22000. Deteriorating Hard Anodizing Tank? [South Africa]
22001. Cleaning of alumina on the surface of metal after the process of tumbling [Malaysia]
22002. Stopping destructive properties upon hot copper by PVC sheeting [California]
22003. WEAR PROBLEM WITH ALUMINUM VACUUM PLATES [New York]
22004. Electroplating brighteners [Texas]
22005. Secondary Electron Emission from Ions Impacting Stainless Steel [Alabama]
22006. Re-nickel a drum in black, saving the engraving [New York]
22007. Brass protection [California]
22008. Anodizing pitting problem [Canada]
22009. Replacing fuses with circuit breakers [Illinois]
22010. Aluminum cathodes for anodizing [Louisiana]
22011. ASSURING STEEL IS UNPASSIVATED [Canada]
22012. Powdercoating aged alodine [Minnesota]
22013. Converting Zinc baths to Zinc-Alloy and Smart Zinc [Arizona]
22014. Need AL flatstock plated, polished or otherwise processed to achieve "mirror" finish [Maryland] {5/23/03}
22015. Need Used Salt Spray Chamber [Minnesota] {5/23/03}
22016. Koyo green buffing compound [Tennessee] {5/23/03}
22017. Electroplating Metals [Texas]
22018. Control methods [France]
22019. Maintaining a shiny brass condition in an adverse environment [New York]
22020. Cleaning a military bronze cemetery plaque [Michigan]
22021. Spearco Mustang intercooler coatings for corrosion protection [Maryland]
22022. Automotive Alusil block piston coating solution request [UK]
22023. Base metal choice [Minnesota]
22024. MIL-C-5541 Class 3 [Germany]
22025. How to dispose/sell Used TCE ? [India]
22026. Alodine 600 rinsing question [California]
22027. Titanio negro [Argentina]
22028. Machined Surface Value Mystery [Texas]
22029. Make steel black without painting [Ohio]
22030. Cleaning oxided solingen steel knive [Texas]
22031. Rhodium plating in my jewelry shop [California]
22032. TT-P-1757 types [California]
22033. New technology replace vacuum metallized process [Thailand]
22034. Consumption of nickel anodes [Egypt]
22035. Need a replacement process for etching aluminum [Florida]
22036. Sulfuric Acid coagulation issue [California]
22037. Masking Technique for Jewelry with Irregular Shape and Cutouts [California]
22038. Internal rust removal [Maryland]
22039. HOW DO YOU PASSIVATE [Virginia]
22040. Etching Pen [Washington]
22041. Need a place to chrome my wheels [North Carolina] {5/27/03}
22042. Acid dip and e coat of automotive sheet metal parts [Ohio] {5/27/03}
22043. Conductive paint for rf shielding [India]
22044. Seeking tinning artisan - craftsman [Connecticut] {5/27/03}
22045. Black Oxide For Furniture Use [New York]
22046. Heat resistant metallic paint [Connecticut] {5/27/03}
22047. Electroplated Black Ru/ Black NiCo / Ni Stripping [China]
22048. Dip clean and lacquer a brass bed [Connecticut] {5/27/03}
22049. FLAME SPRAY ON 365 ALUMINUM CASTING "LARGE" [Pennsylvania]
22050. STEEL BALL MACHINES [India] {5/27/03}
22051. Nickel plated over copper leadframe [Thailand] {5/27/03}
22052. Re-enamel cast iron tub [New York] {5/27/03}
22053. Need ABS chrome plated [Florida] {5/27/03}
22054. Seeking chrome dipping of 4 rims [Washingtgon DC] {5/27/03}
22055. Seeking primer for PVC coating [China] {5/27/03}
22056. Protective coating for vacuum-deposited aluminum [Canada] {5/27/03}
22057. Prospects of a metallurgical and materials engineer [Nigeria]
22058. Copper [Canada]
22059. Gold Glazing like Ishtar Gates [Georgia]
22060. Building a lab scale electrocoagulation unit [Australia]
22061. Glass Phenolic Composite Mold Part Coating [Iran]
22063. How to prevent rusting? [Malaysia]
22064. Reaction mechanism of silver immersion plating [South Korea]
22065. Painting over chrome on bicycle? [New York]
22066. Assaying copper cyanide [India]
22067. Bending 316 stainless rod by heating [Canada]
22068. Should I polish my motorcycle, or should a professional? [California]
22069. Lacquer removal on copper cookware [Michigan]
22070. Chrome detailing interest [Canada]
22071. What to do about crystals in my copper forming tank [California]
22072. Need information on electroplating copper to steel [Nevada]
22073. Testing of Black Chrome Coating [India]
22074. Maintenance of pH of rinse water [Canada]
22075. METALLIC TESTS FOR PLATINUM [Florida]
22076. Stripping of DLC with Ti underlayer [China]
22077. Mechanical plating [UK]
22078. Plasma Nitriding [India]
22079. Antiquing of copper and brass [Indonesia]
22080. Brush Chrome [South Africa]
22081. Crack in tin lead plating [Israel]
22082. Nickel/chromium plating method [Iran]
22083. Chromate conversion coatings [Indonesia]
22084. Selection of Surface Finish For Steel Structure [Jordan]
22085. Need chrome refinisher [California] {5/28/03}
22086. Seeking Chrome Plating for Brand New Range Rover Wheels [Michigan] {5/28/03}
22088. Nickel plating equipment and chemistry [Iran] {5/28/03}
22089. Calibration standards for XRF machine [Malaysia] {5/28/03}
22090. Polyester coating for sublimation [Macedonia] {5/28/03}
22092. Ruthenium Plating Process [California] {5/28/03}
22093. How to bond nickel [Pennsylvania]
22094. Splash anodizing a paintball gun [Colorado]
22095. DISAPPOINTED NEW BRIDE [Illinois]
22096. Polishing a Cast Aluminum Intake Manifold [Michigan]
22097. Request for help fixing water problem [North Carolina]
22098. Polished mild steel [Canada]
22099. Painting galvanized steel swing set [Massachusetts]
22100. Zinc nickel/cobalt plating and hex chrome [Canada]
22101. Teflon for molding [Mexico]
22102. Corrosion in nickel-cadmium plating [Italy]
22103. Seeking anodization/colors/methods for 300 series stainless [Virginia] {5/28/03}
22104. PHILIPPINE ALODINE CLASS 3 DISTRIBUTOR [Philippines] {5/28/03}
22105. Cleaner for ABS plastic molded parts [Indonesia] {5/28/03}
22106. Copper screws [New Jersey]
22107. How to put the bling back in chrome [Illinois]
22108. NiTi market? [Israel]
22109. How to remove magnetism caused by mechanical shaping of stainless steel plate? [Finland]
22110. How to clean ABS plastic parts before plating process [Indonesia]
22111. The repairing process of roller bearing axle [Iran]
22112. Patchiness on black anodized parts [Canada]
22113. Magnesium Alloy Products with Dow 19 Impregnation [Canada]
22114. Looking for PTFE Car Coating Company [Canada] {5/28/03}
22115. Dull dark silver patina for copper [India]
22116. TOP COAT ON GOLD PLATING [India]
22117. Plating Graphite Rod [California]
22118. Adhesion problems [Kentucky]
22119. Looking for a low cost free-boron ion treatment [Malaysia] {5/29/03}
22120. NEED HARD CHROME ELECTROPLATING UNIT [Egypt] {5/29/03}
22121. Cleaning and etching of titanium [Maryland]
22122. Muriatic solution uses in a metallurgical setting [Canada]
22123. Ra and Hardcoat [Idaho]
22124. Replace Arts and Crafts copper on Grandfather Clock [New Zealand] {5/29/03}
22125. Need five Jeep Alloy Wheels Stripped, recoated [Virginia] {5/29/03}
22126. Need motorcycle exhaust rechromed/refinished [Illinois] {5/29/03}
22127. Seeking EPZ mechanical zinc coating of bulk lots of steel clips [Ohio] {5/29/03}
22128. Seeking plating of Zytel 77G33L plastic [Wisconsin] {5/29/03}
22129. GLITTER CUTTING MACHINERY [UK] {5/29/03}
22130. Plastic finishing product [Singapore] {5/29/03}
22131. Can I Refinish a Trombone? [South Carolina]
22132. Does re-plating require removing gemstones [Canada]
22133. Alloy wheel refurbishing [West Virginia]
22134. Prime after Chem Film of Aluminum Parts [New Jersey]
22135. Fumes in Galvanized Plumbing [Maryland]
22136. Mercury disposal treatment [Philippines]
22137. Paint Peeling problems on Prepainted Galvanized Steel Sheets [India]
22138. A-2 CAM PLATING [Tennessee]
22139. Satin Anodized Aluminum [California]
22140. Degreasing copper wire mesh [India]
22141. Phosphorus content after electropolishing [Georgia]
22142. Sterilizing Manicuring Implements Utililizing An Autoclave [Arizona]
22143. Malcomize of 316SS material [Florida]
22144. Baltimore or DC area Metal Plater Needed ASAP [Pennsylvania] {5/30/03}
22145. Plating metal layers over carbon/graphite fiber composite materials [California] {5/30/03}
22146. Plating PVD brass sink [Wisconsin] {5/30/03}
22147. Name of company w/ rust and paint removal dipping process [Washington] {5/30/03}
22148. Lightning conductors [South Africa]
22149. Acid washed anodizing? [Oregon]
22150. Modulus of elasticity without the weight [Arkansas]
22151. Tin Oxide Layer on Hot Tin Dipped Plating Turns Yellow [Massachusetts]
22152. Electroless Nickel Plating for A356.2 aluminum parts [Canada]
22153. Electroforming [India]
22154. Aluminum Cast Finish for Plasma Process Chamber [Florida]
22155. FINISH 6.1.2 OF MIL-STD-171 NEEDED FOR VOLUME JOB [New York] {5/30/03}
22156. Stripping e-coat racks [Colorado] {5/30/03}
22157. Consultant to improve our passivation paste [China] {5/30/03}
22158. Co-efficient of friction for different plating [India]
22159. Copper tungsten [China]
22160. Chrome plating machines price range [South Carolina]
22161. How to preserve the shine on copper [California]
22162. Chrome bath [Pennsylvania]
22163. Rhodium question in a wedding band [New York]
22164. Difference between electro galvanized steel and hot dip galvanized steel [India]
22165. Early Rhodium Plating History [Germany]
22166. "BLACK/WHITE" Stain Elimination [Texas]
22167. Help for setting up a duplex nickel plating line [India]
22168. Parkerizing of rubber to metal bonded parts [India]
22169. Wheel dipping [Connecticut] {6/02/03}
22170. Anodizing sheets of aluminum [Nebraska] {6/02/03}
22171. Looking for an Anodizing Rectifier [Florida] {6/02/03}
22172. Need info on flouropolymer [New Zealand] {6/02/03}
22173. Need a new Polisher and Electro-plating for Stainless [Tennessee] {6/02/03}
22174. Green Engraver Parts [Massachusetts] {6/02/03}
22175. METAL TREATMENT AND BLACKENING PROCESS/PRODUCT [India] {6/02/03}
22176. Removing black oxide [Ohio]
22177. Old Copper Fire Extinguishers [Illinois]
22178. HELP! clear finish for gold plated parts that actually stays on and is durable [Tennessee]
22179. Shiny brass plated to antique brass [Michigan]
22180. Powder coat removal [California]
22181. Refinishing stainless steel with a brush finish [California]
22182. Painting an aluminum swingset [Massachusetts]
22183. Copper's aged look [Arizona]
22184. PETN / Pentastit? [Iran]
22185. Analysis [Malaysia]
22186. Black Organic [Taiwan]
22187. Alternative to 316 SS for a leaf spring [California]
22188. Barrel Plating Anode Design [Philippines]
22189. Copper Oxidation Level [Malaysia]
22190. Industrial Process for Painting Screw Heads [Mexico]
22191. Acrylic Metal Lacquer Breakdown [North Carolina]
22192. Electroless platinum weld to electroless Indium [Canada]
22193. Pits in copper plating [California]
22194. Need for woods nickel strike [Greece]
22195. Pitting? [Minnesota]
22196. Lusterless Black Anodizing [Malaysia]
22197. SURFACE FINISH OF ALUMINUM ALLOY PISTON [India]
22198. I NEED PARTS NICKEL/CHROME STRIPPED [Ohio] {6/02/03}
22199. HOW to get into plating business [Alaska]
22200. Pretreatment steps for hard chromium plating [Algeria]
22201. Looking for copper sulphate for roots. What happens in the sewer pipe [Ontario]
22202. How to get brushed or mirror finish on s.s. BBQ pit? [Texas]
22203. Repainting tin roofs? [Minnesota]
22204. What chemical can I use to turn a copper pipe verdigris? [Washington, DC]
22206. Using hypochlorite to clear murky water [Ireland]
22207. Keep Copper Coating from blackening [Virginia]
22208. Trivalent chromate compounds and international standards [Scotland]
22209. Hazards of pickling in sulphuric acid [Egypt]
22210. Electroless cobalt plating [Oregon]
22211. Etching of Nitinol [Switzerland]
22212. S.S. scratch finishing machine [India]
22213. Help me find a zinc post-plater [Indiana] {6/03/03}
22214. Rechroming artic cat cylinders [Maine] {6/03/03}
22215. HOW, WHERE, WHICH .... TO RHODIUM PLATE? [UK] {6/03/03}
22216. Anti Tarnish S [Massachusetts] {6/03/03}
22217. Sacrificial anode [Libya]
22218. Does deionized water affect nickel plated aluminum [Colorado]
22219. Novice restoring an iron bed [Ohio]
22220. Putting an interesting finish on sheet metal [North Carolina]
22221. Experimental formulas for carbon steel figurative sculptures [California]
22222. German Finish Nomenclature [Texas]
22223. Electrically resistive coating for 316 SS that is UV resistant? [Canada]
22224. Corrosion problems on aluminum ambulance bodies [Alabama]
22225. Antique Stove Re-enamel needed [Texas] {6/03/03}
22226. EN chemical [Singapore] {6/03/03}
22227. Oxide scale formation - copper plated bolts [India]
22228. Electrical circuit model of corrosion with more than one coating on the steel [Iran]
22229. What does happen to an ion? [Iran]
22230. Wastewater Treatment issue [Pennsylvania]
22231. Rust in pipelines [Pakistan]
22232. Electro plating of Cr-Co coatings [California] {6/04/03}
22233. Wood patterned paint on metals [Egypt] {6/04/03}
22234. Test method for tin plating [India]
22235. Need to find M-1085 masking wax [California] {6/04/03}
22236. Black Spots in Chromic Acid Anodizing [Pennsylvania]
22237. Washing concrete floors [New York]
22238. Question on type of gold [Nevada]
22239. Blue finish for iron and steel [England]
22240. 17" damaged rims need filling/dipping [Connecticut] {6/04/03}
22243. Oil rubbed bronze [China]
22244. Need a barrel to plate small batch sizes [Minnesota] {6/04/03}
22245. Machining requirements for part to be electropolished [Pennsylvania]
22246. Hot dip zinc coating on cast iron [China] {6/04/03}
22247. I need very rough plating, like spikes or 40 grid sandpaper [Canada]
22248. Is passivation the cure for identifying weld inclusions? [Virginia]
22249. Follow-up question-powder coat problems [Massachusetts]
22250. Jigging design for anodizing [England] {6/04/03}
22252. Need immersion silver process for copper bus bar [Illinois] {6/04/03}
22253. Refining of Palladium and making its salt [India]
22254. Difference Colour After Passivation [Malaysia]
22255. Help needed on painting brass! [England]
22256. Alternate to Trichloro Ethylene (TCE) [India]
22257. Tributyl tin analysis in paint [Egypt]
22258. Expected problems from chromic acid anodizing [Canada]
22259. Zinc Cyanide [New York]
22260. Seeking Titanium Nitride plating facility. Small 6al-4v Titanium parts [Oregon] {6/05/03}
22261. Plating and coating of plastic components [Florida] {6/05/03}
22262. Need anode suppliers [Philippines] {6/05/03}
22263. Need surface "nonconductive" primer for ABS (pre-chrome) [Tennessee] {6/05/03}
22264. Chemistry concentrations [New Zealand]
22265. Composition of coins [India]
22266. Stainless Steel 304L properties [Puero Rico]
22267. Solder and finishing problem [Rhode Island]
22268. Lack of depth in deep etching stainless steel and aluminum [South Africa]
22269. Copper sheeting [Indiana]
22270. Painting old Winnebago [California]
22271. Nickel [Nigeria]
22272. Starting chrome refinishing business [Kentucky]
22273. Stripping solder [Rhode Island]
22274. Effects of repeated burning off of powder coating to the galvanized steel sheet metal [Pennsylvania]
22275. Variation in black zinc plating on steel cylinders [California]
22276. Problems anodising turned 7075 T6 aluminum [UK]
22278. Help us to improve our passivation paste [China]
22280. Hot dip galvanizing service required [Jordan] {6/06/03}
22281. Aluminum 6061 Deteriorating? [Canada]
22282. Painting Plastic Fender Flares [Texas]
22283. Turning white gold back to yellow gold [Massachusetts]
22284. Paint on metal reference [Switzerland]
22285. Primer for aluminum with hexavalent chromium-free corrosion inhibitors and reduced VOC [Pennsylvania]
22286. Bright Polish of a Brass Casting needed [New York]
22288. Thinning of SS foil [Florida]
22290. Removing rust from inside a bicycle frame [Missouri]
22291. How to make Polyresin items? [Florida]
22293. Request for help--how to recycle spent caustic soda [Indonesia]
22294. Non - cyanide Metal Stripping [Australia]
22295. Welding galvanized steel [Canada]
22296. Can white gold be electroplated? [Washington]
22297. What may be causing Acid Copper to peel from a Cyanide Copper Strike? [California]
22298. Codeposition NiSiC [Switzerland]
22299. High vacuum compatible finish for aluminum? [Vermont]
22300. Burnishing of 300 Series Stainless Steel [Ohio]
22301. Materials for endoscopes [South Africa] {6/09/03}
22302. Silver Bimetal Rivet Manufacturing Machine [India] {6/09/03}
22303. PE coating raw materials, heat shrink sleeves [Pakistan] {6/09/03}
22304. Need technical assistance [Nepal] {6/09/03}
22305. Required Hard Coat Anodizing Plant [India] {6/09/03}
22306. Electroplating in Basic Solution/How pH affects electroplating [California]
22307. Fuzzy pennies are bad for the grade [California]
22308. Creating an inert surface on Inconel 750 ( or ti-6al-4v) [Maryland]
22309. Adhesion of electroplated nickel on gold [Massachusetts]
22310. Scale removal from brass [India]
22311. Sulfamic acid reactions [Iran]
22312. Immediate Chemical Testing of Cobalt and Tungsten in materials [India]
22313. Tungsten alloy dart and playing [China]
22314. Remove Scratches on Mirror Glass [Michigan]
22315. Fine scratch removal [UK]
22316. Rub on brass finish that can withstand heat [Canada]
22317. Help with blue water [New York]
22318. Cleaning / refinishing metal mesh [Texas]
22319. Ebanol-C durability and suppliers [California]
22320. Hull Cell Test [Turkey]
22321. Extreme pH Suitable Tank Material [New Jersey]
22322. Cathodic electro painting [India]
22323. Need a vacuum-compatible aluminum finish [California]
22324. EN Plating Steel for Corrosion and Wear Against Acidic Water [Minnesota]
22325. Plating Nylon 66 as ABS, Is it possible? [West Virginia]
22326. ENIG discoloration for pcb [Philippines]
22327. Copper plating of pcb [Indonesia]
22328. Hot spots [California]
22329. Improvement in Zinc Phosphating [Pakistan]
22330. Acid deburring [Arizona]
22331. Welding spots and finishing techniques in Stainless Steel [India]
22332. Corrosion resistant stainless steel (Magnetic) [India]
22334. Cast Iron Restoration [South Dakota]
22335. Copper sealer to keep fence caps shiny [New York]
22336. Nitrotec surface treatment information request [Michigan]
22337. Alodine Composition [Utah]
22338. Coefficient of Friction for Aluminum Metal Matrix Composite [New Mexico]
22339. Stainless Steel Passivation Needed [Tennessee] {6/10/03}
22340. Looking for "SILVERON" [Canada] {6/10/03}
22341. Need a thin color coating for steel [New Hampshire] {6/10/03}
22342. Electrolysis of Tantalum [Nevada]
22343. Teflon coating cast iron kitchen materials [India]
22344. Alternate Chromate Coating to meet European Counil requirement [Maryland]
22345. Zinc extraction [India]
22346. Permalloy plating bath stabilization [North Carolina]
22347. No plate around contact point [Michigan]
22348. Alumina cleaning [Israel]
22349. Electropolishing [New York]
22350. Nitric Acid Purity for Titanium Passivation [California]
22351. Difference between nickel chrome plating and electroless nickel plating [India]
22352. How do i restore an iron doorknob that has been subject to weather and salt water? [Australia]
22353. Corona treatment [Indonesia]
22354. A to Z about chroming? [Indonesia]
22355. Is PARA-DI-CHLORO-BENZEN carcinogenic ? [Iran]
22356. Brass plating of old microphone[Florida] {6/10/03}
22357. Looking for a place to reporcelin my stove grates [New Mexico] {6/10/03}
22358. FINISHING A CAST IRON FIREPLACE [United Kingdom]
22359. Need source for regalvanizing anchor chain [Florida] {6/11/03}
22360. Plating for boat parts [Florida] {6/11/03}
22361. Seeking Tarniban d [Florida] {6/11/03}
22362. Need 50 gal paraffin wax [Mexico] {6/11/03}
22364. Application method for Ebanol C [Mexico]
22365. Chemicals for Shining Aluminum [Colombia]
22366. Hypo-allergenic 317L ? [Connecticut]
22367. Remove Anodize on Aluminum and Polishing [Mississippi]
22368. Spec for bpl211 [Illinois]
22369. 1,000 lb hazmat exclusion?? [Oregon]
22370. Scummy oxidized aluminum brightener needed [Massachusetts]
22371. Stripping silver [Utah]
22372. Has The Formula For W3700 Optical Paint Changed [California]
22373. NiCaSil coating versus fuel containing alcohol [Brazil]
22376. Carburizing 316 SS [Ohio]
22377. Clear coat [Canada]
22378. product search - fine mesh platinum coated [Maryland] {6/11/03}
22379. Need DSC for measure Tg values [Thailand] {6/11/03}
22381. Role of hexavalent chromium in the inhibition of corrosion of aluminum [France]
22382. Composition of Pickling Solutions [France]
22383. Need to remove muriatic etching in copper [Washington]
22384. Decorative Chrome on Chainmail Fashion Acessories [Philippines]
22385. How to do Invar 36 Passivation? [Taiwan]
22386. Hot dip galvanizing service [Ukraine] {6/12/03}
22387. Plating or metallizing of fishing lures [Oklahoma] {6/12/03}
22388. NEED 900,000 SCREWS PLATED WITH ZINC AND DELTACOLL [Illinois] {6/12/03}
22389. Seeking plater of motorcycle parts [New York] {6/12/03}
22391. Want to Purchase an ISCO Model 6712 Portable Sampler [Florida] {6/12/03}
22392. Brasso Polish [Canada] {6/12/03}
22393. Electro-"diamond-dust" surfacing of stainless steel/titanium [Pennsylvania] {6/12/03}
22394. Cr expansion coefficient [Spain]
22395. Conductive pigment [India]
22396. Help with chemical milling SS [New Jersey]
22397. TIG WELD OF GALVANISED STEEL - SAFETY REQUIREMENTS [England]
22398. Illness from water softener [Alaska]
22399. Checking Methods [India]
22400. Zinc plating conductivity comparison [India]
22401. Powder Coating on Wood [India]
22402. Springs - powder coating vs blackening [India]
22403. Dark Finish to Stainless Steel [Arkansas]
22404. Hardening TiAlV surface [Pennsylvania]
22405. Will chlorine in the air cause electroless nickel plating to tarnish or discolor? [Massachusetts]
22406. Teardrop overplating in copper pulse plating [Canada]
22407. Cold limits for tin plate [Washington]
22408. Shelf Life of PCB's [India]
22409. Electrodeposited Zinc Plating Thickness and Tolerance [Wisconsin]
22410. Alodine on aluminum alloys [California]
22411. 416 passivation problems [California]
22412. RE-CHROME PLATING SPORT TRUCK WHEELS [Florida] {6/12/03}
22414. Flaking issues with Electroless Nickel Plating for A356.2 aluminum parts [Canada]
22415. Paint ingress in tapped holes [England]
22416. Silverplated wire [Minnesota] {6/13/03}
22417. Looking for a company that can blacken #8 polished stainless steel [Utah] {6/13/03}
22418. Seeking brite dip plater capable of plating per ACES 16P15 [Illinois] {6/13/03}
22419. Removing Rust on BMW [Illinois]
22420. JUST NICKEL PLATING [UK]
22421. Looking for the difference between Alodine and Conversion Coating [South Dakota]
22422. Loss of amperage and glowing parts [California]
22423. Alkaline runoff stripping anodized finishes [Florida]
22424. Anodizing of ATV motor cases [Arkansas] {6/13/03}
22425. Cobalt phosphorous on steel prototypes [California] {6/13/03}
22426. Electroless cobalt consultant [California] {6/13/03}
22427. Copper oxide pellets or fines [California] {6/13/03}
22428. Watertight sealants, color additives [Ohio] {6/13/03}
22429. Seeking rectifier [Pakistan] {6/13/03}
22430. How to make NaOCl, 50000 tons/day [Pakistan]
22431. Information regarding barrel tumbling operation [India]
22432. Tantalum wet etch [California]
22433. What are the side effects of electroforming nickel sulphamate with insoluble anodes [Australia]
22434. Anodized aluminum reflectors wanted [China] {6/16/03}
22435. NEED ARCHITECTURAL ALUMINUM PAINTED [New York] {6/16/03}
22436. Wet spray with 250 degree cure oven [Alabama] {6/16/03}
22437. Plating of dried leaves [Massachusetts] {6/16/03}
22438. Need a Green pantograph engraver #106 [Florida] {6/16/03}
22439. Effect Of Urea Reactor On Cast Iron and Stainless Steel [India]
22440. Chrome plating for piston/gas seal [Ireland]
22441. Living in a Faraday Cage [Israel]
22442. How can I coat mugs for sublimation printing on a low budget [Canada]
22443. Restoring old iron [Virginia]
22444. Rhodium Plating over 14 K Yellow Gold [Indiana]
22445. Car exterior protection [India]
22446. Refinishing an old lamp [California]
22447. Metal plated ABS buttons [Florida]
22448. HEAT RESISTANT CHROME PLATE [Delaware]
22449. British Standard Testing method for anodized aluminum [Malaysia]
22450. Properties-Sulfamate-Nickel [California]
22451. CO-CURRENT AND COUNTER-CURRENT REGENERATION COMPARISON [Pakistan]
22452. PTFE coating on steel strips - machinery reqd [India]
22453. Unsolved plating problems [Singapore]
22454. CAN WE ANODIZE ALMUNIUM UTENSILS WITH OUT USING HARMFUL ACIDS? [Pakistan]
22455. NEED ALONISATION TREATMENT? [Quebec, Canada]
22456. Bright Dip process [New York]
22457. Galvanic corrosion of rivets [South Africa]
22458. Need galvalum sheeting [Bahamas] {6/16/03}
22459. Rechroming of motorcycle pipes [New Jersey] {6/16/03}
22460. Seeking gloss meters [Iran] {6/16/03}
22461. Surface finishing of sand-casted aluminium curios [India] {6/16/03}
22462. What are electrolytic black and yellow chromate bath solution for zinc? [Iran]
22463. 1895 Cast Iron Stove - please help me bring it back to its former beauty [Australia]
22464. Determining the copper content of acid/copper sulphate solution [South Africa]
22465. Hexavalent chromium removal by precipitation [India]
22466. Boron and organic compound in the wastewater effluent [Singapore]
22467. Nitrocarburize [China]
22468. Deterioration of bright Ni electrolyte [India]
22469. Chrome plating on aluminium [UK]
22470. Whisker - Pure t Tin [Malaysia]
22471. Color change problem in black anodized parts [Turkey]
22472. Which masking material (tape or lacquer) did not peel off for hard anodizing? [Taiwan]
22473. GEL FOR ACIDS [Spain]
22474. Galling stainless....help [Michigan]
22475. Seeking anodizing of zinc [Ontario] {6/16/03}
22476. Need Help finding Ford Plating Spec - Plate on Plastic [Michigan]
22477. Patinate finishes [Iowa]
22478. Teflon coating for aluminium [Indonesia] {6/17/03}
22479. Protective jewelry coating [Oregon] {6/17/03}
22481. Looking for place to dip rims [Indiana] {6/17/03}
22482. Seeking 2 Lightnin' mixers [Washington] {6/17/03}
22483. Properties of aluminum treated with Alodine process [Turkey]
22484. Is there any alternative for activating plastic for plating? [Spain]
22485. Help! RPP additive analysis [Romania]
22486. Changing the color of an asphalt roof [Pennsylvania]
22487. Want personally designed platinum rings [Oregon]
22488. Cleaning up purple plumbers glue [Texas]
22490. Repainting aluminum swimming pool coping [North Carolina]
22491. Repairing silver corrosion [Ireland]
22492. How to powder coat chrome? [Utah]
22493. Electroplating of flame retardant ABS [Israel]
22494. Repairing Pitted Engine Bore [Australia]
22495. Titanium pressure case coating [Canada]
22496. Process problem [Canada]
22497. Anodising information needed [Australia]
22499. Need magnetic, food-grade stainless steel [Malaysia]
22500. Need non-stick, food grade, permanent coating [Massachusetts]
22501. Silica Removal by RO membranes [Canada]
22502. Propylene Glycol Monoeyhyl Ether as a flux remover [Colorado]
22503. verdis gris [Texas]
22504. Coloring stainless steel black on site application [California]
22505. TEXTURE ETCHING [India]
22506. SEEKING CHROME ON FIBERGLASS PROCESS [California] {6/19/03}
22507. Silver Stripping [Nevada]
22508. Aluminium parts bonding material [Greece] {6/18/03}
22509. Combining Titanium and Carbon [Washington]
22510. Muriatic acid on Brick Pavers [Florida]
22511. Substitute for iron plating material [Philippines]
22512. Eliminating Comtamination from Copper Bath [India]
22513. Pickling of steel coils [U.A.E.]
22514. Copper contamination in pickle [Australia]
22515. Electropolishing machine [Israel]
22516. Alustone DS570 information required [UK] {6/19/03}
22517. Consumption of NaOH in etch tank [Iraq]
22518. Brass coating needed [New Hampshire] {6/19/03}
22519. Moisture effect on 98% sulfuric acid [Pakistan]
22520. Source of chrome plated tube? [Florida] {6/19/03}
22521. Need zinc plating of sheet metal assemblies [Florida] {6/19/03}
22522. Chrome plating a plastic handle on cane [Michigan] {6/19/03}
22523. Need Electroless Palladium Plater [Minnesota] {6/19/03}
22524. What is nickel silver? [Louisiana]
22525. Tub repainting [South Carolina]
22526. ELECTROPLATING STAINLESS IN COLOR [Florida]
22527. Looking for plater to do jewelry and rhinestone crowns [Florida] {6/19/03}
22528. Need my wheels plated [Illinois] {6/19/03}
22529. Need anodizing and conversion coating [California] {6/19/03}
22530. Why Not Alternate Current ? [India]
22531. RUTHENIUM COATING PROCESS [Pakistan]
22532. Need weakly conductive and smooth coating on ceramics [Massachusetts]
22533. Brazing small copper wire to stainless steel [India]
22534. Sea spray resistant paint [California]
22535. Saving natural copper finish [North Carolina]
22536. Hoyt Metal Co of Great Britain thermometer [Wales]
22537. Electroless Decorative Chrome Plating [Philippines]
22538. How to be polite? [Manchuria]
22539. Zinc, Copper, Nickel, Chrome Bath (Cyanide-Free) Composition [Canada]
22540. Use of Nickel Plating in Automobile Restoration [California]
22541. Ceramic Powder Coating? [Ohio]
22542. Rusting Galvanized Nails [North Carolina]
22543. Will Anodized Aluminum outgas in a cleanroom ? [California]
22544. Looking for a quality plater [Texas] {6/19/03}
22545. Need wheels painted [Florida] {6/19/03}
22546. Seeking powder coating of washers [Tennessee] {6/19/03}
22547. Vacuum Sputtering Machine [Pakistan] {6/19/03}
22548. Looking for replacement Cylinder for Jackson Candle Turbidimeter [Minnesota] {6/19/03}
22549. Problem with reiforcing Al6061 with Alumina [England]
22550. Conductive Alumite? [Malaysia]
22551. Is there a danger in Cast aluminum cookware? [Georgia]
22552. bussines expand by starting chrom plating in small and economic way [Indonesia]
22553. Spots in nickle plating [India]
22554. Making stainless parts solderable [United Kingdom]
22555. Sticking trouble on nickel plated molds [Oregon]
22556. Metal Cosmetic Finish Issue : Steel Washer with Black Zinc [Singapore]
22557. Rough etching on anodized 7075-T73 aluminum [California]
22558. Obtaining both Bright & Matt Anodizing on the one sheet [Australia]
22559. Yellowing of stainless steel (304 grade) [India]
22560. Does shotpeening change the previously machined dimensions [California]
22561. Need 3/8 OD decorative chrome plated tube [Florida] {6/23/03}
22562. Show Chrome on Magnesium [California] {6/23/03}
22563. Chrome flash on stainless steel [Michigan] {6/23/03}
22564. Rims dipped in chrome [Maryland] {6/23/03}
22565. Need alloy wheels dipped in chrome [Ohio] {6/23/03}
22566. Seek restoration/recoating of enameled cast iron sink (1 each) [Michigan] {6/23/03}
22567. Auto body parts acid dip [Illinois] {6/23/03}
22568. Seeking anodizing of 5052 H-34 alum. small parts [Indiana] {6/23/03}
22569. Seeking Trivalent Chrome Plating [Illinois] {6/23/03}
22571. Need glitter powder machine immediately [Pakistan] {6/23/03}
22572. Need Electro/Chome Plating Equipment [Canada] {6/23/03}
22573. Powder Paint Booth and related things [Canada] {6/23/03}
22574. Need chemical to turn polished brass finish into antique brass finish [California] {6/23/03}
22575. Acid pickling [India]
22576. How to etch tantalum pentoxide without etching silicon dioxide? [India]
22577. Distilled water versus deionized water [France]
22578. Epoxy for lacquering tinplate [Thailand]
22579. Voltage rise in rectifiers for electroplating [Philippines]
22580. Equations relating electroplating effluent parameters [Nigeria]
22581. Rust remover product? [Minnesota]
22582. How to dye perspex [Scotland]
22584. 1970 Bentwood Rocker - chrome is rusted and pitted [Massachusetts]
22585. Is Brass Statue OK Outside in Winter [California]
22586. How hard is stainless steel? [Australia]
22587. Removal of marine acrylic stain from brass [Massachusetts]
22589. Chroming plastic parts [Michigan]
22590. Refinishing Revere Copper Pans [Texas]
22591. Electroplating science project [Oregon]
22593. Information about Test Method [Turkey]
22594. Instruction courses in anodizing/powder coating [India]
22595. Definition of "architectural quality" stainless steel handrail [Colorado]
22596. Coating for Electropolish Containment Tank [California]
22597. Safe to drink alkaline water [Singapore]
22598. Analysis of aluminum in alum by XRF [India]
22599. Inquiry about pu coating on wood [India]
22600. Recoating carbide end mills [Arizona]
22601. Reworking gold plating [Wisconsin]
22602. Black Anodized parts turning brown after time [Wisconsin]
22603. SS316L contamination - remedies [Kenya]
22604. Understanding Phosphating...help [England]
22605. Sintering the natural diamond for wire drawing dies [India]
22606. Will Molybdenum Disulfide Fix Our Problem? [South Dakota]
22607. Salt spray test [India]
22608. Want to start a brass dipping business- help! [Virginia]
22609. Outsourcing for nickel plating [India] {6/24/03}
22610. Need to architectural anodize some aluminium wire [New York] {6/24/03}
22611. Need my rims chrome dipped / refinished [Illinois] {6/24/03}
22612. Seeking Crodon finishing companies [Illinois] {6/24/03}
22613. NEED PLASTIC PARTS CHROMED [Florida] {6/24/03}
22614. missing or purged
22615. BLACK OX ON STAINLESS [New York] {6/24/03}
22616. Colored Anodization of Nuts -- Six Colors [California] {6/24/03}
22617. High temp paint, need a particular color [Arkansas] {6/24/03}
22618. Need bismuth oxychloride [Illinois] {6/24/03}
22619. Need small copper plating equipment [Canada] {6/24/03}
22620. Water treatment plant enquiry [UAE] {6/24/03}
22621. Acid cleaning paste for stainless steel [Norway] {6/24/03}
22622. Anodizing [England]
22623. Plating copper onto Nb [Ohio]
22624. Request for help: Hastelloy MIG welding? [South Carolina]
22625. Price of machine to chrome plate wheels [Maryland]
22626. Pale Gold Powder Fine Metal Flake Search [California]
22627. Do it yourself silver refinishing [Pennsylvania]
22628. Home Restorers and Powder Coats [California]
22629. CLEARCOAT ON PLEXIGLASS/CLEAN IT OR TRASH IT [Alabama]
22630. Plastic Dive Torch Reflector [Scotland]
22631. Clear coat peeling [South Carolina]
22632. Authenticating bronze work [Switzerland]
22633. Chroming SUV rims [Maryland]
22634. Electropolishing Solutions for Stainless Steel [Philippines]
22635. Tin/Lead accumulation on plastic [Philippines]
22636. Is 316L SS good for Aluminum Sulphatel [South Africa]
22637. Chrome stripping in hydrochloric acid [England]
22638. Passivation Problem [India]
22639. Clear coat on brushed steel [Washington]
22640. Aluminum coating on steel [India]
22641. Difference between galvanized and zinc plated [China]
22642. PVD problem [India]
22643. Cadmium plating vs surface finish [Canada]
22644. USE OF EDUCTORS TO INCREASE PLATING SPEED [California]
22645. Product of Non-Cyanide Alkaline Zinc Plating [California]
22646. Type II anodizing project [Washington]
22647. How to avoid rust while welding steel pots? [India]
22648. Brass Refinishing [Pennsylvania]
22649. Titanium Oxide Removal [North Carolina]
22650. How to avoid finger prints on matt finish pots? [India]
22651. Joining steel and stainless pipe [Singapore]
22652. Help about passivation [India]
22653. Rims Chromed[North Carolina] {6/24/03}
22654. I need to measure the thickness of Epoxy Coating applied on concrete[India] {6/24/03}
22655. Information on adhesion testing of copper electroplating [India]
22656. Waterproof electrically insulating dip-coating enamel [Florida]
22657. Steps and composition for surface cleaning process for nickel electroless in steel samples[Portugal]
22658. Electropolishing molybdenum[Maryland]
22659. Need general information![Ohio]
22660. Inquiry about Nickel-Zinc alloy Electroplating[India]
22661. Rotary brushing of aluminum [Illinois]
22662. Need bead blasted SS panel pricing ASAP [Texas] {6/26/03}
22663. Suppliers of xylan coated studs [India] {6/26/03}
22664. Extrusion honing [India] {6/26/03}
22665. Seeking SUPFINA agent [Malaysia] {6/26/03}
22666. Need manual buffing machine [Washington] {6/26/03}
22667. Phenolic resin for adhesive manufacturing [Pakistan] {6/26/03}
22668. Nickel Waste Procurement [India] {6/26/03}
22669. Conversion factor needed [Tennessee]
22670. Replacement of hexavalent chromium on zamak [France]
22671. Definition of 'Micron' [Tennessee]
22672. Stripping of Vacuum deposited Nickel using a Cyanide Solution [New Zealand]
22673. Carbon coating removal of ceramic devices [California]
22674. Electrophoretic lacquering details [India]
22675. Advice on pre-treatment on powder coating [England]
22676. Corrosion - Powder Coat over Cast Aluminum [California]
22677. STEEL WITH ZINC FINISH [Canada]
22678. Diamond chrome plating? [Iran]
22679. Why is alocrom applied to bare aluminium [England]
22680. Alodine 1200 vs. 1500 [Oklahoma]
22681. Plating Applications for Titanium [Minnesota]
22682. Precleaning of SS Cans [India]
22683. Staining of 303 stainless steel [New Jersey]
22684. Dissimilar metals in air conditioned environment [Florida]
22685. Need anti-corrosion treatment on zamak without hexavalent chromium [France] {6/26/03}
22686. Need a paint job shop in London Ontaria area [Canada] {6/26/03}
22687. Looking for source to Chrome Plate ABS side moldings [Canada] {6/26/03}
22688. Silver Plating a Copper Tube [Colorado] {6/26/03}
22689. Seeking Zinc Ingots [UAE] {6/26/03}
22690. missing or purged
22691. Chromic phosphoric acid to remove neutral anodite [New Jersey] {6/26/03}
22692. Electrical conductivity tester [Malaysia] {6/26/03}
22693. Cleaning/Restoring Copper Roofs to their original color [Texas] {6/26/03}
22694. NEED TO CONTACT: SILVER LION [Massachusetts] {6/26/03}
22695. Need (3) stage phosphate wash line [Oregon] {6/26/03}
22696. Need 36" diameter reels for selective line [Pennsylvania] {6/26/03}
22697. Plating nickel on ceramics and TEFLON [Florida]
22698. Surface treatment of screws [England]
22699. How to get rid of Shiny Aluminium [Turkey]
22700.Need rims dipped in chrome [Ohio] {6/26/03} 
22701. Prelude wipe on paint[Nebraska] {6/26/03}
22702. Refrigerator scratches[Pennsylvania]
22703. D-I-Y DC Rectifier[Canada]
22704. Tricky and riveting question, can you solve it?????[North Carolina]
22705. Electroplate lead[Louisiana]
22706. Rusting out metal [Arkansas]
22707. How can i build a powdercoat oven at home[Missouri]
22708. Aluminum anodite [New Jersey]
22709. Sizing rhodium plated white gold rings.[Canada]
22710. Nitiding 316 Valve Shafts [Massachusetts]
22711. ELECTRODES FOR FISH POND OXYGENATOR? [Missouri]
22712. What is Zinc Clad? [Pennsylvania]
22713. 18 inch rims [New York] {6/27/03}
22714. Impedance and standards [Egypt]
22715. RUST PREVENTIVE FOOD GRADE ADDITIVES [India]
22716. Hologram details [India] {6/27/03}
22717. Surface contaminant and electropolish methods for biomaterials [New York]
22718. Adhesion of ceramic to electroless nickel [North Carolina]
22719. Electrode plating [California]
22720. Electroless tin solution formula [Brazil]
22721. Testing Ammonia Concentration is a Brass Bath [Michigan]
22722. Chemical polishing of brass [India]
22723. Vacuum deposition on powders [California]
22724. Surface roughness values [India]
22725. ABS Painting [Canada]
22726. Trouble on black chromium plating [Portugal]
22727. Silver finish
22728. Looking for suppler of Bis(3-sulfopropyl)-disodium-sulfonate [Arizona]
22729. Refinishing faux brass plumbing fixtures
22730. Engraving system for stainless steel [Malaysia] {6/30/03}
22731. Seeking hard chrome plating [South Carolina] {6/30/03}
22732. FLUOROCARBONS - COATING / LININGS / MOULDINGS [India] {6/30/03}
22733. Density of liquid copper [Texas]
22735. Selective plating [Spain]
22736. Chrome Plating of Work Rolls on Aluminium Cold Rolling Mills [India]
22737. Nickel iron plating bath [California] {6/30/03}
22738. Sulfuric acid damaged rims [North Carolina]
22739. Gold Refining Machines [Nepal] {6/30/03}
22740. Need salt spray chamber [India] {6/30/03}
22741. Acid etching of stainless steel? Help needed! :) [Florida] {6/30/03}
22742. Looking for company to plate 50 Hula hoops [Indiana] {6/30/03}
22743. Luster help needed in anodized al parts [Michigan]
22744. ABS contamination of well [New Mexico]
22745. DESIGN AND CONSTRUCT A GALVANIZING PLANT [Nigeria] {6/30/03}
22746. H2S resistance of nickel-plated aluminum [Colorado]
22747. Aluminum Oxide / Glass Bead Blast problems [New York]
22748. Zinc and powder coating problem [Tennessee]
22749. Remove nickel finish and polish the copper underneath copper? [Connecticut] {6/30/03}
22750. Need Goldwing engine parts redipped [Illinois] {6/30/03}
22751. SEEKING CLEAR ZINC CHROMATE PLATER [Texas] {6/30/03}
22752. Want to import nickel sulphate [Iran] {6/30/03}
22753. Ceramic Coating unit [India] {6/30/03}
22754. Copper Casting Machines [Sweden] {6/30/03}
22755. What are metal alloys? [Australia]
22756. Removing rust from a nail [Philippines]
22758. Ti-O-N phase diagram [Illinois]
22759. Connection of PC to FPC [UK]
22760. Color changes in white gold [Canada]
22761. Antiquing of copper surface [India]
22762. Uses for "Blue Stone" copper sulfate [Georgia]
22763. The ultimate katana [Wales]
22764. How to paint an old tin ceiling [Connecticut]
22765. Looking for sealant protection for copper counters [Ohio]
22767. Speeding the aging of copper [Wisconsin]
22768. Weathered Anodized Aluminium Roof [Virginia]
22769. Keeping the brass bed beautiful [Massachusetts]
22770. Bonn Units [India]
22771. Pretreatment plant design help required [U.A.E.]
22772. Hydrogen peroxide to reduce sludge in effluent treatment [U.K.]
22773. Disposal of liquid paraffin [U.A.E.]
22774. Rust effect [South Africa]
22775. Thin Clad Plating [Michigan]
22776. Gold / Tin Alloy plating [Massachusetts]
22777. Plating connectivity problem [India]
22778. What catalyst can be added to a phosphoric/sulphuric acid mix to achieve a good etch rate and quality? [UK]
22779. Inscribing letter on Tungsten Carbide [China]
22780. Suggest a process to give a cosmetically appealing finish on brass [India]
22781. Need speedy turnaround for powder coating a set of car rims[Massachusetts] {6/30/03}
22782. Replating parts of 48 Riley[Maryland] {6/30/03}
22783. How can I brush plate over plastic[Oklahoma]
22784. Hard Chrome Color?[California]
22785. Electro eching of aluminum[Indonesia]
22786. Hydrogen Peroxide as a possible substitute for HCl as a pickling agent?[Zimbabwe]
22787. Vibratory finishing liquids[Emarat]
22788. Need "Acid Green 3" dye [Connecticut] {7/01/03}
22789. Zinc plating temperature dependance [California]
22790. 6061 Aluminum Extrusion Corrosion protection [Pennsylvania]
22791. Zinc/aluminum-plated sheet treatment to darken finish [California]
22792. TURNING BRASS BLACK? [England]
22793. Need a Brass Bed Refinished [Massachusetts] {7/01/03}
22794. Need 10 kg of Methyltrioxorhenium (VII) [Spain] {7/01/03}
22795. Patina the brass on Model T Ford [Oregon]
22796. Stripping rubber liner out of gas tank [Colorado]
22797. Giving motorcycle abs the bling-bling look [British Columbia]
22798. Re-Finishing Zinc Pot Metal replica guns [New York]
22799. Zinc plating for plane's aluminum floats [British Columbia]
22800. Equivalence between ASTM B-117 vs. ISO 9227 NSS [Mexico]
22801. Powder paint won't charge properly [India]
22802. Powder coated machine skins in a cleanroom [Massachusetts]
22803. How do 'Safer hot black oxides' perform? [Canada]
22804. Keeping castings shiny after machining [India]
22805. Dacromet 320 [Texas]{7/1/03}
22806. Nickel plating on aluminum[Ohio]
22807. Refinishing and repairing stone sculptor by Ike Boring[Georgia]
22808. Ultrasonic Cleaner specs[New York]
22809. Information on MIL-STED-105[Mexico]
22810. Conversion Coating for Tin[Illinois]
22811. Electropolishing [Ohio]
22812. Electro plating or buffing on steel pots[India]
22813. Need High Volume Polisher & Plater [Mexico]{7/2/03}
22814. Need chrome plating on plastic [British Columbia] {7/02/03}
22815. Chrome re-dipping [South Carolina] {7/02/03}
22816. Silver brightener [India]
22817. Stripping chrome to restore authenticity [Alabama]
22818. Faux antique mirror [Nevada]
22820. Pre-weathering of galvanized roofing [Texas]
22821. Plating onto SS416[India]
22822. Treatment for magnesium exterior parts[Spain]
22823. NON STICK COATING MATERIALS FOR COOK WARE [Maryland] {7/02/03}
22824. Need high heat paint for stove[Pennsylvania] {7/02/03}
22825. Electroplating & electropolishing of zirconium [India]
22826. Process for plating electroless nickel on magnesium [Minnesota]
22827. Painting over cadmium bolts [Georgia]
22828. Bilogical Growth in Rinse Tanks [Georgia]
22829. Need custom color coating for Harley pipes[Canada] {7/02/03}
22830. Seeking licensed Kynar applicator [West Virginia] {7/2/03}
22831. POTENTIAL ANTENNAE BASE DISSIMILAR METALS CORROSION PROBLEM? [California]
22832. Need hot dip, high temp. powder coat material[California] {7/02/03}
22833. Does anyone have any idea how to restore enamel on range a cooker? [England]
22834. Machining aluminum and magnesium castings on same CNC [Arkansas]
22835. Need household radiators refinished [Illinois] {7/03/03}
22836. Dielectric Properties of Anodized Aluminum [California]
22837. Need finishing equipment (dipping) [UK] {7/03/03}
22838. Need brass plating of sofa feet [Pennsylvania] {7/03/03}
22839. Gold plating on Magnesium (AZ91D) Die Castings [UK] {7/03/03}
22840. Silicon polyester coated sheet required [India] {7/03/03}
22841. PEWTER PLATING SYSTEM [Turkey] {7/03/03}
22843. Preparation of the XFR samples [Malaysia]
22844. Preservatives for copper [Michigan]
22845. Exterior rust finish [Washington]
22846. Color case hardening [Colorado]
22847. Cross reference RAL to FED-STD-595 [Illinois]
22848. RUST RUST RUST and more RUST [India]
22849. How do I spot galling? prevent galling on 304 on 316? [California]
22850. Seeking Zinc chromate plating on Steel Frame 4' w x 3' d x 3' tall[New York] {7/3/03}
22851. Gold refining & assaying machine [India] {7/3/03}
22852. Engine turned SS sheets [Texas] {7/03/03}
22853. Colorizing molybdenum? [California]
22854. Air Tube Frequent Failure[Saudi Arabia]
22855. Need affordable nickel-plating of cast bronze sculptures [California] {7/07/03}
22856. Pre coated steel coils needed [India] {7/07/03}
22857. Recycling system for solvents [Newfoundland] {7/07/03}
22858. Ultrasonic [Ohio] {7/07/03}
22859. Dive Knives - Titanium vs. Stainless Steel [Australia]
22860. When was galvanized barbed wire available in USA? [New Mexico]
22861. 14k Gold ring changed color after sizing [New Jersey]
22862. Making a shape from a zinc by etching? [Indonesia]
22864. Please explain decorative plating [Canada]
22865. Clear-coating insects [Texas]
22866. 18/8 versus 18/10 stainless flatware [North Carolina]
22867. Why would yellow gold turn silver? [Illinois]
22868. I may have received bad advice about chrome removal [Mississippi]
22869. Etching of aluminum sculpture [Ohio]
22870. Colonial brass chandelier restoration [California]
22871. Starvet Info Required [New Zealand]
22872. How many times can cadmium and chrome be stripped? [Taiwan]
22873. Effect of oxidation on conductivity of ETP Copper [India]
22874. Painting Stainless Steel [California]
22875. Moisture Resistant Powder Coating [India]
22876. Masking problem and pilling off problem in powder coating [India]
22877. Black Staining on Cadmium plating [England]
22878. Immersion silver over copper bus bars [Canada]
22879. Corrosion protection of painted aluminum [Canada]
22880. Pitting in electropolishing of ballbearing steel [India]
22881. Cleaning of 430F stainless steel [California]
22882. Etching tantalum without embrittlement [California]
22883. Cleaning of Stranded Steel Wire Coils [Saudi Arabia]
22884.POWDER ON POWDER WOOD FINISH [Saudi Arabia] {7/7/03} 
22885. Want aftermarket rims chrome redipped [Maryland] {7/07/03}
22886. Need my car headlights re-silvered[United Kingdom] {7/7/03}
22887.Aluminum cleaner and polish for pontoon boats [Kentucky] {7/07/03}
22888. Sandoz Aluminium Wood Dye [Northern Ireland] {7/07/03}
22889. How to measure the unknown quantity of phosphoric acid of soft drinks [Australia]
22890. Mg coatings pretreatment[China]
22891. Tracking degradation of reflective surfaces[Mexico]
22892. Polishing my Yamaha R6 frame [Massachusetts]
22893. Antique brass finish[Nevada]
22894. Sulfuric acid in PE tank[China]
22895. Material for exhaust manifolds of marine engine [India]
22896. Chrome Dipping [Florida] {7/08/03}
22897. WHEELS LOOKIN TO BE DIPPED [Maryland] {7/08/03}
22898. Powder-coat my saxophone [Singapore] {7/8/03}
22899. Need consultant on selective nickel anodizing [Canada] {7/08/03}
22900. Want anodized aluminum plate [Tennessee] {7/08/03}
22901. Titanium alloy for surgical instruments [Pakistan]
22902. Refinish a faucet [California]
22903. Help! phOSPHOric acid prep leaves tacky film [Florida]
22904. WHERE TO BUY POLYVINYL ALCOHOL? [South Carolina]
22905. DI water attack [Texas]
22906. How to prolong the life of my evaporator tanks ? [California]
22907. Anomaly in Nitric/HF analysis [Canada]
22908. Process and techno-economics of Zinc-Nickel plating [India]
22909. Plating Aluminium Wheel [Indonesia]
22910. Anodized aluminum color fading in vacuum [Maryland]
22911. Stainless steel polishing [Wisconsin]
22912. Stainless steel--type 304--in a coastal environment [Illinois]
22913. Brown deposit on 304 stainless steel buckles [India]
22915. Zinc and Copper needed [Georgia] {7/09/03}
22916. Need gloss meter [India] {7/09/03}
22917. Restoring copper gutters [Ohio]
22918. POLISHING MOTORCYCLE BIKES [California]
22919. Pilgrim Silverware Serving Set [Wisconsin]
22920. Is it chrome or stainless steel [Florida]
22921. Business badly needs 50's Chrome table legs and trim [Florida]
22922. Black marks after electropolishing wire [Canada]
22923. Oversize reamed holes [Ohio]
22924. Need 450 MT crystaline powder boric acid [Macedonia] {7/09/03}
22925. I want a gold plating machine [Canada] {7/09/03}
22926. RESIN ULTEM 2300 [India] {7/09/03}
22927. White spot defect on decorative chromium plating [Indonesia]
22928. Minimizing scratches on solid brass [New York]
22929. Refinish almond, textured refrigerator to white [Ohio]
22930. Plating abs plastic [Canada]
22931. Immersion tin issue [Singapore]
22932. Heating up EN Baths [India]
22933. Leaching Test Failure on Terminal [Malaysia]
22934. Care and Cleaning of Aluminum Surfaces [California]
22935. Acceptance Criteria for Passivation of a Mfg Vessel [Canada]
22936. Finishing Weld Seams On Satinless Steel #4 [Oregon]
22937. ALUMINUM MARINE EXPOSURE [New Jersey]
22938. Effect of carbide bonding and morphology on ball bearing steel on SAE52100 [India]
22939. Request for Comparison and Advise [Malaysia]
22940. A-380 Finishing Options for L.E.D. Emergency Lighting [Minnesota]
22941. Finishing per MIL-HDBK-808, table XIII "DG" Final Film [California]{7/09/03}
22942. Want to buy Ross Miles Apparatus [Illinois] {7/10/03}
22944. Zinc plating to code QQZ2325A [Canada]
22945. Federal Color #15090 [Georgia]
22946. Phosphate coating spec [South Carolina]
22947. Keeping cup shaped parts from becoming stuck inside one another [Michigan]
22948. Rinse salt spray before Holiday test [Germany]
22949. Need Infrared clear coatings [California]
22950. Tiny spots in ABS painting [India]
22951. Fresh cement reacting with galvanizing to form hydrogen gas [Canada]
22952. Purged
22953. Chromic anodizing an aluminum assembly [Missouri]
22954. Need to powdercoat my chrome wheels [Illinois] {7/10/03}
22955. Need company to recreate chrome car emblems in mass qtys [California] {7/10/03}
22956. Need used polishing machine [Canada] {7/10/03}
22957. Need consultant for PTFE, FEP, PVDF COATING and MOLDING PROCESS [India] {7/10/03}
22959. Nickel Allergy [Florida]
22960. How To Tarnish Steel [Texas]
22961. Can titanium in ink score gravure cylinders [UK]
22962. Effluent settlement rates [UK]
22963. Finish for aluminum flooring [California]
22964. What enamel for printing on steel oven [Egypt]
22965. Ti 6AL 4v Silver Plated according to MIL standard [Spain]
22966. White Contamination on Flexible Printed Circuit Board [Philippines]
22967. Passivating s/s weld zones [Canada]
22968. Velocity measurement using visualization technique [Indiana]
22969. Recovery or separation of palladium and tin [Germany]
22970. Bronze plating a cast iron bell[Alabama] {7/10/03}
22971. Controlling rust [Washington DC]
22972. Chrome or other plating of steel for awards [Pennsylvania] {7/11/03}
22973. Hobby conductive paint to repair PCB [North Carolina] {7/11/03}
22974. Sea Shell Silverplating [Mexico]
22975. Chrome and possibly paint world-class sportbike [Texas] {7/11/03}
22976. Refinishing (replating) of oil-rubbed bronze (US10B)finished hardware[California] {7/10/03}
22977. Protection of mild-steel during shipping [South Africa]
22978. Desire an aluminum to wood screw with no galvanic action [Florida]
22980. Unknown heat treat spec [Ohio]
22981. Need electroplating of ABS plastics [India] {7/11/03}
22982. Need wheels chrome dipped! [Canada] {7/11/03}
22983. Aluminum rims re-polished and /or chrome plated [North Carolina] {7/11/03}
22984. Removing oxide layer from NiTi wires [Italy]
22985. Sb doped SnO2 coating on metal mesh required [UK]
22986. Etching of titanium dental implants [Argentina]
22987. GOLD [Pakistan]
22988. Etching machinist files [Arkansas]
22989. Aqua Regia Gold and Aluminum [Michigan]
22990. "Frosted Duco" Finish [Rhode Island]
22991. Stripping of Cu/Sn alloy [China]
22992. Print the steel to make good resistant [Egypt]
22993. Pitting and roughness problems in copper plating on abs plastic [India]
22994. Change Zinc plated to be Copper plated on Clinching Fasteners [Thailand]
22995. Nickel Plating on CRCA [India]
22996. COLORING OF STAINLESS STEEL PARTS? [Australia]
22997. Metallic coatings for finished polycarbonate [Australia] {7/14/03}
22998. Need my brass bed restored [Texas] {7/14/03}
22999. Need a steering wheel plated [New York] {7/14/03}

The finishing.com Hotline includes more than 40,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2005