The home page of the finishing industry ®
|
|
|
|
The links above go directly to the book in question when possible. Inventory at book dealers varies; determine if the edition being offered by the dealer is the edition we illustrate/discuss here and the edition you want. If a link doesn't work, the dealer may not have a copy at this time; try another source.
|
Available for review and on-site research in the Joseph Mazia Memorial Research Library at finishing.com in Brick, New Jersey. |
I refer to this volume constantly, as regular visitors to the Hotline may realize. The volume contains 24 chapters on 23 different electrodeposited metals, hundreds of charts, tables, and photomicrographs, and thousands of references. Typically, it answers such questions as: how does a deposit of sulfamate nickel compare to Watt's nickel? What happens to the properties of the plate if I lower the bath temperature, or add a brightener, or increase the agitation? |
|
ISBN |
Edition |
Pub. year |
Publisher |
|
093656900X |
1st |
1986 |
American Electroplaters Society |