The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


17000. Non-condensing humidity cabinet standards [Illinois]
17001. Stalagmometers: Aqueous cleaners [Oklahoma]
17002. Blisters on nickel plated zinc diecastings..copper undercoat missing [India]
17003. Cost hard chrome vs. zinc [Mexico]
17004. Nylon materials suitable to run through e-coat process [Michigan]
17005. Ti interference in Nitric/HF bath [Maine]
17006. Product to release a mineral core [Wisconsin]
17007. Pretreatment and plating Ti6AL4V [Sweden]
17008. Zinc whisker and failed power supplies [Pennsylvania]
17009. ZINC-IRON salt spray hours [Tennessee]
17010. Etching solutions [Mexico]
17011. Seeking nickel anode [Syria] {10/04/02}
17012. Cast iron block sealer [Minnesota]
17013. SEEKING CHROME FINISH FOR HUMMER BRUSH GUARD [Florida] {10/04/02}
17014. Seeking small qtys. of copper cyanide [Nevada] {10/04/02}
17015. Monobasic and dibasic acids [England]
17016. Plating rhodium method [Turkey]
17018. B4A2C, MATERIAL SPECS [New York]
17019. Galvanealed or galvanized doors and frames [New York]
17020. Tin/Zinc Plating with Black Chromate Treatment [Oklahoma]
17021. Special finish on aluminum heat sinks [New York]
17022. COATING OUT PARTS WITH EVERSLIK [Alabama] {10/07/02}
17023. Long term protection against storage corrosion? [Pennsylvania]
17025. Plating of G2 cast iron [Connecticut]
17026. 380 Anodize "Smutty" Finish [Florida]
17027. Pewter Blackning and polishing [So. Africa]
17028. Stop rust on delicate owl bookends, cast iron w/bronze finish [Maryland]
17030. Wanted a rim dipper for my factory alloy rims [Maryland] {10/07/02}
17031. Looking for pewter rechroming companies [So. Dakota] {10/07/02}
17032. WAX STOP OFF FOR ALUMINIUM [India]
17033. Copper Plating for nitride stopoff [India]
17034. Seeking Titanium Foil [China]{10/07/02}
17035. Calcium deposits in tub? [Florida]
17036. Stainless steel 316 corrosion [India]
17037. Seeking nickel-rhodium coating for reflectors [Turkey] {10/07/02}
17038. Need a Brass Plating Refinishing Product [Illinois]
17039. Need info on chrome dipping [New York] {10/07/02}
17040. Need protective coating for hammered copper sheeting [Colorado]
17041. Cryogenic recycling system for chrome plated /pc scrap [Korea]{10/07/02}
17042. The Problems Of Rust [U.K.]
17043. How To Change The Color Of Aluminium [Pakistan]
17044. ROAD MARKING EQUIPMENT [India] {10/07/02}
17045. Yellow chromate treatment [India]
17046. Rechrome fighting chair [Florida] {10/07/02}
17047. Rust repairs [New York]
17048. 440A vs 440C and other choices [Idaho]
17049. HOLOGRAM EQUIPMENT [India] {10/07/02}
17050. Need BLACK CHROME on Plastic and Polyester [California] {10/07/02}
17051. Need lacquer supplier [So. Carolina] {10/07/02}
17052. Coating high density polyethylene with a light weight metal? [N. Ireland]
17053. Electroplating metals questions [Guyana]
17054. Barrel burnishing for paint removal? [Arizona]
17055. Using gold as mirror reflective backing rather than silver [Australia]
17056. Electro-polishing Process [Texas]
17057. Piston & Cylinder Coatings to Eliminate Oil and Increase Life [Hawaii]
17058. Rainbow shade in anodised section [India]
17059. Protection against sulphuric acid attacks on steel structures [India]
17060. Micro-burr in slots 0,5mm width [Italy]
17061. Hardcoat Anodize [Malaysia] {10/08/02}
17062. Hard Chrome OD plated steel tubing [Colorado] {10/08/02}
17063. Chrome Plating Plastic [New Jersey] {10/08/02}
17064. Seeking chiller [Iran] {10/08/02}
17067. Scientific reaction of hydrochloric acid and copper [Washington]
17068. Nickel Stripping [Saudi Arabia]
17070. Help for the aluminum etcher [Florida]
17071. Anodized surgical steel knives [No. Carolina]
17072. Cyanide Antidote Kit [Nevada]
17073. Environment & worker health safety, nickel-chrome plated steel bumper [Canada]
17074. ASTM B-117 Test Interruption [Connecticut]
17075. Testing of Crazing (macro cracks) in Hard Chrome Plating [England]
17076. Finishing of stamped hex nut [Illinois]
17077. Blackening [Thailand]
17078. Sputtering vs. Vapor coating [Florida]
17079. PVD finishing problems [Portugal]
17080. How to eliminate the saccharin to the nickel sulfamate baths [Spain]
17081. Plating vs. anodizing [Hong Kong]
17082. ELECTROPOLISHING CAST CF8M (316 ss) [Pennsylvania]
17083. Galvanic corrosion of aluminum by stainless steel [Ontario]
17084. Need Continuous nitric acid concentration determination equipment [Australia] {10/08/02}
17085. What should I do if it gets on my skin? [Indiana]
17086. Galvanized sheet metal counter tops stained by vinegar [California]
17087. Suitability of poly for tank fab [Rammalah]
17089. Ross Miles Foam Height [Italy]
17090. Hydrogen Embrittlement determination [Malaysia]
17091. Yellow chromating of GS-anodized aluminium [Finland]
17092. WELD FUME TESTING [New York] {10/08/02}
17093. How to Silver/Nickle Plate Stained Glass Angels [Florida] {10/08/02}
17094. Enamel Coating Project [Oman] {10/08/02}
17095. Will solvent-based rust preventive agent dissolve Chromate Sealer? [Singapore]
17096. Nickel plating that could pass one cycle CASS Test? [Singapore]
17097. Ni brightener with fair internal/residue stress? [Singapore]
17098. What is the zinc plating process [Georgia]
17099. I Need a Coating in a Precision Bolted Joint [Connecticut]
17100. Seeking chrome plating of our line of ABS bezels [Michigan] {10/09/02}
17101. FeCl3 from FeCl2 [Italy]
17102. Rx needed for dishwasher sick stainless steel [New Jersey]
17103. Chip-resistant finish [Idaho]
17104. Solution to remove heat discoloration from steel [Ohio]
17105. REMOVING POWDERCOAT PAINT [England]
17106. Laser Edge Quality on Painted Parts [Minnesota]
17107. Plating Spark - How to prove it's a real issue [Ireland]
17108. White run down stain from the decorative chrome tank [Michigan]
17109. Type III anodize/silver plating combination finishing [Vermont]
17110. Anodizing consulting [Mexico]
17111. Electrolysis between aluminum and galvanized [California]
17112. Is chrome plated abs feasible for this application? [Florida]
17113. SEEKING VACUUM METALLIZING EQUIPMENT FOR CHINA PLANT [China] {10/10/02}
17114. Seeking aluminum polishing products, and publications [Washington] {10/10/02}
17115. Electropolishing [Australia]
17117. Separating gold from other metals [Canada]
17118. Food safe techniques for cold bonding aluminum for structural support [California]
17119. Seeking Chrome / Re-chrome [Texas] {10/10/02}
17120. Seeking Wrinkle Paint / Crackle Finish (Black) [UK] {10/10/02}
17121. Planning a hot dip galvanizing installation [Spain] {10/10/02}
17122. Seeking information on trivalent chromate conversion coating [New York] {10/10/02}
17124. What coating material is this? [India]
17125. Clear coat for vintage office furniture [New York]
17126. Chrome dipping wheels [Florida]
17127. GR-63 contamination (corrosive) analysis [New Jersey]
17128. HALAR DE-LAMINATION FROM SST PLATING CLIP [Florida]
17129. Electroless nickel plating 1018 CRS and 304 SST at the same time [California]
17131. Effects of Electropolishing on 410 Stainless Steel [India]
17132. Seeking Porcelain Enamel Supplier [Arizona] {10/10/02}
17133. Help in electroplating project [Canada]
17134. Hazardous Waste Management in electroplating industries [India]
17135. Surface fatigue wear [India]
17136. Aging hardware/hinges [Nebraska]
17137. Methods to remove gypsum scale [Mexico]
17138. HYDROGEN DE-EMBRITTLEMENT OF ZINC PLATED SPOKES [India]
17139. Chrome-plating plastic components [Hungary]
17140. High temperature aluminium blackening process [Australia]
17141. Passivation test, Rust removing [Pakistan]
17142. Seeking 17-7 ph round bar [Argentina] {10/11/02}
17143. Seeking 1000 completed 63" Ductile Iron Cast Stiffener Rings [Canada] {10/11/02}
17144. Determination the concentration of gold solution [The Netherlands]
17145. Adhesion on Polycarbonate /ABS parts [Michigan]
17146. Spec for Titanium Carbide CVD [Tennessee]
17147. A good process sequence for Nickel Plate on Zinc Die Cast [Mexico]
17148. Welded Stainless Steel Finishing [Portugal]
17149. High working temp., wear resistant, dark colored plating [New York]
17151. Seeking powder coating UV for mdf [Austria] {10/11/02}
17152. Seeking process of hard anodizing [Canada] {10/11/02}
17153. Aspencade gas tank rust [New York]
17154. Antique Radio Chassis Rust Inhibitor [California]
17155. Gold repair [Qatar]
17156. Nickel sulphamate questions for wiping contact surface [Australia]
17157. Etching Naval Alloys [England]
17158. Degreaser required [India]
17159. Looks like anodized yet felt rubbery [California]
17160. Chemical Additives Improving Finishing [Italy]
17161. Seeking UV resistant copper lacquer [Montana] {10/11/02}
17162. Safety Inquiry [Alabama]
17163. Corrosion resistance of zinc-dichromate in marine environment [Illinois]
17164. Seeking hot dipping galvanization line manufacturer [Ukraine] {10/11/02}
17165. Seeking anti tarnish lacquer sealant for silver [South Africa] {10/11/02}
17166. SEEKING TIN MILL PRODUCTS [India] {10/11/02}
17167. Blackened copper with hydrochloric acid [Washington]
17168. Stainless Steel Rusting [England]
17169. Tests on Galfan Wire [Russia]
17170. Alumilite 204 [New York]
17171. Coating of optical instruments and black anodization [Turkey]
17172. Paint Adhesion [Northern Ireland]
17173. Chemical burr cleaning [India]
17174. RMS Units [Italy]
17175. Uniformly anodizing titanium [Connecticut]
17176. Seeking to rechrome all chrome on 79 cutlass [Ohio] {10/14/02}
17177. NEED HELP TO CHECKER PLATE MY DASH! [Kentucky]
17178. HELP! Pink ceramic tile invasion [Illinois]
17179. Useful "life" of copper stripping bath [Canada]
17180. Oxidation on Electric Cars [Texas]
17181. Chrome dipping [New York] {10/14/02}
17182. Wanted Dow #7 Dichromate Treatment on magnesium [Wisconsin] {10/14/02}
17183. TiN/TiAlN motorcycle components for race team [Ohio] {10/14/02}
17184. Plating and galvanizing equipment required [Saudi Arabia] {10/14/02}
17185. Phosphate, Granular machine [Georgia] {10/14/02}
17186. Need ion exchange resin [Egypt] {10/14/02}
17187. Need a lab table to measure emissivity [Portugal] {10/14/02}
17189. Source of Galvanized Steel Guy Wire [Saudi Arabia] {10/14/02}
17190. Reduction of Cr(VI) to Cr(III) using FeSO4 or Na-bisulphite [Indonesia]
17191. Hot corrosion of superalloys [Iran]
17192. Aluminum cleaning and brightner [No. Carolina]
17193. Need book, Electrolytic and Chemical Conversion Coatings by Biestek [California]
17194. Corrosion of 304 stainless burner in phosphoric acid tank [Oregon]
17197. IMMERSION SILVER [India]
17198. Photo images on aluminum [Ontario, Canada]
17199. Electropolishing VS. Nitric/Citric Passivation [Pennsylvania]
17200. Stainless Steel Corrosion & Discoloration [Georgia]
17201. Stainless steel in sea water [Iran]
17202. Finding a quality company to powder coat my wrought iron chairs [Delaware] {10/14/02}
17203. What Acids are in fruit juice? [Maryland]
17205. A.S.A.P. [California]
17206. Counterfeiting [Pennsylvania]
17207. Aluminum plating solution [Pennsylvania]
17208. Copper finishing [Michigan]
17209. Stripping Paint & Rust from Antique Auto Rims [Pennsylvania]
17210. Can Black Chrome be used for jewelry decoration? [Thailand]
17211. CORROSION OF E-NI IN LITHIUM BRINE [Argentina]
17212. Flash Copper Plating Failures in Switch Conductors [Florida]
17213. Teflon coating stainless steel vessel [Pennsylvania] {10/15/02}
17214. Need to find ceramic coatings co. [Kentucky] {10/15/02}
17215. Seeking software for corrosion predictions [Iran] {10/15/02}
17216. Enquiry for Powder Coating Machine [India] {10/15/02}
17217. Rubber/Steel Bonding Substitutes [Illinois] {10/15/02}
17218. Ceramic coating material for surgical scissors [Pakistan] {10/15/02}
17219. Seeking Hexavalent Free Chromate Conversion Coating [Virginia] {10/15/02}
17220. Need hard chrome processes for shock absorbors [California] {10/15/02}
17221. Architect seeking decorative stainless samples [Saudi Arabia] {10/15/02}
17222. Alloy 2021 anodizable or not [California]
17223. Need Microscope Photo of Anodized Surface [Washington]
17224. How to paint an antique brass chandelier black? [California]
17225. Flame coloring cast iron [Indiana]
17226. Patinas on zinc [New York]
17227. Stainless steel leaching [Georgia]
17228. VDI30 micron [Florida]
17229. Chromating safety [Michigan]
17230. About CO2 in demin water [Peru]
17231. Soldering Electroless Nickel? [Mexico]
17232. Will epoxy paint support fungus growth? [Georgia]
17233. Delayed Blistering [Indiana]
17234. Zinc-Nickle Plating [Israel]
17235. Testing passivation with meter [Colorado]
17236. Stainless steel finish, high vacuums [Ireland]
17237. 24K gold plate cast aluminum [Iowa] {10/16/02}
17238. Seek chroming of my wheels [Virginia] {10/16/02}
17239. Dealer Needs Sources for Chroming & Clearcoating Aluminum Wheels [New Jersey] {10/16/02}
17240. Potassium cyanide samples required [England] {10/16/02}
17241. URGENT!! Copper coating supplier needed [Hong Kong] {10/16/02}
17242. Coating for Inc718 stem threads [Alberta, Canada] {10/16/02}
17243. Pvc Resin manufacturer and exporter [Bangladesh] {10/16/02}
17244. Hardness of Colbalt [Virginia]
17245. Corrosion of fishing lures [Florida]
17246. Nb electroplating onto carbon [Israel]
17247. Nickel cathode splitting problem [Zimbabwe]
17248. What is the best etchant for brass [Ohio]
17249. Metal radiator problems [Massachusetts]
17251. Hard core -coefficient of friction? [South Africa]
17252. Rectifier Selection [India]
17254. Sudden Salt Spray Failures [Pennsylvania]
17255. Soldering AuSn alloy [Switzerland]
17256. Large scale painting of anodized aluminum [New York]
17257. Chrome etch analysis [England]
17258. Coumarin odor [Ontario, Canada]
17259. GOLD PLATING A KALASH [India]
17260. Clear anodizing large 5052 parts [California]
17261. USP class 6 standards [Israel]
17262. Electropolishing engravings [New York]
17263. Procedure for die polishing [No. Carolina]
17264. Laser Cutting Dross - Magnetic Properties [Ontario]
17265. Cleaning stainless rope [India]
17266. Stainless Steel Finishes [Illinois] {10/17/02}
17267. Plant for Chrome plating on stainless steel [India] {10/17/02}
17268. Decorative treatment imitating wood [Spain]
17269. CHROMIUM DEPOSIT [Tanzania]
17270. Alodine compositional changes in service [California]
17271. Brass ring health risks [Pennsylvania]
17272. Painting a Black Iron Bed [Alabama]
17273. How to remove rust but not paint? [India]
17275. Leaching of lead from brass faucets [Turkey]
17276. Rubber bonding over plating [Illinois]
17277. Coloring aluminium [Pakistan]
17278. The properties of Zinc Phosphate [Louisiana]
17279. Pickling of carbon steel pipe [Brazil]
17280. Infrared enhancing coatings [Newfoundland]
17281. Effects of hydrochloric acid on Galvanized cable? [British Columbia]
17282. ANODIZED ALUMINIUM [Florida] {10/18/02}
17283. Chelators [Illinois]
17284. How to plate the bright nickel over the brass parts [Michigan]
17285. Clear Anodizing [New Hampshire]
17286. Mild steel electrically conductive plating [Illinois]
17287. Flouropolymer etching [Pennsylvania]
17288. Heat Treatment of 440 Stainless Steel [California]
17289. Re-chrome table and chair legs [Connecticut] {10/18/02}
17290. Seeking copper plating of clock parts [Colorado] {10/18/02}
17291. Solder wire making machine [India] {10/18/02}
17292. DIP RIMS [Louisiana] {10/18/02}
17293. Coloring copper and lead greenish [UK]
17294. Brightening kitchen cabinets [New Jersey]
17295. Mu metal tube shield [Massachusetts]
17296. Need supplier of Paramount Brass Lacquer [Florida] {10/18/02}
17297. Zamak, finishing collinox 1010 [Brazil]
17298. White rust and black marks on hot dipped galvanized [Malaysia]
17299. Chrome and Gold Dipping as Business [Pennsylvania]
17300. Different thickness area on plated rhodium ring [Turkey]
17301. TILES WITH A DEFECT [Malta]
17302. Titanium Anodizing Results [Thailand]
17303. How to turn copper patina color [Pennsylvania]
17304. Aluminum screw supplier [Canada] {10/18/02}
17305. Standards on net [India]
17306. Painting Brass Bed [New Jersey]
17307. Corrosion-resistant plating with small through holes [California]
17308. Equipment eet for electrogravimetric to analyze gold [Malaysia] {10/18/02}
17309. Powder coating over e-coated surfaces [Iowa]
17310. Chrome Platting Bumpers [California]
17311. Technological Development on Rotogravure Cylinder Making [India]
17312. Powdercoat Powder color match for Automotive OEM [Colorado] {10/18/02}
17313. Seeking to buy gold electro forming equipment for jewelry [Romania] {10/18/02}
17314. LOOKING FOR PARILENO COATING [Spain] {10/18/02}
17315. Fluoride Concentrations in Zinc Phosphate on steel solutions [Michigan]
17316. How to etch Evanohm? ( High Chromium Alloy ) [UK]
17317. Pulse rectifier technology [India]
17318. Plating of copper on aluminium balls w/o dilution of electrolyte [India]
17319. Spray Pyrolisis Nozzles [California]
17320. Cost to refinish a silver horn [Alabama]
17321. Outgassing during electroless nickel plating process [California]
17322. Conversion of surface finish [Texas]
17323. Need Iron Phosphate [Hawaii] {10/18/02}
17324. Immersion copper plating [Florida]
17325. Shots mass flow [South Africa]
17326. 24 hr. 7 day work shifts [Canada]
17327. Aging Aluminum [Canada]
17328. Titanium Color Standard [China]
17330. Nickel Sulfate Crystals Disposal [California]
17331. DM plant start-up [India]
17333. PTFE impregnation [Singpaore]
17334. Practical Technical Problem [India]
17335. Specification for running Bright Dip at High Al content [Australia]
17336. Need someone to nickel strike, copper plate, black oxide -TITANIUM [Florida] {10/21/02}
17337. Need supplier of electroconducting modeling wax and paint for electroforming/plating of nonmetallic objects [California] {10/21/02}
17338. Need direct fired absorption chiller [Iran] {10/21/02}
17339. Copper backsplash [California] {10/21/02}
17340. Iron Powder [India] {10/21/02}
17341. Different colors of CuSO4 [Kuwait]
17342. Wear-testing electroless diamond coating [India]
17343. Teflon coat for Two Wheeler [India]
17344. Electroplating in stain glass/ tiffany [India]
17345. Rhodium [Illinois]
17347. Antique patina for copper [Washington]
17348. Stripping the original finish off [Michigan]
17350. Humidity failures [Canada]
17351. Phosphating comparison info [Michigan]
17352. Using SNAP AM -Macdermid- as wetting agent for nickel sulfamate [Algeria]
17353. Change aluminum surface look [Texas]
17354. Aluminium coil coating plant [India] {10/21/02}
17355. TECHNICAL DETAILS OF ZINC COBALT PLATING, WITH BLACK PASSIVATION [India]
17356. Effect of Anodising on Teflon Coating of aluminium Pan [India]
17357. Seeking Brush Plating Source [Maryland] {10/21/02}
17358. Toning down the gold on an oxidized aluminum door [Michigan]
17359. Electrostatic spraying with water borne paint [Malaysia]
17360. Adhesion failures [California]
17361. 15-5PH Heat Treated to H-1075 Rusting Hex Flats after Passivation [California]
17362. Acid dipping for auto [Massachusetts] {10/22/02}
17363. Looking for someone who strips chrome [New York] {10/22/02}
17364. Silvering Baby's First Shoe [U.K.] {10/22/02}
17366. Silicon Release Paper [India] {10/22/02}
17367. Seeking water deburring machine for plastic parts [Belgium] {10/22/02}
17368. Seeking permanent color staining for stainless steel chainmail [Massachusetts] {10/22/02}
17369. Need chemicals for hot dip galvanizing [China] {10/22/02}
17370. SEEKING PVC COATING MACHINE [Russia] {10/22/02}
17371. Starch xanthates [Spain]
17372. Black absorber coating or paint to absorb heat [Utah]
17373. Preparing stainless for painting [California]
17374. Surface treatment [Canada]
17375. Heat resistant clear coat paint [Canada]
17376. Maintaining brass cutlery in constant use [Australia]
17377. Best way to clean metal antiques [Michigan]
17378. Painting Polished Brass [North Carolina]
17379. What would cause sparks [Missouri]
17380. Electroless nickel plating on a yellow chromated detail [Sweden]
17381. Non-cyanide alkaline zinc plating [India]
17382. Activation of Nickel prior to Electrolytic Nickel [Singapore]
17383. Corrosion Prevention [India]
17384. Hard anodize thickness [Singapore]
17385. Marking light anodized aluminium [South Carolina]
17386. Removal of Scale / Stain from SS 302 L material [Singapore]
17387. Solution for burr removal and answer for eliminating powder coating [India]
17388. Chrome Removal [Missouri] {10/22/02}
17389. In search of someone to perform a small task with Platinum [Maryland] {10/22/02}
17390. Seek refinishing of wrought-iron furniture [New Jersey] {10/22/02}
17391. Propane flame treater [North Carolina] {10/22/02}
17392. Arthur Brace-Hardcoat Anodizing [Illinois]
17393. Coloring silver [India]
17394. Why Copper for Plating? [Massachusetts]
17395. Wire Basket for Dishwasher needs Recoating [Virginia]
17396. Accelerating copper corrosion [New Hampshire]
17397. Motorcycle polishing [Georgia]
17398. Translucent colored paint for acrylic [Arizona]
17399. Technical infromation [Colorado]
17400. SURSULF PROCESS [Taiwan]
17401. Polishing Hard Anodized Surface [Texas]
17402. 316L stainless is rusting (help) [Tennessee] {10/22/02}
17403. Aluminum Pipe Surfacing Machinery [Indiana] {10/22/02}
17404. Need supplier of Alcor 570 Seal [Massachusetts] {10/23/02}
17405. Silicon Carbide Slurries/Suspension Media [England]
17406. Frosted Finish [Colorado]
17407. Steel cabinets finish suggestions needed [California]
17408. Surface Roughness Question [New Jersey]
17409. Titanium coating [Malaysia]
17410. Silver Plating over Plastic [Canada] {10/23/02}
17411. Protective coating [India]
17412. Finish for an acrylic paint on top of metal [Mexico]
17414. ASTM D3359 [China]
17415. Alodine Processing [California]
17416. How to blue [Oklahoma]
17417. Chroming Caddy Rims [Florida] {10/23/02}
17418. Chrome my rollcage [New Jersey] {10/23/02}
17419. Seeking anodizing of aluminum wheels [California] {10/23/02}
17420. Nickel sulphamate suppliers [Indonesia] {10/23/02}
17421. Need 316L stainless steel plate [Canada] {10/23/02}
17423. Steam Hoist Restoration [Montana]
17424. How do you paint Nylon, 12 [California]
17425. Copper diffusion through Sn/Pb Solder [New York]
17426. ZINC PLATED BB'S! HELP! [Texas]
17427. Advice on steamed wood [Canada]
17428. Green Chrome [Oregon]
17429. Is galvanize poisoning possible? [South Carolina]
17430. Slake lime consumption calculation [Indonesia]
17431. References for black oxide finishing [Georgia]
17432. Effect of black oxide on tight tolerance parts [Missouri]
17433. Vac Cad plating problems and fatigue failures in H-11 tool steel [California]
17434. Scalloping In Heavy Electroless Nickel Deposits [Massachusetts]
17435. What is involved in white brass? [Ohio]
17436. Prevention of titanium galling in spine implant [Texas]
17437. Touching up Alodine1200 [Massachusetts]
17438. Iridite 15 Magnesium Treatment Question [Illinois]
17439. Palladium Cobalt [Arizona] {10/23/02}
17440. Solar reflective material [India] {10/23/02}
17441. Teflon Spray Coating [Florida]
17442. Demineralizer [Saudi Arabia]
17443. Low Zinc Coating on Steel [India]
17444. Improving current efficiency [India]
17445. Bumper rechroming [Illinois] {10/23/02}
17446. Gold anodize needed for large plates [Connecticut] {10/23/02}
17448. C55 sulfide finish [Maine]
17449. Hydrogen Embrittlement on 17-4 PH steel [Kentucky]
17450. Appearance of Chromate Finishes [Pennsylvania]
17451. Standards for iron phosphatizing [Iran]
17452. Optically absorptive coatings for steel or aluminum [Massachusetts]
17454. Stormwater pollution prevention plan [Connecticut]
17455. Tin whiskers on lead [Philippines]
17456. Laminate Cracks Problem [Pakistan]
17457. PET to PET [Canada]
17458. Fasteners training [California]
17459. White coating for stainless steel [UK]
17460. Stainless steel discoloration during heat treating [New Jersey]
17461. Chrome plastic auto grill [Puerto Rico] {10/24/02}
17462. Replate small motorcycle parts [Virginia] {10/24/02}
17463. Need aluminium backsplash [Colorado] {10/24/02}
17464. Quick Cd plating method wanted [Massachusetts]
17465. 5S and Kaizen [Tennessee]
17466. Copper Oxidation [Utah]
17467. Re-use of DI water from solder plating process to electrolytic deflashing process [Philippines]
17468. Testing for free iron content in acidic solutions [Utah]
17469. Anodize test [California]
17470. Bright Dip Pitting [Texas]
17471. Phosphate coating surface affect on seal life [Wisconsin]
17472. Electropolishing for stainless steel vessels [Michigan] {10/24/02}
17473. Carbonia Bluing Processor [Connecticut] {10/24/02}
17474. Searching for supplier of RUST PEL 51 [China] {10/24/02}
17475. Coin plating for commercial use [California]
17476. Can I make a copper countertop? [Ohio]
17477. Coatings that are non-permeable to hydrogen [The Netherlands]
17478. How to rust steel on purpose [Colorado]
17479. Muriatic acid to turn copper green [South Carolina]
17480. In chamber top coat [Australia]
17481. Surface conductivity of water [New York]
17482. Corrosion [Missouri]
17483. Endurance [Connecticut]
17484. SETTING UP NICKEL PLATE LINE FOR ALTERNATORS [Mississippi]
17485. Tank Water Evaporation Estimates [Canada]
17486. Who is the clearest of them all? [Colorado]
17487. Plating peeling off [Taiwan]
17488. Flexi circuit gold edge connector oxidation [Texas]
17489. Separating electroformed Ni replica from mandrel [Massachusetts]
17490. Self tapping screws through hard anodize [Oregon]
17491. Nonconductive plating on Be-Cu [California]
17492. Patchy Coverage, Apparently Random Anodize [California]
17493. Sputter Coater Wanted [California] {10/25/02}
17494. Seeking molybdenum coating [India] {10/25/02}
17495. DIRHODIUM TRISULFATE [Korea] {10/25/02}
17496. Want to rubber coat my rear spoiler (polyester) [California] {10/25/02}
17497. Need Vendor for Coating Plastic w/ Metal [Massachusetts] {10/25/02}
17498. What dissolves Pennies? [Florida]
17499. Internal coating for tubes to hot water [Israel]
17500. Painting Brass Bed [California]
17502. Aluminium etching formulas for sculptors [California]
17503. Detail of BS1615 [China]
17504. Chemical solution for locating welds [Ireland]
17505. Electroless nickel problems in plating [India]
17506. Copper Electroforming on silver mandrels [India]
17507. Corrosion of chrome plated parts [India]
17508. Chloride Induced Corrosion of CS Tank [India]
17509. Need Mustang side scoops chromed [Kansas]{10/28/02}
17510. Seeking baked enamel finish [Massachusetts]{10/28/02}
17511. Remanufacturer Seeking Cadmium Plating services {10/28/02} [Louisiana]
17512. Requirement of Ceramic tube and cold weld material [India] {10/28/02}
17513. Where to locate a flex mask known as "cheese"[Illinois] {10/28/02}
17514. Seeking Nitric Test Equipment for acid bright dip [Australia] {10/28/02}
17515. Seeking consumer plating supplies [UK] {10/28/02}
17516. Finishing of Tweezers [India] {10/28/02}
17517. High impact resistance coatings [Singapore] {10/28/02}
17518. What type of vinegar cleans a penny better? [Guam]
17519. Aluminum Pot Dangers [Australia]
17520. Patinas on Naval brass [New York]
17521. Pure gold by electrochemical means [Ghana]
17522. Strong material [Holland]
17524. Dyeing aluminum computer case [New York]
17525. Painted Aluminum Oxidation [Florida]
17526. Can Chrome be Plated on aluminum wheels? [California]
17527. The Zinc-Coated Penny Dilemma [Illinois]
17528. Brass lamp cleaner [Colorado]
17529. Motorcycle frame polishing help [Illinois]
17530. Removing old paint from aluminum boat [Virginia]
17531. Silver Antiquing [Washington]
17532. Oil Can Finish [Indiana]
17533. How to restore the appearance of an old mirror [New Jersey]
17534. Galvanizing Thickness Standards [India]
17535. Layout of e-polish line [Virginia]
17536. Testing for embrittlement with a microscope [Massachusetts]
17537. Interchanging anhydrous and hydrated products [New York]
17539. Lubricant specifications Question [Virginia]
17540. Want to do Ceramic Coating & Cryogenic Metal Treatment [Georgia]
17541. Bluing as in Blue instead of black [Arizona]
17542. Alloy selection for patina brass parts [Florida]
17543. Avoiding Hydrogen Embrittlement in Galvanizing - how? [England]
17544. Matt-Less Spots defects in Skin Passing [India]
17545. PLATING COPPER ON ALUMINUM [Massachusetts]
17546. Alternative passivation for electroless nickel electroforming [Minnesota]
17547. Electrogalvinizing of welded joints [Israel]
17548. Dull spots on bright tin plated copper [Egypt]
17549. Procedure for plating [Philippines]
17550. Pitting Problem [Texas]
17551. FPL ETCH RATE [Connecticut]
17552. Indelible titanium tube marking [Spain]
17553. Ammonium Biflouride vs. HCl or HF [New Jersey]
17554. Specs for "Pickled and Oiled"? [So. Carolina]
17555. Polishing of stainless steel [California]
17556. 17-7 PH Stainless Steel with Deionized Water [California]
17557. Electro-Galvanized Staples with Western Red Cedar Shingles [Wisconsin]
17558. Sacrificial anodes and tomatoes [Florida]
17559. Recycled content in stainless steel [California]
17560. Best clear lacquer for unusual bottlecap tabletop [Pennsylvania]
17561. Nickel with stray currents [South Africa]
17562. SILVER CARBONATE FOR HEEF-25 [Illinois]
17563. Preventing tarnish of jewelry by sulfur [Kentucky]
17564. Teflon spray to resurface pots and pans [United Kingdom]
17565. Defects in silver casting/polishing [India]
17566. Rust Formation Post Phosphate Pressure Wash [California]
17567. Seeking adhesive tape coating line [Yugoslavia] {10/29/02}
17568. Citric Acid [Illinois]
17569. Electroplated Pd, etchants, grain structure [Idaho]
17570. Re-plating copper bus bars [Canada] {10/29/02}
17571. Refinishing Bathroom Faucets [Louisiana]
17572. Need finisher for Phos/Oil, GM4435W, for springs [Michigan] {10/29/02}
17573. Can 6061-T6 be anodized to natural color? [India]
17574. How to begin in bronzing baby shoes [Singapore]
17575. Seeking Anodizing of Various Auto Engine Accessories For Show-Car [Wisconsin] {10/29/02}
17576. NEED a Copper/Bronze Color Restorer and Bright Shiny Finish [Michigan]
17577. Rusting prevention [England]
17578. Refinishing dirt bike gas tank [Canada]
17579. Boric acid analysis method [Guatemala]
17580. Brush Conversion Coatings [England]
17581. Seeking Fiat Spider bumper repair/replate [Maryland] {10/29/02}
17582. Electroless nickel on aluminum bodies [Massachusetts]
17583. Corrosion control in aluminium window frames [Australia]
17584. Tank stripping of kitchen cabinets [New Jersey] {10/30/02}
17585. Wheel dipping [Virginia] {10/30/02}
17586. Alloy wheels dipped in chrome [Minnesota] {10/30/02}
17587. Powder coating glass bottles [New Hampshire] {10/30/02}
17588. Seeking tin immersion coating of Al Alloy 850 [Texas] {10/30/02}
17589. Seeking alochrome pen [UK] {10/30/02}
17590. Looking for Plastisol [Venezuela] {10/30/02}
17592. Pennies [Arizona]
17593. Project on cleaning pennies [Texas]
17594. I need silver recovery method [Michigan]
17595. Experiments with titanium coatings [Michigan]
17596. Technical info on silver stain reacting to the tin side of float glass [North Wales]
17598. How to obtain the grain structure of Al6061-T651? [Kentucky]
17599. Solubility of Zn(HPO4)2 [California]
17600. Aluminum Oxidized Trim [California]
17601. What substrate and coating should I use for an outside plinth [China]
17602. POLISHING WHEEL RIMS [Louisiana]
17603. CLEAN PAINT OFF ALUMINUM WHEELS [South Carolina]
17604. Stain removal from doorknobs [Louisiana]
17605. How do I tumble a copper coin [Georgia]
17606. How do we go from Yellow to White Gold [Connecticut]
17607. Electroless Nickel Mil Spec Needed [Washington]
17608. Validity of ASTM B117 requirement [Arizona]
17609. Painting of channel structures [India]
17610. PVD [India]
17611. Zinc Plating Deposition in Holes [Michigan]
17612. White Spots on Cadmium Plating? [England]
17613. Chrome plating on diecast aluminum [New York]
17614. Alodining to MIL-C-5541E [Canada]
17615. Passivation of SAE 420 steel balls [India]
17616. Citric passivating [Illinois]
17617. Deburr - Drilled holes in round stock [Wisconsin]
17618. SALT-SPRAY TEST ON PRE-PLATED ZINC ON STEEL [California]
17619. NSF61.9 certified coating for brass tube and EPDM Hoses [Canada]
17620. Range Rover brush guard coating [Oklahoma]
17621. Mechanical means of SS Decorroding [Washington]
17622. Gold plating [Australia] {10/31/02}
17623. Zinc Stannate Process [Canada]
17624. Purchasing a powder coating business [Australia]
17625. Want to do powder coating on wood furniture [India]
17626. Impregnation of zinc parts [Canada]
17627. Maximum Thickness of Hard Anodizing [Turkey]
17628. Passivation testing [Pakistan]
17629. 316L is rusting [Tennessee]
17630. Satellite Centrifuge [Italy]
17631. Contaminating stainless with countersink [Michigan]
17632. Seeking rechroming shops [Louisiana] {10/31/02}
17633. Oil Rubbed Bronze [Michigan] {10/31/02}
17634. Seeking Anodizers [North Carolina] {10/31/02}
17635. IRIDIZE [Belgium] {10/31/02}
17636. Deburring of hydraulic valves [Belgium] {10/31/02}
17637. Electrostatic Painting Primer [Pennsylvania] {10/31/02}
17638. Need a chemical to re-wash galvanneal [Indiana] {10/31/02}
17639. Antique Refinishing [Texas]
17640. Caustic Recovery [South Africa]
17641. Chromate rinse filtration [New Jersey]
17642. Statistic (6Sigma, SPC etc) in Corrosion test/appearance evaluation [Singapore]
17643. Porcelain enamel on 6063 aluminum alloy [Canada]
17644. Water absorption [Indonesia]
17645. Cathodic electrodeposition film [California]
17646. Plating Copper on Tantalum Sheet [Georgia]
17647. Magnetic property of stainless steel affected by plating [New York]
17648. MICROCRACKS PER INCH [India]
17649. Food Grade Anodized Aluminum [Minnesota]
17650. Hardcoat problem on 6061-T6 tubing [New York]
17651. Reaction of aluminium with nitric and sulphuric acids and water [India]
17652. Staining and Pitting of 304/304L Stainless Steel after clean [Arizona]
17653. Fine resolution etching of stainless steel [Georgia]
17654. Chemical Etching of Tantalum Sheet [Georgia]
17655. Sulfate attack on stainless steel pipe [Malaysia]
17656. Can patina affect chromed plated stainless steel? [U.A.E.]
17657. Powder coating adhesiveness and thickness checking [India]
17658. Photo-etching [Hawaii] {11/01/02}
17659. Supplier of raised lettering in metal or plastic [Minnesota] {11/01/02}
17661. Seeking kynar paint applicator [California] {11/01/02}
17662. Electrostatic paint [Canada] {11/01/02}
17663. Need a used anodizing line [Canada] {11/01/02}
17664. Surface treatments for electroplating over Molybdenum [California]
17665. Filling and powdercoating pot metal (automotive) [California]
17667. Remove Cr/Au from stainless steel [Washington]
17668. Protecting copper from sunlight [Alabama]
17669. Plating on A356 aluminum [Massachusetts]
17670. Tolerance change due to anodizing [Singapore]
17671. Problems of staining with iron phosphate [Mexico]
17672. Ral70004 brush aluminum [Rhode Island]
17673. Sandblasting tortilla machine rolls [Texas]
17674. Seeking Proposals to Apply Metal to Liquid Crystal Polymers [Ohio] {11/04/02}
17675. Seeking a ceramic coating service [Taiwan] {11/04/02}
17676. PVC Dipping to form thin transparent product [UK]
17677. Anodize increasing adhesive [Taiwan]
17678. Bath Life and Control of Alkaline Permanganate Solution [Connecticut]
17680. Platinum plating [Taiwan] {11/04/02}
17681. Refinishing Metal Golf Clubs [Texas] {11/04/02}
17683. GOLD PLATING [Massachusetts] {11/04/02}
17684. Seeking conductive paints [Saudi Arabia] {11/04/02}
17685. High Security Registration Plate Technology Requirement [India] {11/04/02}
17686. Seeking powder coating equipment [India] {11/04/02}
17687. Seeking Titanium Anode Mesh [India] {11/04/02}
17688. Need a manual installation for zinc metallizing [Romania] {11/04/02}
17689. Want porcelain enamel manufacturer [Egypt] {11/04/02}
17690. COPPER WASTE [Pennsylvania]
17691. Acid vs. Alkaline Copper Plating [Australia]
17692. Deoxidation [India]
17693. H type crimp clamps [Sri Lanka]
17694. How Do I Repaint the Background of Brass Plaque [Connecticut]
17695. Stainless Steel Polishing [Australia]
17696. Brass pulls [Maryland]
17697. Is Blue Alodine Bad? [Florida]
17698. Welding on aluminum wheels [Alabama]
17699. Failure concern related to ASTM D 3359 [Kentucky]
17700. How and what to do for copper patina (dark brown) [North Carolina]
17701. N3 finish [California]
17702. AFP [Taiwan]
17703. Seeking Plating [California] {11/05/02}
17704. Re Chrome Bumpers - Show Quality [Ohio] {11/05/02}
17705. Restoring Oldsmobile [Michigan] {11/05/02}
17706. Estimate for rechroming my rims [Maryland] {11/05/02}
17707. Chromate coating needed (28' extrusions, 100,000#) [Maryland] {11/05/02}
17708. Stainless steel powder [Ohio] {11/05/02}
17709. Polishing heads [Canada] {11/05/02}
17710. Science project how does voltage travel [Illinois]
17711. PENNY RESEACH [Ohio]
17712. Control Valve Stem with PTFE Coating [England]
17713. Coil coating report [Germany]
17714. Adhesion of chromium with gold in metallization [Texas]
17715. Stove enamel resurfacing [New York]
17716. Anodizing dyes [Algeria]
17717. Help with hammered copper texture [Utah]
17718. Silver refinishing [Texas]
17719. Polishing Steel - Buffs and Compounds [Australia]
17720. Tin Drag-Out Recovery [New York]
17721. Adhesion test for painted plastics [Michigan]
17722. Simple test for presence of clear chromate [Massachusetts]
17723. Testing for Residual Aluminum After Etching [Florida]
17724. EN activation [New York]
17725. Resin/metal bonds grinding wheels, diamond tools [India]
17726. How hard is hard? [UK]
17727. Clean Au/Sn deposits from Al substrate [California]
17728. Finishing for Polymers and Ceramics [China]
17729. Electroplated tin-zinc alloy coatings [California] {11/06/02}
17730. Need my rims re-chromed [New York] {11/06/02}
17731. Replating fasteners for automobiles [Ohio] {11/06/02}
17732. Electropolishing of Chamber [New York] {11/06/02}
17733. Plating a very large part [Florida] {11/06/02}
17734. How to hardcoat with Teflon anodize for food grade service [Tennessee] {11/06/02}
17735. Rust Remover and Rust Preventer [India] {11/06/02}
17736. Chemicals for etching [India] {11/06/02}
17737. Caustic Etch Recovery [England]
17738. Pennies and the Economy [Canada]
17739. Analysis of a precipitated containing NaHCO3 and (NH4)2CO3 [Guatemala]
17740. Steel Pickling Information [Kentucky]
17741. BRASS WASH FINISH [Nebraska]
17742. Powder Coating [Canada]
17743. Field service of anodized surfaces [California]
17744. Restoration [Australia]
17745. Water electrolysis project [Canada]
17746. High-temp copper coating/plating [New York]
17747. Candle wax stains on brass [North Carolina]
17748. Trivalent Chromate Conversion for EMC properties [New York]
17749. Need a method for determination of chloride in nitric acid [Iran]
17750. Plating rack stripper [Massachsusetts]
17751. Catalyst S.G. [Malaysia]
17752. Control for Predip and Catalyst bath [Malaysia]
17753. Gold bath brightener [Iran]
17754. Electro copper coating [India]
17755. Plating peel off [India]
17756. Zinc Plating [Ohio]
17757. Mixing the chrome tank [Turkey]
17758. Plating C12L14 and making it red [Nevada]
17759. Titanium Anodising [England]
17760. METAL WIRE ONLINE CLEANING AND PREHEATING PRIOR TO EXTRUSION COATING [India]
17761. Na CN Solution is it dangerous [Indonesia]
17762. Problem in drawing electro galvanized wire [India]
17763. TOLERANCING FOR SURFACE ROUGHNESS [California]
17764. Need mirror-like mass surface preparation on zinc die-cast parts [Massachusetts] {11/07/02}
17765. Electroplating machines/supplies [California] {11/07/02}
17766. Electroplating/DME Research [Ohio]
17767. Semiconductor photoresist process [Vietnam]
17768. Glass Paint AB [California]
17769. Hook problem [Texas]
17770. Fail salt spray on aluminium test vs process [Canada]
17771. Need help with Kovar and Cu/Au alloys [Massachusetts]
17772. Anodizing polished aluminum [Colorado]
17773. Vapour degreasant alternatives [England]
17774. 303 Vs 304 [Wisconsin]
17775. Chemical passivation for stainless steel parts [Michigan]
17776. Aluminum/steel interaction [Georgia]
17777. Piston and cylinder wall finishings [Hawaii]
17778. Cleaning zamak carburetors [France]
17779. Copper sheeting [Wisconsin]
17780. Cleaning solutions for jewelry with gemstones [Florida]
17781. ALUMINUM DUST [California]
17782. Iridium coating for acrylic plastic sheet [Australia] {11/07/02}
17783. Cleaning procedure for ITO [India]
17784. Removal of Teflon from cookware [Texas]
17785. Electro-flocculation for domestic installations [Australia]
17786. Coating without hexavalent chromium, dull silver, 240 h corrosion resistance minimum [Poland]
17787. Garlic odor. Is it Arsine? [Maine]
17788. Kesternich test for copper/nickel plating [Spain]
17789. Immersion tin plating [India]
17790. SS 316L zinc kettle performance [India]
17791. COMPOSITE ELECTROLESS OF NICKEL-PTFE ON ALUMINIUM [Iran]
17792. Alodine finish [Germany]
17793. Gravell test, stamping painting surfaces [Poland]
17794. Seeking Nikasil Plating [Texas] {11/08/02}
17795. Polishing wheels [New York] {11/08/02}
17796. Adhering brass to brass [Mexico]
17797. Seeking chrome dipping [Florida] {11/08/02}
17798. Zinc dichromate plating with epoxy powder top finish in Mexico for Mexico auto parts [Mexico] {11/08/02}
17799. Need Aluminum to near mirror finish [California] {11/08/02}
17800. Sublimation Coatings [Georgia] {11/08/02}
17801. Seeking ZnS supplier [South Africa] {11/08/02}
17802. Looking for Black Oxide Solution -Require Spec. Mil-C-13924 [Korea] {11/08/02}
17803. Crystallizing from several different solutions [Pennsylvania]
17804. Rusting metal [Maryland]
17805. Silver peeling off from copper [Korea]
17806. Metal recovery from pickling liquor [India]
17807. Electrostatic Spray Gun Functional Description [New Jersey]
17808. Corrosion testing of marble [Australia]
17809. Plastic Conductivity [New York]
17810. Is this etching? [Canada]
17811. Restoration [England]
17812. Cost/delivery differences for Hexavalent/Trivalent Chromate and Molyphos [Tennessee]
17813. Reduction of fumes emission [India]
17814. Material Of Construction [India]
17815. Analyzing Ni and Au of electroless Ni, immersion Au bath [Malaysia]
17816. Fastener coatings [India]
17817. Zinc pretreatment [France]
17818. Source for Dacromet 500 LC Class A [Canada] {11/11/02}
17819. Cianeto de Potassio Aurico (g.p.c) [Brazil]
17820. Discoloration on stainless steel edges [California]
17821. How can I accelerate the oxidation of brass and copper? [California]
17822. Converting resistance to temperature [Arkansas]
17823. Painting over nickel plate [Virginia]
17824. Rust prevention question [California]
17825. Setting up Electroplating Bath [Vermont]
17826. Phosphate Coating Weight Specifications [Kansas]
17827. Ruthenium coated titanium? [New Zealand]
17828. Japan Black [Washington] {11/11/02}
17829. Seeking patina supplies [Florida] {11/11/02}
17830. New Pennies and Several Acids; an Observation [Massachusetts]
17831. Equipment costs for water electrolysis [India]
17832. Fiber optic cladding removal [China]
17833. IP Plating [China]
17834. Oxidation rate of copper [New Hampshire]
17835. What is the process to extract silver from x-ray traps? [Washington]
17836. Refinishing bathroom faucets [California]
17837. Waste Hydrochloric Acid [UAE]
17838. Plating Bubble Problem [China]
17839. How can I get a satin finish on aluminum using an acid solution? [Brazil]
17840. Titanium oxide removal after hermetic sealing [California]
17841. Problems etching 304 stainless steel [Illinois]
17842. Aluminum Polishing [California] {11/12/02}
17843. Second hand graphite furnace [Iran] {11/12/02}
17844. Import sulphuric acid [Bangladesh] {11/12/02}
17845. Need galvanized steel coils [Canada] {11/12/02}
17846. Standard test for adherence of products to electrode? [England]
17848. Bath Temperature Affecting Plating Speed [Texas]
17849. Aqua Regia Etch Rate [Nevada]
17850. Texture coating powders [Iran]
17851. Non-Tarnishing Spray [New Jersey]
17852. Aluminum paint and copper sheeting [Pennsylvania]
17853. Clear coat on metal [Oregon]
17854. Stripping paint from antique brass register [California]
17855. What is TURCO DECON 4182-A [Washington]
17856. Galvanizing cosmetic tubes [New York]
17857. Chrome Plating Car Wheels [New Jersey] {11/12/02}
17858. Large Drag Finisher [Nebraska] {11/12/02}v
17860. Copper Cathode / Copper Tape / Polyester Tape / High Carbon Steel [South Africa] {11/12/02}
17861. Solder failure in pure tin [Thailand]
17862. Effect of hard anodized coating to the furnace [Malaysia]
17863. Galvanizing plant [Uganda]
17864. Bright dip liquid required [Australia]
17865. Rusting Problem [India]
17866. Hydrogen embrittlement? [Australia]
17867. Seeking refinishing of a triple chrome show (roll) bar [Florida] {11/12/02}
17868. Polishing an aluminum intake manifold and water pump [Maryland] {11/12/02}
17869. 5 oz copper, tin plated [California] {11/12/02}
17870. Need an e-coat contact [Mexico] {11/12/02}
17871. Tantalum/Tantalum Nitride Etch [Georgia]
17872. "Anadiczenda" process for steel tubes [Illinois]
17873. Manual for Harshaw/Filtrol salt spray cabinet needed [Canada]
17874. Need Stress Measurement Panels [New Hampshire] {11/13/02}
17875. Seeking non chip paint for airgun targets [Florida] {11/13/02}
17876. Researching information on nail corrosion [Florida]
17877. White Gold or Palladium? [Mexico]
17878. Patina for bright brass fireplace surround [Canada]
17879. Copper Inserts for Kitchen Cupboards [Washington]
17880. What to do when brass lamps start to get black spots [Indiana]
17881. EPOXY PAINT FINISH [Massachusetts]
17882. Fixing anodized aluminum color problems [New York]
17883. Passivating Super Invar (32-5) [California]
17884. Chrome guitar finish [England] {11/13/02}
17885. Need Alodine [Illinois] {11/13/02}
17886. Applying Brushed Aluminium Finish [England]
17887. Need some permalloy help please [Iran]
17888. Electrodeposition [Iran]
17889. Refinish cabinet knobs to brushed nickel [Alabama]
17890. Ebonal 'c' plating process [UK]
17891. Anodising on Titanium [UK]
17892. Formula for Chelants [California]
17893. Oxidation / resistivity of metals [Switzerland]
17894. 0.5M SODIUM HYDROXIDE PREP [California]
17895. SOLDERING FLUX REMOVAL [California]
17897. Replacement For Hard Chrome Plating [California]
17898. Problems with Black Oxide on CRES 304 [Illinois]
17899. Tinted Hard Coat of T6 [Connecticut]
17900. Seeking plating machine [Vietnam] {11/14/02}
17901. SEARCHING FOR SOURCE OF LP86 LUBRICANT AND LP114 SEALENT [California] {11/14/02}
17902. Basic understanding of the purpose of electroplating [California]
17903. Corrosion of Stainless Steel [South Carolina]
17904. HOW TO POLISH ALUMINUM [Maine]
17905. OLD BRASS BED [Ohio]
17906. Copper reducing agent [Illinois]
17907. Nickel-Free Men's Jewelry [Hawaii]
17908. Teflon spray coatings [Canada]
17909. Zinc rich primer under ripple finish powder coat [Australia]
17910. Ideas on applying color to hand made steel [Oklahoma]
17911. Zinc Whiskers [Australia]
17912. Burr free product [California]
17913. Pickling spec. for 15-5 stainless [Florida]
17914. Removal of burrs/dirt from anodized aluminum [Pennsylvania]
17915. Stainless steel fasteners salt spray test [New Hampshire]
17916. Sulphuric acid pipeline [Chile]
17917. Pistolsmith seeks anodizing Ti frames [Michigan] {11/14/02}
17918. Service for ION Exchange Regeneration Service [Pennsylvania] {11/14/02}
17919. Gilt bronze, electrolysis, yellow gold finish in bronze [New Jersey]
17920. Cracking pattern in old brass [Ohio]
17921. Stripping "mechanically" deposited cadmium [Massachusetts]
17922. Etching of galvanized steel [UK]
17923. Maximum impurities in steel to be plated [Chile]
17924. Hard Anodizing Al. 7075 [Arizona]
17925. Change in Surface Structure of 304L Stainless Steel [Arizona]
17926. MIRROR FINISHING LONG BORES [India]
17927. Regeneration time [Peru]
17928. Using sodium bi carbonate in continuous galvanizing line [Bangladesh]
17929. Nickel plating over copper flash [Taiwan]
17930. Need to black rhodium our dog pin - 14kt. [New Jersey] {11/14/02}
17931. Need aluminum finishing/polishing services for hitch products [Idaho] {11/14/02}
17932. Need a shop to do UV cure coatings [Colorado] {11/14/02}
17933. Etching electrolyt [Bosnia and Hercegovina] {11/14/02}
17934. Acid Hydrometer [Vietnam] {11/14/02}
17935. Low temperature resistant protective coatings [California]
17936. Commutator plating [Massachusetts]
17937. Getting started in the chroming business [Pennsylvania]
17938. Brushed Aluminum [Arkansas]
17939. Cleaning brass with the non liquid Brasso [Massachusetts]
17940. Long lasting stainless steel polish [Texas]
17941. Want Book on Solder plating [New York]
17942. Stainless steel 316 corrosion [India]
17943. Distilled water vs Reverse Osmosis water in Pharmaceutical Company [Philippines]
17944. Finding the purity of silver in silver alloys [India]
17945. Compatibility of D-2 tool steel and TiCN coatings [Ohio]
17946. Corrosion appears on SS303 after nickel plating [India]
17947. Chemical Composition of Anodized Aluminum [California]
17948. Bead blast surface finish [California]
17949. Fluorides in water and toothpaste [Lebanon]
17950. Lacquered Brass restoration and Metal Bluing [Australia]
17951. Relevance of Salt Spray Test [India]
17952. Metallic Powders used in Automotive Paints [Iran]
17953. Bronzed Knee Caps [Massachusetts] {11/15/02}
17954. Interested in having cooking pots anodized [Texas] {11/15/02}
17955. Need to Alkaline/Acid Dip a 1977 280Z [Nevada] {11/15/02}
17956. Seeking powder coat shop [South Carolina] {11/15/02}
17957. Zinc Nickel Sources [North Carolina] {11/15/02}
17958. Alkaline zinc nickel process [Ohio] {11/15/02}
17959. Di-valent chromium? [Scotland]
17960. Ferric chloride etch for preparation of brazing surfaces [Massachusetts]
17961. Chromium solution electrodeposits [Brazil]
17962. Anodizing aluminium- resist [England]
17963. Need to now about refinishing cast iron tea kettle [Kentucky]
17964. Bluing solution problems [England]
17965. Magnesium finishes needed [Canada]
17966. Citric acid as a chelating agent for nozzles spraying tap water [Tennessee]
17967. Removal of cadmium coated bolts [UK]
17968. Refinishing Oil Rubbed Bronze [Michigan]
17969. Cracking of thick vs thin anodized 6061 [California]
17970. Non-porous Alternative to Hard Chrome Plating [Rhode Island]
17971. How do I coat the inside of a plastic tube during extrusion? [Georgia]
17972. EMBOSSED NUMBER PLATES [India] {11/18/02}
17973. Need DI seal tester [California] {11/18/02}
17974. Rust rate project [Georgia]
17975. WHAT'S AN ALLOY AND WHAT DO YOU USE IT FOR [England]
17976. Cleansing pennies...INTERNET IS WRONG I AM RIGHT! [Florida]
17977. How to make bronze [Nevada]
17978. Depositing metal with low diffusion content [Singapore]
17979. Aluminum coloring [Colorado]
17980. Can you paint cookware? [Pennsylvania]
17981. Satin vs. hairline finish [Kuwait]
17982. MIL-C-5541E or AMS-C-5541 [Kansas]
17983. Anodizing Fume Capture and Treatment [Iran]
17984. UV-test [Belgium]
17985. Removing CARC paint [South Carolina]
17986. Copper anodizing [Indiana]
17987. Estano ennegrecen [Spain]
17988. Welding of zinc iron coated metal [Tennessee]
17989. Passive Ni deposit [Mexico]
17990. Chem-Film Facility [Taiwan] {11/18/02}
17991. Color range for Mil-A-8625F Satin Clear Ty II Class I [California]
17992. Seeking Refinishing of Knife [Michigan] {11/18/02}
17993. Regeneration of pickling liquor (HCl) [Mexico]
17994. Inhibitors for acid-metal reaction [Philippines]
17995. Wet Chlorine and Pulp [New Zealand]
17996. SULPHURIC ACID PIPE LINE LINER [Chile]
17997. Hard coating [Connecticut]
17998. Selective plating or anodizing [Hong Kong]
17999. Chrome plate my boots [Texas] {11/19/02}

The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.