Letter 9052 Black diamond+ I an looking for information on black diamond plating. I would like to find out is there a company that offers it and or the procedure. Gregg Neufeld
+ Hello Gregg! If what you're looking for is a boron carbide PVD coating, then see letter 582 at: http://www.finishing.com/0400-0599/582.html >From the Thomas Register,
If you buy from these folks, tell them you saw them here, OK? Then maybe they'll help support Ted's fine site. Hope this helps!
+ Hello Gregg: You probably already got the answer to your need. But according to your company I assume that what you are looking for has to deal with resistance to corrosion or to other degradation problem asociated with fuels. If this is correct you should also look to electroless nickel technologies. Specifically, I saw several applications in this field some three years ago. Refer to Surface Technology, Inc., Trenton, NJ. You should not have trouble. Regards, Guillermo Marrufo