187. Need theatrical mask chrome plated [New York] {2/5/04}
27188. Reduction of an oxidized copper layer (100nm thickness) [Belgium]
27189. How do I remove anodizing from a large area? [North Carolina]
27190. About bright dip process for copper [Mexico]
27191. Plating for High Strength Steels [Oregon]
27192. Ways to minimize defects in electroplating [Philippines]
27193. Putter Mfgr. seeks nickel plating shop for golf clubs [Georgia] {2/5/04}
27194. Seeking protection for electroplated shoes to withstand harsh weather [UK] {2/5/04}
27195. Need help on Teflon coating cars [India] {2/5/04}
27196. How to get rid of calcium deposits from cement [California]
27197. What stainless steel mesh alloy should I use for frying? [New York]
27198. Handgun dechroming [New York]
27199. How do we strip kitchen pulls and hinges? [Ohio]
27200. Stripping rust with alkaline solution [Canada]
27201. MIL-STD-105E interpretion [China]
27202. Ion Vapor Deposition over Electroless Nickel Plate [California]
27203. Tungsten metallization problem [California]
27204. High stress strike nickel [Indonesia]
27205. Rust spots on dripline [Kentucky]
27206. Vibratory tumbler/motor size and load [California]
27207. Transparent Coating Material for Silicon Carbon [Hong Kong]
27208. Wanted - rechroming equipment and information [Missouri] {2/6/04}
27209. Body shop needs side-exhaust paintbooth [Ohio] {2/6/04}
27210. How much zn, ni and cu are electroplated annually? [California]
27211. Etching of NiAlMn alloys [Germany]
27212. Plating/Finishing test standards [Minnesota]
27213. FLUOROCARBON GM6046M/18T336 [Canada] {2/6/04}
27214. Chrome Dipping [Arkansas] {2/6/04}
27215. Electrodeposition of diamond particles [Texas]
27216. Coating aluminum to withstand temp and vib changes [Iowa]
27217. Need to find powder water softener [Georgia]
27218. Refinishing musical brass instruments [Maryland]
27219. How to repair scratches in brass finish [Iowa]
27220. Making wood finials look like brass [New York]
27221. Hand dip metal roses? [Missouri]
27222. Can waste hydrochloric acid be used for hex chrome reduction [Pennsylvania]
27223. How To De-Anodize? [Pakistan]
27224. Need to buy 150,000 pounds of white painted aluminum [Michigan] {2/9/04}
27225. Black anodizing of bicycle components [Missouri] {2/9/04}
27226. Need for BORON REMOVAL [Oklahoma] {2/9/04}
27227. Ag recovery (method or equipment) [Malaysia] {2/9/04}
27228. Request for chemical suppliers and quotation [Zimbabwe] {2/9/04}
27229. Acid marking pen [India] {2/9/04}
27230. Grams of copper in a penny [North Carolina]
27231. Silver Safety Pin Piercing [Canada]
27232. Galvanized coma [South Carolina]
27233. Metal finishing process wastewater treatment regs [South Carolina]
27234. Burning paint off 17-7 PH SS Spring [Texas]
27235. Black Oxide and Surface Finishes [Ohio]
27236. GELLING NITRIC AND HYDROFLUORIC ACID [Croatia]
27237. Convert Rz in mKm to micro-inches [Illinois]
27238. Al 6061T6+Hardcoat anodizing+Saltwater fog= still not working [Illinois]
27239. LASER SCALE REMOVAL [Illinois]
27240. Magnesium Mated to Printed Circuit Board [California]
27241. Need auto body acid dipping [New York] {2/10/04}
27242. Need chrome plating of 5000 small pieces [Michigan] {2/9/04}
27243. Need supplier for alonizing [Pennsylvania] {2/9/04}
27244. Need Help Looking for Software/Analysis Chemicals [California] {2/9/04}
27245. Need Bronze Paint that can be patinized [Arkansas] {2/10/04}
27246. What protects nails from rusting best in different solutions? [Oklahoma]
27247. Electroless nickel references [Saudi Arabia]
27248. TiN etchant [Iran]
27249. Upgrading copper/brass statues with a coating [South Africa]
27250. Metal vacuum sealing [California]
27251. Increased conductivity of DM water generated [India]
27252. Removing nickel and repairing decorative chrome plating [Slovenia]
27253. Effect of hydrogen de-embrittlement on plating life [India]
27254. Zn-Ni-P alloy plating process [Slovenia]
27256. Electrically conductive finish (in black this time) [Latvia]
27257. Bright silver finish after anodizing [Illinois]
27258. Chemical Cleaning of New Boilers [Singapore]
27259. Chromium solvent contamination or passive film solvent dissolution [France]
27260. Non- uniform results in needle/cannulae electropolishing [India]
27261. Sand blasting media for clear anodize pre-prep [Illinois]
27262. Reconditioning of worn out molds [India]
27263. Discoloration of Arcap in deionized water rinsing [UK]
27264. Distributor looking for Electroplating machines and supplies [Saudi Arabia] {2/10/04}
27265. Estimate of installing a powder coating plant [India] {2/10/04}
27266. Sodium hypophosphite [Australia] {2/10/04}
27267. Need reel-to-reel plating equipment from Japan [Taiwan] {2/10/04}
27268. Project on zinc-cobalt plating [India]
27269. Fixing Electrolysis in boat [Cambodia]
27271. Permit requirements for powdercoating [Alabama]
27272. Removing oxidation from aluminum sheets [Missouri]
27273. Powder coating plant [India] {2/10/04}
27274. Electroless Deposition on Graphite Powder [India]
27275. Passivation color [India]
27276. Bath for EN with Teflon [Iran]
27277. If solder is plated on silver [China]
27278. Bubbled plating? [Indiana]
27279. Premature tarnishing of Bright Dip finish on aluminum [Singapore]
27280. 316 vs 316L for see water use [UAE]
27281. Nickel Teflon Plate on Composite Parts [California] {2/11/04}
27282. NEED ANODIZING PLANTS FOR 20-22 FEET RAIL [India] {2/11/04}
27283. Need a 40 Ford acid dipped [Texas] {2/11/04}
27284. Need whole car acid dripped to remove paint for restoration [Pennsylvania] {2/11/04}
27285. Music shop needs nickel plating for brass instruments [Texas] {2/11/04}
27286. Need hologram system for registration plates [India] {2/11/04}
27287. Need product to replace brass appearance of interior hardware [Indiana] {2/11/04}
27288. Looking for anodizing additive [Taiwan] {2/11/04}
27289. UV coating system for MDF [Turkey] {2/11/04}
27290. Seeking trivalent black chromate [Illinois] {2/11/04}
27291. Oxidation of copper during plating [Ohio]
27292. Unexpected copper plating effects [California]
27293. What do they use when you car is acid dipped [Canada]
27295. Aluminum home radiators versus steel wood-stove boiler - what to do? [France]
27296. MIL-T-10727 vs. ASTM B545 [California]
27297. Controlling solder dipping thickness on a round flatten lead [New Jersey]
27298. Black color coating by PVD [India]
27299. Ni plating on Ni-fe alloy withoutaffecting lead-based glass [Washington]
27300. How to remove chloride contamination from acid tin bath [Poland]
27301. Gold plating thickness on high abrasion parts [Colorado]
27302. Cost difference between Polished Solid Brass and US15 Satin Nickel plating [California]
27303. Decorative aluminum etching (eg orange peel texture) [South Africa]
27304. Making an Aluminum Wear Strip [Pennsylvania]
27305. Patches on cold rolled sheet [India]
27306. BELT ZINC PHOSPHATE ADVANTAGES AND DISADVANTAGES [Canada]
27307. Stainless Steel Finish [UAE]
27308. Jeweler needs TITANIUM COATING of DRUSY AGATE [Connecticut] {2/11/04}
27309. Black stainless fasteners needed [Oregon] {2/11/04}
27310. Sand blasting and powder coating of Spin Cycles [California] {2/11/04}
27311. Electroplating onto Titanium [Singapore]
27312. Odor suppressant for paint stripper [Philippines]
27313. Need a 'clear' metal treatment [Georgia]
27314. Anodizing Aluminum for Artist [California]
27315. Use of Ferric Sulfate as a coagulant [Pakistan]
27316. Sodium orthophosphate analysis [Singapore]
27317. Standards and Test procedures for checking and acceptance of PTFE coating [India]
27319. Silver plating of Kovar for a high temperature application [Vermont]
27320. Private mint seeks silver plater of copper coins [Canada] {2/11/04}
27321. Brass bed refinishing needed [West Virginia] {2/11/04}
27322. Medcoat 200 , 500 +/- pieces [California] {2/11/04}
27323. Parkerizing touch up [Texas]
27324. Cadmium Oxide In Granular Or Briquette Form [Arizona]
27325. Gold adhesion on work hardened area different [Connecticut]
27326. Voltage for hard coat failure [New York]
27327. Green spots in silver plating [Puerto Rico]
27328. Any active activator for Pd deposition on stainless steel [Bangladesh]
27329. Peeling of hot dip galvanizing coils [Egypt]
27330. Bright dip for brass [Arkansas]
27331. Paint adhesion problems to bare cast iron [Pennsylvania]
27332. Mirror polishing of die casted aluminum [Denmark]
27333. Chrome plating of brass kitchen cabinet hinges [Arizona] {2/12/04}
27334. CHROME PLATING ON PLASTIC REFLECTOR [India] {2/12/04}
27335. Need paintable peel coat for over painting (automotive) [England] {2/12/04}
27336. How to accelerate rust on steel [California]
27337. Gold Bullion Moisture Effect [Malaysia]
27338. Can you powder coat an engine after it's assembled? [Australia]
27339. Raise pH in Trivalent Chromium [Florida]
27340. Galvanizing half a built up letter [England]
27341. Chemical composition of B-Ni electroless Plating Bath [Indonesia]
27342. Troubleshooting Barrel Plating [Australia]
27343. Masking and Nickel Plating [Canada]
27344. Aluminum 6082-T6 vs. 6060-T66 [The Netherlands]
27345. Need chroming of plastic bumper valance [Maryland] {2/12/04}
27346. Seeking acid bath/galvanized coating for a pickup cab [Florida] {2/12/04}
27347. Need electroplating additives, copper bright dips, dyestuffs [China] {2/12/04}
27348. Copper oxide on pennies [South Carolina]
27349. Cu plating for small grid structures [Virginia]
27350. Black rhodium plating problems [Philippines]
27351. Pulse plating paper by Andy Lesko [Sweden]
27352. Electropolishing Solution Analysis [Arizona]
27353. Hydrogen Embrittlement Relief Test for Manganese Phosphate [New York]
27355. Repairing a hydraulic cylinder by chrome plating [Texas]
27356. Silver Cyanide Solution Turning Dark Brown [California]
27357. Joining steel pipe to galvanized pipe [California]
27358. PVD Glow Discharge for In Process Cleaning Uses [England]
27359. Making zinc electroplating bright [Indonesia]
27360. Hot water sealing problem [India]
27361. Coating anodized aluminum [England]
27362. Hardness vs Thickness [India]
27363. NEED chrome plating of plastic on classic cycle [Maryland] {2/12/04}
27364. Dissolving just the aluminium, not the anodizing [Oregon]
27365. Black Anodizing an Aluminum 2017 [Philippines] {2/12/04}
27366. EMBRITTLEMENT RELIEF OF STAINLESS STEELS [Ohio]
27367. Suggestions for start up of zinc phosphating buisness [New York]
27368. Need good industrial powder gun [Ohio] {2/12/04}
27369. Anodizing Metal for Lasering [Jamaica]
27370. Need copper plating on Kovar [California] {2/12/04}
27371. Need reflective glass beads as additive for powder coating [Florida] {2/12/04}
27372. Darkening polished brass [Texas]
27373. Retinning of antique dairy equipment [Virginia] {2/13/04}
27374. Anodize bleed out [New York]
27375. Wanted Edwards 2001/2002/2011 vacuum contoller [Ireland] {2/13/04}
27376. Plating for fluoropolymers molds [Pennsylvania]
27377. Time requirements between plate and post-bake? [Arizona]
27378. Color Changing Paint Due To Current [New York]
27379. NEED help POLISHING and ROUNDING stainless steel [South Carolina]
27380. Zinc plate on rubber/metal motor mount [Ohio] {2/13/04}
27381. Anodizing Question [England]
27382. Architect seeks best finish for exterior hand rails [Maine]
27383. Problems with stainless steel cut wire media in magnetic tumbler [Oregon]
27384. Cyanide zinc plating / Chloride zinc [Arkansas] {2/13/04}
27385. Titanium anode baskets in LHE Alkaline Cadmium [UK]
27386. Sign company needs large aluminum numbers powder coated [Florida] {2/13/04}
27387. Rusting of stainless turnstiles [Michigan]
27388. Need brittle coating lacquer for stress test [Hong Kong] {2/13/04}
27389. Alodine As per MIL-C-5541, Class 3 [India]
27390. Non-chromate conversion coating for aluminum [India] {2/13/04}
27391. Chemical removal of Parylene C from aluminum surfaces [New York]
27392. Mil. Spec., Powder Coat [Minnesota]
27393. Need better than Ra 1 surface on ceramic part [Canada] {2/16/04}
27394. Electroless plating to smooth surface finish [UK]
27395. Alternatives to chromate conversion coatings [New York]
27396. Chroming, I'm so confused [Tennessee]
27397. Plating cobalt on titanium [UK]
27398. Galvanize plating [Michigan] {2/16/04}
27399. Recommended B-Ni Electroless Bath [Indonesia]
27400. Aluminum galling problem [Finland]
27401. Looking for company that can acid dip entire car for restoration [Pennsylvania] {2/16/04}
27402. Chrome plater needed for classic truck bumper [Maryland] {2/16/04}
27403. Teflon re-coating for aluminum cookware [California] {2/16/04}
27404. Chrome dip plastic parts [Canada] {2/16/04}
27405. ABS chrome plater [Pennsylvania] {2/16/04}
27407. Looking for Acid/Chemical Etching Machine Vendor [Pennsylvania] {2/16/04}
27408. Need plastic media blaster [North Carolina] {2/16/04}
27409. Used vacuum metalizing equipment [California] {2/16/04}
27410. Copper Corrosion [Canada]
27411. Tarnishing of copper versus zinc plated object [Canada]
27412. Stainless steel 304 grade details [India]
27413. Water Break Test [California]
27414. Spherodizing annealing of sae 52100 bearing wires [India]
27415. MgB2 by Sol-Gel technique [India]
27416. Alumina membrane [India]
27417. Safe antiquing for zinc? [California]
27418. Enamel to re-finish Pavoni expresso machine [UK]
27419. How to rechrome golf clubs in my shop [California]
27420. Worn aluminum rims [Louisiana]
27421. Painting Galvanized Gutters [Illinois]
27422. Removal of gold plating [Arkansas]
27423. Wanting to build a electrolytic gold scrap refining machine [Iowa]
27424. Buffing Raw Copper [Pennsylvania]
27425. Removal of rust ring on cast iron woodburning stove [Michigan]
27426. Appraisal [Alabama]
27427. Polishing and anodizing of casted aluminum [Sweden]
27428. Oversize tap for anodizing [Utah]
27429. Keep Rinse Waters Neutral [Colombia]
27430. Electropolishing of stainless steel process in details [Egypt]
27431. Can you plate brass with Pt without a sub-plating? [Massachusetts]
27432. Chloride Corrosion in SS 304L piping in Sugar Refinery [Bangladesh]
27433. Pmma authenticity test [Canada]
27434. Protection against stress corrosion cracking of H13 [New York]
27435. Electrostatic Powder Coating [Colorado] {2/16/04}
27436. Air, Burning and Rusting [India]
27437. Equilibrium diagram of Inconel 718 [India]
27438. Lacquer needed for applying rare earth compounds to neon tubing [Ohio]
27439. Clear coat over hammered paint [Canada]
27440. Test to reveal oxides on steel surface [Ohio]
27441. Seeking electroplater who does Rhodium Plating on Sterling Silver [Georgia] {2/17/04}
27442. Chrome plating my plastic Mustang parts [Florida] {2/17/04}
27443. Need chrome-free conversion coating [Virginia] {2/17/04}
27444. Need Basic Yellow 1, cas:2390-54-7 [China] {2/17/04}
27445. FOR EFFECTIVE RINSING, THE QUANTITY OF RINSE WATER PER DM SQ [India]
27446. Enamel Coating [Malaysia]
27447. Rust preventive coatings for horns [India]
27448. Repainting church's tin ceiling [New York]
27449. My line of silver necklaces is tarnishing [Florida]
27450. Books on Boriding or Boronizing [Vietnam]
27451. Could cadmium contamination be due to airborne zinc breaking down in rinse water [England]
27452. Salt spray test parameters [India]
27453. Etching chrome castings for inspection [Virginia]
27454. Metal to rubber adhesion [India]
27455. 'Dust' on the components in Acid Copper Tank [India]
27456. Dissolving Silicon in Hard Anodizing [India]
27457. Fungus Formation on Cast Aluminum [India]
27458. Etchant needed for etching Nylon-11 [Arkansas]
27459. Electrochemical potential of stainless steel bolts [Philippines]
27460. Iridium coating sunglasses [New York] {2/18/04}
27461. Can powdercoating be used on exhaust systems? [Ohio]
27462. Anodize Cracking [Washington, DC]
27463. WANTED POWDERCOATING MACHINES [India] {2/18/04}
27464. Setting up a Nicasil coating shop [Greece] {2/18/04}
27465. Electroless Ni-B [Canada]
27466. Repairing titanium shaft by plating [Oregon]
27467. Wanted - Used UV pilot coater line [Alabama] {2/18/04}
27468. Electroplating nickel on aluminum [Ohio]
27469. Chrome plating plastic car parts [Tennessee] {2/18/04}
27470. Preventing flash rust on sculptures [Oregon]
27471. Need rims powder coated [Texas] {2/18/04}
27472. Seeking Cold Blackening Chemical Supplier [Malaysia] {2/18/04}
27473. Need 400 amp rectifier [Maine] {2/18/04}
27474. Electroplating thesis [China]
27475. How do I sell iridium? [Arizona]
27476. E-coating vs. galvanizing for security doors [South Africa]
27477. WHITE SPOTS ON ZINC PLATED CAST IRON BODIES [Italy]
27478. Zinc plating - plating peel off issue [India]
27479. Zinc cobalt plating: alkaline vs acid [India]
27480. Assuring Chrome Plate Integrity [Massachusetts]
27481. Salt spray test on anodizing coating for 2014 [Malaysia]
27482. How to clean heated iron [India]
27483. Which sealer and how to obtain a rust finish on metal, which will not rub off [Texas]
27484. Strip n' spray a mountain bike [Ireland]
27485. Hard coat anodizing of ASME SA356-T6 [Ohio]
27486. Screen printer require stainless steel engraving advise [Kuwait]
27487. Seeking Black Chrome plating of rims [New Jersey] {2/20/04}
27488. Real silver vs. sterling silver [North Carolina]
27489. Chrome Plating Exhaust Tips [Ohio] {2/20/04}
27490. Testing bond strength of HVOF coating [India]
27491. GI sheets uses [UAE]
27492. Helping poor Filipinos via silver antibiotic [Philippines]
27493. Abrasive cloth and polishing equipment for aluminum cookware factory [Ghana] {2/20/04}
27494. Information request for coatings on cylinders walls? [Belgium]
27495. Cycle accessories mfgr. seeks chrome plating on ABS plastic [Oregon] {2/20/04}
27496. How to speed up the hard anodizing process [Taiwan]
27497. Rechroming of my rims [Nebraska] {2/20/04}
27498. Re-Chroming Plastic [California]
27499. Getting copper pan re-tinned [Arkansas] {2/20/04}
27500. Panel plating chemical stain [Malaysia]
27501. Finger print problem on stainless steel [China]
27502. Stripping plating from zinc [Maine]
27503. Low pH in Nickel Tank [Maine]
27504. WHAT CAUSES LARGE CRYSTALS TO FORM IN THE ANODIZE TANK [Ohio]
27505. Horse farm needs 6 new stall fronts powder coated [Pennsylvania] {2/20/04}
27506. Zinc phosphate vs. inorganic zinc primer for mailboxes? [Virginia]
27507. Chrome dipping wheels for a '92 s-10 blazer 4x4 [West Virginia] {2/20/04}
27508. Need Sermagard on small screws [Alabama] {2/20/04}
27509. This is a heat transfer problem for processing composite materials [Alabama]
27510. Immersion silver on continuous strip electrical contacts [Colorado] {2/20/04}
27511. Looking for an industry workmanship standard for Yellow Chromate [Virginia]
27513. Teflon-Copper reaction [Connecticut]
27514. 1st Grade Science Experiment: Removing Rust from Nails [Washington]
27515. Seeking Hard Chrome Plate for very large steel shaft [New York] {2/20/04}
27516. PHOSPHATE NEEDED ON GALVANIZED SHEET? [India]
27517. Need plating in tapped holes [Oklahoma]
27518. Geothermal pipe coating and insulation [Philippines] {2/20/04}
27519. Nitriding of steam turbine blades [India]
27520. Test Methods for Heavy Metals (ELV requirement) [Malaysia]
27521. Architect needs info on metal stair finishing options [California]
27522. "Stoning machine" for Plastic Injection Mold Polishing [Canada] {2/20/04}
27523. Metal anodizing near Mexico City [Michigan] {2/23/04}
27524. Seeking coatings for plating racks [Poland] {2/23/04}
27525. Tin electroplating on nickel coated material [Philippines]
27526. Percentage and quantity of etchants required for Inconel 718 [India]
27527. Coloring aluminum like gold [India]
27528. Hobbyist needs help getting started [Florida]
27529. 316L Stainless on Mortar and Grout [South Carolina]
27530. Airborne emissions calculations: Emissions factors? [New York]
27531. Hydrogen embrittlement bake [Canada]
27532. Zinc plate/Yellow Chromate appears green in color [Michigan]
27533. Equipment and parameters for hard anodizing [Italy]
27534. Citric Acid Passivation rinse waters [Ohio]
27535. Problem in zinc phosphate coating bath [Turkey]
27536. Metal coating for glass substrate [Pennsylvania]
27537. Who and what can be black chromed [Oregon]
27538. Seeking Black Nickel plating of Italian Bicycle Frameset [Kansas] {2/23/04}
27539. Equipment for powder coating [Syria] {2/23/04}
27540. Testing the difference between anodized and alodined coatings [Texas]
27542. Aluminum galling situation [Canada]
27543. Need rims chrome dipped [Virginia] {2/23/04}
27544. Chrome dipping of one wheel [North Carolina] {2/23/04}
27545. Polyester coating to make sublimation printables [UK] {2/23/04}
27546. How to make 4% Picric solution? [California]
27547. Chrome of 1966 Nova parts [Michigan] {2/24/04}
27548. Need aluminum intake manifolds chromed [Vermont] {2/24/04}
27549. Painting thermoformed polycarbonate - pebbled [Canada] {2/24/04}
27550. Need copper anodes and aluminum anodes [Philippines] {2/24/04}
27551. Need Copper Cathode [Turkey] {2/24/04}
27552. Coating graphite onto optical fiber [Iran]
27553. How to copper plate steel welding rods [India]
27554. Etching aluminum, stainless and zinc plaques [Indonesia]
27555. Automotive Paint Finish [Texas]
27556. Reducing reflectivity of copper camera parts at home [Michigan]
27557. Stripping EN from aluminum [Georgia]
27558. Pebbled finish on plastic (polycarbonate?) [Canada]
27559. Painting zinc plated valves [Texas]
27560. Surface defects on powder coated panels [New York]
27561. Ti inhibition to HF [India]
27562. Oxidation of silver nickel electrical contact [Singapore]
27563. POLISHING OF SILVER ARTICLES [India]
27564. Biotech company needs multi-color anodizing [California] {2/24/04}
27565. Need plater for Miralloy finish [China] {2/24/04}
27566. Seeking anodizing of Suzuki LT80 frame [California] {2/24/04}
27567. Need manufacturers of nc thinner [India] {2/24/04}
27568. Is Core-Ten Steel Used In Large "I Beams"? [Florida]
27569. Equivalent to QQ-P-35 TYPE IV (Type 4) [Illinois]
27570. Dissolving Silicon Carbide Scale [Canada]
27571. Help repairing cement floor in anodize shop [New York]
27572. Problems plating over silver braze [Kentucky]
27573. Powder Coat Hooks Lose Conductivity [Minnesota]
27574. Determining pH and Orthophosphite level in Electroless Nickel Plating Process [Texas]
27575. Preparing electroless nickel surface for better adhesion [England]
27576. Looking for (black) plating that will pass 200 hr salt spray on zinc [California]
27577. Comparison - Acid and Alkali Zinc Plating [India]
27578. Dissimilar metals - stainless steel and nickel plated brass [New York]
27579. Teflon coating of small parts [Texas] {2/25/04}
27580. Chrome plating ABS for a hobbyist's passion of cars [New Jersey] {2/25/04}
27581. Rechroming my rims [New Jersey] {2/25/04}
27582. Re-chroming of my truck rims [New Jersey] {2/25/04}
27583. Electro static painting equipment wanted [New Mexico] {2/25/04}
27584. OPENING NEW CHROMING SHOP [Kentucky] {2/25/04}
27585. Conductive Paints [Ohio] {2/25/04}
27586. Art student needs to print on steel [Northern Ireland]
27587. Different RH at different temperatures [Sweden]
27588. What Is White Brass? [Massachusetts]
27589. How to dissolve gold potassium cyanide for coating purpose [India]
27590. Chrome Plating Exhaust Systems [Ohio]
27591. Rusting Patina for Cast Iron [Texas]
27592. Rust to Gunmetal [Massachusetts]
27593. Mechanical finishing of body jewelry [Oregon]
27594. Need to color steel shotgun barrel [Texas]
27595. Painting a scene on corrugated steel building [Louisiana]
27596. Removal of copper electroplating [Kentucky]
27597. Indium alloy solder adhering to titanium tip [Singapore]
27598. Removing powder coat from aluminum [Vermont]
27599. Improving de-smut for chromate conversion coating [Korea]
27600. Seeking electrostatic painter [Georgia] {2/25/04}
27601. Equipment to differentiate grade of stainless steel [Singapore] {2/25/04}
27602. Difficulty finding tinting ratios for '65 Mini Cooper [California]
27603. Removing gold plating from brass [Oregon]
27604. Gold under Nickel [Idaho]
27605. USA regulations or guidelines for jewelry plating? [New Zealand]
27606. Plastic dipping and powder coating of RC components [Washington] {2/25/04}
27607. Equipment and technical resources for hot dip galvanizing [Vietnam] {2/25/04}
27608. STAINLESS STEEL VS MARINE GRADE ALUMINUM [Iran]
27609. Ceramic coat motorcycle pipes [Massachusetts] {2/25/04}
27610. Zinc plater [Australia] {2/25/04}
27611. Teflon coating [Turkey] {2/25/04}
27612. RVS corrosion due to copper reaction? [The Netherlands]
27613. Sublimation coating formula and process [Indiana]
27614. Tintillate Process [Singapore]
27615. How hard is "Hard Anodizing" [Australia]
27616. Low friction coating for solder mask [France]
27617. Seeking vintage refrigerator painter [Washington] {2/26/04}
27618. Decorative chrome refinish muscle car console [Indiana] {2/26/04}
27619. Need Used Abrasive Media [New Mexico] {2/26/04}
27620. My pennies are floating [Ohio]
27621. Remove surface oxide of Al-alloy [Kentucky]
27622. Chemically stable and highly conductive metal films [Illinois]
27623. Brass help [Michigan]
27624. Polishing Brass Tabernacle [Pennsylvania]
27625. Tank material of Electroless Ni Solution [Indonesia]
27626. Petrol resistance - 2k PU system [India]
27627. Why nickel/copper coating peeled off aluminum [China]
27628. Fatigue strength loss due to hard anodize treatment [Pennsylvania]
27629. Alodine/Iridite Issues [Wisconsin]
27630. Supplier for Phenolic Resin [Mauritius] {2/26/04}
27631. JEWELER NEEDS ELECTROPLATING MACHINES [China] {2/26/04}
27632. Students seek So. African form with cobalt in wastewater [South Africa]
27633. Silkscreen Peel Test Description [Singapore]
27634. Analytical test method for Alkalis (K2O and Na2O) [Tanzania]
27635. Reliable method and supplier for painting zamak 5 component [Bulgaria]
27636. What is Galvanneal? [Virginia]
27637. Chrome cracking [Canada]
27638. Production of silver cyanide from silver nitrate [Turkey]
27639. Anodizing on Aluminum EPS dies [India]
27640. Cleaning bond areas of nickel/silver plated lead frames [Michigan]
27641. Electrical Resistance Testing for Chromate Conversion [Malaysia]
27642. Need parts salt bath nitrided by NADCAP shop [Illinois] {2/27/04}
27643. What salt is formed from iron? [UK]
27644. FeO processes [Indiana]
27645. Non Cyanide Copper Plating of 14 ga Mild steel art work [Washington]
27646. I want galvanized bumpers [Canada]
27647. Choosing anode material for electrocleaning tank [Singapore]
27648. Health effects from an artesian water well cased with galvanized pipe [California]
27649. 17-4ph discolors upon heat treatment [Washington]
27650. Need Two sets of Rims Rechromed [South Carolina] {2/27/04}
27651. Grinding equipment for plug valves [Texas] {2/27/04}
27653. Rate of penny corrosion [California]
27654. How can I test for genuine plating? [Massachusetts]
27655. Painting Golf Clubs [Tennessee]
27656. Surface finish formula [Michigan]
27657. Anodizing MX quad racer in a 5 gallon bucket [Canada]
27658. Corrosion Protection for Aluminum in Water [Wisconsin]
27659. Enquiry for galvanizing plant [India] {3/1/04}
27660. Plating [Pennsylvania]
27661. Need plating thickness gauge [India] {3/1/04}
27662. Booster club needs penny clean up help [Texas]
27663. Problem in kanigen plating [India]
27664. Best cleaner for brass radiator mfg. [Saudi Arabia]
27665. Need chrome plating on custom chopper parts [North Carolina] {3/1/04}
27666. Machine shop needs tefni coating [New York] {3/1/04}
27668. Need a Teflon coating for heated aluminum plates [Lebanon] {3/1/04}
27669. Need Teflon paint thinner [Iran] {3/1/04}
27670. Redip spoke wheels for '88 Mustang [Pennsylvania] {3/1/04}
27672. Immersion tin plating too thin [Pennsylvania]
27673. Chrome plating carbon composites [New Zealand]
27674. Cylinder bore hard anodizing questions [Ohio]
27675. Powder Coating builds around masked holes [Iowa]
27676. Rechrome my 20 inch rims [New Jersey] {3/1/04}
27677. Inquiry for high temperature paints in multi colors [Texas] {3/1/04}
27678. Need supplier of zinc blocks for galvanizing [UK] {3/1/04}
27679. Changing brass to chrome or patina [New Mexico]
27680. Spent Citric Acid Disposal [Pakistan]
27682. Titanium nitride coating on rotary blades [India] {3/1/04}
27683. Need chroming of grill and headlight covers [Pennsylvania] {3/1/04}
27684. Thickness meter for magnetic card [Iran] {3/1/04}
27685. Need a used AA Sprectrometer [India] {3/1/04}
27686. Wrinkle paint by Sherwin Williams [Texas] {3/1/04}
27687. TO WAX OR NOT TO WAX? [Kentucky]
27688. Quantitative analysis of nitric acid in a mixture of nitric and sulfuric acid [India]
27689. How to seal the edge of a PVC laminate [Australia]
27690. Out-gassing in aluminum castings [Florida]
27691. Nickel electroplating on polyaniline (conductive polymer) [Denmark]
27692. Need Mazda frame powder coated or painted [Nebraska] {3/2/04}
27693. Photo resist to be used to etch solid steel [India] {3/2/04}
27694. Low coefficient of friction paint for pinewood derby car [Arizona]
27695. Titanium plating on steel products like manicure items [UAE]
27696. Copper plating steel wire equipment [Peru] {3/2/04}
27697. Water pipe connectors turning green [North Carolina]
27698. Trouble with NADCAP Audits [California]
27699. Recovery of cyanide from Ag effluent [India]
27700. HOW TO SOLDER TITANIUM [New York]
27701. Zero defects in plating aluminum [India]
27702. Silver corrosion by zinc based additives in lubricants [California]
27703. PVC MIST ELIMINATOR [India] {3/2/04}
27704. Adhesive applied on glass at 700 C [Pakistan]
27705. Metal finishing [New York]
27706. Need inorganic sealant after HVOF process [Taiwan]
27707. Plating Finish for Shields used on Connectors [Philippines]
27708. Dark spots in nickel and how to lower my ph level in nickel bath [Louisiana]
27709. Chrome my '94 Corvette wheels [Alabama] {3/2/04}
27710. Need OPC Drum Tester and Recoating and Refurbishing Portable Machine [Philippines] {3/2/04}
27711. Cyanide for aromatherapy [England]
27712. Natural rust patina, use and care [Washington]
27713. Is this yellow ring my stolen white gold ring? [Illinois]
27714. Cleaning the "golding effect" on 304 stainless exhaust tips [Mississippi]
27715. Changing polished chrome to brushed [South Carolina]
27716. Can you re-finish a brass finish by 'dipping' it into a satin nickel finish? [Colorado]
27717. Painting 304SS lumber kilns with epoxy coatings [Florida]
27718. Anodizing titration automation [Idaho]
27719. Clear anodizing aluminum appearance flaws [Washington]
27720. 303 stainless steel to brass galling [Missouri]
27721. Metal printing and can printing machines [China] {3/2/04}
27722. R O deionizer [Pakistan]
27723. Silver coating glass with silver nitrate [Florida]
27724. Clear protective coating for sand cast aluminum [Australia]
27725. Electroplating wood [Washington]
27726. Aluminum Finish called AMM43 Medium Matt [California]
27727. Need my rims dipped [Illinois] {3/2/04}
27728. Want to know information about aluminum powder and paste [South Korea] {3/2/04}
27729. Electrophoretic lacquer as gold plate alternative [California] {3/2/04}
27730. Ni-diamond composite powder with spiky [Korea]
27731. Nitriding valve springs [Michigan]
27732. Acids and elements [California]
27733. Etching tantalum for metallography [Australia]
27734. Interlead short during soldering [Thailand]
27735. Acid copper plating void holes [Malaysia]
27736. Silver plating thickness [India]
27737. Need salt spray machine [China] {3/3/04}
27738. Alumina research for underground cables [Italy]
27739. Black finish for cast iron [Michigan]
27740. Finishing Method for Bright (mirror surface of) Aluminum Sheets [Korea]
27741. How can I get good adhesion of organic coatings to anodized surfaces [Indiana]
27742. Need stainless steel coating to fight static [Massachusetts]
27743. Activator for PCB and PTH not stable [Iran]
27744. Wanted vendors for aluminum alloy hard anodizing [New York] {3/3/04}
27745. Abralon 180 pads [France] {3/3/04}
27746. Need used Nordson powder guns [Wisconsin] {3/3/04}
27747. How to macro etch stainless steel 316 [Michigan]
27748. Laser Burning Galvannealed Steel [Kentucky]
27750. Need silver/white anodize process [California] {3/3/04}
27751. Need basecoat and topcoat lacquers for vacuum metalizing [Pakistan] {3/3/04}
27752. Galvanic action on cooling coils [Missouri]
27753. Seeking bronze plater of Zinc/Al castings [Illinois] {3/3/04}
27754. Coefficient of expansion of hardened oils [Canada]
27755. Electroplating for engine block repair [Australia]
27756. PVD and Plating Differences [Maryland]
27757. Who has a good nonchrome desmut? [Oregon] {3/3/04}
27758. Mirror finish water based chrome paint [Australia]
27759. Will a clear anodized finish hold up in either / both chromatic and sulfuric acids? [Minnesota]
27760. Prolonged UV resistant coating with good release properties [California] {3/3/04}
27761. NIKASIL PLATING [Wyoming] {3/3/04}
27762. Iron-Chrome Co-Deposition [Argentina]
27763. Aluminum Protection from Corrosion [Illinois]
27764. Anisotropic etching of aluminum [Indiana]
27765. Switching my refrigerator door [Utah]
27766. Details on hydrogen embrittlement [India]
27767. HOT DIP [Iran]
27768. Zinc chrome same as Zinc Ni alloy? [Thailand]
27769. Zinc Plated carbon steel (gr) bolts to 304 sst [New York]
27770. Applicable material to be welded on carbon steel [Philippines]
27771. Plastisoling service required [Canada] {3/4/04}
27772. Aluminum irridite thermal conductivity [California]
27773. Outdoor use of colored anodized aluminum embedded in concrete [California]
27774. Looking to buy Versa Spray powder guns [Wisconsin] {3/4/04}
27775. Using Muratic Acid to etch concrete [California]
27777. Plating of Engineering Plastics [Arizona]
27778. MIL-R-7575C resin [Oregon] {3/4/04}
27779. Aluminum clad cleaning or refinishing [Maryland]
27780. Refinishing Vinatage Steel Desk [California]
27781. Black Oxide Specification and Drawing Description [New Jersey]
27782. Treatment of 416 SS [Georgia]
27783. Need clear coating on zinc die castings [Michigan] {3/4/04}
27784. Silver, mechanical, hot dip and delta tone plating [China] {3/4/04}
27785. Need platinum black electroplating [New Jersey] {3/4/04}
27786. Substitution of stainless or aluminum for plated steel grating [California]
27787. Durable Black Finish for 303 Stainless Golf /Putters [Ohio]
27788. Jeweler getting brown spots in rhodium plating [Indiana]
27789. Alocrom1200 and Alocrom1000 [China]
27790. Standard for zinc plating [Thailand]
27791. Need "nickel seal" for bright nickel plating [India] {3/4/04}
27792. Research lab needs brightener for bronze plating [Singapore]
27793. Remove and prevent rust [Texas]
27794. Achieving even black patina on zinc [Florida]
27795. Water drop test for silver migration detection [Israel]
27796. Plating options to avoid cadmium [India]
27797. Composite plating for diamond [India]
27798. Zinc peels off at bending corners [Egypt]
27799. Aluminum H2S [UK]
27800. Seeking company that can nikisil steel liners for V-12 aircraft [California] {3/4/04}
27801. Information about electroplating [India]
27802. Nickel Plating vs. Chrome Plating SLA Parts [Ohio]
27803. Powdercoat outcasting [Pennsylvania]
27804. Ammonium bifluoride wastewater [South Carolina]
27805. NEED BRASS BED REFINISHED [Florida] {3/5/04}
27806. Sublimation On Plywood [Maryland] {3/5/04}
27807. Diffuse coating on smooth surface [Massachusetts]
27808. Etching of Ni-alloy billet material [New York]
27809. Have 50,000 small aluminum clips that need inexpensive dark coating [Kansas] {3/5/04}
27810. Sourcing for nickel flake or powder for black conductive paint [Malaysia] {3/5/04}
27811. Dulling anodizing to permit infrared temperature noncontact measurement [Texas]
27812. Determination of silver concentration in ppm levels [Delaware]
27813. How to color aluminum for jewelry purposes [Massachusetts]
27814. HOW TO RECOVER PLATINUM FROM CATALYTICS CONVERTERS [Mexico]
27815. Distilling hydrochloric acid [Australia]
27816. Dissolving aluminum [Minnesota]
27817. COPPER PLATING WITH SULFURIC ACID [New York]
27818. Pitting problem in nickel sulfamate bath [Pennsylvania]
27819. Chipped Nickel Plate on Stainless Steel [Illinois]
27820. Titanium Plating [Illinois]
27821. Jagged edge on plating [Singapore]
27822. ID burnishing on Hard coat anodizing, before? or after? to achieve RA of 15 max [Wisconsin]
27823. Dust collection from aluminum and steel grinding [Nebraska]
27824. Need Indian Suppliers/Distributors of Armohib and Amchem [India] {3/5/04}
27825. Need Gloss Meter 20/60 [India] {3/5/04}
27826. Need zinc cobalt coating process [India] {3/5/04}
27827. Chef needs titanium re-coating of high-heat kitchen pans [Canada]
27828. Setting up hard anodizing on 7075 aluminum alloys [Italy]
27829. Electropolish on 17-4PH [Israel]
27830. Casting Material Selection [UK]
27831. Plating plastic auto trim [Canada] {3/8/04}
27832. Need "Spray on chrome coating" [Ohio] {3/8/04}
27833. Type of paint for hand art on a vehicle [Texas]
27834. IPS or wet plating [England]
27835. Suspension agents for glycol ether systems [New Jersey]
27836. Researcher needs plasma chamber anodized [Texas] {3/8/04}
27837. Gold refine machine [India] {3/8/04}
27838. Painting PVC pool jets [Michigan]
27839. Re-dip my titanium facemask [Maryland] {3/8/04}
27840. Looking for a company who could reproduce an oiled bronze finish [Illinois] {3/8/04}
27841. Chrome failure on '02 Harley V-rod [Louisiana]
27842. Nickel coating layer thickness control [Egypt]
27843. Having trouble finding raw Zinc (solid) [California]
27844. Finding a good chrome shop [Georgia]
27845. Want alternative to manual buffing in stainless steel [India]
27846. 2nd tier auto supplier needs electrochemical deburring machines [England] {3/8/04}
27847. Finishing Machines Manufacturer [India] {3/8/04}
27848. Compare galvanized to powder coat please [California]
27849. Seeking anodizing of exhaust cans for Suzuki TL1000R [Florida] {3/8/04}
27850. Aircraft hardware needs H-11 plating process [New Jersey] {3/8/04}
27851. Stainless steel cages for exotic birds are failing [Florida]
27852. Coating copper to inhibit tarnishing. How? [Canada]
27853. Black chrome wheels for Lexus [Missouri] {3/8/04}
27854. Conductive Copper Paint [Maryland] {3/8/04}
27855. How to make a corrosion in a stainless steel needle [Brazil]
27856. Creating a homemade plastic coating setup [Pennsylvania]
27857. Sterling silver plating of cabinet hardware [Massachusetts]
27858. Porosity Post - machining [India]
27859. Bacteria in Electroclean Rinse [Arkansas]
27860. E-coating standards for sterling silver? [Israel]
27861. Iron contamination in chrome plating baths [UAE]
27862. Passivation vs. bead blast [Texas]
27863. Polishing of stainless steel scrub stations [India]
27864. Question on plasma nitriding of steel [Egypt]
27865. Copper Conductivity [Canada]
27866. Removing scratches from white gold ring [UK]
27867. Building a shower stall with liquid vinyl [Pennsylvania]
27868. Standard for black trivalent chromate [Malaysia]
27869. Analysis of surfactants by MBAS and CTAS [India]
27870. How to remove pits from stainless steel vessels [Indiana]
27871. Mil Spec Heavy Phosphate 20k lb [Florida] {3/9/04}
27872. Simultaneous plating of two different metals [UK]
27873. Re-plating an engagement ring with accent diamonds [Texas]
27874. Infrared curing of solvent sprayed in sheet metal [India]
27875. Powder coating pre treatment process after galvanizing [India]
27876. Nickel-Iron Plating for perforated Nickel Rotary Screen [India]
27877. Can silver plated bus bar be tin plated? [Singapore]
27878. Cyanide copper plating [Australia]
27879. Need suitable MOC for ammonium chloride at high temp [India]
27880. Seeking gold plater of plastic parts [Minnesota] {3/9/04}
27881. Chrome plate ABS plastic, or provide equivalent appearance, for motorcycle shop [Michigan] {3/9/04}
27882. Aluminum anodized pore diameter [Canada]
27883. Chrome plating problem- wavy metal [Michigan]
27884. Oxalic acid testing of black oxide [Indiana]
27885. Pre-treatment Problem [India]
27886. User experience with chemical grafting [New York]
27887. Durability of plating a brass sink [Washington]
27888. Stress relieving of magnesium to prevent warpage [New York]
27889. Cracks on corners of 316 SS phosphoric solution tank [Connecticut]
27890. Need a recommended process spec for painting zinc castings [California]
27892. Is tin a problem in galvanized coatings? [Massachusetts]
27893. Avoiding waviness on the finished stainless steel surface [UAE]
27894. Platinum plating of inconel wire [Belgium] {3/10/04}
27895. Retro-reflective coating of small beads [Singapore] {3/10/04}
27896. Need Salt spray test on Zinc plated CRCA Sheet (yellow passivation) [India] {3/10/04}
27897. Need electroless nickel service [China] {3/10/04}
27898. Artist wants chrome plating on fiberglass [New York] {3/10/04}
27899. Re-chrome my vehicle wheels [UK] {3/10/04}
27900. Need bronze plating of boots, one pair [Wisconsin] {3/10/04}
27901. Need Nikasil Equipment [Wyoming] {3/10/04}
27902. Need help with proposed zinc plating plant [Thailand] {3/10/04}
27903. Gold assaying machine [India] {3/10/04}
27904. Need a roller as specified in MIL-STD-141, Method 6301 [Massachusetts] {3/10/04}
27905. Copper Cyanide bath/plating help [Australia] {3/10/04}
27906. Need nickel-free hematite plating process [Rhode Island] {3/10/04}
27907. Roughness of a zinc plate surface [South Africa]
27908. Aluminum Alloy Plating [China]
27909. Anodizing of aluminum pigeon leg rings [Saudi Arabia]
27910. Hardfacing a steel cam [California]
27911. Streaky anodizing [UK]
27912. Contamination between 304 and 316 stainless [England]
27913. Possibility of reaction of nitrogen with Ti-Al-V [Mexico]
27914. Pin holes in 316SS heat exchanger in amine service [India]
27915. Automotive Acid Dipping Needed [Pennsylvania] {3/10/04}
27916. Powder coat my bike frame [Kentucky] {3/10/04}
27917. Need paint or anodizing of rivets [Pennsylvania] {3/10/04}
27918. Starting a cylinder plating and repair business [Canada] {3/10/04}
27919. Calibrating pH meter [India]
27920. 304 Stainless Steel Heat Colouring Thesis [Canada]
27921. Connecting copper pipes to chromed ones [Washington]
27922. Yellow vs. blue chromated screws [Germany]
27923. Preparing copper for patina finish [Pennsylvania]
27925. Space qualified high temp silver plating [India] {3/11/04}
27926. Needing chrome work, information about preparation of metal [California] {3/11/04}
27927. GM Spec Autophoretic [Massachusetts] {3/11/04}
27928. NEED USED FINISHING/POWDER EQUIPMENT/SYSTEMS [Ohio] {3/11/04}
27929. Need clearcoat for faux wood finish [Florida] {3/11/04}
27930. Chrome plate my Monte Carlo plastic ground effects [Indiana] {3/12/04}
27932. Passivation [New Mexico]
27933. Polish anodized tumblers [Ohio]
27934. Removing oxidation from a tinned chocolate mold [Canada]
27935. Chrome removal [Canada]
27936. Barbeque kit coating/finishing [India]
27937. Painting aluminum sheet metal [North Carolina]
27938. Powder coating on galvanized sheet [Jordan]
27939. Want non-CN diffusion brass plating on wire [India]
27940. Need to increase chrome hardness [Bangladesh]
27941. Chrome vs. Nickel plating of keychains [North Carolina]
27942. Comparing the advantages of different finishes [Portugal]
27943. Copper extraction from copper sulfate [Iran]
27944. Repair chrome rim [Maryland]
27945. Restore interior of rusting cast iron teapot [New Jersey]
27946. Rhodium plating directly on silver [New York]
27947. Adhesive doesn't stick to Chemfilm [California]
27948. What type of tumbling media should I use? [Texas]
27949. Electrolytic corrosion of dome [Australia]
27950. Conversion shop needs custom plating of plastic [Michigan] {3/12/04}
27951. Re-plating my Rogers Co goldplated flatware [California] {3/12/04}
27952. Rechroming of my auto wheels [Missouri] {3/12/04}
27953. Looking to introduce oil rubbed bronze finish on our kitchen and bath hardware [Texas] {3/12/04}
27954. Urgently need PVD system [Turkey] {3/12/04}
27955. Oxygen-free copper [Egypt] {3/12/04}
27956. Furniture mfgr. needs clearcoat for mild steel furniture [Illinois] {3/12/04}
27957. Need SPCC panels immediately [Indiana] {3/12/04}
27958. TITANIUM COLOR TECHNOLOGY REQUIRED [Pakistan] {3/12/04}
27959. Stainless steel glue [Canada] {3/12/04}
27960. Need waste penetrant treatment plant [UK] {3/12/04}
27962. Fire Suppresion Agents Corrosiveness on Different Materials [New Jersey]
27963. Removal of heat treatment scale [Arkansas]
27964. Risk from heavy metals [India]
27965. Green Stains on Enamel BathTub [UK]
27966. Can I faux paint a table top to look like galvanized metal? [New York]
27967. Silver nitrate coating [UK]
27968. Rate of corrosion to imports and aluminum cars [New York]
27969. European Finishing Specs [Alabama]
27970. "Standards Documentation" for Powder Coating [India]
27971. Type of non-conductive media to be used between Stainless Steel and A36 Steel [Maryland]
27972. Stripping chrome from alloy steel (41) [Canada]
27973. How to keep copper parts bright and shiny for at least 6 months? [India]
27974. Remove nickel comtamination from immersion gold bath [Colorado]
27975. Sodium hypophospite [Indonesia]
27976. Cost of pickling pipe [Ohio]
27977. Diffusion of oxygen in silver platings during post-plate heating [California]
27978. Which hand tool plating for aerospace [India]
27979. Plating Peel Off [India]
27980. Bubbles under Hard Coat [California]
27981. Bright dip for Aluminum [Canada]
27982. Testing efficacy of passivation on stainless steel parts [Mexico]
27983. Will magnetism in 304L stainless steel cause corrosion? [Massachusetts]
27984. Removing weather stain from stainless steel [Canada]
27985. Rechrome my '66 Bonneville parts [Massachusetts] {3/12/04}
27986. Clear coating carbon steel to prevent rust [Georgia]
27987. Polyester treated tiles [California]
27989. Anodizing Specification UN-D 469 18+-2 Micron [Michigan]
27990. Anodizing Flakes Off of 7075 Parts [Brick, NJ]
27991. Need Automatic Polishing Machine for Stainless Steel Sinks [India] {3/15/04}
27992. Advantages of cashew nut sheath as sorbent for defluoridation of water [India]
27993. Nickel-Alumina composite coating [Iran]
27994. Electroplating brass to lead [Canada]
27995. Zn removal from wastewater [Slovenia]
27996. Lacquer coating over Brass/Copper to avoid tarnish [India]
27997. Pitting nickel plating [Thailand]
27998. 7 Tank process, surface preparation process [India]
27999. Galvanic corrosion of building [Australia]

The finishing.com Hotline includes more than 40,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2005