14000. Polishing of small 304 stainless steel pressed components [India]
14001. Seeking palladium chloride solution [Iran] {4/16/02}
14002. A report on the production of sodium hypochlorite industrially [Nigeria]
14003. Hallmarks? Silver or pewter? [West Virginia]
14004. Stainless steel finishing [Texas]
14005. Electroplating Nonmetal Objects/Commercially Producing Metals from Electrolytic Cells [USA]
14006. Melted rain suit on exhaust pipe [Pennsylvania]
14007. Copper tubing patina [North Carolina]
14008. Seeking an ion exchange resin 'Duolite ES-63' [Netherlands] {4/16/02}
14009. Seeking cathodic immersion painting process [Taiwan] {4/16/02}
14010. Removing lacquer [Japan]
14011. Darken pennies [Canada]
14012. Electropolish 316L [California]
14013. COATING OF OIL FIELD TOOLS [Canada]
14014. Brass Bed Refinishing [North Carolina]
14015. Black Dull Nickel Plate [UK]
14016. No thickness aesthetic surface treatment for grey cast iron [Italy]
14017. Galling of 718 threads in non-permanent connections [Texas]
14018. 7075 aluminum pin hole corrosion [California]
14019. Removing tile sealers [Maine]
14020. Which tumblers are the best [Texas]
14021. Seeking equipment for decorative chroming [India] {4/17/02}
14022. Gold plating removal [Vermont]
14023. O-ring seal on hard coat anodize [Minnesota]
14024. Cold bluing vs cold black oxide finish [California]
14025. Seeking tinning of an old copper sauce pan [North Carolina] {4/17/02}
14026. Red indicates corrosion site in hard chrome deposit [Canada]
14027. Polish Motorcycle Rims [New Jersey]
14028. Galvanic couple between Al6061T6+Alodine1200 and AISI316L or AISI304L [France]
14029. Diamond electro plating on gear [India]
14030. Is it normal to plate platinum jewelry [England]
14031. Seeking coating (3M EC2290) [Malaysia] {4/17/02}
14032. Hard anodizing problem, aluminum alloy [Turkey]
14033. Crystal varathane purported to be carcinogenic [Canada]
14034. Blacodizing Process [India]
14035. Neutralizing nitric acid with sodium bicarbonate [Florida]
14036. CLEANING PENNIES - Substances that don't work [New York]
14037. Disposal methods of MSDS [Texas]
14038. How much of copper sulphate do you consume before you die [Canada]
14039. Sodium hydroxide [Australia]
14040. How to protect Mild Steel [England]
14041. Undo my polishing on antique brass hardware [Ohio]
14042. HCL vs. Muriatic Acid [Illinois]
14043. Seeking paint instead of electroplating [Poland] {4/17/02}
14044. Need antique brass heat resistant paint [Oklahoma]
14045. Titanium / Tungsten etching [Oregon]
14046. Seeking metallic plated fine fiber [Colorado] {4/18/02}
14047. Seeking Liquid Honing [Illinois] {4/18/02}
14048. Ti-SBR bonding [India]
14049. Cladding through welding process [India]
14050. Cleaning a burned stainless steel surface [Hong Kong]
14051. Effects of Hydrogen Embrittlement [Florida]
14052. On the lookout for "Nextel Suede-Coating" [Denmark]
14053. Anodization [India]
14054. Powder Coating Plugging Hole [Canada]
14055. White Rust on Sheeting [South Africa]
14056. Seeking used e-coat systems [Canada] {4/18/02}
14057. Mill Scale Use [North Carolina]
14058. Steel, Aluminum, Plastic Chroming [Illinois]
14059. PAINTING OVER HOT DIP GALVANIZE [Texas]
14060. Sulfamate Nickel Strike Help Needed [Maine]
14061. Anodising assistance [UK]
14063. Seeking shop to powdercoat diamond mesh expanded metal [New York] {4/18/02}
14064. Seeking anodizing and laser etching on 6061 extrusion [Nevada] {4/18/02}
14065. Substances for Cleaning Pennies [California]
14066. Chromate Recovery [Oklahoma]
14067. Piston Tin Plating Problem [Australia]
14068. Stain on nickel plated surface [Hong Kong]
14069. Blow mold texturizing, help! [Mexico]
14070. Ti-SBR bonding [India]
14071. SEEKING SMALL SALT SPRAY CABINET [Utah] {4/18/02}
14072. Degree of cleanness of stainless steel [Thailand]
14073. Seeking concentric hot dip tin plating machine [India] {4/18/02}
14074. Seeking High Alumina Refractory Sintering Boat [Switzerland] {4/18/02}
14075. Etching silver [Isle of Wight, England]
14076. Ideal temperature for hot dip tinning [India]
14077. Solder plating [Thailand]
14078. Problem with soft anodic coating [New Zealand]
14079. Thin film coating of a small inside diameter [New Hampshire]
14080. Removing sheen on ceramic tile [Minnesota]
14081. Metal tiles [Spain]
14082. Galvanic Corrosion between Nickel Plating and 17-4 SS [Florida]
14083. Help cleaning stainless steel tanks [Virginia]
14086. Seeking m/c wheels chrome plated [Michigan] {4/19/02}
14087. Seeking chrome wheel refinishing [Louisiana] {4/19/02}
14088. Seeking magnesium anodizing technology [Japan] {4/19/02}
14089. Seeking lab-scale roll coating equipment [Massachusetts] {4/19/02}
14090. Seeking platinized Ti anodes [Russia] {4/19/02}
14091. TTE and Hexane [Canada]
14092. Teflon recoating [Michigan]
14093. Small bluing operation [Arizona]
14094. Vacuum metallizing [New Zealand]
14095. Nickel Plating Brass [Canada]
14096. Help with blue dye over zinc plate [Minnesota]
14097. Films of Cobalt Iron Soft Magnetic Alloys [Illinois]
14098. Phosphate pretreatment [New Jersey]
14099. Need preparation chemicals for powdercoating [Florida]
14101. How to separate the anodic alumina from the underlying aluminum substrate [Illinois]
14102. Dependence of deposited mass on temperature during electroplating [Scotland]
14103. What's in 7up or Mountain Dew to dissolve a paper clip? [Arizona]
14104. Copper plating nail experiment [New York]
14105. Aluminum Polishing Question [New York]
14106. Aluminium oxide wood finishing [Macau]
14107. Refinishing a brass bed [Pennsylvania]
14108. Thermal conductive powder [California]
14109. How do we plate nickel over nickel [Michigan]
14110. Plating on TiW [Singapore]
14111. Tufftriding [Malaysia]
14112. Seeking foil printing plates [UK] {4/22/02}
14113. Seeking ultra filter for e-coat process [Iran] {4/22/02}
14115. Electroplating [Saudi Arabia]
14116. Rechroming plastic [Australia]
14117. Passivation contamination [Canada]
14118. Rusting problem [Turkey]
14119. Stabilizer for hydrogen peroxide [India]
14120. Seeking polyester coating for sublimation [Saudi Arabia] {4/22/02}
14121. Australian AS 1231 1985 [North Carolina]
14122. Aluminum re-anodize [Virginia]
14124. Plastic chrome plating [Canada]
14125. Seeking acid dipping for 300zx hood [Ohio] {4/22/02}
14126. Seeking Ti-based ACTIVATOR BATH [Iran] {4/23/02}
14127. Spotting after vacuum heat treatment [UK]
14128. Aluminium pretreatment [India]
14129. Filling rust pitted area on metal before chroming [Belgium]
14130. CrVI Anti-Tarnish Process [Malta]
14131. Conductive Aluminum Finish [Michigan]
14132. How can you monitor or measure amount of chrome in water [Kentucky]
14133. Pressure Washer Deanodizing [Rhode Island]
14134. Seeking chemicals for Chromate Conversion Coating [Pakistan] {4/23/02}
14135. Chrome appearance in a plastic paint [Virginia]
14136. Galvanization Repair Suggestions [Tennessee]
14137. Gold property [California]
14138. Need info. on "plater's wax" [Virginia]
14139. Aluminum patinas [Washington]
14140. SEEKING CHROME PLATING PLASTIC [California] {4/23/02}
14141. Seeking zeolites to bind divalent cations [Vermont] {4/23/02}
14142. How to cast a smooth bore iron cannon [Canada]
14143. Old stainless steel stove top refurbishing [California]
14144. Electrostatic painting with aqueous coatings [India]
14145. Etch square corners [South Africa]
14146. Stainless Steel Scratches [Illinois]
14147. Charge of a nickel dithiocarbamate complex molecule [Pennsylvania]
14148. Zinc galvanizing [India]
14149. How do you check bonding strength between sputtered metal and ceramic [Texas]
14150. Gold plating on SS component (spring steel wire component) [India]
14151. Improving the reflectivity of anodised surfaces [UK]
14152. Methods of finishing for vacuum and vibration work [UK]
14153. Mirror finish on die-cast aluminium [Singapore]
14154. Seeking tabletop style Electro Chemical Deburring machine [Connecticut] {4/24/02}
14155. Need to know what materials/chemicals for electroplating [Oregon]
14156. Need really clear clearcoat [Nevada]
14157. Painting ABS [Maryland]
14158. Removing scratches from a polished parts [North Carolina]
14159. Method to color concrete to near white [Canada]
14160. E Coat vs Autophoretic [Tennessee]
14161. Acid corrosion [Canada]
14162. Bismuth / tin plating questions [North Carolina]
14163. Bright dip acting as lubricant [Pennsylvania]
14164. Ruthenium/Iridium coated Titanium anodes [Canada]
14165. Seeking hi-temp but removable paint [Taiwan] {4/24/02}
14166. Seeking titanium and nickel pump Spanish vendors [India] {4/24/02}
14167. Electrode polarization [California]
14168. Finishing pewter buckles [England]
14169. Clear coat on aluminium surfaces [England]
14170. Seeking Decoral finish for aluminium profiles [Saudi Arabia] {4/24/02}
14171. Seeking supplier for polypropylene ball [Florida] {4/24/02}
14172. Painting over a hot-dipped galvanized surface [Connecticut]
14173. Painting a plastic (polyethylene) motorcycle gas tank [Michigan]
14174. Inert carbon canister coating [Texas]
14175. Cost of aluminum fume treatment [India]
14176. Difference between lacquer and papier mache [Singapore]
14177. Non-sticking coating for welding blade [Taiwan]
14178. High frequency metal plating issue [California]
14179. Spectral emissivity measurements for 3M Nextel [UK]
14180. Searching for alternatives to dipping for magnesium chromate plating [UK]
14181. Sensitizing Paste for Electroless Nickel Deposition [Louisiana]
14182. Frosted appearance on passivated parts [Arizona]
14183. Bright dip or what? [California]
14184. A hydrogen embrittlement and coated wire puzzler [Oregon]
14185. Tarnish prevention of copper [Minnesota]
14186. SAE AMS-A-8625 and MIL-A-8625 [France]
14187. Powder coating plastic [Iowa]
14188. Refinishing wrought iron furniture [New York]
14189. Thermal vs Chemical Black Oxide [Connecticut]
14190. Final finish problems during fishing reel manufacturing [Canada]
14191. Seeking rechroming of bumpers and wheels [Michigan] {4/25/02}
14192. Seeking refinishing of aluminum automotive trim [California] {4/25/02}
14193. SEEKING P.S PLATE SINGLE SHEET LINE [Pakistan] {4/25/02}
14194. Seeking Turn-key CHROME PLATING Installation [U.A.E.] {4/25/02}
14195. WATER RESISTIVITY [Texas]
14196. Information about synthetic diamond powder from Chinese companies [India]
14197. Advice reagrding electroplating wastes and inline systems [New Zealand]
14198. Anti reflective paint for 400-700 nm [New York]
14199. Sealing of anodize [Mexico]
14200. Paint that reflects lights [Illinois]
14201. White Patina Wanted [Massachusetts]
14202. Soldering Electroless Nickel [North Carolina]
14203. Best brass finish for outdoors-goldleaf or e-coat? [New Jersey]
14204. Enamel Coating [Hong Kong]
14205. Edge Building of Nickel Deposit Problem [India]
14206. Gold plating on stainless steel battery contacts [India]
14207. Dow#7 /Dichromate treatment [Hong Kong]
14208. Need lubricant to aid in stripping process [Florida]
14209. Chromate Conversion Coating [Massachusetts]
14210. "Home" powdercoating over chrome plate [Maryland]
14211. PAINT ISSUES OVER PLATED PARTS [Minnesota]
14212. Question on Zinc Olive Drab Plate [Indiana]
14213. Seeking zinc phosphate with PPG Powercron 640 electrocoat [New York] {4/26/02}
14215. Seeking Ni-W plating services [California] {4/26/02}
14216. Seeking Dip Spin Machines [New Jersey] {4/26/02}
14217. Seeking adhesive for metalbonding [Romania] {4/26/02}
14218. Seeking phenolic resin 12687 [China] {4/26/02}
14219. Seeking suppliers of SUS303 and Oxygen-Free Copper [Thailand] {4/26/02}
14220. Seeking Cobalt Rounds [Canada] {4/26/02}
14221. Activation [India]
14222. Procesos químicos en la línea de galvanizado [Ecuador]
14223. Which type/grade of Aluminum [Pennsylvania]
14224. Polishing flat Aluminium [Australia]
14225. Chemicals for etching [India]
14226. Electrostatics precipitators security [France]
14227. Laser removal of Teflon FEP problem [Massachusetts]
14228. Any ideas about aluminum finish shine removal? [Utah]
14229. Clear Anodizing - Matching 6061 and 6063 [Oregon]
14230. ALUMINIUM DISSOLUTION IN CAUSTIC [Australia]
14231. Galvanic Problems - Zinc substituted for Cadmium [Pennsylvania]
14232. Seeking vacuum plating ABS [Florida] {4/26/02}
14233. Chrome horse [Spain]
14234. Cleaning cedar and water spots [Vermont]
14235. Matte black finish stainless [Wisconsin]
14236. Seeking vacuum metalize or chrome plate 96" long fiberglass parts [Texas] {4/29/02}
14237. Seeking small quantities of AeroGlaze [California] {4/29/02}
14238. Mix olive drab and yellow [Argentina]
14239. Red Tint to Black Oxide Holders [Ohio]
14240. Seeking Chrome Lining for Cylinders [Connecticut] {4/29/02}
14241. Nickel sulfate build up in nickel tank [Michigan]
14242. Seeking enamel coating [Taiwan] {4/30/02}
14243. Manufacturer seeking representation in Pakistan [Pakistan] {4/30/02}
14244. Clear coat finish needed for copper [North Carolina]
14245. NH4OH and Silver Chloride [Virginia]
14246. Plasma Nitriding [India]
14247. Aluminum etching [Connecticut]
14248. Seeking equipment for decorative chroming [India] {4/30/02}
14249. Removal of Sodium Carbonate [Singapore]
14250. Seeking el materials -phosphor and barium titanate ink [Taiwan] {4/30/02}
14251. Seeking silver brighteners [India] {4/30/02}
14252. Chemical stripping of chrome from aluminum substrate [Pennsylvania]
14253. Electroless nickel plating [India]
14254. Seeking ultrasonic polisher, pneumatic polisher (SIG) and Flex-poli machine [Australia] {4/30/02}
14255. Enamel coating [Taiwan]
14256. Seeking glitter cutting machine [India] {4/30/02}
14257. Chrome plating in deep holes [Australia]
14258. Machining terminology [Australia]
14260. Seeking Glossmeter [India] {4/30/02}
14261. PP compatibility with sulphuric acid [India]
14262. Seeking silver cyanide [India] {4/30/02}
14263. Carbon mark defect on piping product after pickling [Malaysia]
14264. Open fire barbecue with galvanized mesh [Australia]
14265. Where to buy equipment for chrome plating plastic [Missouri]
14266. Degreasing of SS 304 Parts [India]
14267. Seeking powder coat aluminum tubing off-white [Kansas] {4/30/02}
14268. Plating of copper on tin [New Jersey]
14269. Discoloration of Stainless Steel [Japan]
14270. Putting logo on stainless steel products [China]
14271. Seeking prototyping shop/lab [California] {4/30/02}
14272. Seeking paint coating line for sheet metal [Greece] {4/30/02}
14273. Biodegradable steel [Australia]
14274. Bronze memorial [Australia]
14275. Seeking a special plating [California] {4/30/02}
14276. Seeking Dirilyte Polish [Virginia] {4/30/02}
14277. Facility to make NAOCI [Malaysia]
14278. Electroplating for kids [Washington, DC]
14279. How can I refinish my wrought iron railing [Utah]
14280. Rusting carbon steel [North Carolina]
14281. Restoring the chrome base on a 1950's style table [Florida]
14282. Foil finish [Arizona]
14283. LOOKING FOR ASTM STD [Michigan]
14284. Zr:N coating, How to strip it [Belarus]
14285. Coatings on glass [Massachusetts]
14286. Bondable, wearable under extreme pressures [Minnesota]
14287. Ammonia in Watts Nickel Plating Bath [Tennessee]
14288. Removing copper from nickel anodes [Massachusetts]
14289. Cast iron compressor in marine environment [New York]
14290. Anodizing brass [Minnesota]
14291. Pickling of stainless steels like SS304, 316, 310 - HOW? [India]
14292. Seeking electroplating plant for ABS and Polypropylene [UAE] {4/30/02}
14293. Ni-P-Alumina electroless composite coating [Iran]
14294. Copper plating in my kitchen...can it be done? [California]
14295. Anodising WS3.2315.72 [England]
14296. Seeking waste from anodizing of aluminium [Mexico] {4/30/02}
14297. Anodizing Industry-Phosphoric Acid [India]
14298. NaAu simple procedure to obtain [Arizona]
14299. Paint filling engraved plates [Australia]
14300. Aluminium and magnesium wheel clearcoating [Canada]
14301. Removing Chrome from an Antique [Pennsylvania]
14302. Plating corrosion [India]
14303. What is/was CHEMPLATE? [California]
14304. Seeking specific hydrometer for sulfuric acid concentration measurement in %v/v [Malaysia] {5/01/02}
14305. Cadmium plating [UK]
14306. Seeking Gold Plating/Finishing of LPs for framing [Illinois] {5/01/02}
14307. Seeking phosphoric acid [Egypt] {5/01/02}
14308. Seeking chrome plated or vacuum deposited on carbon fiber [New Mexico] {5/01/02}
14309. Seeking Koroseal tank lining materials and training [Australia] {5/01/02}
14310. Seeking titanium nitride coating [California] {5/01/02}
14311. Light color fastness [China]
14312. Citrus information urgent [California]
14313. Chrome over brass [Canada]
14314. Aluminum Sailboat Mast Refinishing [Ohio]
14315. Base metals stuck in solution, need them out! [Virginia]
14316. Zinc Whiskers [Canada]
14317. PVD and oil rubbed bronze [California]
14318. Making sulfuric acid anodizing solution [Canada]
14319. Clean burn/great taste wanted [Australia]
14320. Paints for corroded machinery [India]
14321. Seeking galvanized sheet metal [Germany] {5/01/02}
14322. New Stainless Steel [Tennessee]
14323. Electroless coatings for tubing [Georgia]
14324. Failure of bond between rubber and brass [India]
14325. What is difference between silver oxidation and corrosion [Canada]
14326. Seeking plating of fishing lures [Tennessee] {5/03/02}
14327. Seeking investment casting/chrome plating-small part prod [California] {5/03/02}
14328. Seeking chrome painting [Wisconsin] {5/03/02}
14329. Seeking brass plating of lucky horseshoe [California] {5/03/02}
14330. Seeking local vacuum metalizing services [Ohio] {5/03/02}
14331. Seeking printing/lettering on 2'' round anodized parts [Canada] {5/03/02}
14332. Seeking Chromic Acid Masking [Canada] {5/03/02}
14333. Pricing of 6063 T5 Aluminum Extrusion [New York]
14334. 1100 Alum composition [Massachusetts]
14335. Price of sheet of aluminum [Mexico]
14336. Electroplating [Canada]
14337. Cost of aluminum alloy for bicycle [Illinois]
14338. Relation between thickness and height [India]
14339. Chemical resistant tanks or lining for NaOH sol. up to 90% [Iran]
14340. Chemistry project [North Carolina]
14341. How to give brass an antique finish [Idaho]
14342. Stiffle lamp restoration [New York]
14343. Removing "Rust" on Stainless 304 [Michigan]
14344. Patination of zinc sheet [Arizona]
14345. Rinsing Water Criteria [Malaysia]
14346. ALGAE FORMATION INSIDE PVC PIPES [California]
14347. Sump liners [Michigan]
14348. Etchant for Nickel and Copper [Texas]
14349. Colored plating/conversion finishes for Zinc ZA-8 [California]
14350. Help to plate aluminum cast [Illinois]
14351. Electroplating ceramic surfaces [Sweden]
14352. Grain structure visible through black anodising [Australia]
14353. Aluminum content upper limit in sulfuric acid anodizing baths [Iran]
14354. This tape will self destruct.... any alternatives? [UK]
14355. Product to increase adhesion of metal finish (eg chrome over chrome) [New York]
14356. Differences between 316 and 316L [Singapore]
14357. Seeking CHEM FILM / LARGE TANK [California] {5/06/02}
14358. Seeking Anodizing (Grey) to Fed Std [New York] {5/06/02}
14359. Seeking hot dip equipment [Turkey] {5/06/02}
14360. Seeking LOCK FORMING/ROLL FORMING MACHINE FOR SHEET METAL [U.A.E.] {5/06/02}
14361. Seeking Bearing Quality Steel [Ohio] {5/06/02}
14362. Seeking portable/compact polishing-buffing machine [Australia] {5/06/02}
14363. Seeking paint stripper [Turkey] {5/06/02}
14365. Seeking hardened stainless steel press plates [Iran] {5/06/02}
14366. ANTICORROSIVES [India]
14367. Silver from silver nitrate? copper? [Missouri]
14368. Aluminum alloy used in coating cds [Egypt]
14369. Shotpeening and boiling heat transfer [India]
14370. CLEANING EXPERTS FOR SALTWATER [California]
14371. Electrolysis in water wood stove, and how to prevent [California]
14372. Lead/tin nickel or chrome plating [Wisconsin]
14373. What does the name RAL stand for [Israel]
14374. Microwave Oven Interior Reflective Materials [California]
14375. Electroforming [Australia]
14376. Patinizing copper pipes [California]
14377. Mil-a-8625f [Canada]
14378. Health effects of Sodium Hypochloride [Maine]
14379. Electro-coagulation process [Mexico]
14380. Strip nickel from stainless steel [Michigan]
14381. Alternative for for Hydrofluoric acid (HF) to remove silver coated surface [Malaysia]
14382. How to remove white gold or platium over gold jewelry [Tanzania]
14383. Powder Coating on galvanized mild steel sheets [India]
14384. Anodising vs Powder Coating [New Zealand]
14385. Bronze-like finishes for architectural stainless steel [England]
14386. Black conductive finish [Hong Kong]
14387. Shopping Cart Plating [Kuwait]
14388. Pin hole corrosion in 7075 Aluminum [California]
14389. ELECTROPOLISHING [India]
14390. Need idea for science project [Canada]
14391. Darkening Brass Candlesticks [Missouri]
14392. Electro black finish, is it? [Argentina]
14393. Acid to reveal a filed off stamping on steel [Florida]
14394. Harder deposit [Pakistan]
14395. SEEKING PREGRAINED AND ANODIZED ALUMINIUM STRIPS OR SHEETS TO PRODUCE P.S LITHO PLATES [Pakistan] {5/07/02}
14396. SEEKING INFORMATION ON ZINC ALLOY PLATING [Turkey] {5/07/02}
14397. SEEKING COATING LINE TO PRODUCE P.S PLATES -USED / SECONDHAND [Pakistan] {5/07/02}
14398. Seeking clear glossy lacquer dry curing [Argentina] {5/07/02}
14399. Water stain on wood [Maryland]
14400. PLASTIC REFINISHING [Michigan]
14401. Aluminum Polish [Missouri]
14402. Powder Coat Mil Specs [New York]
14403. CORROSION RESISTANCE OF CED COATING [India]
14404. Electroforming mold life [India]
14405. Electropolishing [South Africa]
14406. DETERMINATION OF INHIBITOR CONCENTRATION IN PICKLING [India]
14407. Seeking Wrought Iron Refinishing [Massachusetts] {5/07/02}
14408. Passivation on Titanium [Virginia]
14409. Seeking finishing mirrored bronze [Georgia] {5/07/02}
14410. Weathered look on corrugated metal [Georgia]
14411. Barrel brass electroplating [Pakistan]
14412. Seeking information for silver extraction business and machine [India] {5/07/02}
14413. Seeking Electropolish Supplier [Mexico] {5/07/02}
14414. Test for Citric Acid [California]
14415. Seeking brass statue finishing [India] {5/07/02}
14416. Seeking acid cleaning of various substrates [Ohio] {5/07/02}
14417. Electroplating experiment(iron and copper) unsure of how [Australia]
14418. How can I dye metal cable different colors [California]
14419. Metal recovery from electroplating industrial waste [India]
14420. Removing corrosion from Supercharger [California]
14421. Bike frame [Indiana]
14422. Vintage Motorcycle Aluminum Deox and Finish Restoration [Washington]
14423. ELECTROPLATING SOLUTION TEMPERATURE [Australia]
14424. Optical black [China]
14425. Need way to preserve luster of copper sheet [Arizona]
14426. Electrolytic polishing [Ohio]
14427. Pitting corrosion on steel after molding acrylic plastics [Singapore]
14428. Ultrasonic cleaning and contamination [England]
14429. Surgical Steel [Turkey]
14430. Field test for verifying anodizing [New York]
14431. Volkswagen colour [The Netherlands]
14432. Citric Acid in plating solution [California]
14433. Leadfree plating [Hong Kong]
14434. Adhesion between Ni and Au plating [Virginia]
14435. Bright zinc plating over industrial steel [Iowa]
14436. Zinc and trivalent + clear and seal salt spray protection level [UK]
14437. SEEKING CHROME PLATER(s) [MEXICO] {5/08/02}
14438. Seeking replating of binacle and winches on sailboat [Florida] {5/08/02}
14439. Copper coating for welding wire [Saudi Arabia]
14440. Acceptable reject rates [New York]
14441. White spots in black anodizing [New Jersey]
14442. How to Cut before Color [Texas]
14443. Seeking flat mirror finish [New Jersey] {5/08/02}
14444. Seeking colored chromate bronze plating [Canada] {5/08/02}
14445. Seeking Zinc Rich Paints [India] {5/08/02}
14446. Seeking Whiteness Tester [Indonesia] {5/08/02}
14447. Copper Plating a Quarter [Nebraska]
14448. Cyanide colorimetry [Indonesia]
14449. Aluminum Deburring Ideas [Utah]
14450. Defects on plated components [India]
14451. Hazards of welding galvanized metal and e-coat primer [Iowa]
14452. Stain on EN-plated surface [Singapore]
14453. Silver coating replacement [Turkey]
14454. Al anodizing for small fuse [Taiwan]
14455. Need help on copper parts brightening [India]
14456. Ferroxyl alternative [Australia]
14457. Flat mirror finish [New Jersey]
14458. Tank Heating Design [Ohio]
14459. Masking tape for anodize without chromating first [New York]
14460. Nickel Barrier Thermistors [California]
14461. Hard Chrome Peel Off On Inconel [Singapore]
14462. Need a spot type seal check for black anodized aluminum [California]
14463. Plating aluminum water coldplates [New Jersey]
14464. Cleaning Contaminated Anodized Aluminum [California]
14465. Sulfonic acid compatibility [Virginia]
14466. Small business offering metal cleaning and lacquering [Singapore]
14467. FTIR of Polyetherimide [Singapore]
14468. Need a formula used in polishing and buffing stainless steel [India]
14469. Copper Roof Cleaning [Ohio]
14470. Polishing equipment or accessories [North Carolina]
14471. Seeking equipment for decorative chroming [India] {5/09/02}
14472. Is electrowinning an alternative? [Minnesota]
14473. Seeking anodizing or powder coat of 6061 mt. bike frame [Massachusetts] {5/09/02}
14474. Seeking small poly factory [Arkansas] {5/09/02}
14475. Differences between thermal spraying and PVD [Australia]
14476. Seeking titanium rods [India] {5/09/02}
14477. Aluminium deposit in a plate heat exchanger [UK]
14478. Nicked chrome handle bars [Texas]
14479. CLEAR CHROMATE THAT MEETS MIL-SPEC [New York]
14480. Titanium oxidation cleaning procedure [Norway]
14481. Nickel Free Specification in Europe [Hong Kong]
14482. Citric Acid Passivation - Disposal and Reclamation of Effluent [Iowa]
14483. Masking hard anodized part [California]
14484. Using Citric Acid as an Electrolyte [Massachusetts]
14485. Seeking DLC coating on 316L stainless steel [Pennsylvania] {5/10/02}
14486. Oiled Bronze Finish on Copper [Washington]
14487. Degreaser reconfiguration [New York]
14488. Salt Spray Standards - What do they really indicate? [Arizona]
14489. What's the cheapest best way to clean dirty (organic stained) anodized aluminum? [California]
14490. Autophoretic and C.E.D painting process [India]
14491. Iron content in a fluxing bath [Colombia]
14492. Seeking PU finish factory [U.A.E.] {5/13/02}
14493. Brush Metal Look [New York]
14494. Seeking Potassium Cyanide [India] {5/13/02}
14495. How to Nicasil [South Africa]
14496. Performance Metric for powder coat and E-Coat process [North Carolina]
14497. Hot dip galvanizing [Turkey]
14498. Seeking Passivation of Grill Tops [Georgia] {5/13/02}
14499. Galvanneal vs. Hot Dipped process [Massachusetts]
14500. PAINT REFLECTIVITY [Massachusetts]
14501. Seeking hot dip galvanizing bath [California] {5/14/02}
14502. How does aluminum foil clean silverware [Australia]
14503. Cabinets [Alabama]
14504. Storing muriatic acid [North Carolina]
14505. Material of pickling tanks [India]
14506. Dun Blackening [Louisiana]
14507. Plating contaminants [California]
14508. Zinc Anodize [Canada]
14509. Request of information about thermal deburring [Brazil]
14510. Painting a forced hot air duct [Rhode Island]
14511. Stained dishwasher door [Canada]
14512. Chrome contamination of nickel bath [Canada]
14513. Seeking re-chrome of a Leica camera [Australia] {5/14/02}
14514. Seeking Mil-spec Parkerizing help [Florida] {5/14/02}
14515. SEEKING SUPPLIER OF FOIL LACQUERING LINE [China] {5/14/02}
14516. METAL STAMPING QUESTION [Ohio]
14517. Plating of wood [South Africa]
14518. Re-finish new brass hardware to give it an antique distressed look [California]
14519. Pulse anodizing [India]
14520. Anodizing parameters to get 50 micron thickness [India]
14521. RHR to Ra, Rz conversion [Saudi Arabia]
14522. Seeking spectrometer [India] {5/14/02}
14523. Seeking controllers for electroless plating [India] {5/14/02}
14524. High Wear Resistance Coating Needed [Indonesia]
14525. Seeking chrome plating shop for auto parts [Florida] {5/14/02}
14526. Seeking someone to chrome plate a candelabrum [New Jersey] {5/14/02}
14527. Seeking GMW14 and GMW3359 [Illinois] {5/14/02}
14528. Seeking chromate conversion finishing for aluminium chassis [Thailand] {5/14/02}
14529. Darkening aluminium [Denmark]
14530. Stripping brass parts [New York]
14531. Chroming cromemolly [Canada]
14532. Aged, oxidized brass finish [Washington]
14533. DO YOU KNOW HOW TO GET OUT BUFFING MARKS [Michigan]
14534. Detailing aluminum rims [Texas]
14535. Patent access [Maryland]
14536. How to analyze salt spray solution [New York]
14537. Standards for Hydrogen Embrittlement Relief after Zinc Plating [Canada]
14538. Aluminum consumed / coating formed ratio [Colorado]
14539. Sensitizing and the Brashear process [North Carolina]
14540. Electroless deposition in organic suspension [India]
14541. Plating Brass Trouble [Wisconsin]
14542. Chromating metal matrix composites [Colorado]
14543. WOODEN FINISH DESIGNS ON POWDER COATED ALUMINIUM PROFILES [Saudi Arabia]
14544. Bluish sparkle on red anodize [Arizona]
14545. Matte anodizing of machined aluminium parts [Mexico]
14546. Surface Finish Options for CF-3M S.S. [New Jersey]
14547. Seeking manufacturers for electroless gold solutions [India] {5/15/02}
14548. Acid neutralizing solution [California]
14549. Rebuild of axle shaft bearing seats [Illinois]
14550. ANODIZING vs. CHROMATE PLATING [Thailand]
14551. Black electrically conductive finish over temperature [UK]
14552. Additive acid for copper coating [China]
14553. Seeking SPI-SPE Mold Comparison Kit [Massachusetts] {5/15/02}
14554. Cyanide destruction in spent strippers [South Africa]
14555. Coating burr problem [Malaysia]
14556. Hard Coat Info [Massachusetts]
14557. Etch process to roughen 316 SS for glue adhesion [Pennsylvania]
14558. Seeking large item anodizer, olive drab color [New York] {5/15/02}
14559. Seeking chrome plating source [California] {5/15/02}
14560. Thermoplastic motorcycle seat construction [Michigan]
14561. Brass table [Illinois]
14562. Removal of brass/gold finish [South Carolina]
14563. Stained gold-plated flatware [California]
14564. PAINTING AN INTERIOR FIREPLACE AND CHIMNEY [Canada]
14565. Need acceptance criteria spec; Class A, Type II, etc. [California]
14566. Electropolishing books [Germany]
14567. Adhesion of paint on galvanizing sheets [Indonesia]
14568. Stains on Nickel Plating [Arizona]
14569. Hard chrome on titanium- help [Arizona]
14570. Silvery spots (visible crystals) in matte anodized machined parts [Mexico]
14571. Seeking refinishing a cast iron tub [Texas] {5/15/02}
14572. High nickel contain [Singapore]
14573. When to heat treat [Arkansas]
14574. Seeking chrome dipping [Ohio] {5/15/02}
14575. Seeking Zinc Cyanide and Zinc Anode [Iran] {5/15/02}
14576. Seeking Rubber Coating Equipment for the internal of pipelines [Hong Kong] {5/15/02}
14577. Powder coating reactivity [Portugal]
14578. Polished brass fixture recoating [New Jersey]
14579. Stainless Steel Polishing [California]
14580. Using palladium chloride in plating ABS plastic [Vietnam]
14581. PLATING PROBLEMS [Canada]
14582. Laser Scale Removal [Michigan]
14583. Unable to achieve finish [India]
14584. Metal finish [Ireland]
14585. Rhodium vs. silver plate [Georgia]
14586. Collet project [Illinois]
14587. Seeking brass plating drawer pulls [Michigan] {5/16/02}
14588. Bonding of brass to rubber [India]
14589. Disadvantage of Electroplating in Powder Coating Vs. Advantage of Zinc Phosphating in Powder coating [India]
14590. Seeking Gold Plating [New York] {5/16/02}
14591. FEDERAL OR MILITARY SPECIFICATION FOR NICKEL PLATING [California]
14592. Metal finishes [Idaho]
14593. How to achieve a dark bead blasted and anodised surface [UK]
14594. Seeking electrolytic tin plates sheets [India] {5/16/02}
14595. Albert Gnehm (Swiss Made) Rockwell Tester user instructions [Florida]
14596. Standard Average Thickness for Anodizing [New York]
14597. Seeking trichloroethylene replacement - vapour degreasing [Canada] {5/16/02}
14598. De-rhodium [Canada]
14599. Seeking wheels polished or chromed [Pennsylvania] {5/16/02}
14600. Chromating zinc die cast parts [India]
14601. Tarnishing Copper [UK]
14602. Viscosity of paint and atmospheric temperature correlation [India]
14603. Seeking chrome plated ABS part for sign facia [New Jersey] {5/17/02}
14604. Seeking for tinning service--copper tinning [South Carolina] {5/17/02}
14605. Seeking Automating Anodizing Line for Aluminum Extrusion Plant [Indiana] {5/17/02}
14606. Clean rust off metal [Florida]
14607. Stainless steel "Tea Staining" [Australia]
14608. Waste Water Treatment [India]
14609. Do the two consecutive layers of the same material deposited by PVD behave as one [India]
14610. Marine copper plating [Idaho]
14611. Electro-Galvanizing [New York]
14612. Surface Finish Question [Nebraska]
14613. Removing of oxide layer on the SS316L surface [Canada]
14614. Seeking copper sheet metal screws [Lake George, CO] {5/20/02}
14615. Partial discharge [Washington DC]
14616. Phenyle Formulation [India]
14617. Request for paint spec recommendation for high temp/steam environment [New Jersey]
14618. Seeking chroming of alloys [England] {5/20/02}
14619. Seeking nikasil plating for motorcycle cylinder [Texas] {5/20/02}
14620. Seeking powder coating [Louisiana] {5/20/02}
14621. SEEKING STAINLESS STEEL POWDER PLANT [India] {5/20/02}
14622. Seeking USED dip spin equipment [Michigan] {5/20/02}
14623. Qwicksilver [New Jersey]
14624. GREEN PATINA STAINS [California]
14625. Chroming of plastic scooter parts [Philippines]
14626. Removing of hard chrome coating [Iran]
14627. Passivation of galvanized steel surface [Canada]
14628. Electroless Nickel Information [Massachusetts]
14629. Another choices instead of Trichloroethylene for Cleaning Process [Thailand]
14630. Electropolishing of phosphorous bronze [India]
14631. Seeking chrome plate of golf heads [New Jersey] {5/20/02}
14632. Seeking Platinized Titanium Anodes [India] {5/20/02}
14633. Seeking tnemic [Georgia] {5/20/02}
14634. Safety aspects of a fun experiment [Wisconsin]
14635. Mirror antiquing [New York]
14636. Titanium surface pitting [England]
14637. Trumpet refinishing [Mississippi]
14638. Seeking Liver of Sulfur [New Zealand] {5/20/02}
14639. Metal cleaning-degreasing [Ohio]
14640. Request information about procedure of auditing 5S [Iran]
14641. Trouble shooting on tin plating [India]
14642. Solution proof trimline coating [UK]
14643. Can you cover tin/zinc with something that has better appearance [Illinois]
14644. Seeking info on recovering silver from x-ray films [U.A.E.] {5/21/02}
14645. Stainless steel valves [Mexico]
14646. The effect of potential drop across the anode double layer on the thickness of double layer [Alabama]
14647. Mild Steel Information [Australia]
14648. Coutellererie [Canada]
14649. How to clean anodised aluminium [UK]
14650. Refinishing an old metal floor lamp [New York]
14651. Brightener for nickel electroplating [Egypt]
14652. Seeking Plating Indium onto Aluminum [California] {5/22/02}
14653. Seeking hardcoat anodizing with Teflon coating [China] {5/22/02}
14654. SEEKING PLATING FIBERGLASS [UK] {5/22/02}
14655. Seeking rechroming of old motorcycle parts [Minnesota] {5/22/02}
14656. Seeking mag wheels refinished [New York] {5/22/02}
14657. Seeking Teflon Coating Service [China] {5/22/02}
14658. Seeking razor blade machinery [India] {5/22/02}
14659. Seeking ornamental cast iron baths [Australia] {5/22/02}
14660. Fabrication of multi junction thermocouple [India]
14661. NOXON WHERE HAVE U GONE? [Florida]
14662. Does rust affect the pH of water? [Virginia]
14663. Kitchen Counter Finishes [New York]
14664. May I decoat pvd? [Italy]
14665. Coating PP on Al in seal-peel application [Croatia]
14666. NC THINNER [India]
14667. How to make copper stick to silicon/titanium nitrite with good adhesion [Texas]
14668. Tungsten process list required [Connecticut]
14669. Chrome Plating: Corrosion Resistance [California]
14670. Process or chemical required to make stainless steel wire cloth bright and shiny [India]
14671. Tin/ Zinc or EN for corrosion resistance [Illinois]
14672. Seeking nickel anode [Russia] {5/22/02}
14673. Seeking electrophoretic equipment [India] {5/22/02}
14674. Difference between metallization and PVD [Spain]
14676. DI water pH at 7 after polisher [Philippines]
14677. CASS TEST [Argentina]
14678. Chrome Free Passivation [India]
14679. PVDF [India]
14680. Post strike nickel is blue [Ohio]
14681. Seeking brass lamp refinishing [Minnesota] {5/22/02}
14682. Liability issues for platers regarding customers' parts [New Hampshire]
14683. Exposure to zinc chromium [New York]
14684. Cadmium plating of stainless steel components [India]
14685. Need to polish and deburr 6061 aluminum [New Jersey]
14686. Seeking anodizing of aluminum tubes [Maryland] {5/22/02}
14687. Electroless Nickel [India]
14688. Galvanize steel in aluminum and then anodize [Pakistan]
14689. Seeking conductive silver paste [China] {5/22/02}
14691. Bad Filter Cake [Arizona]
14692. Silica removal [Germany]
14693. Factors affecting the Quality of Ultra Pure DI water [Singapore]
14694. Chemical post-treatment (di-chromate) for zinc plating [Ohio]
14695. Electrodeposition on Aluminium [Belgium]
14696. Anodised aluminium temperature resistance [Australia]
14697. Electro-polishing pipe bores [South Africa]
14698. Anode and articles position [Turkey]
14699. Hydrogen Embrittlement Baking Cycles After Nickel Electroplating [Georgia]
14700. Seeking Brass Plating [Wisconsin] {5/23/02}
14701. Etching Aluminum Plate [Texas]
14702. More questions about removing copper oxidation [Minnesota]
14703. Allergic reaction to exposed 'white gold' where rhodium faded [Canada]
14704. Haze [Michigan]
14705. Equipment and methods to control purity [Belarus]
14706. Gold on platinum [Utah]
14707. Soldered parts problem [Turkey]
14708. Information about the anodization process [Egypt]
14709. Seeking UHMWPE POWDER [India] {5/24/02}
14710. Seeking Polyethelyne Powders, Powder Coating Resins [Saudi Arabia] {5/24/02}
14711. Smell in the bathroom [Kansas]
14712. Black coating for stainless steel stamped parts [New York]
14713. Difference between chromating alumina and brass [Australia]
14714. ALUMINIUM BOAT REFINISHING [New Zealand]
14715. Job coating rates for E coat [India]
14716. Cu and EN plating on Zinc Die-Cast Part [Singapore]
14717. Is trivalent chromate conductive [Australia]
14718. Scratch removing [Iran]
14719. Silver plate and bleach [Louisiana]
14720. Painting aluminum wheels [Virginia]
14721. Seeking plating a set of model tabernacle furniture [Canada] {5/24/02}
14722. Solderability issue on battery contact [Indiana]
14723. How often to clean the chrome anodes [Michigan]
14724. PCB coating [California]
14725. Tarnishing problem on silver plated copper material [Alabama]
14726. Anodize - Solvent/Contaminant resistance [Canada]
14727. Seeking Alodine 600 [Israel] {5/24/02}
14728. Inconel 625 D [Massachusetts]
14729. Stainless Steel 304 #4 polish to #8 mirror finish, how to [California]
14730. Bright dip on clear chromate parts [Mexico]
14731. Seeking Salt Bath Nitriding [Canada] {5/24/02}
14733. Treatment of Zinc/Nickel Rinse Waters [Ohio]
14734. FPL Etch Solution [New York]
14735. Chromate/Zinc Coatings [Florida]
14736. Bench top Conversion Coating and Painting [Texas]
14737. NICKEL PLATING LOW CARBON STEEL WITH STAINLESS STEEL HARDWARE [Utah]
14738. COPPER COATING [Saudi Arabia]
14739. Simplify surface finish explanation [Tennessee]
14740. Seeking chrome dipping [Maryland] {5/24/02}
14741. Seeking COIL COATING LINE [India] {5/24/02}
14742. SEEKING COATING OF LEAD DIOXIDE/MANGANESE DIOXIDE ON CERAMIC SUBSTRATE ROD [Pakistan] {5/24/02}
14743. Separation of Potassium Pyrophosphate and Potassium Orthophosphate [Kentucky]
14744. Hairline finish on aluminium [Thailand]
14746. SEEKING ORGANIC COLOR ANODIZING LARGE TANKS [New York] {5/28/02}
14747. Seeking Wheel Dipping [Missouri] {5/28/02}
14748. Seeking Chrome Dipping [New Jersey] {5/28/02}
14749. Seeking Chemical Conversion Coating using Alodine 5200 or 5700 [Colorado] {5/28/02}
14750. Seeking Chromated Al2024 Test Panels [Ohio] {5/28/02}
14751. Seeking electroforming of copper on pvc components [India] {5/28/02}
14752. Seeking razor blade manufacturing machines [India] {5/28/02}
14753. Seeking GPC Price and Address [India] {5/28/02}
14754. Gold Powder [Nepal]
14755. Drum coating [Iran]
14756. Application electroless nickel in non metals [Chile]
14757. Corroded cast aluminum versus cast pewter [Florida]
14758. How to prepare a chrome surface to paint over [New York]
14759. Remove rust from chrome [Rhode Island]
14760. Repair brushed stainless finish [New York]
14761. Changing the finish on a brass bed [Illinois]
14762. Is it possible to dissolve aluminum? [California]
14763. Sand blasting of steel tank [Egypt]
14764. Chrome removal from phosphoric acid [California]
14765. Molarity [Kentucky]
14766. Strip tungsten from brass [North Carolina]
14767. TIN deplating [India]
14768. Hydrogen embrittlement problem [Malaysia]
14769. UV absorbing paint [Turkey]
14770. Auto head/tail lens coating [California]
14771. Autophoretic painting [India]
14772. Poor paint adhesion on shocks [India]
14773. Localized No IG [California]
14774. Hard chrome over electroless nickel [India]
14775. To remove Zinc from Nickel Sulphate [India]
14776. Finger prints on black nickel finish [California]
14777. Trivalent chromate, zinc nickel [South Carolina]
14778. Plating-masking-painting [India]
14779. Aluminum electropolish [Iran]
14780. Passivation pre-cleaning and multiple materials in same bath [Minnesota]
14781. Polish for Polygon mirror of Laser units [India]
14782. MATERIAL FOR SPRING SUITABLE FOR HIGH pH VALUE PRODUCTS [India]
14783. Aluminum anodizing [Greece]
14785. HELP...MY STAINLESS CASTINGS ARE "RUSTING" [England]
14786. Seeking aerospace approved inorganic decontaminator for waterborne coatings [UK] {5/29/02}
14787. Seeking ceramic shafts [India] {5/29/02}
14788. Seeking Microporosity Tests [India] {5/29/02}
14789. SEEKING MASKING OF BORES [England] {5/29/02}
14790. Seeking Nycote [Australia] {5/29/02}
14791. Salt spray fog cleaner [Portugal]
14792. RENEWING PARQUET FLOORS [South Carolina]
14793. Over painting interior wrought iron [Minnesota]
14794. OXIDIZATION ON AUTOMOBILE [Michigan]
14795. 900F Heat Treatment of Electroless Nickel [Minnesota]
14796. Corrosion of Al Alloy [India]
14797. Corrosion caused by deionized water [Ohio]
14798. RAL powder coating touch up paint [Illinois] {5/29/02}
14799. Fading away [Canada]
14800. Nickel Strike Process/Application [Ohio]
14801. Coating Material Needed for Sublimation [Philippines]
14802. Brush plating solution recipes [Peru]
14803. CrIII to CrVI [California]
14804. Name of aluminum finish [California]
14806. Seeking Electropolishing SS 304 63 rms [Australia] {5/29/02}
14807. Seeking Black Chrome Plating [Sweden or Germany] {5/29/02}
14809. Need Free Energy of Formation Data for Load Dioxide [New York]
14810. AP Physics/Chemistry electroplating experiment [Virginia]
14813. Problems whit Kesternich test and Zn/Ni alloy finishing [Spain]
14814. Surface preparation of Silver for PC Teflon layer bonding [Israel]
14815. Surface Finishing [Hong Kong]
14816. BEST NON CYANIDE BATH FOR PLATING STEEL BOLTS [Peru]
14817. Gold Plated Beryllium Copper [Singapore]
14818. Potentiel electrochimique de l'aluminium revetu d'alodine 1200 [France]
14819. Chromate - 2024 Aluminum Alloy [Texas]
14820. Stainless steel passivation [India]
14821. How to reclaim my polishing dust etc [Indonesia]
14822. Black oxided steel / anodising aluminium: bimetal corrosion? [Illinois]
14823. Seeking Black Oxidation [Tennessee] {5/30/02}
14824. Seeking Re-Dow coating of Magnesium auto parts [Maryland] {5/30/02}
14825. Seeking Plating Non-Conductive Prototypes [California] {5/30/02}
14826. Seeking Phosphoric Acid Anodizing [Ohio] {5/30/02}
14827. SEEKING CHROME PLATING [MEXICO] {5/30/02}
14828. Spring to it [UK]
14829. Sketching of mirrored glass [Michigan]
14830. Black coating on bismuth plating [Florida]
14831. Bluing of double barrel guns [West Virginia]
14833. RA to SPI comparison charts [Wisconsin]
14834. Chloroform from NaOCl [New York]
14835. Etch rate drop after filtration [UK]
14836. Seeking Zinc Coating Plant [U.A.E.] {5/31/02}
14837. Salt Spray Tests for Measuring Pitting Corrosion Rates [Venezuela]
14838. Bismuth electroplating [California]
14839. Painting Anodized car wheels-can it be done [Missouri]
14840. Anodize Dye Problem [Ohio]
14841. Seeking company to recover palladium [India] {5/31/02}
14842. Seeking Electrolytic Tinplate [Italy] {5/31/02}
14843. Seeking Aluminum Blue 2LW Dye [Kansas] {5/31/02}
14844. How to Recover Gold from Silver Sludge [India]
14845. Electroless coating, modeling [India]
14846. Time lines [California]
14847. Safe acid etching [California]
14848. Copper onto Stainless Steel [Australia]
14850. Nitinol electropolishing [Massachusetts]
14851. Alodine Salt Spray Results vs. Panel Preparation [Idaho]
14852. Plating 4140 [Wisconsin]
14853. Thickness Problem [Philippines]
14854. Post plate treatment to blacken silver plating [California]
14855. Closed-loop water recycling cause of salt spray failure [Idaho]
14856. Removing a scratch from stainless steel [England]
14857. Remove blue discoloration from motorcycle exhaust? [Virginia]
14858. Seeking chemical coloring process on stainless steel [Korea] {5/31/02}
14859. HAE BLISTERS [Indiana]
14860. Seeking decorative chroming [Michigan] {6/03/02}
14861. Seeking gold electroforming on plexiglass [Korea] {6/03/02}
14862. Seeking Electro Polishing Vendors for Stainless Steel and Anodising for Aluminium [India] {6/03/02}
14863. Seeking Dacrotizing equipment [Iran] {6/03/02}
14864. Seeking knife over roll coating machine for textiles [India] {6/03/02}
14865. Seeking adhesive to Teflon [Mexico] {6/03/02}
14866. Seeking heating furnace [India] {6/03/02}
14867. Seeking stainless steel modular bracelets [Hong Kong] {6/03/02}
14868. Remove Solder from Gold Coins [Virginia]
14869. Replating saltwater reel [Iowa]
14870. Copper sealant [Australia]
14871. How to stress anneal polyester resin [Canada]
14872. Wanted: matching antique cast iron and brass bed [Massachusetts]
14873. Removing Tin Ceiling [New York]
14874. Copper in cement [Mexico]
14875. Corrosion encrusted U.S. pennies [Texas]
14876. Tin Ceiling Restoration [Canada]
14877. Fiber Glass Powder Booth [Mexico]
14878. Aluminium electroplating [India]
14879. Soft soldering to aluminium [Australia]
14880. Low friction conductive aluminum coating [Minnesota]
14881. Seeking processes to put metal films onto glass [California]
14882. Seeking Applying Cadmium to Aluminum [Tennessee] {6/03/02}
14883. Corrosil technique? [China]
14884. Spinning ring plating / F.F.plating [India]
14885. Causes of resistivity increase in iridium oxide coated titanium anodes [Turkey]
14886. Gypsum as coagulant [South Africa]
14887. Help with high concentration of Calcium in a bright Nickel bath [Nevada]
14888. Surface Preparation Needed for Paint Scratch Touch-Up? [California]
14889. SEEKING ANODISING DYES [Australia] {6/04/02}
14890. ELECTROLYSIS PROCESS INVOLVED [India]
14891. Scratch removal on aluminum wheels [California]
14892. Clear-coat dilemma [Canada]
14893. Stripping chrome plating from metal [South Africa]
14894. Adhesion test [Singapore]
14895. WHITE RUST [Singapore]
14896. Maximum Nickel Thickness for Solderability Applications [Arizona]
14897. Understanding Nitric Acid Passivation [Oregon]
14898. Passivating stainless steel [South Africa]
14899. Alternatives for zinc coating? [Maryland]
14900. Zinc-based epoxy for stainless steel painting [Malaysia]
14901. Seeking caustic etch of 3003 grade aluminum [Texas] {6/05/02}
14902. Seeking large part EN capability for aluminum [Illinois] {6/05/02}
14903. Silver extraction [India]
14904. Internal combustion engine part hydrogen de-embrittlement [Montana]
14905. Emissivity VS absorptivity [Illinois]
14906. Tye-dying in cold water [California]
14907. Repair pit marks on Coleman lanterns [Canada]
14908. Tank Material for Hot Blacking Process [Brazil]
14909. Dissolving Copper Not Nickel [Massachusetts]
14910. Absorbing light at 890nm [UK]
14912. ANODIZE STRIP [Ohio]
14913. Removing the blue from blue spring steel [New York]
14914. Removal of glass bead blast residue [Mexico]
14915. Difference in Durability and Rate of Oxidation of a 440A Grade Carbon Stainless Blade and a 300 Grade [South Dakota]
14916. Seeking Teflon Coating [Ireland] {6/06/02}
14917. Porous anodized alumina [Massachusetts] {6/06/02}
14918. Seeking photo engraved tubing [Massachusetts] {6/06/02}
14919. Seeking Electro-Polishing [Oklahoma] {6/06/02}
14920. Seeking acid marking pens/markers [Canada] {6/06/02}
14921. Seeking air heating {recirculating} for batch type powder paint oven New or Used [U.A.E.] {6/06/02}
14922. Preventing rust on bare metal car body [Oregon]
14923. EN plating specifications for offshore use [The Netherlands]
14924. Hot Tank Evaporation Rates [Kansas]
14925. Thickness Measurement Methods Question [Colorado]
14926. Measuring Chrome Thickness [Canada]
14927. Preventing Discoloration of Low Alloy Steel during embrittlement relief [Israel]
14928. Black cad help [Ohio]
14929. Chromate treatment of zinc-nickel plating [Massachusetts]
14930. Bonding Preparation for 2014 {forged} Aluminum Inserts [Indiana]
14931. Type II black anodizing discoloration {gold} [Wisconsin]
14932. Liquid paraffin as rust preventer [India]
14933. Stainless steel rusting [Canada]
14934. Steel Selection for use in chemically harsh environment {Fertilizer Industry} [Australia]
14935. Matchbox car scratch marks in stainless steel appliances [Wisconsin]
14936. Dissolve Al from Au and Ni [Kansas]
14937. Ti adhesion [Italy]
14938. Charmille Surface Finish Chart [Louisiana]
14939. Seeking Brass and Chrome Plated Tubing [Washington] {6/07/02}
14940. Seeking Napgard Epoxy [Colombia] {6/07/02}
14941. Electropolishing Nickel 200 [Washington]
14942. Galvanizing bars and pipes [Brazil]
14943. Passivate per G1041 [Malaysia]
14944. Bright dip stack emissions [Canada]
14945. Need vapor degreaser wiring diagram [Mexico]
14946. How to darken gold plated item [New York]
14947. Chromium substitute [Mexico]
14948. Mirror finish to an aluminium disk [Australia]
14949. Stellite machining [India]
14950. Finish for compressor blade erosion prevention [Florida]
14951. Seeking Tin Pre-plated CRS [Europe and Asia] {6/07/02}
14952. Seeking Electroplating Suppliers [Australia] {6/07/02}
14953. Seeking consultant for manufacture of brighteners [India] {6/07/02}
14954. Surface finish for parts to be electroless Ni plated Vs. adhesion [California]
14955. Change from Trico to what [England]
14958. Seeking decorative chrome plating [Texas] {6/10/02}
14960. Recovery of silver from fixer [Iran]
14961. Density of CuSO4? [England]
14963. Chemical impurities in deionized water [Pakistan]
14964. Teflon coating [Pakistan]
14965. Zinc oxide removal with household products [Florida]
14966. Changing bright brass finish to antique brass [New Jersey]
14967. Stopping rust on galvanized steel roof decking [British Columbia]
14968. Teflon recoating at small scale [Cameroon]
14969. Removing Rust & Re-Paiting Wrought Iron Railings [Maryland]
14970. Coloring Titanium [Wisconsin]
14971. Hot tank Solution [Florida]
14972. Process needed for Alumium & Zinc die cast parts [So. Carolina]
14973. Protecting aluminum frames from copper [Lebanon]
14974. Phosphating on steel parts [U.A.E.]
14975. Need Chrome on abs in big sizes [Mexico] {6/10/02}
14977. Seeking 5 Rims to be chrome dipped [New York] {6/10/02}
14978. Seeking GM 988-4132 plating [California] {6/10/02}
14979. Technology & Training for Hard Chrome Plating [India] {6/10/02}
14980. Treatment of Magnesium Corrosion [Texas]
14981. Granite counter damaged by cleaner containing citric acid [Mass.]
14982. Gold Plating to prevent scaling [California]
14983. Seeking Brush Satin Chrome services [Washington] {6/11/02}
14984. POWDER COATING OF DOMESTC LPG CYLINDERS [India] {6/11/02}
14985. Seeking Titanium Gold service [Australia] {6/11/02}
14986. Seeking Electro-Chemical Deburring Machine [India] {6/11/02}
14987. Seeking Cobalt/Tin process [So. Africa] {6/11/02}
14988. Seeking Sublimation Coating Polymers [Mexico] {6/11/02}
14989. MicroSeimens converted to megaOhms [Wisconsin]
14990. Anodizing color [Indonesia]
14991. Removing scratches from stainless steel appliances [England]
14992. Removing anodization from aluminum motorcycle parts [Minn.]
14993. Fixing break in small pieces of chrome plated pot metal [Kansas]
14994. How is mirror glass aging done? [Missouri]
14995. Excessive Iron in Swimming Pool Water [Illinois]
14996. How can I finish a copper table top [Pennsylvania]
14997. Seeking dye sublimation coatings and equipment [Australia] {6/11/02}
14998. Can you plate white gold with platinum? [Florida]
14999. Ballizing Process Needed [No. Carolina]

The finishing.com Hotline includes more than 40,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2005