HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 9037
Sealing rust patina finish
+
Having a hard time finding a sealer or clear finish to seal in real rust finish on items we produce. Have tried everything from poly to Tung Oil [linked by editor to product info at Amazon]. Cannot contain the rust.
Please help!
Mark D. LyonWish Craft - Rock Springs, WY
+
Dear Mark,
A good polyurethane should do the trick. I would usually recommend an acrylic basecoat followed by a urethane. This makes the urethane much easier to strip, when it comes time to repair/maintain the patina and substrate. Contact me if you would like more information.
Regards,
|
Jake Koch G. J. Nikolas & Co., Inc. Bellwood, Illinois |
+++++++
Furnishing a very rustic cabin. I have 1/4' thick steel plate I am using as a countertop and an old steel plow disc I am using as a wash basin. Both are rusted to perfection. How can I seal the rust and maintain it's current appearance and water proof?
Ray skinnerHobbyist - koosheram, utah, usa