Concrete Mixer Paddle Wear Problems.

+

To Whom It May Concern,

Currently I am conducting a research of improving Concrete Mixer Paddle (Maker : SIMEM, Italy) with Hard surfacing materials but the results seen not much improvement. Hard facing coating applied have the following Chemical composition; 5%C, 28% Cr, 1%Mo rest Fe. The paddle base materials is 12% Cast Manganese.

Suggestion and past experience from those even come across this problems and the solution is very much welcomed. Any advise is very appreciated.

Chiong Kung Kwong
- Kuala Lumpur, Malaysia


Dear Reader, please --

Post a question on a different subject.
 
Answer this question (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com