21000. Titanium and Stainless side by side [Vermont]
21001. Chroming of sidecovers for my motorcycle [Massachusetts] {4/07/03}
21002. Bumper in need of chroming [Illinois] {4/07/03}
21003. Chrome plating of my motorcycle parts [Canada] {4/07/03}
21004. Bonding rubber to spring steel! [Georgia] {4/07/03}
21006. Seeking re-chroming of valve covers [Maryland] {4/07/03}
21007. Chrome plating, a pair of wheels [New York] {4/07/03}
21008. Bronze and nickel plating of pebbles and stones [California] {4/07/03}
21009. Classic/Satin plating vendor in Central or Eastern Europe? [Yugoslavia] {4/07/03}
21011. Small plating equipment for stained glass work [Texas] {4/07/03}
21012. BLACK ONE-COAT SOLAR PANEL PAINT [California] {4/07/03}
21013. SPECIAL PRE-PLATED COPPER/BRASS SHEETS [India] {4/07/03}
21014. Italian modular link [Texas] {4/07/03}
21015. Needed - 5/16-18 aluminum hex socket cap screws [Wisconsin] {4/07/03}
21016. Chrome look on soft materials? [Canada]
21017. Normes d'echantillonnage pour controle par attributs [Morocco]
21018. Lubricating Soap Box Derby Wheels [Maryland]
21019. Pontoon Boat - Aluminum Panel Repainting [Massachusetts]
21020. Nickel plating removal [Florida]
21021. Superlight/Superstrong model airfoil contruction [Massachusetts]
21023. Need pp-plating baths or sheets [Iran]
21024. Chromate poisoning [Ohio]
21025. Lab test procedure for Watt's nickel [Pakistan]
21026. Measure Surface Area of 3D parts? [Illinois]
21027. Primer Colour Selection [India]
21028. Looking for inexpensive paint method [Georgia]
21029. CRACKS IN CLEAR POWDER COATING [Israel]
21030. Zinc plating separation during powder coating heat treatment [Texas]
21031. White Rust and Discoloration on Zinc Plated Parts [Texas]
21032. Powdercoat as mask for plating [California]
21033. "Parkerizing" on WWII electric torpedoes [Florida]
21034. Etching solution for P20 [Michigan]
21035. AISI 316 steel polishing problem [Turkey]
21036. Clear lacquering brushed stainless steel [UK]
21037. Can passivated stainless steel cause oxidation using silver epoxy? [California]
21038. Looking for a supplier to barrel plate screws with chrome plate [California] {4/08/03}
21039. FAA repair station seeks nickel plating per PW SPOP 26 to SPOP 321 [Indiana] {4/08/03}
21040. Need CORICONE CLEAR COATING for aluminum [New Jersey] {4/08/03}
21041. Green chromating [France]
21042. Surface preparation on a custom motorcyle frame [California]
21043. Galvanized cooker [Illinois]
21044. Audit format for 5S [India]
21045. Corrosion and heat treatment [India]
21046. Painting Brass and Nickel for underwater use [Pennsylvania]
21047. Treating galvanized steel sheets to avoid white rust [India]
21048. Gold Plating Thickness [Alabama]
21049. Nickel and chrome plating fail to pass 96 hrs acid salt spray test [Canada]
21050. Chemical pretreatment of titanium alloys before anodizing [Austria]
21051. Zinc Aluminum (85/15%) Metallising [India]
21052. Painting and heating of zinc-plated details [Texas]
21053. Looking for a chroming company for Edsel parts [Texas] {4/08/03}
21054. Need my wheels chromed [Oahu, Hawaii] {4/08/03}
21055. Need powder coating on aluminum items [Tijuana, Mexico] {4/08/03}
21056. Looking for a cataphoresis provider [Spain] {4/08/03}
21057. Requirement of Electrolytic Tin Plate Sheets [Pakistan] {4/08/03}
21058. Bluing a Winchester for gunsmithing class [Canada]
21059. Picture Reproduction in copper or metal? [Illinois]
21060. Searching for a clear zinc spec [California]
21061. Dirtness due to corona treatment [Italy]
21062. Brush plating experience [Israel]
21063. Reactions in anodizing bath [Bosnia and Herezgovina]
21064. Solder plating of nickel plated leadframe [Philippines]
21065. Finding the rms value for the entire object [India]
21066. 22" rims to be redipped in chrome [Georgia] {4/09/03}
21067. Equipment to print holograms [Iran] {4/09/03}
21069. Science Project-What's oxidation? [Massachusetts]
21070. Need Antique Brass Decorative Finish on Nickel Coated Hardware [Colorado]
21071. Fast aluminum polishing [Massachusetts]
21072. Looking for aluminum brightener [New Jersey]
21074. Aluminium Motorcycle wheel treatment and care [England]
21075. Brilliant gold picture frame [Scotland]
21076. Bronzing a skull-- or giving one a "bronze" look [California]
21077. How to remove lead from wastewater [Minnesota]
21078. Bonding rubber seal to phenolic based fiber glass surface [Pakistan]
21079. White rust appears in galvanized pipes [Pakistan]
21080. DLC [Ohio]
21081. Need gold plated glass [Arizona]
21082. Hard plating of cast lead bullets [Pennsylvania]
21083. Hard Anodize Colors [Canada]
21084. Extend life of phosphate tank chemicals [Michigan]
21085. What does a satin finish look like? [Massachusetts]
21086. Need re-chroming done in Belgium or Holland for plastic and metal [Belgium] {4/09/03}
21087. Chroming of plastic emblem on my car [New York] {4/09/03}
21088. Need phosphating and electrocoating to Ford spec [Illinois] {4/09/03}
21090. Tin rolls of gauge 0.22 mm [India] {4/09/03}
21091. Separating a mix of gold and iron powder [UK]
21092. Building a gas fired convection oven for powdercoating [Jamaica]
21093. Copper finish for pewter chess pieces, how to? [New Jersey]
21094. Protecting the shine on brass [Virginia]
21095. EDP Process [Indonesia]
21096. SN/PB PLATING PEEL OFF FROM NICKEL SUBSTATE [Philippines]
21097. Ti6Al4V Anodizing versus Fatigue behavior [Brazil]
21098. Aluminum Anodizing and Chemical Conversion Coating same part? [Canada]
21099. Corrosion Resistance of Stainless Steel on Chromate Solution? [China]
21100. 316 L SS, SS300, SS304 in saline solution for 72 hrs [India]
21101. Chrome redipping of old rims [Illinois] {4/10/03}
21102. Need chrome plating of wheels and Harley parts! [New Jersey] {4/10/03}
21103. Powder coating of small zinc die castings [Tennesee] {4/10/03}
21104. Need supplier who can Nickel Chrome plate large ABS parts [Illinois] {4/10/03}
21105. Aluminum polish [South Dakota] {4/10/03}
21106. Need increase in cure capability [South Carolina] {4/10/03}
21107. Bizarre reaction at the mining claim [Georgia]
21108. Stripping Baldwin Brass clearcoat [California]
21109. Hydrogen embrittlement of nuts [Tennessee]
21110. Zinc die cast painting [Tennessee]
21111. Patina help [Texas]
21112. Need durable, solderable finish for spring steel contact [Indiana]
21113. EFFECTS OF CAUSTIC BLEACH ON ANODIZED SURFACE [Virginia]
21114. Treatment of Magnesium Skins with Selenous Acid [Australia]
21115. New chrome plating needs finishing [Arizona]
21116. Need aluminium case and anodizing services for audio product [Indonesia] {4/10/03}
21117. Need metal tooling coated for extended wear [Mississippi] {4/10/03}
21118. Deburring of Needle Roller Thrust Bearing Cages [India] {4/10/03}
21119. Material Spec RU4 SECC 21 [Malaysia]
21120. Dye sublimation coating [Egypt]
21121. Electroless Nickel Heat Treatment [Israel]
21122. Time saving hot rolled steel [Ohio]
21123. Brass plating of interior door handles [Georgia] {4/11/03}
21124. Reflective glass beads [India] {4/11/03}
21125. Seeking pre-anodize masking alternatives [Virginia] {4/11/03}
21126. Spray Paints for Glass [New Jersey] {4/11/03}
21127. Aluminum sheet A6061 [Singapore] {4/11/03}
21128. Need one Aluminum Sheet [California] {4/11/03}
21129. UHMWPE properties? [South Africa]
21130. Information of fluidized bed coating equipment [Pakistan]
21131. Dendrites phenomena with immersion silver finishes on PCBs [France]
21132. Chemical etching [Malaysia]
21133. Bird Bath [Louisiana]
21134. Lettering a brass plaque [Canada]
21135. Specifying vibratory deburring and etching processes [Oregon]
21136. ELECTROLOID chrome plating equipment value? [Jamaica]
21137. BAKING AND HYDROGEN EMBRITTLEMENT [India]
21138. Nitric acid passivation [Texas]
21139. Stainless thermowell galling at high temperatures [Canada]
21140. Ardox [Alabama]
21141. Information on corrosive attack on 316L Stainless Steel [California]
21142. Plastic Chrome Plating [California]
21143. Need 4 rims chrome plated [Connecticut] {4/14/03}
21144. Need 4 alloy wheels chrome plated [Texas] {4/14/03}
21145. Need 3 copper pans re-tinned [Arizona] {4/14/03}
21146. Need gold refinery plant [UAE] {4/14/03}
21147. Need some raised lettering [Michigan] {4/14/03}
21148. Nickel based single crystal grain etching equipment [Utah] {4/14/03}
21149. Analysis of unknown aqueous solutions [England]
21150. Help me remember an old science project [Florida]
21151. Chemically coloring cold-rolled steel [Nevada]
21152. Chrome plating of aluminum Corvette wheels [Illinois] {4/14/03}
21153. Clear coat finish [D.C.]
21154. How to copper plate steel handles [England]
21155. Finishing a rough finished, flat casted bronze medal [New Jersey]
21156. Using wrong line source voltage and frequency [UAE]
21157. ASTM A764 Coating Weight Measurement [New York]
21158. Copper coatings-UV resitant and reflective [Colorado]
21159. Heat resistant paint for a firepit [Michigan]
21160. Rusting Iron and Copper [So. Dakota]
21161. Not adherent copper film in welding wire [Venezuela]
21162. Plating onto rusted steel procedure? [California]
21163. Black Nickel Versus Chrome on Motorcycle Aluminum [California]
21164. Casting alloy for anodizing [Malaysia]
21165. How to prevent discoloration on aluminium surface [Malaysia]
21166. Iridite 14 vs. 14-2 [Ohio]
21167. Polishing an Industrial mixing tank [Iowa]
21168. Diamond burnishing of chrome plating [India]
21169. Best sanding discs for cutting 304L stainless? [Oklahoma]
21170. Best way to polish 304L Stainless? [Oklahoma]
21171. Magnetism vs. 316 stainless steel properties [New Mexico]
21172. Finish/sealer for intentionally-rusted structural steel [Utah]
21173. Chrome plating mororcycle engine parts [Pennsylvania] {4/15/03}
21174. Need one aluminum rim chrome plated [Illinois] {4/15/03}
21175. Need chrome dipping of four rims [Florida] {4/15/03}
21177. Automotive Organic Coatings [Minnesota]
21179. Durability of oil-rubbed bronze finish [Nevada]
21180. Needing to darken pewter [Texas]
21181. Smoke free muriatic acid [Philippines]
21182. Iron oxide erupting through tin plating [California]
21183. Seeking: Nickel plated fine aluminum wire (0.001"-0.005") [Maryland]
21184. Better options to zinc passivate plating? [New Zealand]
21185. Bright spotting in satin nickel finish [New Zealand]
21186. Increasing plating hardness [India]
21187. Nickel chrome plating issue [California]
21188. CHEMICAL MILLING OF TITANIUM [India]
21189. Tarnishing of plated products [South Africa]
21190. Protective finish for copper molds [South Carolina]
21191. Cleaning weld marks on stainless steel [Illinois]
21192. ULTRASONICS TO INCREASE PLATING SPEED [California]
21193. Seeking chrome plating [Texas] {4/15/03}
21194. Cleaning of hard metal substrates before PVD coating [France]
21195. Solvent for CF4 plasma deposited PMMA layer [Switzerland]
21196. On-site flat black wrinkle finish [Washington]
21197. Maximum chlorides in cooling water [Spain]
21198. Dichromate sealing set-up [Canada]
21199. Rainbow Titanium-Oxide Coating [Virginia] {4/16/03}
21200. Mil-C-5541 Chem Film on terminal blocks [China] {4/16/03}
21201. Need Nikasil replating for Honda NSR 250cc cylinder [Greece] {4/16/03}
21202. Control of nickel tank [Egypt]
21203. Brass corrosion prevention in marine conditions [California]
21204. Passivation alternative [UAE]
21205. Ceramic coating over stainless steel for a medical instrument [India]
21206. Spray paint that gives anodized look? [New Jersey]
21207. Need Langsol Products [Indonesia] {4/16/03}
21208. Conductivity of CR 304 Stainless Steel [England]
21209. Stripping the paint off a wrought iron table and chairs and repainting [New York]
21210. Using the paint for the body of the gas household appliances those expose to heat [Iran]
21211. Legs need refreshing-rust removal and added shine [New York]
21212. Scale Removal Methods [Iran]
21213. TIN PLATING COPPER PANS [Arizona]
21214. Starting a SIM card factory [India]
21215. Black dye for hard coat anodized forgings [Maine]
21216. Galvanized Sheet Metals [Ohio]
21217. Soldering zinc plate [UK]
21218. How do I paint my action figure? [India]
21219. Motorcycle chrome rims [Illinois] {4/16/03}
21220. Corrosion protection of Aluminium without Cr6 [Great Britain] {4/16/03}
21221. Need 12" Spin Dryers [Michigan] {4/16/03}
21222. Electrophoretic [Malaysia]
21223. Coating Ospho? [Oregon]
21224. Custom vinyl interior [Canada]
21225. Removing chrome from the insides of my wheels [New York]
21226. Let the Chrome Shine Through! [Alabama]
21227. Sealing Cast Iron Fireplaces Once Restored [UK]
21228. Chrome-free coatings [Indiana]
21229. Runoff from copper roofing [California]
21230. CrN Stripping [Canada]
21231. Bonding with MEK [Mexico]
21232. Kinds of treatment superficial Cr6 free [Brazil]
21233. Blackened, bronzed or colored finishing black of the stainless steel [Spain]
21234. Problem with bright nickel [Egypt]
21235. Need pickle and passivate of stainless forgings [Canada] {4/17/03}
21236. Need vacuum metallizing of polycarbonate lighting fixtures [India] {4/17/03}
21237. Blue-coloured electrolytic brightening agent [Russia] {4/17/03}
21238. Impregnation Resin for aluminum wheels [India] {4/17/03}
21239. Polycarbonate cryogenic deflashing equipment [Philippines] {4/17/03}
21240. Need 25-50 grams of PdCl2 [Spain] {4/17/03}
21241. Need valmet thickness gauge [South Korea] {4/17/03}
21242. Using Laser to Produce Thin Oxide Coating on glass [UK]
21243. Inclusions and polishing defects [Iran]
21244. How to check the gold concentration in a gold bath instead of using AAS? [China]
21245. Black color on silver item [Turkey]
21246. Anodized al for high load applications [New York]
21247. Cookware mirror finish [UAE]
21248. How anodizing, galvanising and powder coating is done [India]
21250. Why is Zinc Plating changing colors? [South Dakota]
21251. Need clear finish for polished aluminum item [Maine] {4/18/03}
21252. Iridium and or Platinum coated anodes [Wisconsin] {4/18/03}
21253. Can only electroform mush, not hard metal [Pennsylvania]
21254. Determination of Na by AAS [UK]
21255. Cubic Printing System [India]
21256. Paint handlebars [Canada]
21257. Prepping metal for paint [Wisconsin]
21258. Magnetism of electroplating processes [Oregon]
21259. Alternative to chromating for white rust protection [Oklahoma]
21260. Chemical cleaning of boiler [Poland]
21261. MIL STD 105E method [Malaysia]
21262. Understanding chromate passivations [Michigan]
21263. Electrophoretic paint and hydrogen embrittlement [Michigan]
21264. Electroforming substrates [UK]
21265. Corrosion of nickel plating [West Virginia]
21266. Is copper or nickel flashing a must for good solderability of tin plated steel [Texas]
21267. Manganese Phosphate sludging problem [North Carolina]
21268. Electropolishing is not shiny [Pakistan]
21269. Looking for corrosion performance chart for steel [Washington]
21270. Seeking Powder Coating Service [Ohio] {4/18/03}
21271. Improvement of colour change of bromophenol blue indicator in glycerine [Malaysia]
21272. Oxidizing copper [New York]
21273. Allergies to Castrol Alusol? [Indiana]
21274. Anodize vs Paint [California]
21275. Hologram effect (AKA holographic buffing tails) in automotive paint [Australia]
21276. Oil Rubber Mild Steel Finish Process? [Florida]
21277. Nitride Leakage through Copper Plate Stop Off [Massachusetts]
21278. Die cast repair/acid copper [Kansas]
21279. Molding elastomer to anodized Al [New York]
21280. Phosphating 3-4% chromium steel [Argentina]
21281. STAINLESS STEEL FINISH FOR ADHESION [California]
21282. Zinc --Prime Western Grade [Iran] {4/18/03}
21283. Improved microwave fabrication methods [China]
21284. Regenerate resin [Indonesia]
21285. Copper Plating Issue [India]
21286. Hard chrome plate on I.D. of 304 stainless steel tube [Minnesota] {4/21/03}
21287. Need a metal mold mangrane coated [California] {4/21/03}
21288. RFQ to chem film and paint [Utah] {4/21/03}
21289. Seeking vinyl powder for powder coating [California] {4/21/03}
21290. Seeks info about advanced chrome/nickel and galvano plating systems [Iran] {4/21/03}
21291. Need Used Spray Booth for Ceramic Enameling Powder [Brazil] {4/21/03}
21292. Green wheel source? [Virginia] {4/21/03}
21293. Silver Solution polishing kit by Sheffield Silver [Georgia] {4/21/03}
21294. Need literature on standards for surface roughness [India] {4/21/03}
21296. REFLECTIVE GLASS BEADS [India] {4/21/03}
21297. Steel wool corrosion, unexpected results [Norway]
21298. How to electroplate [Saudi Arabia]
21299. Oxygen scavengers [Minnesota]
21300. Laptop painting [Massachusetts]
21301. Paint/sealer adherence to "non-metallic" gas tank [Nevada]
21302. Paint removal from leather [Florida]
21303. Removing lacquer from brass [Florida]
21304. Metal finishing [California]
21305. Refinish Computers? [Louisiana]
21306. Copper rust remover [Canada]
21307. Trash to Treasure Antique Iron Bed [Georgia]
21308. Mast Refinishing [Michigan]
21309. Want rhodium plating over yellow gold [New York]
21310. What is Jewelers rouge and where can I get it? [India]
21311. Rust Area on Galvanized Metal [Pennsylvania]
21312. Metal for Robotics [Washington DC]
21313. Need copy of plating specification [Michigan]
21314. Needing diagram and dimensions for a Pour Foam Test Apparatus, LX4140 [Texas]
21315. NFPA 33 Unclear about powder booth [Virginia]
21316. HCL fumes [Pakistan]
21317. Barrel-plating on plastics [India]
21318. Tin plating surface finish [India]
21319. Aux. anode placement and LCDs [Arizona]
21320. Black anodizing ESD hazard of fast moving parts [Canada]
21321. Heat shock resistant of hard anodized coating and scratch resistant property of hard anodized when hot [India]
21322. Black anodizing problem [Maine]
21323. Can anodization cause brittleness? [India]
21324. Polishing Stainless Steel [Illinois]
21325. Electropolishing know how [India]
21326. Stainless Steel vs. Zinc Plated Fasteners [Wisconsin]
21327. Brass plated on candlelabras gone bad [North Carolina] {4/22/03}
21328. NEED TO BUY PASSIVATING SYSTEM [New York] {4/22/03}
21329. Need lacquer for gold plating [Pakistan] {4/22/03}
21331. Painting Graphics and Plastics [Ohio]
21332. Table top refinish -- to urethane or not? [Massachusetts]
21333. Stripping Gold Plating from Beryllium Copper without damaging the GOLD [Texas]
21334. Ink in wood [Texas]
21335. Specification for Black Chromate over Zinc Plating [Canada]
21336. Painting Fiberglass [California]
21337. Knoop Microhardness Tester [Malaysia]
21338. Chromate testing for zinc plate [California]
21339. Stripping [India]
21340. Set-up of Teflon coating plant [Indonesia]
21341. Clear lacquering tints [Pennsylvania]
21342. Process for electroless Ni-Cu-P [Indiana]
21343. Chrome electroplating vs. electroless nickel in mirror finishes [Canada]
21344. Electroforming [Turkey]
21345. Acid complexing agent for aluminum? [Washington]
21346. International Standard for Stainless Steel Purity? [Singapore]
21347. Non magnatic tranfurable steel [New Zealand]
21348. Pearl gold color which is applied on the base of brass plating [Pakistan]
21349. Need powder coating of my Harley parts [Tennessee] {4/22/03}
21350. Need hard gold plating [Singapore] {4/22/03}
21351. Source for Tungsten Carbide Coatings in Mumbai [India] {4/22/03}
21352. Seeking anodizing of stainless steel parts [Missouri] {4/22/03}
21353. Need local source for consumable parts of plating line [Malaysia] {4/22/03}
21354. Need Plating Additives for distribution [Pakistan] {4/22/03}
21355. Aluminum Boat Frame and Wire Brushing [Delaware]
21356. Trouble with my french polishing [Canada]
21357. How to remove stains of Tremclad [Canada]
21358. Interested in the small business aspect of ceramic coatings and powder coatings [Canada]
21359. COR-TEN steel sealer to control oxidation [Washington]
21360. Electrodeposition of nickel [West Virginia]
21361. ALTERNATIVE METHOD FOR CLEANING THE HEAT TREATMENT BURN MARKS ON AISI 304 STAINLESS STEEL [Turkey]
21362. Removing Zinc Phosphate [Oregon]
21363. Re-anodizing feasible? [Canada]
21364. How to antique wrought iron furniture [Mississippi]
21365. Need "gold" chromate (?) finish applied to cast magnesium parts [California] {4/23/03}
21366. Dyanco Process #C-13 [California]
21367. Weathering brass to a bronze color [Pennsylvania]
21368. Corrosion of anodized coating, cookware [New York]
21369. Silver plating for copper bus bar [Canada]
21370. Looking for a place to chrome motorcycle parts [Minnesota] {4/23/03}
21371. Need AR-1500 (or equal) Rust Inhibitor [Georgia] {4/23/03}
21372. Brass bed refinishing [California] {4/23/03}
21373. LOOKING FOR SOURCE OF ELECTROFORMED BEADS [New Jersey] {4/23/03}
21374. Need reel to reel plater with reflow tin capability [Oregon] {4/23/03}
21375. PRE TIN PLATED STAINLESS STEEL [UK] {4/23/03}
21376. Titanium Processing for Lockheed Martin [California] {4/23/03}
21377. Need auto or semi-auto polishing machines [India] {4/23/03}
21378. Looking for software for my ggx-6b atomic absorbtion spectrometer [Australia] {4/23/02}
21379. LOOKING FOR PASSIVATION AND ELECTROPOLISHING SYSTEM [Florida] {4/23/03}
21380. How to paint hog panels [Missouri]
21381. What are the five metals of panchalogam [India]
21382. POWDER COTING DEFECTS: ORANGE PEEL OFF [India]
21383. Plating copper and /or nickel on low temp lead eutectics [Louisiana]
21384. White Corrosion on 6061 Alodine 1500cc, Salt Spray [Idaho]
21385. How to determine the frequency of chemical solution recharge? [South Korea]
21386. Seeking shop to powder-coat custom car grills [Pennsylvania] {4/24/03}
21387. Fireplace equipment polished and lacquered [New Jersey] {4/24/03}
21388. Field applied passivation gels [Ohio] {4/24/03}
21389. Interested in plating business [Canada]
21390. Re-Painting a wrought iron bed [Minnesota]
21391. Water based metal coatings [Washington]
21392. Best repair/paint process to match factory application [Rhode Island]
21393. Information and restoring info on antique wood stove [Missouri]
21394. Acid dipping my '55 Chevy [New York] {4/24/03}
21395. HIGH TEMP BONDING [Oregon]
21396. SEARCH FOR DURABLE RESIN SYSTEM [Georgia] {4/24/03}
21397. Electroless Nickel Plate of B7 Alloy Bolts [Massachusetts]
21398. Using Magnesium Hydroxide for Acid Streams [Nevada]
21399. Chrome carbide coating of ball valve balls [Pennsylvania] {4/24/03}
21400. Volume of collected salt solution condensate [Canada]
21401. Look for Electro Deburring Company [Japan] {4/24/03}
21402. Fluoride Phosphate per FPS-0116 quote needed [New York] {4/24/03}
21403. PORCELAIN ENAMEL PAINTING [UAE] {4/24/03}
21404. Looking for inexpensive, used wet paintline [Georgia] {4/24/03}
21405. Looking for a solvent for cleaning metals [Israel] {4/24/03}
21406. GCSE information needed please! [England]
21407. Electropolishing [Israel]
21408. Ni electroless plating on fibers [Singapore]
21409. Antique Metal Resotoration [Maryland]
21410. Suitable anodizing power supply question [Ireland]
21411. Chrome dipping procedures /chemicals and equipment [Florida]
21412. Etching cast aluminum [New York]
21413. Bumpers [California]
21414. Concentration of HF in the presence of SO2 [China]
21415. Pits in acid copper plating [Arizona]
21416. Removing anodization without spoiling the aluminum [UK]
21417. Dielectric strength of hard coat black anodized aluminum [Canada]
21418. Passivation testing [India]
21419. Electropolishing for part used in medium vacuum condition [Singapore]
21420. Repair of Spectrophotometer [Nepal] {4/25/03}
21421. WATER EVAPORATOR [New York]
21422. Alkaline nickel electrostrip etches and pits [California]
21423. Ni/Pd/Au finishing lead failed dipping solderability, possible causes [Malaysia]
21424. P.V.D.F. coating - investment cost [India]
21425. Stenciling on Powder Coat [Tennessee]
21426. Chemical Nickel Plating [Ohio]
21427. Alodine 1000, 1001, and 1500 [Singapore]
21428. Impact of exterior scale buildup on rotary kiln performance [Louisiana]
21429. Rechroming rims for 95 Gt [New York] {4/25/03}
21430. Need local seller of Nybco spray paints [Ohio] {4/25/03}
21431. SEEKING MACHINE FOR COPIER DRUM COATING [Mexico] {4/25/03}
21432. NEED BARRELS FOR PLATING ABS SMALL COMPONENTS [India] {4/25/03}
21433. Need Inexpensive Vibratory Finishing Machine [Delaware] {4/25/03}
21434. Info about copper electropolishing [Belgium]
21435. Method of mirroring by spraying [Pakistan]
21436. Removing oxidation from bronze [Alabama]
21437. "Rainbowing" and "Bluing" Stainless Steel [Louisiana]
21438. Nickel plating removal [Florida]
21439. Painting galvanized pipe handicap railing [Massachusetts]
21440. Want to know about chrome plating on abs plastic process [Pakistan] {4/28/03}
21441. How to polish SS304 in phos/sul acids soln [India]
21442. Rechrome my 17" Boyd rims [California] {4/28/03}
21443. Plating stainless steel onto aluminum [Tennessee]
21444. Dissimilar Metals [Pennsylvania]
21445. Rust treatment for large areas [Australia]
21446. Request to buy automatic zinc electroplating line [Iran] {4/28/03}
21447. Removal of Epoxy Based Powder Coatings [Michigan]
21448. Copper restoration [New Jersey]
21449. Inquiry for surface roughness [India]
21450. Small electrorefining equipment for gold [Nicaragua]
21451. Solder wire machine [India] {4/28/03}
21452. STRIPPING OF GOLD [India]
21453. Brass protection [Utah]
21454. Powder Coated Cabinets Quality Issues [India]
21455. NEED TO GET YAMAHA FENDERS CHROMED [California] {4/28/03}
21456. Rechrome Porsche Boxster Rims [California] {4/28/03}
21457. Electro galvanizing Versus Hot Dip [Singapore]
21458. Why does Ni prevent Cu migration to Au? [Hong Kong]
21459. Rechroming table legs [New York] {4/28/03}
21460. How can I build a "hot" oxide system? [Alabama]
21461. Request for information on the seven tank process [India]
21462. Copper work [Canada]
21463. Pure Tin and Tin-Lead [Malaysia]
21464. Satin finish on stainless castings [India]
21465. Removal of rust from vinyl siding [Indiana]
21466. Need info about yellow dye to be used with passivation [India]
21467. Whitewash on Bright Nickel/Chrome Plated Parts [Indiana]
21468. 5S Audit sample [Canada]
21469. Sandblasting - powder coating needed [New Jersey] {4/29/03}
21470. Need brass brite dip finishing services [Indiana] {4/29/03}
21471. Blister after powder coating on zinc chromated surface [India]
21472. Refinish metal door [Arkansas]
21473. I need a red patina [India]
21474. Molleting tool/knurling tool for nickel screen making [India] {4/29/03}
21475. Need 4 rims chrome plated [Indiana] {4/29/03}
21476. Sn-Ni Jobshop [China] {4/29/03}
21477. Need conductive glue [Arizona] {4/29/03}
21478. Acid + Carbonate = what reaction? [Australia]
21479. Organometallic precipitation [Sweden]
21480. Copper Electroformed Layer "Upset" by Extreme Heat [Texas]
21481. BLACK ANODIZED PROBLEM [Massachusetts]
21482. Need help with very serious tarnish [Oklahoma]
21483. Question on re-finishing cymbals [Michigan]
21484. Cleaning a salt looking crust off of polished aluminum [Pennsylvania]
21485. Electroplating Holly Leaves [UK]
21486. Seeking references for nickel plated copper clad aluminum [France]
21487. Electropolishing [Ireland]
21488. Sursulf Quenched Water Treating System [India]
21489. Enamel painting [Egypt]
21490. Sticky Sludge Problem [India]
21491. Chroming shop for motorcycle wheels and parts [Minnesota] {4/30/03}
21492. Phosphate coat 22 pieces per Mil STD 16232 Type M or Z Class 3 [Maine] {4/30/03}
21493. Need a company who can remove silver and aluminum from copper [Massachusetts] {4/30/03}
21494. High volume Ni chrome platers [Ohio] {4/30/03}
21495. Motor cylinder bore plating or anodizing (hard chrome, nikasil...) [Turkey] {4/30/03}
21496. Vacuum metalizing equipment for plastic chrome plating [Canada] {4/30/03}
21497. PACVD or PECVD system [Mexico] {4/30/03}
21498. Locate Green engraver model #106 [Florida] {4/30/03}
21499. Tarnishing Chain (Making Antique Silver Jewelry Chain) [California]
21500. Resurfacing with enamel [England]
21501. Restoring ATP luster [Alabama]
21502. Painting over Plated Brass Shower Enclosure Frame [Texas]
21503. Graphite suspension [Canada]
21504. Oil rubbed bronze finish [New Hampshire]
21505. Dry Film PTFE on Aluminium alloy 6061-T6 [Singapore]
21506. Plating versus solderability issues [New York]
21507. Ethanol resistant lacquers [India]
21508. High Temperature Baking of Nickel Chrome Plating and its Possible Effect [Ohio]
21509. WOULD A FINE-SILVER PLATING CUT DOWN ON THE TARNISHING OF POLISHED STERLING JEWELRY? [Nevada]
21510. Aluminum electropolishing [France]
21511. Looking for answers on Phos and Oil [Wisconsin]
21512. Molten Sulfur Storage in 304L SS [Pennsylvania]
21513. NICKEL PLATING TITANIUM WITHOUT O2 PROBLEM [Florida] {5/01/03}
21514. Elecrophoretic jobworker wanted [India] {5/01/03}
21515. Acid dipping [Pennsylvania] {5/01/03}
21516. Vaccum plate a Chevelle dash bezel [California] {5/01/03}
21517. REFURBISHING BAKED ENAMEL FINISH ON ANTIQUE HIGH CHAIR TRAY [Pennsylvania] {5/01/03}
21518. Chroming of alloy wheels [Australia] {5/01/03}
21519. Seeking PTFE coaters [Thailand] {5/01/03}
21520. Require polishing equipment [New Jersey] {5/01/03}
21521. Want to buy RO-59 [Washington] {5/01/03}
21523. Sealer to keep copper caps for turning black? [South Carolina]
21524. Dye wipes off anodized parts! [Florida]
21525. Help with prep anodizing [Michigan]
21526. Is there a fix to stainless steel pitting? [California]
21527. Body chemistry and sterling silver [Georgia]
21528. Looking for a brick to fit back of cast iron fireplace [South Africa]
21529. Chromed fenders and gas tank on a Harley? [Ohio]
21530. QQZ325C Alive or Dead? [Pennsylvania]
21531. Steel grade EN8D [India]
21532. CITY INSPECTORS!! HELP! [Oklahoma]
21533. How to qualify a metallic plating-substrate system regarding its diffusion properties? [France]
21534. Removal of Platinum [Texas]
21535. Chloride contamination of galvanize steel and removal methods [California]
21536. Titanium dry etch [France]
21537. Med or high phos [Indiana]
21538. Purification of SnPb plating bath [Arizona]
21539. Decorative Chrome plating 304 Stainless steel foot pegs [Washington]
21540. Needed: Nickel corrosion performance with Tin ductility [Arizona]
21541. Nickel plating loses continuity [India]
21542. Silicon Dioxide Coating [India]
21543. Aluminium finishing for saline weather [Malaysia]
21544. Teflon impregnated hard anodising [New Zealand] {5/01/03}
21545. Fluoropolymer / PTFE [Indonesia]
21546. Removing Magnetism in Stainless 304 Grade Fasteners [India]
21547. Start Own Teflon Re-Coating Business [Thailand] {5/02/03}
21548. Seeking chiller unit, capacity 3tons [India] {5/02/03}
21549. Rhodium plating [Massachusetts]
21550. Sodium hydrosulphite (dithionite) [UK]
21551. Matte tin - what is the criteria appearance or thickness which determines coverage [Maryland]
21553. Rims re-chromed [New Jersey] {5/02/03}
21554. Need sodium gold (I) sulfite [New Mexico] {5/02/03}
21555. Glue for Copper Caps [Alabama]
21556. OK TO JUST USE BLACK PAINT? [Oregon]
21557. Copper paint for plating [Texas]
21558. Blue coloring on cast aluminum [Washington]
21559. Stainless steel weakened by chlorine gas [Florida]
21560. Need help in identifying Cr3t [Indiana]
21561. Collinox for Zamac diecasting [Illinois]
21562. Pure Zr PVD coating required [New York]
21563. Immersion silver adhesion to copper? [Massachusetts]
21564. Question on Cleaners: Where is this white haze coming from?
21565. Metalized Finish on Aluminum [California]
21566. Corrosion and adhesion. Shotblast vs no shotblast [Indiana]
21567. Removing/Preventing graphite from sticking to Kovar [Maryland]
21568. Plating copper, zinc, or gold onto an styrofoam/epoxy sphere! [Washington]
21570. Comparison between Powder Coatings and Electrodeposition [India]
21571. Help on Polishing and Lacquering Small Brass Boilers [New Zealand]
21572. Can a part be black hard anodised after chemical film finish ? [Singapore]
21573. Acid Copper over Zinc Die-cast cut through during buffing [Wisconsin]
21574. Teflon coating inside the SS piping [Singapore] {5/05/03}
21575. Rechroming of Harley parts [Vancouver, Canada] {5/05/03}
21576. Polish Airstream [Texas] {5/05/03}
21577. Seeking small quanity alloy anodizing [Alabama] {5/05/03}
21578. Need oil rubbed bronze refinish with tarnish and wear resistant finish [Colorado] {5/05/03}
21579. Polyester coating [Florida] {5/05/03}
21580. Seeking nickel [Venezuela] {5/05/03}
21581. Need the Silver Solution [New York] {5/05/03}
21582. Need a used or surplus nickel, chrome soln [India] {5/05/03}
21583. Reducing weight whilst maintaining stiffness and strength? [UK]
21584. Electrolysis [England]
21585. Growth rate of gold [India]
21586. Formulation of plating chemicals [India]
21587. Teflon inserts on punch tips [India]
21588. Questions on aluminum pontoons [California]
21589. Aluminum cylinder fins clear finish [Brazil]
21590. Polishing Aluminum Wheels on BMW r100rs (1981)...help! [Ireland]
21591. Corrosion resistant coating for stainless steel wanted [Pennsylvania]
21592. Amateur doing some aluminum polishing [Louisiana]
21593. Removing rhodium plating [Connecticut]
21594. Amount of resin needed to saturate fiberglass mat [Illinois]
21595. Removing black antiquing from a gold ring [Massachusetts]
21596. What is Liver of Sulphur? [South Africa]
21597. Chrome repair [Texas]
21598. Silver polished rims [Georgia]
21599. Can a patina be applied to chrome [Virginia]
21600. Steel foil required [India]
21601. Foil tape-Copper works [Florida]
21602. Seeking Salt Bath Nitriding specification [Minnesota]
21603. Toxin INFO on Yellow Dichromate [Canada]
21604. Salt Spray Life of powder coat vs zinc olive green passivation [India]
21605. Etching brass plates [New Zealand]
21606. How to paint copper downspouts, gutters, flashing, etc. [California]
21607. Black Oxide on Stainless Steel [California]
21608. How to make Matte finish Hot Dip Tinning [UK]
21609. Chrome Plating Stainless Steel [Missouri]
21610. Machine coolant etching aluminum? [Connecticut]
21611. Pretreatment process [Saudi Arabia]
21612. Type of acid/solution for s.s etching [Pakistan]
21613. Steel pickling and side effects [Massachusetts]
21614. Tube Failure in 2nd Stage Intercooler Compressor [Saudi Arabia]
21615. 304SS with H2S [England]
21616. ELECTROPLATED COPPER/BRASS SHEETS IN DEMAND [India] {5/06/03}
21617. Sn (tin) [U.A.E.] {5/06/03}
21618. Looking for Small Powder Coating Turn-key system [Florida] {5/06/03}
21619. Glue/Adhesive Copper/Brass etc. [Maryland]
21620. Problems with blister packing [India]
21621. Reflective paper for solar cooker applications [Michigan]
21622. How does one "Low Tech" pickle descale #9 gauge wire? [Nebraska]
21623. High heat resistant coating [North Carolina]
21624. European Union's "End of Life Vehicle" standard for Cr6 chromates [California]
21625. Finishing aluminum [New York]
21626. Rust Removal Product? [North Carolina]
21627. Ollard Testing or Modified Ollard Testing [Connecticut]
21628. Painting galvanized windmill sails [Michigan]
21629. The origin of Corrosion coatings [England]
21630. Muric acid as a cleaner [Florida]
21631. Clear Resin Coating On Bright Zinc Plating [India]
21632. Verification of hexavalent plating and timing for phase-out [Michigan]
21633. Searching Nickel Electroforming Events [Spain]
21634. Imitation gold (brass salt) [Indonesia] {5/07/03}
21635. Finishing cast aluminum [Italy]
21636. THROWING POWER IS INCREASED? [Pennsylvania]
21637. Sources for hot dip galvanizing [Maine] {5/07/03}
21638. Tub legs chromed [Massachusetts] {5/07/03}
21639. Seeking zinc plating on Oahu for rod iron railing [Hawaii] {5/07/03}
21641. Ospho Primer Distributor [North Carolina] {5/07/03}
21642. Instrument for Paint Thickness Measurement [Hong Kong] {5/07/03}
21643. Flat black paint IR absorbing adherence to aluminum [Missouri] {5/07/03}
21644. Technology of car plastic parts [Israel]
21645. Termocouples cleaning [Italy]
21646. Force curing cor-ten steel and copper metalizing spray [Texas]
21648. Deopsiting a boron thin film [Australia]
21649. Au wire bonding question [Florida]
21650. Improving EN adhesion to steel [Israel]
21651. Enquiry of setup hologram label industry [India] {5/07/03}
21652. Screen printing machine for piston skirt [Iran] {5/07/03}
21653. Need adhesive plastic to protect metal from scratches [Indonesia] {5/07/03}
21654. Boundary condition on bipolar electrode [Russia]
21655. What kind or kinds of surface treatment technology can be operated on shell of notebook PC ? [China]
21656. Zinc Peeling [India]
21657. How volatile is H2O [Pennsylvania]
21658. ADC 12 query [Pakistan]
21659. Distressing brass wall sconces [New York]
21660. Process Of SandBlasting [India]
21661. Low Friction Metal Clothing Racks [Texas]
21662. How can we evaluate zinc corrosion [Libya]
21663. Making paint stick to nickel without hex chrome? [Canada]
21664. Plating problem? [Singapore]
21665. Caustic etching for aluminum shores [Korea]
21666. Etching aluminum with a matte surface [Iran]
21667. Fungus formation after exposure to Brake Fluids [India]
21668. Surface treatment of G.I. steel [India]
21669. Iron Phosphating [Iran]
21670. Carbon Fiber Corrosion on Metal? [Delaware]
21671. Heat staking pins - recommended materials [Canada]
21672. Need anti-corrosion coating for low quality stainless steel posts [New York] {5/9/03}
21673. Seeking conversion coating/anodizing of aluminum extrusions [Oregon] {5/9/03}
21674. Need Everslik 1201 and 1301 [Florida] {5/09/03}
21675. How to dissolve Tin Oxide [Rhode Island]
21676. Non-amenable cyanides in wastewater [New York]
21677. Titanium Nitride Coating Standards? [Montana]
21678. Problem of high variation of coating thickness in barrel plating [India]
21679. Cobalt Chrome [Ohio]
21680. Cyanide in gold deposit? [Tennessee]
21681. How to print on anodized aluminum sheet without using Film [Ontario]
21682. Burnishing of Cast Aluminum [Georgia]
21683. Nitric Acid attack on Carbon Steel [Pennsylvania]
21684. Nickle wire dining room chairs need dipping in chrome [New Jersey] {5/9/03}
21685. Need Dry Film Resist [Singapore] {5/09/03}
21686. Trouble making a metallic pigment hammertone finish [France]
21687. Non-toxic Stove Top Paint [Ontario]
21688. Pursuit of Shiny Parts [Maine]
21689. What Steel handbook do I need? [India]
21690. Replacement for 304 SS hooks in jig [Massachusetts]
21691. Etching of titanium for microscopic examination [Egypt]
21692. CONVERTING GRAM/SQ MT TO MICRONS [India]
21693. Sealing Aluminum to prevent oxidation? [Nebraska]
21694. Chroming of an Exhaust Tip [Mississippi] {5/9/03}
21695. Need Trivalent Black [Michigan] {5/9/03}
21696. Low Cost Anodizing Service Needed [No. Carolina] {5/9/03}
21697. Need Chroming Company for rims & other things [New Jersey] {5/9/03}
21698. Furniture manufacturer looking for mass finishing of aluminum parts [Ohio] {5/9/03}
21699. Need a 2nd-hand powder paint oven [Ireland] {5/09/03}
21700. Extracting zinc from a penny [Wyoming]
21701. Chrome dipping: How long lasting and how costly? [Georgia]
21702. Coloring of stainless steel [So. Africa]
21703. Toxic effects from galvanized food preparation utensils [British Columbia]
21704. Deionized water making procedures [Washington]
21705. Refining solder [So. Africa]
21706. Leakage of oil after powder coating steel tubing frame [Texas]
21707. Surface Finish Conversions [Michigan]
21708. Comparison between ED and Powder Coatings [India]
21709. Titanium dipping [North Carolina]
21710. Small dia. rubber coated slugs [Minnesota] {5/10/03}
21712. Deburring of Aluminum components [India]
21713. Plating of brass with electroless nickel and gold [Canada]
21714. Sur-Sulf on engine shaft [Italy]
21715. Powder coat applied over zinc plating [Indiana]
21716. Role of a Chemical Engineer [India]
21717. Everslik [California]
21718. Acid chemistry [Texas]
21719. Copper plating self casted lead objects [Massachusetts]
21720. Machine Manufacturer for electroplating of copper wire (solder plated wire) [India] {5/10/03}
21721. Bright Dip problem [Texas]
21722. Porosity and die castings [Minnesota]
21723. Need tungsten carbide coating [Italy] {5/10/03}
21724. How to remove scratches from stainless steel refrigerator doors? [California]
21726. Oxidizing a cobalt thin film [Vietnam]
21727. Electropolished part dimensional tolerance [Michigan]
21728. Aluminum Surface Quality Improvement [New Zealand]
21729. Tarnished Stainless Steel with Muratic Acid! Please help! [California]
21730. Is it possible deposit SiO2 by PVD cathodic arc? [China]
21731. Salt spray test on MS and SS [India]
21732. Formulating phosphate pretreatment solutions [India]
21733. Looking for a chemical to dissolve EVA [California]
21734. Embossed metal sheeting for birdhouse roofs [Wisconsin]
21735. Brass Chandelier [Florida]
21736. Seeking used RECTIFIER 1000 AMP 40 VOLT [Louisiana] {5/10/03}
21737. The three leading elements in electroplating [Minnesota]
21738. Air Tubes Failure in 2nd Stage Air Compressor [Saudi Arabia]
21739. Water spot remover suggestions for windows, paint on car [Hawaii]
21740. ASTM Electrochemical test for rebar in concrete [Ohio]
21741. Chrome Plating Motorcycle Parts [Mexico] {5/12/03}
21742. Asymmetrical current [Russia]
21743. Rechrome motorcycle rims [Kansas] {5/12/03}
21744. Info wanted: carburetor zinc dichromate refinishing [Michigan]
21745. Looking for barrel electropolishing [Illinois] {5/12/03}
21746. Need advice how to polish my motorcycle frame properly by hand [North Carolina]
21747. Moderately high causticity a problem for clear anodize? [Illinois]
21748. Brass Sealer [Michigan]
21749. Restoration of aluminum covers [Vietnam]
21750. Mill scale recovery [Iran]
21751. Discoloration on Plated Leadframe [Singapore]
21752. Black brass [Washington]
21753. ALUMINIZED STEEL PRODUCTION FACTORY [Iran] {5/12/03}
21754. Chrome paint and cellulose paint [Scotland]
21755. Shining old Brass Trumpet the easy way [Tennessee]
21756. Titanium woks [UK]
21757. NEED MOLYBDENUM SULPHATE SURFACE TREATMENT ON STEEL [India]
21758. ALUMINIUM GRADE FOR PERFUME/COSMETIC INDUSTRY [India]
21759. How to remove haze from engine degreaser on stainless steel [Nebraska]
21760. Aluminized Steel [Iran]
21761. Nickel free finishing of hardware [India]
21762. BLACK ANODIZED ALUMINUM TUBING [Arkansas] {5/12/03}
21763. Need Dacro coating: D2008 grade 1 [Connecticut] {5/12/03}
21764. White spot after grinding process [Malaysia]
21765. Sculptor seeking Steel (anti rust) finish [Australia]
21766. Continuous monitoring of specific gravity during a plating process [New Jersey]
21767. Stripping the anodize coat [New York]
21768. Electropolishing of aluminum dicast alloy [Egypt]
21769. Silver to chrome? [New Mexico]
21770. Removal of Heavy Metals from Contaminated Water [UAE]
21771. Why does hydrochloric acid rust nails? [Sweden]
21772. Which type of juice cleans pennies the best? [South Carolina]
21773. Heavy metals in our environment [Nigeria]
21774. Powder coat maintenence [Texas]
21775. Refinish exterior brass light fixtures [Tennessee]
21776. Is there difference between Alocrom 1200 and Alodine 1201? [UK]
21777. Finishing brass stock to mirror finish [New York]
21778. Small cans of spray, gray wrinkle finish paint? [California]
21779. What is mechanical zinc plating? [Pennsylvania]
21780. Fix for a failing powder coat? [California]
21781. Request for substitute of chromate conversion of zinc-plating [China]
21782. Antistick treatment to steel mold for painted parts [Mexico]
21783. Coating for sole plate of electric iron [Hong Kong]
21784. SPI #2 to RMS number? [Utah]
21785. Clear coat protection for ultaviolet fading of aluminum [New York]
21786. Tinplating line [Nepal] {5/13/03}
21787. Need old car parts anodized [Colorado] {5/13/03}
21788. Seeking plating shop that plates on plastic [Canada] {5/13/03}
21789. Need clear and brite-dip red anodizing, plasma electrolytic oxidation [Michigan] {5/13/03}
21790. Search for Nikasil and Hard Cr plating and deplating equipment [Turkey] {5/13/03}
21791. Need technical assistance for powder coating plant [India] {5/13/03}
21792. Need water based varnish, 40 tons/mo [China] {5/13/03}
21793. Pulse plating in cyanide based baths [Sweden]
21794. New to Chrome - Repairing Pits [Texas]
21795. Copper cleaning and restoration [California]
21796. Surface finish definition for stainless steel [Canada]
21797. Brazing brass to brass [Oregon]
21798. Internal painting of pipes [Turkey]
21799. Liquid and powder coating comparison [Pakistan]
21800. Basic definition of galvaneal steel [Pakistan]
21801. Electroless Nickel Plating Pips [England]
21802. Thickness of tin/lead plate (Mil-P-81728) [Massachusetts]
21803. Aluminum blades treatment [India]
21804. White list passivation chemical, toner, inhibitor [India]
21805. Surface Finish Chart [Canada]
21806. What's construction material resist to Sodium Hydroxide (caustic soda) ? [France]
21807. Need copper polishing service for my building [Illinois] {5/14/03}
21808. Chrome Resurfacing [New York] {5/14/03}
21809. Seeking Chrome Finisher [Canada] {5/14/03}
21810. Seeking Source to Chrome Plastic Parts [Massachusetts] {5/14/03}
21811. Electropolishing for Laser Cut Stencils [Philippines] {5/14/03}
21812. SALT SPRAY CABINETS [Illinois] {5/14/03}
21813. Source of gold plating solution [U.K.] {5/14/03}
21814. Need to establish a Black- Chromatizing system [Egypt] {5/14/03}
21815. Science experiment [Ohio]
21816. Spring failures [New Zealand]
21817. Help me remove burn mark on bath made by tealight [UK]
21818. STAINLESS : Help with heat-treating and annealing [Tennessee]
21819. Enamel repair [Michigan]
21820. Help... need non toxic clear coat for metal [Canada]
21821. Cr6 Emissions from Conversion Coating tank process [California]
21822. Non-Cr strike pre-plating process for Mo [Singapore]
21823. Zn plate w/ tri-chrome passivation, temp at which delamination of plating will occur? [California]
21824. Oil in cadmium plating bath [Kansas]
21825. Chrome plating on aluminum for wear resistance [India]
21826. Better metallizing alloy wire [India]
21827. Material identification [New Zealand]
21828. Seek hot galvanization process expert [Minnesota] {5/15/03}
21829. How can I make steel threaded rod black? [Connecticut]
21830. Yellow Chromate adhesion problems [Wisconsin]
21831. Coloring zinc plated sheet steel [New Mexico]
21832. Yellow chromate stripping [Massachusetts]
21833. White Rusting on Galvanized Surface [India]
21834. Vacuum metalizing costs [Connecticut]
21835. Conversion coating for pure magnesium [California]
21836. Electrically insulating, wear resistant coating for titanium [Utah]
21837. Galvanic action between carbon and stainless steel [Florida]
21838. Aluminium Clad SAE 1006 cold rolled steel strips/Bronze Clad SAE 1010 deep drawing quality cold steel strips [India] {5/15/03}
21839. Stabilizer for Oil Rubbed Bronze finish [New Mexico] {5/15/03}
21840. Oxidation of immersion silver coating on PCB [Canada]
21841. What kind of chemical do I need to pressure wash my concrete driveway [Alabama]
21842. Looking for PLX Clean Wax or like product [Kansas]
21843. Painter seeks insight [California]
21845. White gold turning yellow after bath [Vermont]
21846. Salt Spray [Malaysia]
21847. Alky resin question [Pennsylvania]
21848. Masking for vibratory finishing process [Italy]
21849. Synthetic sea water [France] {5/16/03}
21850. Stainless Steel Spray Paint needed! [Georgia] {5/16/03}
21851. 440C stainless steel heat treatment problem- surface effects [New York]
21852. Data required for DI water used as rinsing water [India]
21853. Finishing Galvaneal Sheet [South Dakota]
21854. 316 SS temperature by color at max temp [Canada]
21855. Formula for plating sol'n using Chromic acid, Phosphoric acid and Urea? [Ohio]
21856. Need my rims chromed [Wisconsin] {5/16/03}
21857. Need attractive outdoor metal fencing material [California] {5/16/03}
21858. # 6 finish on stainless steel [California] {5/16/03}
21859. PTFE [0.3micron powder] EMULSION [India] {5/16/03}
21860. Nickel allergy [Pennsylvania]
21861. Restoring chrome finish [Ohio]
21862. How can a person anodize aluminum at home? [Virginia]
21863. Removing Paint from Brick Fireplace [California]
21864. Lacquer to spray aluminum yacht for protection [Thailand]
21865. Refinishing wrought iron chairs [Florida]
21866. Anodized titanium [Canada]
21867. Tarnished silver [Ohio]
21868. How do you oxidize silver? [Hawaii]
21869. Guitar chroming [California]
21870. Reactions in Copper Plating [Australia]
21871. Alternative to chrome plating [India]
21872. Chromium plating - heating coil material [UK]
21873. Emission factors pickle bath [Canada]
21874. Determination of chlorides [Italy]
21875. Corrosion on 2024 Chromate, Salt Spray Test [Korea]
21876. Gold plating inquiry [Philippines]
21877. Flexible Coating with UL rating and high dielectric strength [North Carolina]
21878. How to handling copper-plated parts to prevent oxidation [Illinois]
21879. Medical devices, passivation and manufacturing [California]
21880. Need a source for Zinc-Iron plating [Illinois] {5/19/03}
21881. Dacromate process provider [India] {5/19/03}
21882. Wheel Chroming [Florida] {5/19/03}
21883. Change chrome plated shower parts to brass [South Carolina] {5/19/03}
21884. ACIDIC COPPER BRIGHTENERS AND ADDITIVES [Pakistan] {5/19/03}
21885. Seeking pure tin plating process (lead free solder plating) [Malaysia] {5/19/03}
21886. Corten or equivalent required [Australia] {5/19/03}
21887. Rusting nails experiment [Tennessee]
21888. Mild Steel [England]
21889. Electropolishing cast NiAl [Canada]
21890. Gold purity [India]
21891. Urgent Requirement of Technical Support [India]
21892. Glossiness caused by scrubbing siding [Iowa]
21893. Red coloration of any titanium alloy using any method [Canada]
21894. Stainless Steel Paint for White Refrigerator? [California]
21895. 1995"w" American silver eagle. Can you help me? [New York]
21896. Using citric acid as an etching mordant [Alabama]
21897. Removing Rust or Corrosion on Lamp [Iowa]
21898. How to repair minor surface corrosion? [Florida]
21899. Surface imperfections 304ss #4 finish [Ohio]
21900. Safety of hydrochloric acid [New Jersey]
21901. ASTM B-117 SALT SPRAY FAILURES AND ORIENTATION IN A SALT CABINET [Ohio]
21902. Paint for Polycarbonate [Texas]
21903. Powder coating problems [Turkey]
21904. Zinc Ammonium Chloride Solution Specific Heat Capacity [UAE]
21905. Brass electroplating [Saudi Arabia]
21906. Irradiation Process and Steps in Electroplating [India]
21907. Electroplating defect [Malaysia]
21908. Why Nickel Chrome on Stainless Steel? [Illinois]
21909. Nikasil coating [Portugal]
21910. BARREL CHROME ELECTROPLATING [Pakistan]
21911. Iron electroforming Tips and Tricks [Iran]
21912. How does a passivation layer get produced on stainless steel [Pennsylvania]
21913. PICKLING [India]
21914. Grinding and polishing bar formula [India]
21915. How to choose between different scale removal techniques? [Connecticut]
21916. Finishing of stainless steel [India]
21917. Ni plating vs Powder Coating for corrosion resistance and conductivity [California]
21918. Seeking zinc plate [Texas] {5/20/03}
21919. NEED PLATING CHEMICALS [Indonesia] {5/20/03}
21920. Science project not doing well [California]
21921. Need plastic transparent to Infra red [Israel]
21922. Restoring White Gold Coloring [Illinois]
21923. Request for the definition of chromate plus sealer [Singapore]
21924. Is there any alternative to HydroFluoric Acid? [Pakistan]
21925. Cladding of paper cutting machine bed [India] {5/20/03}
21926. Want wholesale quantities of gold and silver plated roses [Pennsylvania] {5/20/03}
21927. In Need of Bright Dip Anodizers [Indiana] {5/20/03}
21928. HELP! Need to passivate tungsten electrodes [Massachusetts] {5/20/03}
21929. Chrome Plating Chemicals [India] {5/20/03}
21930. Pt grid needed [Singapore] {5/20/03}
21931. Need a large rack zinc line [New York] {5/20/03}
21932. Painting public bathroom as an outhouse [Wisconsin]
21933. Electroplating Stained Glass [Canada]
21934. The Polishing of Anodized Aluminum [Delaware]
21935. Is my ring really platinum? [Canada]
21936. Aluminum oxide hazards in fake wood flooring [Washington]
21937. Chrome conversion on zinc-plating [New York]
21938. Brass German polished spec. [England]
21939. Comparing results obtained by various corrosion test methods ? [Australia]
21940. Adhesion of Tire Bead Wire with Rubber [India]
21941. Blackening Process; uniqueness? [Singapore]
21942. Aluchrome corrosion resistance against DI water [UK]
21943. Painting Brass Lamps [Texas]
21944. Shelflife of platings wrt solderability [Holland]
21945. Can stainless be re-passivated? [California]
21946. Paint and Bake Cure [Michigan] {5/21/03}
21947. Need Nearby Source to Clean and Polish Knife Blades [Wisconsin] {5/21/03}
21948. RE-CHROMING MY FORD BUMPERS [North Carolina] {5/21/03}
21949. Need our armatures Teflon coated [Tucson, AZ] {5/21/03}
21950. Seeking MIL-A-8625C anodizing on 6005-T6 handrail components [California] {5/21/03}
21951. PAINT RECIPE [New York]
21952. Recovery of Ni from electroplating waste materials [Pakistan]
21953. Cleaning and Polishing Bronze sailboat hardware [Ohio]
21954. Metal to gold [Utah]
21955. Does Corona treatment make PP adhere better with Acrylic glue? [California]
21956. Black oxide coating won't take [Pennsylvania]
21957. Hard silver plating [Oman]
21958. Anodized Aluminum, brightening aluminum [Wisconsin]
21959. Anodic coating sealing [Israel]
21960. Huntington Alloy IAI-21, How do we make pickling solution? [Ohio]
21961. Where can I find Kelite SprayWhite C aerospace cleaner? [Kentucky]
21962. Zinc phosphate with olive drab seal [Minnesota]
21963. Chrome dipping of engine parts [Pennsylvania] {5/22/03}
21964. Electrostatic powder and liquid paint for wood [Egypt] {5/22/03}
21965. Concrete floor cleaning agent [India] {5/22/03}
21966. MEK-P [California] {5/22/03}
21967. FILTER PRESS REQUIRED [Ohio] {5/22/03}
21968. HELP - WHITE WHISKER LIKE GEL AFTER TIN PLATING [Ireland]
21969. Restoration of zinc tabletop [Georgia]
21970. Paint removal [California]
21971. Black rhodium bath [Portugal]
21972. MSDS request for Tremclad [Canada]
21973. Tiger Drylac [Maine]
21974. Aluminum/Silver Compatibility [Texas]
21975. Nickel /Lead Combination Coatings [Israel]
21976. Looking for Orange Aluminum Coating [Illinois] {5/22/03}
21977. Seeking fabricated canopy anodizing [New Jersey] {5/22/03}
21978. CHEMICALS, ELECTROPLATING, NaCN ETC [Pakistan] {5/22/03}
21979. I need magnesium etching equipment suppliers [Canada] {5/22/03}
21980. Chemical Required [India] {5/22/03}
21981. White streaking buildup [Alabama]
21982. Copper tabletop [Colorado]
21983. ANTIQUING COPPER [Florida]
21984. GOLD PLATING WITH HEAT [Georgia]
21985. IVD Coated Fasteners [Florida]
21986. Hot seal or cold seal? [England]
21987. Portable laser marker for steel [Texas]
21988. Fastening stainless steel to carbon steel [Florida]
21989. BMW wheels [Pennsylvania] {5/22/03}
21990. Aluminum stain or dye [Australia]
21991. Seeking chroming of hard bag lids [Georgia] {5/23/03}
21992. Need finisher for green/black variable color tinting of copper sheet [Missouri] {5/23/03}
21993. Brighteners for Ni and Cu plating solutions [Egypt] {5/23/03}
21994. Need Copper Brightener and Polish [Mexico] {5/23/03}
21995. Need rectifiers, polishing machines, anything for plating shop [Ohio] {5/23/03}
21996. Technical Information on Electroforming Plant set-up and Operations [India]
21997. High Zinc Levels [Virginia]
21998. Odor in plasma metallizing [India]
21999. Zinc nickel reel to reel plating [Ohio]

The finishing.com Hotline includes more than 50,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2009